CN118009829A - A construction method for filling and charging mixed emulsion explosives on site - Google Patents

A construction method for filling and charging mixed emulsion explosives on site Download PDF

Info

Publication number
CN118009829A
CN118009829A CN202410245237.XA CN202410245237A CN118009829A CN 118009829 A CN118009829 A CN 118009829A CN 202410245237 A CN202410245237 A CN 202410245237A CN 118009829 A CN118009829 A CN 118009829A
Authority
CN
China
Prior art keywords
temperature sensor
medicine
drug delivery
construction method
filling
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN202410245237.XA
Other languages
Chinese (zh)
Inventor
冯保国
王南焰
刘瑶
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Longyan Minhua Engineering Blasting Co ltd
Original Assignee
Longyan Minhua Engineering Blasting Co ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Longyan Minhua Engineering Blasting Co ltd filed Critical Longyan Minhua Engineering Blasting Co ltd
Priority to CN202410245237.XA priority Critical patent/CN118009829A/en
Publication of CN118009829A publication Critical patent/CN118009829A/en
Pending legal-status Critical Current

Abstract

The invention relates to the technical field of blast hole charging construction, in particular to a field mixed emulsion explosive filling and charging construction method; a first temperature sensor and a second temperature sensor are sequentially arranged on the outer circumferential surface of the drug delivery rubber tube close to the drug outlet along the drug outlet direction; when the medicine conveying rubber tube stretches into the bottom of the blast hole to convey medicine, the medicine surface can sequentially permeate through the second temperature sensor and the first temperature sensor, when the temperature difference between the first temperature sensor and the second temperature sensor is reduced to a set threshold value, the medicine surface is indicated to permeate through the first temperature sensor, the medicine surface is used as a trigger signal for lifting the medicine conveying rubber tube, when the medicine surface is lifted to only permeate through the second temperature sensor, the temperature difference between the first temperature sensor and the second temperature sensor is larger than a preset threshold value, the actual height of the medicine surface in the blast hole can be accurately obtained, the lifting of the medicine conveying rubber tube is controlled according to the actual height, the medicine outlet end of the medicine conveying rubber tube is always buried in a proper depth range of the medicine surface, and the medicine loading quality is ensured.

Description

Filling and charging construction method for on-site mixed emulsion explosive
Technical Field
The invention relates to the technical field of blast hole charging construction, in particular to a field mixed emulsion explosive filling and charging construction method.
Background
At present, a powder charge of the on-site mixed emulsion explosive for blasting engineering is mainly characterized in that a powder delivery rubber tube is placed into a blast hole, emulsion explosive is pumped, the powder charge speed is measured by a flowmeter, the powder charge speed is matched by manually setting parameters to control the pulling and lifting of the powder delivery rubber tube, and in order to ensure the powder charge quality, the powder delivery rubber tube mouth is generally buried in the range of 0.4-0.6 m of the on-site mixed emulsion explosive, and the depth of the powder delivery rubber tube mouth buried in the blast hole cannot be directly observed through vision because the blast hole is a blind hole; if the medicine conveying rubber tube is lifted at a constant speed, when the conditions of crushing, cracking, karst cave and the like exist on the wall of a blast hole, the charging position in the blast hole cannot rise at a constant speed, so that the rising speed actual value and the calculated value of the on-site mixed emulsion explosive charging surface in the blast hole are inconsistent, the proper and accurate embedding depth of the medicine conveying rubber tube in the charging process is difficult to ensure, the adverse conditions of medicine breaking, improper charging height control, insufficient filling length and the like in the charging process are caused, and the potential safety hazards of large orifice blocks, blind cannons, flying stone out of control and the like are caused.
Disclosure of Invention
The technical problems to be solved by the invention are as follows: the on-site mixed emulsion explosive filling and charging construction method is provided, so that when the emulsion explosive is filled and charged, the mouth of a medicine conveying rubber pipe is ensured to be always buried into a specific depth of a medicine surface, and the charging quality is ensured.
In order to solve the technical problems, the invention adopts the following technical scheme:
The on-site mixed emulsion explosive filling and charging construction method is based on a drug delivery rubber tube, wherein a first temperature sensor and a second temperature sensor are sequentially arranged on the outer circumferential surface of the drug delivery rubber tube, which is close to a drug outlet, along the drug outlet direction;
The filling and charging construction method comprises the following steps:
Extending the medicine outlet end of the medicine delivery rubber tube into the bottom of the blast hole;
controlling a drug delivery rubber tube to fill mixed explosive into the blast hole;
Acquiring a temperature value T1 of a first temperature sensor and a temperature value T2 of a second temperature sensor;
Calculating a temperature difference delta t=t2-T1 monitored by the first temperature sensor and the second temperature sensor;
When the delta T is smaller than a preset threshold value, controlling the medicine delivery rubber tube to slowly lift out of the blast hole;
When the delta T is larger than a preset threshold value, the medicine delivery rubber tube is controlled to stop lifting out of the blast hole.
Further, in the above-mentioned on-site mixed emulsion explosive filling and charging construction method, the filling and charging construction method further includes: according to the depth of the blast hole, the aperture of the blast hole and the charging speed, calculating the predicted medicine surface height H1 in the blast hole, calculating the actual medicine surface height H2 in the blast hole according to the actual lifting height of the medicine conveying rubber tube and delta T, and calculating the height difference delta H between the actual medicine surface height H2 and the predicted medicine surface height H1; if delta H is larger than a preset threshold value, judging the abnormal conditions of broken walls, cracks, abnormal pore diameters or karst cave of the blast hole walls.
Furthermore, in the on-site mixed emulsion explosive filling and charging construction method, the first temperature sensor is annular, and the first temperature sensor is embedded in the outer wall of the drug delivery rubber tube.
Further, in the on-site mixed emulsion explosive filling and charging construction method, the second temperature sensor is annular, and the second temperature sensor is embedded in the outer wall of the drug delivery rubber tube.
In the on-site mixed emulsion explosive filling and charging construction method, the distance between the first temperature sensor and the second temperature sensor is 30cm.
Further, in the on-site mixed emulsion explosive filling and charging construction method, the distance between the second temperature sensor and the drug outlet end of the drug delivery rubber tube is 40cm.
Further, in the on-site mixed emulsion explosive filling and charging construction method, an annular heat insulation material layer is arranged between the first temperature sensor and the drug delivery rubber tube.
Furthermore, in the on-site mixed emulsion explosive filling and charging construction method, an annular heat insulation material layer is arranged between the second temperature sensor and the drug delivery rubber tube.
The invention has the beneficial effects that: by utilizing the characteristic that the temperature of the mixed emulsion explosive can reach 80 ℃, a first temperature sensor and a second temperature sensor are sequentially arranged on the outer circumferential surface of the drug delivery rubber tube, which is close to the drug outlet, along the drug outlet direction; when the medicine conveying rubber tube stretches into the bottom of the blast hole to convey medicine, the medicine surface sequentially penetrates through the second temperature sensor and the first temperature sensor, when the temperature difference between the first temperature sensor and the second temperature sensor is reduced to a set threshold value, the medicine surface is indicated to be not through the first temperature sensor, the medicine surface is used as a trigger signal for lifting the medicine conveying rubber tube, when the medicine surface is lifted to be not through the second temperature sensor, the temperature difference between the first temperature sensor and the second temperature sensor is enabled to be larger than a preset threshold value, the medicine surface is used as a trigger signal for controlling the medicine conveying rubber tube to stop lifting, so that the actual height of the medicine surface in the blast hole can be accurately obtained, the lifting of the medicine conveying rubber tube is controlled according to the actual height, the adverse conditions of medicine breaking, improper medicine loading height control, insufficient filling length and the like are avoided, the medicine outlet end of the medicine conveying rubber tube is always buried into a proper depth range of the medicine surface, and the medicine loading quality is ensured.
Further, according to the depth of the blast hole, the aperture of the blast hole and the charging speed, calculating the predicted medicine surface height H1 in the blast hole, and according to the actual lifting height of the medicine conveying rubber tube and delta T, calculating the actual medicine surface height H2 in the blast hole, and calculating the height difference delta H between the actual medicine surface height H2 and the predicted medicine surface height H1; if delta H is larger than a preset threshold value, judging the abnormal condition of the broken wall, the crack, the pore diameter abnormality of the hole or the karst cave, wherein when the broken wall, the crack, the pore diameter abnormality of the hole or the abnormal condition of the karst cave occur, the filled explosive can infiltrate into the crack or the karst cave, so that the actual powder surface height is lower than the predicted powder surface height, the aperture is reduced, the actual powder surface height is higher than the predicted powder surface height, and the height difference delta H between the actual powder surface height H2 and the predicted powder surface height H1 is used as the basis for judging the abnormal condition of the hole.
Drawings
FIG. 1 is a schematic diagram of a drug delivery hose and a blasthole structure related to a construction method for filling and charging on site of mixed emulsion explosive according to an embodiment of the invention;
Fig. 2 is an enlarged view of a portion a of fig. 1;
description of the reference numerals:
1. A drug delivery rubber tube;
2. A first temperature sensor;
3. a second temperature sensor;
4. A layer of insulating material;
5. A blast hole;
6. And (5) mixing and loading the explosive.
Detailed Description
In order to describe the technical contents, the achieved objects and effects of the present invention in detail, the following description will be made with reference to the embodiments in conjunction with the accompanying drawings.
Referring to fig. 1 and 2, the specific embodiment of the invention relates to a construction method for filling and loading an emulsion explosive on site, based on a drug delivery rubber tube 1, a first temperature sensor 2 and a second temperature sensor 3 are sequentially arranged on the outer circumferential surface of the drug delivery rubber tube 1, which is close to a drug outlet, along the drug outlet direction;
The filling and charging construction method comprises the following steps:
The medicine outlet end of the medicine delivery rubber tube 1 extends into the bottom of the blast hole 5;
controlling the drug delivery rubber tube 1 to fill the mixed explosive 6 into the blast hole 5;
Acquiring a temperature value T1 of the first temperature sensor 2 and a temperature value T2 of the second temperature sensor 3;
calculating a temperature difference Δt=t2-T1 monitored by the first temperature sensor 2 and the second temperature sensor 3;
when the delta T is smaller than a preset threshold, for example, the threshold can be set to be 1-2 ℃, and the drug delivery rubber tube 1 is controlled to be slowly lifted out of the blast hole 5;
when the delta T is larger than a preset threshold value, the medicine delivery rubber tube 1 is controlled to stop lifting out of the blast hole 5.
In the above embodiment, the outer diameter of the drug delivery hose 1 is 50mm, and the inner diameter is 38mm. The drug delivery rubber tube 1 is connected to a tube rolling machine, and the tube rolling machine drives the drug delivery rubber tube 1 to lift or stop in the blast hole 5.
In the above embodiment, by utilizing the characteristic that the temperature of the mixed emulsion explosive can reach 80 ℃, a first temperature sensor 2 and a second temperature sensor 3 are sequentially arranged on the outer circumferential surface of the drug delivery rubber tube 1, which is close to the drug outlet, along the drug outlet direction; when the medicine conveying rubber tube 1 stretches into the bottom of the blast hole 5 to convey medicine, the medicine surface sequentially passes through the second temperature sensor 3 and the first temperature sensor 2, when the temperature difference between the first temperature sensor 2 and the second temperature sensor 3 is reduced to a set threshold value, the medicine surface is indicated to be over the first temperature sensor 2, the medicine surface is used as a trigger signal for lifting the medicine conveying rubber tube 1, when the medicine surface is lifted to be over the second temperature sensor 3, the temperature difference between the first temperature sensor 2 and the second temperature sensor 3 is enabled to be larger than a preset threshold value, the medicine surface is used as a trigger signal for controlling the medicine conveying rubber tube 1 to stop lifting, the actual height of the medicine surface in the blast hole 5 can be accurately obtained, the lifting of the medicine conveying rubber tube 1 is controlled according to the actual height, the medicine outlet end of the medicine conveying rubber tube 1 is always buried in a proper depth range of the medicine surface, and the medicine loading quality is ensured.
As a preferred embodiment, the method for filling and charging construction further comprises: according to the depth of the blast hole 5, the aperture of the blast hole 5 and the charging speed, calculating the predicted medicine surface height H1 in the blast hole 5, calculating the actual medicine surface height H2 in the blast hole 5 according to the actual lifting height of the medicine conveying rubber tube 1 and delta T, and calculating the height difference delta H between the actual medicine surface height H2 and the predicted medicine surface height H1; if the delta H is larger than a preset threshold value, judging the abnormal conditions of broken walls, cracks, abnormal pore diameters of the blast holes 5 or karst cave.
In the above embodiment, because the wall of the blast hole 5 is broken, cracked, the pore diameter of the hole is abnormal or the karst cave is abnormal, the filled explosive can infiltrate into the crack or the karst cave, so that the actual powder surface height is lower than the predicted powder surface height, and the height difference delta H between the actual powder surface height H2 and the predicted powder surface height H1 is calculated as the basis for judging the abnormality of the blast hole 5, so that the method has the advantages of simplicity and high efficiency.
As a preferred embodiment, the first temperature sensor 2 is annular, and the first temperature sensor 2 is embedded in the outer wall of the drug delivery rubber tube 1.
As a preferred embodiment, the second temperature sensor 3 is in a ring shape, and the second temperature sensor 3 is embedded in the outer wall of the drug delivery rubber tube 1.
As a preferred embodiment, the distance between the first temperature sensor 2 and the second temperature sensor 3 is 30cm.
As a preferred embodiment, the second temperature sensor 3 is 40cm away from the drug outlet end of the drug delivery tube 1, i.e. the first temperature sensor 2 is 70cm away from the drug outlet end of the drug delivery tube 1.
Through improving the setting position of first temperature sensor 2 and second sensor, can further make the play medicine mouth end of defeated medicine rubber tube 1 imbed the suitable degree of depth scope of medicine face all the time, further improve the loading quality.
As a preferred embodiment, an annular heat insulation material layer 4 is arranged between the first temperature sensor 2 and the drug delivery tube 1.
As a preferred embodiment, an annular heat insulation material layer 4 is arranged between the second temperature sensor 3 and the drug delivery tube 1.
In the above embodiment, since the first temperature sensor 2 and the second temperature sensor 3 are used for sensing the temperature of the explosive filled in the blast hole 5, by providing the heat insulation material layer 4, the temperature of the mixed emulsion explosive in the drug delivery rubber tube 1 can be prevented from influencing the sensing temperature of the first temperature sensor 2 and the second temperature sensor 3.
The foregoing description is only illustrative of the present invention and is not intended to limit the scope of the invention, and all equivalent changes made by the specification and drawings of the present invention, or direct or indirect application in the relevant art, are included in the scope of the present invention.

Claims (8)

1.一种现场混装乳化炸药灌装装药施工方法,其特征在于,基于输药胶管,所述输药胶管靠近出药口处的外圆周面沿出药方向依次布设有第一温度传感器和第二温度传感器;1. A construction method for filling and charging mixed emulsion explosives on site, characterized in that, based on a drug delivery hose, a first temperature sensor and a second temperature sensor are arranged in sequence on the outer circumferential surface of the drug delivery hose near the drug outlet along the drug delivery direction; 所述灌装装药施工方法包括以下步骤:The filling and charging construction method comprises the following steps: 将输药胶管的出药口端伸入炮孔内的底部;Insert the medicine outlet end of the medicine delivery hose into the bottom of the blast hole; 控制输药胶管向炮孔内灌装混装炸药;Control the explosive delivery hose to fill the mixed explosive into the blast hole; 获取第一温度传感器的温度值T1和第二温度传感器的温度值T2;Acquire a temperature value T1 of a first temperature sensor and a temperature value T2 of a second temperature sensor; 计算第一温度传感器和第二温度传感器监测到的温度差ΔT=T2-T1;Calculate the temperature difference ΔT=T2-T1 detected by the first temperature sensor and the second temperature sensor; 当ΔT小于预设的阈值时,控制输药胶管向炮孔外缓慢提拉;When ΔT is less than the preset threshold, the drug delivery hose is controlled to be slowly pulled out of the blast hole; 当ΔT大于预设的阈值时,控制输药胶管停止向炮孔外提拉。When ΔT is greater than a preset threshold, the drug delivery hose is controlled to stop being pulled out of the blast hole. 2.根据权利要求1所述的现场混装乳化炸药灌装装药施工方法,其特征在于,所述灌装装药施工方法还包括:根据炮孔深度、炮孔孔径和装药速度,计算炮孔内的预计药面高度H1,根据输药胶管的实际提升高度以及ΔT计算炮孔内的实际药面高度H2,计算实际药面高度H2与预计药面高度H1的高度差ΔH;若ΔH大于预设的阈值时,判断炮孔孔壁破碎、裂隙、孔内孔径异常或溶洞的异常情况。2. The on-site mixed emulsion explosive filling and charging construction method according to claim 1 is characterized in that the filling and charging construction method also includes: calculating the expected powder surface height H1 in the blasthole according to the blasthole depth, blasthole aperture and charging speed, calculating the actual powder surface height H2 in the blasthole according to the actual lifting height of the drug delivery hose and ΔT, and calculating the height difference ΔH between the actual powder surface height H2 and the expected powder surface height H1; if ΔH is greater than a preset threshold value, judging the abnormal situation of the blasthole wall breakage, cracks, abnormal aperture in the hole or abnormal cave. 3.根据权利要求1所述的现场混装乳化炸药灌装装药施工方法,其特征在于,所述第一温度传感器为圆环形,所述第一温度传感器嵌设于输药胶管的外壁。3. The on-site mixed emulsion explosive filling and charging construction method according to claim 1 is characterized in that the first temperature sensor is annular and is embedded in the outer wall of the drug delivery hose. 4.根据权利要求1所述的现场混装乳化炸药灌装装药施工方法,其特征在于,所述第二温度传感器为圆环形,所述第二温度传感器嵌设于输药胶管的外壁。4. The on-site mixed emulsion explosive filling and charging construction method according to claim 1 is characterized in that the second temperature sensor is annular and is embedded in the outer wall of the drug delivery hose. 5.根据权利要求1所述的现场混装乳化炸药灌装装药施工方法,其特征在于,所述第一温度传感器和第二温度传感器的间距为30cm。5. The on-site mixed emulsion explosive filling and charging construction method according to claim 1 is characterized in that the distance between the first temperature sensor and the second temperature sensor is 30 cm. 6.根据权利要求1所述的现场混装乳化炸药灌装装药施工方法,其特征在于,所述第二温度传感器距离输药胶管的出药口端40cm。6. The on-site mixed emulsion explosive filling and charging construction method according to claim 1 is characterized in that the second temperature sensor is 40 cm away from the drug outlet end of the drug delivery hose. 7.根据权利要求3所述的现场混装乳化炸药灌装装药施工方法,其特征在于,所述第一温度传感器与输药胶管之间设有环形的隔热材料层。7. The on-site mixed emulsion explosive filling and charging construction method according to claim 3 is characterized in that an annular heat insulation material layer is provided between the first temperature sensor and the drug delivery hose. 8.根据权利要求4所述的现场混装乳化炸药灌装装药施工方法,其特征在于,所述第二温度传感器与输药胶管之间设有环形的隔热材料层。8. The on-site mixed emulsion explosive filling and charging construction method according to claim 4, characterized in that an annular heat insulation material layer is provided between the second temperature sensor and the drug delivery hose.
CN202410245237.XA 2024-03-05 2024-03-05 A construction method for filling and charging mixed emulsion explosives on site Pending CN118009829A (en)