CN1267614C - 玉石纳米粉体、晶体颗粒合成建筑装饰材料的方法 - Google Patents
玉石纳米粉体、晶体颗粒合成建筑装饰材料的方法 Download PDFInfo
- Publication number
- CN1267614C CN1267614C CN 03133933 CN03133933A CN1267614C CN 1267614 C CN1267614 C CN 1267614C CN 03133933 CN03133933 CN 03133933 CN 03133933 A CN03133933 A CN 03133933A CN 1267614 C CN1267614 C CN 1267614C
- Authority
- CN
- China
- Prior art keywords
- jade
- parts
- powder
- nano
- crystal grain
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明涉及一种玉石纳米粉体、晶体颗粒合成建筑装饰材料的方法,其特征在于:是按下列步骤完成的:原料制备:(1)玉石废料粗粉碎、(2)精粉碎、(3)精细粉碎制成玉石纳米微粉;合成方法:(1)配料:原料(重量的百分比):取玉石晶体颗粒占85%、玉石纳米微粉占15%为100份;添加(按原料重量比):环氧树脂6101 3~6份、固化剂:650树脂胶2~3份、溶剂:丁醇7~8份、丁酯8~10份;(2)混合搅拌、(3)成型、(4)加工初磨。本发明利用天然玉石加工剩余的废弃料生产建筑装饰材料,可以制成地面砖、墙面装饰板和生产家具的型材,其工艺方法简单、产品晶体透明、美观大方、价格低廉、使用寿命长,还具有防暑降温、对人体有保健的作用。
Description
技术领域
本发明涉及一种加工方法,特别涉及一种玉石纳米粉体、晶体颗粒合成建筑装饰材料的方法。
背景技术
目前,国内在建筑装饰材料领域,主要用于室内地面或墙面的装饰材料,传统采用木材、石材、陶瓷等制成地板块、地面砖、墙面装饰板等。在现有技术中天然玉石在加工时剩余的废弃料原本没有什么利用价值,本发明则是利用这些废弃的物质作为原料,制成精美的室内装饰材料。
发明内容
本发明的目的是利用天然玉石在加工时剩余的废弃的物料作为原料,生产精美的室内装饰材料,解决了加工、合成的技术问题,提供一种玉石纳米粉体、晶体颗粒合成建筑装饰材料的方法。
本发明玉石纳米粉体、晶体颗粒合成建筑装饰材料的方法内容简述:
本发明玉石纳米粉体、晶体颗粒合成建筑装饰材料的方法,其特征在于:是按下列步骤完成的:
一、原料制备:
(1)、玉石废料粗粉碎:对天然玉石在加工时剩余的废弃的物料在粉碎机内进行粉碎,加工成2~3cm3的玉石晶体颗粒;
(2)、精粉碎:玉石晶体颗粒在雷蒙粉碎机内进行精粉碎,得到玉石粉体粒度为325目;
(3)、精细粉碎:将精粉碎后的玉石粉末投入到纳米微粉设备中进行精细粉碎加工,制成玉石纳米微粉粒度达到15000目;
二、合成方法:
(1)、配料:按重量的百分比取原料:玉石晶体颗粒占85%、玉石纳米微粉占15%为100份;再按100份玉石晶体颗粒和玉石纳米微粉的重量比添加:环氧树脂6101 3~6份、固化剂:650树脂胶2~3份、溶剂:丁醇7~8份、丁脂8~10份;
(2)、混合搅拌:投入搅拌机内进行混合、充分搅拌;
(3)、成型:将搅拌后的原料放入成型模具内经液压机挤压成型,常温下干燥一周;
(4)、加工:初磨、抛光、打蜡、包装、出厂。
本发明综合利用天然玉石在加工时剩余的废弃料生产的建筑装饰材料,可以制成地面砖、墙面装饰板和生产家具的型材,其工艺方法简单、产品晶体透明、美观大方、价格低廉、使用寿命长,还具有防暑降温、对人体有保健的作用。
具体实施方式
本发明生产玉石纳米粉体、晶体颗粒合成地面砖是这样实现的,原料制备:首先对天然玉石在加工时剩余的废弃的物料在粉碎机内进行粗粉碎,加工成2~3cm3的玉石晶体颗粒;将玉石晶体颗粒在雷蒙粉碎机内进行精粉碎,得到玉石粉体粒度为325目;再将精粉碎后的玉石粉末投入到纳米微粉设备中进行精细粉碎加工,制成玉石纳米微粉粒度达到15000目。
配料:以玉石纳米微粉、玉石晶体颗粒为原料,添加环氧树脂、650树脂胶固化剂、溶剂为丁醇、丁脂。
其组份为:玉石纳米微粉15份、玉石晶体颗粒85份、环氧树脂6101 5份、650树脂胶固化剂2.5份、溶剂为丁醇8份、丁脂9份。
上述成分投入搅拌机内进行混合、充分搅拌;将搅拌后的原料放入地面砖成型模具内经液压机挤压成型,常温下干燥一周;初磨、抛光、打蜡、包装。
Claims (2)
1、一种玉石纳米粉体、晶体颗粒合成建筑装饰材料的方法,其特征在于:是按下列步骤完成的:
一、原料制备:
(1)、玉石废料粗粉碎:对天然玉石在加工时剩余的废弃的物料在粉碎机内进行粉碎,加工成2~3cm3的玉石晶体颗粒;
(2)、精粉碎:玉石晶体颗粒在雷蒙粉碎机内进行精粉碎,得到玉石粉体粒度为325目;
(3)、精细粉碎:将精粉碎后的玉石粉末投入到纳米微粉设备中进行精细粉碎加工,制成玉石纳米微粉粒度达到15000目;
二、合成方法:
(1)、配料:按重量的百分比取原料:玉石晶体颗粒占85%、玉石纳米微粉占15%为100份;再按100份玉石晶体颗粒和玉石纳米微粉的重量比添加:环氧树脂6101 3~6份、固化剂:650树脂胶2~3份、溶剂:丁醇7~8份、丁脂8~10份;
(2)、混合搅拌:投入搅拌机内进行混合、充分搅拌;
(3)、成型:将搅拌后的原料放入成型模具内经液压机挤压成型,常温下干燥一周;
(4)、加工:初磨、抛光、打蜡、包装、出厂。
2、根据权利要求1所述的玉石纳米粉体、晶体颗粒合成建筑装饰材料的方法,其特征在于:所说的合成方法:
配料:按原料重量比组份为:玉石纳米微粉15份、玉石晶体颗粒85份、环氧树脂5份、650树脂胶固化剂2.5份、溶剂为丁醇8份、丁脂9份。