CN110791907A - Production process of pitaya fabric - Google Patents

Production process of pitaya fabric Download PDF

Info

Publication number
CN110791907A
CN110791907A CN201910970705.9A CN201910970705A CN110791907A CN 110791907 A CN110791907 A CN 110791907A CN 201910970705 A CN201910970705 A CN 201910970705A CN 110791907 A CN110791907 A CN 110791907A
Authority
CN
China
Prior art keywords
ironing
temperature
softening
rolling
production process
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201910970705.9A
Other languages
Chinese (zh)
Inventor
沈洪良
丁月明
孙金根
沈王振
王佳俊
夏东明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Tonghui Textile Co Ltd
Original Assignee
Zhejiang Tonghui Textile Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Tonghui Textile Co Ltd filed Critical Zhejiang Tonghui Textile Co Ltd
Priority to CN201910970705.9A priority Critical patent/CN110791907A/en
Publication of CN110791907A publication Critical patent/CN110791907A/en
Pending legal-status Critical Current

Abstract

The invention discloses a production process of a pima velvet fabric, which comprises the following process flows of blank preshrinking, preshaping, napping, ironing, shaping, over-softening, dehydrating, rolling-softening, loose drying, hanging a frame, shearing, hanging a frame, ironing for the first time, ironing for the second time, coiling, cropping, shaping finished product, inspecting and rolling. The production process of the pile fabric is a brand new fabric with a leather effect formed by after-finishing on the basis of common textiles.

Description

Production process of pitaya fabric
The technical field is as follows:
the invention relates to the technical field of spinning, in particular to a production process of a pima velvet fabric.
Background art:
due to the gradual improvement of the daily living standard, people pursue the clothes day by day. In view of the pursuit of people for leather clothing at present, and the fact that leather products are resisted by animal protective tissues, the development of a textile with leather effect becomes the development direction of the mass consumption fabric.
The invention content is as follows:
the invention aims to solve the technical problem of providing a production process of a pima pile fabric with a leather effect formed by after-finishing on the basis of a common textile.
The technical scheme of the invention is that a production process of a pima velvet fabric is provided, which comprises the following process flows of blank preshrinking, presetting, napping, ironing, setting, softening, dehydrating, softening by rolling, loose drying, hanging on a frame, shearing, hanging on a frame, ironing for the first time, ironing for the second time, rolling, cropping, setting of finished products, checking and rolling, wherein the blank preshrinking temperature is 80 ℃, and the time is 30 minutes; presetting parameters, rolling 1.5 percent of 821 raising agent at the temperature of 210 ℃ and the speed of 28 meters per minute; the ironing light adopts double-roller ironing, and the parameters are that the temperature is 180 ℃, the vehicle speed is 13 m/min, and the gauge is 36%; setting temperature is 210 ℃, and vehicle speed is 40 m/min; when the soft is finished, 829 softening agent of 10 g/l is adopted, and the vehicle speed is 12 m/min; roll soft with 20 g/l 527 softener; the setting temperature of the finished product is 170 ℃, and the vehicle speed is 40 m/min.
Preferably, the first scalding adopts a hair falling mode, and the temperature is 180 ℃; the second time of ironing adopts a hair smoothing mode, and the temperature is 150 ℃.
Compared with the prior art, the invention has the following advantages after the process is adopted: on the basis of the original common textile, a brand new product with leather effect is formed through a plurality of times of after-finishing processing.
The specific implementation mode is as follows:
the invention is further illustrated with respect to specific embodiments below:
a production process of a pima velvet fabric is characterized by comprising the following steps: the process flow comprises the following steps of white blank preshrinking, presetting, napping, ironing, setting, over-softening, dehydrating, rolling and softening, loose drying, hanging a shelf (the shelf cannot touch a bottom plate in a suspended way), shearing (the shelf cannot touch a cross strip in a shearing way), hanging the shelf (the shelf cannot touch the bottom plate in a suspended way), performing primary ironing, performing secondary ironing, coiling and cropping, setting a finished product, and inspecting and coiling, wherein the white blank preshrinking temperature is 80 ℃ and the time is 30 minutes; presetting parameters, rolling 1.5 percent of 821 raising agent at the temperature of 210 ℃ and the speed of 28 meters per minute; the ironing light adopts double-roller ironing, and the parameters are that the temperature is 180 ℃, the vehicle speed is 13 m/min, and the gauge is 36%; setting temperature is 210 ℃, and vehicle speed is 40 m/min; when the soft is finished, 829 softening agent of 10 g/l is adopted, and the vehicle speed is 12 m/min; roll soft with 20 g/l 527 softener; the setting temperature of the finished product is 170 ℃, and the vehicle speed is 40 m/min.
The invention has the following advantages: on the basis of the original common textile, a brand new product with leather effect is formed through a plurality of times of after-finishing processing.
The foregoing is illustrative of the preferred embodiments of the present invention only and is not to be construed as limiting the claims.

Claims (2)

1. A production process of a pima velvet fabric is characterized by comprising the following steps: the process flow comprises the steps of white blank preshrinking, presetting, napping, ironing, setting, over-softening, dehydrating, rolling and softening, loose drying, hanging, shearing, hanging, first ironing, second ironing, coiling and cropping, finished product setting, inspecting and coiling, wherein the white blank preshrinking temperature is 80 ℃ and the time is 30 minutes; presetting parameters, rolling 1.5% of raising agent at the temperature of 210 ℃ and the speed of 28 m/min; the ironing light adopts double-roller ironing, and the parameters are that the temperature is 180 ℃, the vehicle speed is 13 m/min, and the gauge is 36%; setting temperature is 210 ℃, and vehicle speed is 40 m/min; softening by using 10 g/L of softening agent at the speed of 12 m/min; rolling and softening by using a softening agent of 20 g/L; the setting temperature of the finished product is 170 ℃, and the vehicle speed is 40 m/min.
2. The production process of the piquan fabric according to claim 1, characterized in that: the first scalding adopts a hair falling mode, and the temperature is 180 ℃; the second time of ironing adopts a hair smoothing mode, and the temperature is 150 ℃.
CN201910970705.9A 2019-10-13 2019-10-13 Production process of pitaya fabric Pending CN110791907A (en)