CN114714646A - Production method of printing gloss oil composite film - Google Patents
Production method of printing gloss oil composite film Download PDFInfo
- Publication number
- CN114714646A CN114714646A CN202110000818.3A CN202110000818A CN114714646A CN 114714646 A CN114714646 A CN 114714646A CN 202110000818 A CN202110000818 A CN 202110000818A CN 114714646 A CN114714646 A CN 114714646A
- Authority
- CN
- China
- Prior art keywords
- gloss oil
- film
- original
- composite film
- films
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention provides a production method of a printing gloss oil composite film, which comprises the following steps: s1): slitting and layering: the original film with insufficient strength between films is separated into A, B two rolls by a splitting machine; in the process of cutting the original film by the aid of the cutting machine in S1, the original film is firstly soaked in hot water at the temperature of 70-80 ℃ for 10-15 minutes, and two rolls of cut raw materials A, B are respectively sent to an air heater to be air-dried; s2): coating gloss oil: coating the gloss oil full plate on the original binding surface of the roll A by a printer; the gloss oil used in the step S2 is environment-friendly UV gloss oil, so that the strength between films of the film can be effectively improved, the performance of the film meets the requirement of long-time storage, and the problem that the existing printed film is only scrapped due to performance reduction caused by long-time storage in production can be solved; after the film is cured, the strength between films of the film is obviously improved, and various technical requirements and customer use requirements of the casing film can be completely met.
Description
Technical Field
The invention relates to the technical field of packaging film production processes, in particular to a production method of a printing gloss oil composite film.
Background
The share of plastic packages and plastic package products in the market is getting larger and larger, and especially the composite plastic flexible packages and the printing composite films are widely applied to the fields of food, medicine, chemical industry and the like, wherein the proportion of the plastic packages is the largest, such as beverage packages, quick-frozen food packages, steamed and cooked food packages, fast food packages and the like, and the plastic packages and the printing composite films bring great convenience to the life of people.
After being produced, the printed film in the prior art can be placed in a dust-free storehouse for a long time for some reasons and cannot be sold in time, the strength between films cannot meet the requirement due to long-term placement, and if a method for improving the strength between films cannot be found effectively, the printed film produced in the prior art becomes waste after being stored for a long time, cannot reach the factory standard, and has no value.
Meanwhile, after the film is produced, the strength between films can be weakened after a period of time, so that the quality problems of the product, such as bubbles, are caused in the using process of a client. Therefore, it is necessary to find a process method for improving the strength between films of a thin film so that the properties of the thin film can meet the requirement of long-term storage.
Disclosure of Invention
The technical problem to be solved by the invention is to overcome the existing defects and provide a production method of a printing gloss oil composite film, which can effectively solve the problems in the background technology.
In order to achieve the above object, the present invention provides: a production method of a printing gloss oil composite film comprises the following steps:
s1): slitting and layering: the original film with insufficient strength between films is separated into A, B two rolls by a splitting machine;
s2): coating gloss oil: coating the gloss oil full plate on the original binding surface of the roll A by a printer;
s3): compounding: carrying out high-temperature pressing on the roll A of the gloss oil coated surface and the roll B of the original binding surface;
s4): curing in an inner printing process: placing the compounded film into a curing box for curing, and adopting an inner printing process; after the curing is finished, the strength between films of the film is obviously improved, and all technical requirements and customer use requirements of the casing film can be completely met.
Further, the gloss oil used in step S2 is an environment-friendly UV gloss oil, and the gloss oil comprises the following components: 25-30 parts of ultraviolet photosensitive resin, 5-8 parts of photoinitiator, 8-20 parts of active monomer and 3-5 parts of auxiliary solvent.
Furthermore, the thickness of the roll A coated with the original laminating gloss oil is controlled to be 2 microns.
Further, in the process of cutting the original film by the cutting machine in the step S1, the original film is firstly soaked in hot water at 70-80 ℃ for 10-15 minutes, and the cut A, B rolls of raw materials are respectively sent to an air heater for air drying.
Further, the step S2 gloss oil applying process is performed in a dark box.
Further, the high-temperature pressing in the step S3 is performed in four stages, the surface temperature of the first section of control pressing roller is 100 to 120 ℃, the surface temperature of the second section of control pressing roller is 120 to 140 ℃, the surface temperature of the third section of control pressing roller is 140 to 180 ℃, and the surface temperature of the fourth section of control pressing roller is 180 to 220 ℃.
Further, in the step S4, the temperature of the curing box is controlled to be 180-220 ℃, and curing is carried out for 20-30 minutes.
Compared with the prior art, the invention has the beneficial effects that: the invention can effectively improve the strength between films, enables the performance of the films to meet the requirement of long-time storage, and simultaneously can solve the problem that the performance of the existing printed films is reduced and only can be scrapped due to long-time storage; after the film is cured, the strength between films of the film is obviously improved, and various technical requirements and customer use requirements of the casing film can be completely met.
Drawings
FIG. 1 is a flow chart of a method for producing a printed gloss oil composite film according to the present invention.
Detailed Description
The technical solutions in the embodiments of the present invention will be clearly and completely described below with reference to the drawings in the embodiments of the present invention, and it is obvious that the described embodiments are only a part of the embodiments of the present invention, and not all of the embodiments. All other embodiments, which can be derived by a person skilled in the art from the embodiments given herein without making any creative effort, shall fall within the protection scope of the present invention.
Referring to fig. 1, the present invention provides the following technical solutions:
a production method of a printing gloss oil composite film comprises the following steps:
s1): slitting and layering: the original film with insufficient strength between films is separated into A, B two rolls by a splitting machine; in the process of cutting the original film by the aid of the cutting machine in S1, the original film is firstly soaked in hot water at the temperature of 70-80 ℃ for 10-15 minutes, and two rolls of cut raw materials A, B are respectively sent to an air heater to be air-dried; s2): coating gloss oil: coating the gloss oil full plate on the original binding surface of the roll A by a printer; the gloss oil used in the step S2 is environment-friendly UV gloss oil, the thickness of the original gluing gloss oil of the roll A is controlled to be 2 micrometers, and the environment-friendly UV gloss oil comprises the following components: 25-30 parts of ultraviolet photosensitive resin, 5-8 parts of photoinitiator, 8-20 parts of active monomer and 3-5 parts of assistant, and the ultraviolet photosensitive resin is prepared by composite processing; the whole process of coating the gloss oil is operated in a dark box; s3): compounding: carrying out high-temperature pressing on the polished oil surface of the roll A and the original binding surface of the roll B; the high-temperature pressing in the step S3 is carried out in four stages, the surface temperature of a first section of control pressing roller is 100-120 ℃, the surface temperature of a second section of control pressing roller is 120-140 ℃, the surface temperature of a third section of control pressing roller is 140-180 ℃, and the surface temperature of a fourth section of control pressing roller is 180-220 ℃; s4): curing in an inner printing process: placing the compounded film into a curing box for curing, and adopting an inner printing process; and S4, controlling the temperature of the curing box at 180-220 ℃, curing for 20-30 minutes, and after curing is completed, obviously improving the strength between films, so that various technical requirements and customer use requirements of the casing film can be completely met.
The invention has the advantages that: the invention can effectively improve the strength between films, enables the performance of the films to meet the requirement of long-time storage, and simultaneously can solve the problem that the performance of the existing printed films is reduced and only can be scrapped due to long-time storage; after the film is cured, the strength between films of the film is obviously improved, and various technical requirements and customer use requirements of the casing film can be completely met.
Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that changes, modifications, substitutions and alterations can be made in these embodiments without departing from the principles and spirit of the invention, the scope of which is defined in the appended claims and their equivalents.
Claims (7)
1. A production method of a printing gloss oil composite film is characterized by comprising the following steps: the method comprises the following steps:
s1): slitting and layering: the original film with insufficient strength between films is separated into A, B two rolls by a splitting machine;
s2): coating gloss oil: coating the gloss oil full plate on the original binding surface of the roll A by a printer;
s3): compounding: carrying out high-temperature pressing on the polished oil surface of the roll A and the original binding surface of the roll B;
s4): curing in an inner printing process: placing the compounded film into a curing box for curing, and adopting an inner printing process; after the curing is finished, the strength between films of the film is obviously improved, and all technical requirements and customer use requirements of the casing film can be completely met.
2. A method of producing a printed gloss oil composite film according to claim 1, characterized in that: the gloss oil used in the step S2 is environment-friendly UV gloss oil, and comprises the following components: 25-30 parts of ultraviolet photosensitive resin, 5-8 parts of photoinitiator, 8-20 parts of active monomer and 3-5 parts of auxiliary solvent.
3. A method of producing a printed gloss oil composite film according to claim 1, characterized in that: the thickness of the roll A coated with the original laminating gloss oil is controlled to be 2 microns.
4. A method of producing a printed gloss oil composite film according to claim 1, characterized in that: in the step S1, the cutting machine firstly soaks the original film in hot water of 70-80 ℃ for 10-15 minutes in the process of cutting the original film, and the A, B rolls of the cut raw materials are respectively sent to an air heater to be air-dried.
5. A method of producing a printed gloss oil composite film according to claim 1, characterized in that: the step S2 gloss oil application whole process is operated in a dark box.
6. A method of producing a printed gloss oil composite film according to claim 1, characterized in that: the high-temperature pressing in the step S3 is carried out in four stages, the surface temperature of the first section of control pressing roller is 100-120 ℃, the surface temperature of the second section of control pressing roller is 120-140 ℃, the surface temperature of the third section of control pressing roller is 140-180 ℃, and the surface temperature of the fourth section of control pressing roller is 180-220 ℃.
7. A method of producing a printed gloss oil composite film according to claim 1, characterized in that: and in the step S4, the temperature of the curing box is controlled to be 180-220 ℃, and curing is carried out for 20-30 minutes.