Prior art keywords
plasticine
rosin
normal temperature
microcrystalline wax
white vaseline
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 00123233
Other languages
English (en)
Other versions
CN1132880C (zh
Inventor
刘毅
吴德臣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 00123233 priority Critical patent/CN1132880C/zh
Publication of CN1352217A publication Critical patent/CN1352217A/zh
Application granted granted Critical
Publication of CN1132880C publication Critical patent/CN1132880C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Links

Landscapes

  • Compositions Of Macromolecular Compounds (AREA)
  • Toys (AREA)

Abstract

本发明是涉及雕塑材料的改进。本发明就是按照一定比例,将微晶蜡、白凡士林、松香放入金属容器中加热,当达到一定熔点后,倒入粉末填料搅匀,冷却后即得。本发明的优点是,密度高,粘度好,手感好、塑形肯定,手不易粘泥、粘色,常温下不易变形,无菌无毒,不污染。不仅适用于雕塑,也适用于工业造型设计、建筑设计、工艺美术、模具制作、美术教育及儿童玩具等。

Description

一种常温橡皮泥的制作方法
本发明是涉及雕塑材料的改进。
橡皮泥又称油泥、油土、油粘土。目前国产橡皮泥在操作时偏软,手易粘泥,粘色,常温下易变形。国外进口橡皮泥也不理想,如韩国橡皮泥虽然不太受气温影响,但使用时手仍易粘泥、粘色;日本同类产品有仅塑形不稳定,还含有一定的有毒物质。如日本玩具协会生产的油粘土在说明书中明确的提示:“在手、胳臂等上有伤肿、湿疹等时,请别使用。”甚至在操作时不可接触鼻子、眼睛和嘴。由此可见,上述都不能成为目前较为理想的材料。本发明的目的就是提供一种手感好、常温易变形、无毒的常温橡皮泥。
本发明的目的是这样实现的:将微晶蜡140-155g、白凡士林90-110g、松香18-20g放入金属容器中加热,当熔点升至120-140℃时离火,倒入粉末填料300-450g搅匀,冷却后即得。
根据本地区气候条件和实际需要,可在所限比例范围内随意调解。加大微晶蜡和松香比例可增材料强度高,加大矾士林的比例可使材料硬度减弱。其色彩差别取决于填料。
下面对本发明的所用材料说明:
(1)微晶蜡
微晶蜡有两种,一种是氧化微晶蜡,另一种是80#精白微晶蜡。氧化微晶蜡为浅黄色,有韧性的固体,滴点为70-115℃。80#精白微晶蜡是我国黄色地蜡的深加工,滴点为82.5℃。两者的密度在0.85-0.95g/cm3左右。微晶蜡在配方中的作用是利用软化后,在常温下的密度、粘度、硬度、拉伸粘度和运动粘度以及所特有的亲合力。
(2)白凡士林
白凡士林属于医用严格控制酸值、含硫量和不含稠环化合物的一种膏状石油产品。熔点为38-56℃。其作用是使微晶蜡等软化,形成可塑性手感。
(3)松香
松香,俗称熟松香或熟香。透明玻璃状脆性物质,带有松香脂香气。密度1.05-1.10g/cm3熔点110-135℃。温热变软而粘。在配方中的作用是增加粘度、密度、和硬度。
(4)粉末填料
粉末填料,如泥粉、水泥粉、大白粉,各种矿石粉等。一般在200#以上都是可利用的对象。在配方中,粉状填料是橡皮泥的基质。
本发明的主要优点:本发明是雕塑家根据自己的实践研制的,其优点为密度高,手感好、塑形肯定,手不易粘泥、粘色,在常温下不易变形,无菌无毒、不污染。本发明除用于雕塑外,也适用于工业造型设计、建筑设计、工艺品设计、模具翻制、美术教育及儿童玩具等。
实施例1:
微晶蜡    150g
白凡士林  100g
松香      19g
粉末填料  400g
实施例2:
微晶蜡    145g
白凡士林  90g
松香      18g
粉末填料  370g
实施例3:
微晶蜡    152g
白凡士林  105g
松香      18g
粉末填料  380g

Claims (4)

1、一种常温仿青铜橡皮泥的制作方法,将微晶蜡140-155g、白凡士林90-110g、松香18-20g放入金属容器中加热,当熔点升至120-140℃时离火,倒入粉末填料300-450g搅匀,冷却后即得。
2、根据权利要求1所述的一种常温仿青铜橡皮泥,其特征在于微晶蜡150g、白凡士林100g、松香19g、粉末填料400g。
3、根据权利要求1所述的一种常温仿青铜橡皮泥,其特征在于微晶蜡145g、白凡士林90g、松香18g、粉末填料370g。
4、根据权利要求1所述的一种常温仿青铜橡皮泥,其特征在于微晶蜡152g、白凡士林105g、松香18g、粉末填料380g。
CN 00123233 2000-11-10 2000-11-10 一种常温橡皮泥的制作方法 Expired - Fee Related CN1132880C (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 00123233 CN1132880C (zh) 2000-11-10 2000-11-10 一种常温橡皮泥的制作方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 00123233 CN1132880C (zh) 2000-11-10 2000-11-10 一种常温橡皮泥的制作方法

Publications (2)

Publication Number Publication Date
CN1352217A true CN1352217A (zh) 2002-06-05
CN1132880C CN1132880C (zh) 2003-12-31

Family

ID=4589697

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 00123233 Expired - Fee Related CN1132880C (zh) 2000-11-10 2000-11-10 一种常温橡皮泥的制作方法

Country Status (1)

Country Link
CN (1) CN1132880C (zh)

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101177531B (zh) * 2007-12-18 2010-06-02 东莞市汇欣工贸有限公司 一种彩色油泥及制备方法
CN101195691B (zh) * 2008-01-08 2010-06-02 山西大学 可变色面泥粉及其制备方法
CN101875548A (zh) * 2010-03-26 2010-11-03 许庆华 彩色凹凸棒橡皮泥及其生产方法
CN102220019A (zh) * 2011-04-29 2011-10-19 东莞市汇欣工贸有限公司 工业油泥及其制备方法
CN101768314B (zh) * 2009-01-05 2012-08-22 惠州海翔文教用品有限公司 水溶性橡皮泥组合物及其制造方法
CN104877358A (zh) * 2015-06-16 2015-09-02 张学锋 环保型雕塑模具材料
CN104960368A (zh) * 2015-06-16 2015-10-07 张学锋 一种环保型雕塑模具的制作方法及浮雕制作方法
CN107033395A (zh) * 2017-05-22 2017-08-11 河南机电高等专科学校 一种橡皮泥及制备方法和使用该橡皮泥的可循环使用沙盘

Cited By (12)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN101177531B (zh) * 2007-12-18 2010-06-02 东莞市汇欣工贸有限公司 一种彩色油泥及制备方法
CN101195691B (zh) * 2008-01-08 2010-06-02 山西大学 可变色面泥粉及其制备方法
CN101768314B (zh) * 2009-01-05 2012-08-22 惠州海翔文教用品有限公司 水溶性橡皮泥组合物及其制造方法
CN101875548A (zh) * 2010-03-26 2010-11-03 许庆华 彩色凹凸棒橡皮泥及其生产方法
CN101875548B (zh) * 2010-03-26 2011-07-20 许庆华 彩色凹凸棒橡皮泥及其生产方法
CN102220019A (zh) * 2011-04-29 2011-10-19 东莞市汇欣工贸有限公司 工业油泥及其制备方法
CN102220019B (zh) * 2011-04-29 2012-12-05 东莞市汇欣工贸有限公司 工业油泥及其制备方法
CN104877358A (zh) * 2015-06-16 2015-09-02 张学锋 环保型雕塑模具材料
CN104960368A (zh) * 2015-06-16 2015-10-07 张学锋 一种环保型雕塑模具的制作方法及浮雕制作方法
CN104877358B (zh) * 2015-06-16 2017-11-10 深圳市联想空间艺术工程有限公司 环保型雕塑模具材料
CN107033395A (zh) * 2017-05-22 2017-08-11 河南机电高等专科学校 一种橡皮泥及制备方法和使用该橡皮泥的可循环使用沙盘
CN107033395B (zh) * 2017-05-22 2019-06-14 河南机电高等专科学校 一种橡皮泥及制备方法和使用该橡皮泥的可循环使用沙盘

Also Published As

Publication number Publication date
CN1132880C (zh) 2003-12-31

Similar Documents

Publication Publication Date Title
CN1132880C (zh) 一种常温橡皮泥的制作方法
CN109265887A (zh) 一种超轻粘土及其制备方法
CN1273531C (zh) 一种透明质感树脂粘土的制造方法
CN108793948B (zh) 一种彩陶制品的加工方法
CN111977978A (zh) 一种仿玉宝石蓝玻璃及其制备方法
CN101177531B (zh) 一种彩色油泥及制备方法
CN1125855C (zh) 一种超常温橡皮泥的制作方法
CN1123604C (zh) 一种常温仿青铜橡皮泥的制作方法
CN107737865A (zh) 一种铸造型砂
CN1045179C (zh) 琉璃雕琢饰品的制作方法
CN107572785A (zh) 玻璃瓶制作工艺
CN1132882C (zh) 一种超常温仿青铜橡皮泥的制作方法
CN104445942A (zh) 一种无铅仿瓷玻璃酒瓶及其制造工艺
CN1132881C (zh) 一种常温仿石橡皮泥的制作方法
CN110436778A (zh) 一种骨科修复用生物活性玻璃材料制备方法
CN1117924A (zh) 不饱和树脂工艺品的制作方法
CN107117815A (zh) 一种高韧性耐摔玻璃碗的生产工艺
CN113492614A (zh) 一种琉璃器具成型模具及其制备工艺
TW202242029A (zh) 可捏塑之彈性蠟
CN102464816A (zh) 贴面装饰砖加工模具的制备方法及其用途
CN1245732A (zh) 可重复捏塑的儿童玩具泥
CN1373052A (zh) 人体仿真塑造工艺
CN107737864A (zh) 一种环保型铸造型砂
CN101973731B (zh) 发光凹凸棒软陶泥的生产方法
CN118006134A (zh) 一种diy粘土及其制备方法

Legal Events

Date Code Title Description
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C06 Publication
PB01 Publication
C14 Grant of patent or utility model
GR01 Patent grant
C19 Lapse of patent right due to non-payment of the annual fee
CF01 Termination of patent right due to non-payment of annual fee