CN1394760A - 中纤杆铅笔及其生产方法 - Google Patents

中纤杆铅笔及其生产方法 Download PDF

Info

Publication number
CN1394760A
CN1394760A CN 01126114 CN01126114A CN1394760A CN 1394760 A CN1394760 A CN 1394760A CN 01126114 CN01126114 CN 01126114 CN 01126114 A CN01126114 A CN 01126114A CN 1394760 A CN1394760 A CN 1394760A
Authority
CN
China
Prior art keywords
pencil
production method
fine shaft
mdf
shaft
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 01126114
Other languages
English (en)
Inventor
李枝官
黄榕生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 01126114 priority Critical patent/CN1394760A/zh
Publication of CN1394760A publication Critical patent/CN1394760A/zh
Pending legal-status Critical Current

Abstract

一种中纤杆铅笔及其生产方法,其特征是,笔杆部分是用人造中密度纤维板材料制成。其工艺步骤依序是先将规边后的中密度纤维板材制成符合尺寸规格的铅笔板-刨槽-用胶粘剂胶芯-置入笔芯后束板烘干-磨头-刨杆-磨光成白杆铅笔-外表油漆装饰-包装得成品。与已有技术比较,本发明的中纤杆铅笔不仅可达到(或优于)木材原料的性能,使整根笔杆各处切削性能保持一致,满足铅笔国家标准的要求,还可简化加工工序,提高木材综合利用率,有利保护林木资源和改善生态环境。

Description

中纤杆铅笔及其生产方法
本发明涉及一种笔具生产技术,特别是一种中纤杆铅笔及其生产方法。
现有市场上出售的铅笔多采用木材为笔杆原料,据有关统计,近年我国铅笔行业采用木杆的铅笔产量超过70亿支,每年都要向自然界索要20万立方米以上木材,而且还要采用适于制作铅笔的树种,如果采用其它树种,因材质问题,木材利用率十分低下,仅24%左右。另外,近几年由于铅笔市场竞争激烈,个体和乡镇铅笔厂大批出现,大量劣质铅笔向市场倾销,更造成木材资源的严重浪费和生态环境的破坏。为保护森林资源和生态环境,目前有些企业在积极地寻找木材的替代品,已出现纸卷杆铅笔和笔芯可换的全塑活动铅笔替代木杆铅笔,但还未见有采用中密度纤维板制造木杆铅笔的报道。此外,生产纸卷(杆)铅笔,存在着几乎要更新整套工艺设备、生产工艺较复杂的缺点,全塑活动铅笔在书写手感方面不如传统木杆铅笔的手感好。
本发明的目的是提供一种新型中纤杆铅笔及其生产方法,它不仅具有与木杆铅笔一样的纤维粗细度和密度适中、均匀性好,各处切削(笔)性能一致,不亚于原木材料制的木杆铅笔,还可简化现有木杆铅笔的加工工序,减轻环境污染,提高木材综合利用率,有利森林资源的保护和生态环境的改善,实现绿色产品的目标。
本发明是以如下技术方案实现的:它仍包括笔芯和笔杆两部分,其特征是铅笔的笔杆部分是用人造中密度纤维板(简称中纤板)材料制成。
由于制作木杆铅笔的树种与资源缺口越来越大,随着人们重视对生态环境的保护,特别重视对森林资源的保护,采用其它材料来替代制造木杆铅笔的木材已是一种发展趋势,本发明采用上述中纤板(中密度纤维板)来替代木材,是比较合适的,中纤板具有一定强度(可经过解纤和加入适当添加剂处理),便于各种机械加工,当将其替代传统的木材原料制作木杆铅笔,还可减化加工工序,不需对现有设备作大的改动,工艺性好,其具体的加工工艺步骤依序仅仅是:将规边(整形)后的中密度纤维板材制成符合尺寸规格的铅笔板-刨槽-用胶粘剂胶芯-置入笔芯后束板烘干(燥)-磨头-刨杆-磨光成白杆铅笔-外表油漆装饰-包装得成品。
与现有技术比较,本发明利用人造的中纤板替代制造木杆铅笔的木材,不仅可达到(或优于)木材原料的性能,使整根笔杆各处切削性能保持一致,满足铅笔国家标准的要求,还可简化加工工序,减少环境污染,提高木材综合利用率,有利保护林木资源和改善生态环境,有利实现绿色产品的目标。
以下结合具体生产实例对本发明作进一步详细说明。
附图1为本发明制成一种无皮头HB圆杆铅笔的剖面示意图。其中:1-笔杆部分(为人造中纤板材料制成),2-笔芯。
本发明所选用的人造中密度纤维板(中纤板)材料的整体密度应是控制在620-700kg/m3,而其断面密度应尽可能均匀,以保证切削性能的一致性。在进行刨槽工序时,可将一定规格的铅笔板用自动刨槽机借助各种规格的刨槽刀具刨出适合镶嵌铅笔芯的槽眼(芯槽)。在进行胶芯时是在槽板(指刨好槽眼的铅笔板)表面涂刷一层胶液后,将笔芯嵌入芯槽中,再合上另一块涂有胶液(或不涂胶液)的槽板。在进行束板烘干工序时,是将一定块数的湿胶板放在束板干燥机上,把它们夹紧到一定松紧程度,送入干燥机进行胶板的烘干,束夹烘干房的温度控制为100-110℃,束夹时间为0.7-1.5小时。接着进行磨头工序时,将烘干后的胶板用胶板磨头机上的砂轮把胶板两端磨齐整,使胶板的长度保持一致,接着进行刨杆工序,将磨头的胶板经过刨杆机(又称铅笔成型机)借助刨杆刀具刨削成各种不同形状的白杆铅笔,最后选取合格的白杆铅笔进行上漆印字等外观装饰,经包装即得成品铅笔。
利用本发明技术可以制造各种不同规格形状尺寸和不同用途的铅笔,如可制成各种石墨铅笔和彩色铅笔,只要改变人造铅笔板的厚度还可制成各种不同形状笔杆的铅笔,如圆杆、中圆杆、大圆杆、细杆、六角杆、大六角杆的铅笔等,甚至可按不同用途需要制成化妆笔、缝纫笔、炭画笔、特种用途笔等等。

Claims (4)

1、一种中纤杆铅笔,它包括笔芯和笔杆两部分,其特征是铅笔的笔杆部分是用人造中密度纤维板材料制成。
2、根据权利要求1所述的中纤杆铅笔,其特征是所述人造中密度纤维板材料的整体密度是控制在620-700kg/m3,而其断面密度也应均匀。
3、一种如权利要求1所述的生产中纤杆铅笔的生产方法,其特征是其生产的工艺步骤依序仅是:先将规边整形后的中密度纤维板材制成符合尺寸规格的铅笔板-刨槽-用胶粘剂胶芯-置入笔芯后束板烘干-磨头-刨杆-磨光成白杆铅笔-外表油漆装饰-包装得成品。
4、根据权利要求3所述的中纤杆铅笔的生产方法,其特征是在进行束板烘干工序时,束夹烘干的温度控制为100-110℃,束夹时间为0.7-1.5小时。
CN 01126114 2001-07-09 2001-07-09 中纤杆铅笔及其生产方法 Pending CN1394760A (zh)