CN1270886A - Spray painted cloth for lamp box and its production process - Google Patents

Spray painted cloth for lamp box and its production process Download PDF

Info

Publication number
CN1270886A
CN1270886A CN 00114165 CN00114165A CN1270886A CN 1270886 A CN1270886 A CN 1270886A CN 00114165 CN00114165 CN 00114165 CN 00114165 A CN00114165 A CN 00114165A CN 1270886 A CN1270886 A CN 1270886A
Authority
CN
China
Prior art keywords
skeleton
temperature
raw material
accounts
lamp box
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 00114165
Other languages
Chinese (zh)
Other versions
CN1114526C (en
Inventor
李德荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN00114165A priority Critical patent/CN1114526C/en
Publication of CN1270886A publication Critical patent/CN1270886A/en
Application granted granted Critical
Publication of CN1114526C publication Critical patent/CN1114526C/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The present invention relates to a decoration technology. By using PVC as base material, titanium oxide powder, whitener No.1857, stabilizer calcium carbonate and anti-againg agnet styrene (ABAS-60), and adopting different formulation for two sides of skeleton, the present invention produces spray-painted cloth through the technological process of raw material throwing, laminated feeding, sectional controlled heating, pressing to adhere, sectional cooling, marking and rolling and packing. The spray-painted cloth has firm surface layer, clear picture, high weather resistance and high illumination resistance and is suitable for advertising lamp box.

Description

Spray painted cloth for lamp box and preparation method thereof
Spray painted cloth for lamp box of the present invention and preparation method thereof belongs to the technology field that produces decorative effect, particularly a kind of lamp house cloth that is used for the painting advertisement use.
The lamp house cloth of use in the lamp box advertisement is to be used at its surperficial air brushing picture, lamp house cloth is used for painting advertisement and has two big technical barriers for many years, first, the less calcium carbonate of lamp house cloth intensive amount can generate the powder of one deck trace on its surface through chemical reaction in PVC, second, skeleton in the lamp house cloth can evenly not wait to produce powder as time passes yet, because the effect of powder, just make the picture of air brushing occur incomplete, can air brushing not go up picture when serious, the picture of air brushing is difficult for preserving, through wind, drench with rain, illumination, along with powder produces, picture moves back and takes off eclipsedly, has influence on the effect of painting advertisement, often will often change.
The objective of the invention is to avoid the deficiencies in the prior art part and provide a kind of top layer absorption affinity good, picture is difficult for moving back and takes off, and the picture of air brushing is clear, be not afraid of wind, drench with rain, illumination, picture is not eclipsed, can keep for a long time, is applicable to lamp house cloth that painting advertisement uses and preparation method thereof.
The objective of the invention is to reach by following measure, spray painted cloth for lamp box is to adopt PVC to make raw material, be equipped with plurality of raw materials and additive, adopt different batchings to combine on the two sides of skeleton, both built-in lamp with outward play lamp and combine, the segmentation cooling is made after utilizing the method pressurizing attaching of the different temperature temperature control of multistage, spray painted cloth for lamp box of the present invention is to add Cornstarch in the PVC raw material, the brightening agent that has added whitening effect, control transparency and stable elements have been added, the stabilizing agent of filling waterproof action, the age resister that adds uvioresistant and anti-aging effect is formed, and brightening agent adopts 1857#, stabilizing agent adopts calcium carbonate, age resister adopts styrene (ABAS-66), and Cornstarch accounts for 2-5%, and brightening agent accounts for 0.5-2%, stabilizer comprises 0.5-15%, age resister accounts for 1-5%.Calcium carbonate can be used as simultaneously.
In the one side employing PVC of skeleton raw material, add Cornstarch and account for 2-5%, the brightening agent 1857# that has added whitening effect accounts for 0.5-2%, control transparency and stable elements have been added, the stabilizing agent calcium carbonate 0.5-2% of filling waterproof action, the age resister styrene (ABAS-66) that adds uvioresistant and anti-aging effect accounts for 1-5%, in the another side employing PVC of skeleton raw material, add Cornstarch and account for 2-5%, the brightening agent 1857# that has added whitening effect accounts for 0.5-2%, the stabilizing agent calcium carbonate 2-15% that has added control transparency and stable elements effect, the age resister styrene (ABAS-66) that adds uvioresistant and anti-aging effect accounts for 1-5%, after utilizing the different temperature temperature control heating of multistage, pressurizing attaching, the segmentation cooling is made, and the longitude and latitude D of skeleton is 200 * 500-500 * 800.
Preparation method of the present invention is to adopt raw material to throw in, and------the temperature-gradient method temperature control------pressurizing attaching is finished in segmentation cooling---rolling of note sign indicating number---by finished product packing in the layering conveying, one deck was thrown in skeleton in the middle of raw material was thrown in, in the one side employing PVC of skeleton raw material, add Cornstarch and account for 2-5%, brightening agent 1857# accounts for 0.5-2%, stabilizing agent calcium carbonate 0.5-2%, age resister styrene (ABAS-66) accounts for 1-5%, in the another side employing PVC of skeleton raw material, add Cornstarch and account for 2-5%, brightening agent 1857# accounts for 0.5-2%, stabilizing agent calcium carbonate 2-15%, age resister styrene (ABAS-66) accounts for 1-5%, the layering conveying is that the PVC raw material on skeleton and skeleton two sides is separately carried, the temperature-gradient method temperature control is that the temperature with the skeleton heated wheel is controlled at 90-99 ℃, the PVC raw material on skeleton two sides is divided into three sections intensification temperature controls, the temperature of first section heated wheel is controlled at 170-178 ℃, the temperature of second section heated wheel is controlled at 180-187 ℃, the temperature of the 3rd section heated wheel is controlled at 165-170 ℃, at the 3rd section heated wheel place the PVC raw material and the skeleton on skeleton two sides are fitted, pressurizing attaching is the PVC raw material pressurization that will be fitted in the skeleton two sides at the 3rd section heated wheel place, pressure remains on the 6-7 kg/cm, the speed that spray painted cloth for lamp box passes through be 13-19 rice/minute, segmentation cooling is that the spray painted cloth for lamp box with pressurizing attaching is divided into three sections coolings, first section chilling temperature is controlled at 70-60 ℃, the temperature of second section cooling is controlled at 45-40 ℃, the temperature of the 3rd section cooling is controlled at 20-12 ℃, with the rolling of spray painted cloth for lamp box note sign indicating number, finished product packing.
Top layer of the present invention absorption affinity is good, and picture does not move back and takes off, and the picture of air brushing is clear, be not afraid of wind, drench with rain, illumination, picture is eclipsed, can keep for a long time, can satisfy the requirement of high, medium and low shelves spray drawing apparatus precision and definition, be a kind of lamp house cloth that is applicable to that painting advertisement uses.
Accompanying drawing 1 is a process chart of the present invention.
Accompanying drawing 2 is applying schematic diagrames of the present invention.
The invention will be further described below in conjunction with accompanying drawing.
As shown in Figures 1 and 2, spray painted cloth for lamp box of the present invention is to adopt PVC to make raw material, is equipped with too white Powder, brightening agent 1857#, stabilizing agent calcium carbonate, age resister styrene (ABAS-66), at skeleton 1 Different prescription batchings is adopted on the two sides, adopts the method pressurizing attaching of three sections different temperature temperature controls after the segmentation cooling make Become, preparation method of the present invention is to adopt raw material to throw in, and---layering conveying---temperature-gradient method temperature control---adds and overlays Finished product packing is finished to close---segmentation cooling---note code a rolling---, and raw material is thrown in and adopted layering to carry the centre What one deck was thrown in is skeleton 1, in the one side input employing PVC of skeleton raw material, add Cornstarch and account for 3%, Brightening agent 1857# accounts for 1%, stabilizing agent calcium carbonate 1%, and age resister styrene (ABAS-66) accounts for 2%, Add Cornstarch in the another side input employing PVC raw material of skeleton and account for 3%, brightening agent 1857# accounts for 1%, and is steady Decide agent calcium carbonate 13%, age resister styrene (ABAS-66) accounts for 3.5%, layering carry be with skeleton and The PVC raw material on skeleton two sides is separately carried, and forms three layers of conveying, and middle one deck is skeleton, temperature-gradient method Temperature control is that the temperature with skeleton heated wheel 2 is controlled at 95-98 ℃, and the PVC raw material on skeleton two sides is divided into three Duan Shengwen temperature control, the temperature of first paragraph heated wheel 3 are controlled at 173-175 ℃, the temperature of second segment heated wheel 4 Be controlled at 182-185 ℃, the temperature of the 3rd section heated wheel 5 is controlled at 167-169 ℃, the 3rd section heated wheel The place fits PVC raw material and the skeleton on skeleton two sides, and pressurizing attaching is will fit at the 3rd section heated wheel place Pressurize with press roll 6 at the PVC on skeleton two sides raw material, pressure remains on the 6.5-7 kg/cm, spray Painting the speed that lamp house cloth passes through is 13-19 m/min, and the segmentation cooling is that the spray painted cloth for lamp box with pressurizing attaching is divided into Three sections coolings, first paragraph 7 chilling temperatures are controlled at 65 ℃, and the temperature of second segment 8 coolings is controlled at 43 ℃, the The temperature of three section 9 cooling is controlled at 15 ℃, after the cooling spray painted cloth for lamp box is remembered a yard rolling, finished product packing.
The invention will be further described below in conjunction with an embodiment.
The present invention is used for the lamp box advertisement and uses, and the lamp house cloth that uses in advertisement is to be used at its surperficial air brushing picture.
The centre of spray painted cloth for lamp box of the present invention is a skeleton, in the one side employing PVC of skeleton raw material, add Cornstarch and account for 3%, brightening agent 1857# accounts for 1%, stabilizing agent calcium carbonate 1%, age resister styrene (ABAS-66) accounts for 2%, in the another side employing PVC of skeleton raw material, add Cornstarch and account for 3%, brightening agent 1857# accounts for 1%, stabilizing agent calcium carbonate 13%, age resister styrene (ABAS-66) accounts for 3.5%, adopt different prescription batching layerings to carry on the two sides of skeleton, adopts behind the method pressurizing attaching of three sections different temperature temperature controls segmentation to cool off and make, the longitude and latitude D of skeleton is 200 * 500.
Preparation method of the present invention is to adopt raw material to throw in, and------the temperature-gradient method temperature control------pressurizing attaching is finished in segmentation cooling---rolling of note sign indicating number---by finished product packing in the layering conveying, raw material is thrown in and is adopted layering to carry, what middle one deck was thrown in is skeleton, in the one side input employing PVC of skeleton raw material, add Cornstarch and account for 3%, brightening agent 1857# accounts for 1%, stabilizing agent calcium carbonate 1%, age resister styrene (ABAS-66) accounts for 2%, in the another side input employing PVC of skeleton raw material, add Cornstarch and account for 3%, brightening agent 1857# accounts for 1%, stabilizing agent calcium carbonate 13%, age resister styrene (ABAS-66) accounts for 3.5%, the layering conveying is that the PVC raw material on skeleton and skeleton two sides is separately carried, form three layers of conveying, middle one deck is a skeleton, and the longitude and latitude D of skeleton is 200 * 500, and the temperature-gradient method temperature control is that the temperature with the skeleton heated wheel is controlled at 95 ℃; The PVC raw material on skeleton two sides is divided into three sections intensification temperature controls, the temperature of first section heated wheel is controlled at 173 ℃, the temperature of second section heated wheel is controlled at 182 ℃, the temperature of the 3rd section heated wheel is controlled at 167 ℃, at the 3rd section heated wheel place the PVC raw material and the skeleton on skeleton two sides are fitted, pressurizing attaching is the PVC raw material pressurization that will be fitted in the skeleton two sides at the 3rd section heated wheel place, pressure remains on 6.5 kg/cm, the speed that spray painted cloth for lamp box passes through is 14 meters/minute, segmentation cooling is that the spray painted cloth for lamp box with pressurizing attaching is divided into three sections coolings, first section chilling temperature is controlled at 65 ℃, the temperature of second section cooling is controlled at 43 ℃, the temperature of the 3rd section cooling is controlled at 15 ℃, after the cooling spray painted cloth for lamp box is remembered a yard rolling, finished product packing.

Claims (7)

1, a kind of spray painted cloth for lamp box, it is characterized in that adopting PVC to make raw material, be equipped with plurality of raw materials and additive, adopt different batchings to combine on the two sides of skeleton, the segmentation cooling is made after utilizing the method pressurizing attaching of the different temperature temperature control of multistage, spray painted cloth for lamp box of the present invention is to add Cornstarch in the PVC raw material, the brightening agent that has added whitening effect, control transparency and stable elements have been added, the stabilizing agent of filling waterproof action, the age resister that adds uvioresistant and anti-aging effect is formed, brightening agent adopts 1857#, and stabilizing agent adopts calcium carbonate, and age resister adopts styrene (ABAS-66), Cornstarch accounts for 2-5%, brightening agent accounts for 0.5-2%, stabilizer comprises 0.5-15%, and age resister accounts for 1-5%.
2, spray painted cloth for lamp box according to claim 1, it is characterized in that adding Cornstarch in the one side employing PVC of skeleton raw material accounts for 2-5%, the brightening agent 1857# that has added whitening effect accounts for 0.5-2%, the stabilizing agent calcium carbonate 0.5-2% that has added control transparency and stable elements effect, the age resister styrene (ABAS-66) that adds uvioresistant and anti-aging effect accounts for 1-5%, in the another side employing PVC of skeleton raw material, add Cornstarch and account for 2-5%, the brightening agent 1857# that has added whitening effect accounts for 0.5-2%, the stabilizing agent calcium carbonate 2-15% that has added control transparency and stable elements effect, the age resister styrene (ABAS-66) that adds uvioresistant and anti-aging effect accounts for 1-5%, after utilizing the different temperature temperature control heating of multistage, pressurizing attaching, the segmentation cooling is made.
3, a kind of spray painted cloth for lamp box and preparation method thereof is characterized in that adopting raw material to throw in, and------the temperature-gradient method temperature control------pressurizing attaching is finished in segmentation cooling---rolling of note sign indicating number---by finished product packing in the layering conveying.
4, according to described spray painted cloth for lamp box of claim 3 and preparation method thereof, one deck is thrown in skeleton in the middle of it is characterized in that the raw material input, in the one side employing PVC of skeleton raw material, add Cornstarch and account for 2-5%, brightening agent 1857# accounts for 0.5-2%, stabilizing agent calcium carbonate 0.5-2%, age resister styrene (ABAS-66) accounts for 1-5%, in the another side employing PVC of skeleton raw material, add Cornstarch and account for 2-5%, brightening agent 1857# accounts for 0.5-2%, stabilizing agent calcium carbonate 2-15%, age resister styrene (ABAS-66) accounts for 1-5%, the layering conveying is that the PVC raw material on skeleton and skeleton two sides is separately carried, the temperature-gradient method temperature control is that the temperature with the skeleton heated wheel is controlled at 90-99 ℃, the PVC raw material on skeleton two sides is divided into three sections intensification temperature controls, the temperature of first section heated wheel is controlled at 170-178 ℃, the temperature of second section heated wheel is controlled at 180-187 ℃, the temperature of the 3rd section heated wheel is controlled at 165-170 ℃, at second section heated wheel place the PVC raw material and the skeleton on skeleton two sides are fitted, pressurizing attaching is the PVC raw material pressurization that will be fitted in the skeleton two sides at the 3rd section heated wheel place, pressure remains on the 6-7 kg/cm, the speed that spray painted cloth for lamp box passes through be 13-19 rice/minute, segmentation cooling is that the spray painted cloth for lamp box with pressurizing attaching is divided into three sections coolings, first section chilling temperature is controlled at 70-60 ℃, the temperature of second section cooling is controlled at 45-40 ℃, the temperature of the 3rd section cooling is controlled at 20-12 ℃, with the rolling of spray painted cloth for lamp box note sign indicating number, finished product packing.
5, spray painted cloth for lamp box according to claim 2, the centre that it is characterized in that spray painted cloth for lamp box is a skeleton, in the one side employing PVC of skeleton raw material, add Cornstarch and account for 3%, brightening agent 1857# accounts for 1%, stabilizing agent calcium carbonate 1%, age resister styrene (ABAS-66) accounts for 2%, in the another side employing PVC of skeleton raw material, add Cornstarch and account for 3%, brightening agent 1857# accounts for 1%, stabilizing agent calcium carbonate 13%, age resister styrene (ABAS-66) accounts for 3.5%, adopts different prescription batching layerings to carry on the two sides of skeleton, adopts behind the method pressurizing attaching of three sections different temperature temperature controls segmentation to cool off and makes.
6, according to described spray painted cloth for lamp box of claim 4 and preparation method thereof,------the temperature-gradient method temperature control------pressurizing attaching is finished in segmentation cooling---rolling of note sign indicating number---by finished product packing in the layering conveying to it is characterized in that adopting raw material to throw in, raw material is thrown in and is adopted layering to carry, what middle one deck was thrown in is skeleton, in the one side input employing PVC of skeleton raw material, add Cornstarch and account for 3%, brightening agent 1857# accounts for 1%, stabilizing agent calcium carbonate 1%, age resister styrene (ABAS-66) accounts for 2%, in the another side input employing PVC of skeleton raw material, add Cornstarch and account for 3%, brightening agent 1857# accounts for 1%, stabilizing agent calcium carbonate 13%, age resister styrene (ABAS-66) accounts for 3.5%, the layering conveying is that the PVC raw material on skeleton and skeleton two sides is separately carried, form three layers of conveying, middle one deck is a skeleton, the temperature-gradient method temperature control is that the temperature with the skeleton heated wheel is controlled at 95 ℃, the PVC raw material on skeleton two sides is divided into three sections intensification temperature controls, the temperature of first section heated wheel is controlled at 173 ℃, the temperature of second section heated wheel is controlled at 182 ℃, the temperature of the 3rd section heated wheel is controlled at 167 ℃, at the 3rd section heated wheel place the PVC raw material and the skeleton on skeleton two sides are fitted, pressurizing attaching is the PVC raw material pressurization that will be fitted in the skeleton two sides at the 3rd section heated wheel place, pressure remains on 6.5 kg/cm, the speed that spray painted cloth for lamp box passes through is 14 meters/minute, segmentation cooling is that the spray painted cloth for lamp box with pressurizing attaching is divided into three sections coolings, first section chilling temperature is controlled at 65 ℃, the temperature of second section cooling is controlled at 43 ℃, the temperature of the 3rd section cooling is controlled at 15 ℃, after the cooling spray painted cloth for lamp box is remembered a yard rolling, finished product packing.
7, spray painted cloth for lamp box according to claim 1 is characterized in that being used for the lamp box advertisement and uses, and is used in advertisement at its surperficial air brushing picture.
CN00114165A 2000-03-31 2000-03-31 Spray painted cloth for lamp box and its production process Expired - Fee Related CN1114526C (en)