CN110616866A - Environment-friendly wood grain waterproof mosaic and manufacturing process thereof - Google Patents

Environment-friendly wood grain waterproof mosaic and manufacturing process thereof Download PDF

Info

Publication number
CN110616866A
CN110616866A CN201810855635.8A CN201810855635A CN110616866A CN 110616866 A CN110616866 A CN 110616866A CN 201810855635 A CN201810855635 A CN 201810855635A CN 110616866 A CN110616866 A CN 110616866A
Authority
CN
China
Prior art keywords
environment
waterproof
aluminum
veneer
mosaic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810855635.8A
Other languages
Chinese (zh)
Inventor
赖展勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nanhai District Foshan Branch Building Materials Co Ltd
Original Assignee
Nanhai District Foshan Branch Building Materials Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanhai District Foshan Branch Building Materials Co Ltd filed Critical Nanhai District Foshan Branch Building Materials Co Ltd
Priority to CN201810855635.8A priority Critical patent/CN110616866A/en
Publication of CN110616866A publication Critical patent/CN110616866A/en
Pending legal-status Critical Current

Abstract

An environment-friendly wood grain waterproof mosaic and a manufacturing process thereof are mainly characterized in that: the hot-melt adhesive film is compounded on one aluminum-plastic plate, and a veneer is compounded on one hot-melt adhesive film. Compounding an aluminum-plastic plate, a hot-melt adhesive film and a veneer on a compounding machine platform from bottom to top in sequence, covering a plastic bag for sealing, vacuumizing, pushing into the compounding machine, heating (100-; the main advantages of the invention are: 1. radiation protection, high temperature resistance, no water absorption and environmental protection; 2. the compression resistance, the tensile resistance, the water resistance and the acid resistance all accord with the national standard; 3. the anti-skid rubber is anti-skid, not easy to break, not easy to fall off, environment-friendly and safe.

Description

Environment-friendly wood grain waterproof mosaic and manufacturing process thereof
Technical Field
The invention relates to the field of building decoration materials, in particular to a manufacturing process of an environment-friendly wood grain mosaic.
Background
The mosaics used in the market at present mainly comprise glass mosaics, ceramic mosaics, marble mosaics and the like, the mosaics can be divided into different types according to materials and processes, the mosaics made of glass can be divided into machine single-face cutting, machine double-face cutting, manual cutting and the like according to the processes, the mosaics made of non-glass materials can be divided into ceramic mosaics, stone mosaics, metal mosaics and the like according to the materials, and the ceramic mosaics are the most traditional mosaics and are small and exquisite, but dull and low in grade. The marble mosaic is a mosaic variety developed in the middle period, is rich and colorful, but has poor acid and alkali resistance and poor waterproof performance, so the market reflection is not good. A glass mosaic is divided into multiple small-class glass mosaics, molten glass mosaics, glass mosaics which are melted and formed at high temp. by silicate as main raw material and contain a small amount of bubbles and non-molten particles, sintered glass mosaics which are made up by using glass powder as main raw material and adding a proper quantity of adhesive through isobaric shaping, glass mosaic which is sintered at a certain temp. and contains a small amount of bubbles and a certain quantity of metal crystal particles. But present mosaic can not paste with white cement, and white cement is more crude, and first easy scratch glass surface, and second, white cement time is of a specified duration, and easy yellowing can corrode the mosaic, and is whole not beautiful, and the glass mosaic is breakable, easily drops, and is not safe enough, when with wall brick match, because the thickness of wall brick all is 8 millimeters generally, so need once make level, take time and take a lot of work.
Aiming at various defects of the Marseke manufacturing process, the appearance of the novel Marseke manufacturing process is urgently expected by the market and people, and the Marseke manufacturing process not only has convenient manufacturing process and cost saving, but also has the advantages of environmental protection, water resistance and durability.
Disclosure of Invention
Aiming at the defects of the traditional mosaic manufacturing process, the inventor of the invention has been engaged in the building and decoration material industry for many years, and finally obtains the environment-friendly wood grain waterproof mosaic and the production of the manufacturing process thereof through repeated research and demonstration.
Aiming at the problems, the invention aims to solve the problems that: the mosaic manufacturing process has the advantages of simple manufacturing process, cost saving, environmental protection, water resistance and durability.
In order to solve the problems, the environment-friendly wood grain waterproof mosaic and the manufacturing process thereof are mainly characterized in that: mainly comprises an aluminum-plastic plate, a veneer, a hot melt adhesive film and a vacuum compound machine. And compounding the aluminum-plastic plate, the hot-melt adhesive film and the wood veneer on a compounding machine platform from bottom to top in sequence, covering a plastic bag for sealing, vacuumizing, pushing into the compounding machine, heating to the temperature of 100 plus 130 ℃, preserving heat for 40-70 minutes, and taking out of the machine for cooling and forming.
In order to solve the problems, the technical scheme of the environment-friendly wood grain waterproof mosaic and the manufacturing process thereof is as follows: flatly placing the aluminum-plastic plate on a compound machine platform, covering the hot melt adhesive film on the aluminum-plastic plate, and cutting off the redundant hot melt adhesive film to enable the size of the hot melt adhesive film to be the same as that of the aluminum-plastic plate; flatly covering a wood veneer on a hot-melt adhesive film, then covering a silk screen and a plastic bag, and pressing four edges of the plastic bag to enable the compound machine platform to be in a sealing state; putting the sealed adhesive bag on a platform of the compound machine, starting the compound machine, opening an air extraction switch, checking whether the adhesive bag leaks air, pushing the platform into the compound machine after confirming that the adhesive bag does not leak air, closing a machine door, heating to the temperature of 100 plus 130 ℃, and preserving the heat for 40-70 minutes; after the heat preservation time is over, pushing the whole plastic bag out of the compound machine platform, cooling for 30 minutes, opening the plastic bag, taking out the formed veneer aluminum-plastic plate, brushing the mixed pigment on the surface of the veneer, and waiting for 24 hours until the pigment is completely dried; and conveying the formed veneer aluminum-plastic panel dyed with the pigment to a paint spraying workshop, putting the panel in order, conveying the panel into a paint spraying track, spraying a protective environment-friendly paint layer, conveying the panel into the paint spraying track again after the formed veneer aluminum-plastic panel is dried completely, spraying a waterproof agent layer, performing quality inspection after the waterproof agent is dried completely, and checking the quality to obtain a finished wood grain mosaic product.
The manufacturing process of the environment-friendly wood grain waterproof mosaic has the advantages that:
1. radiation protection, high temperature resistance, no water absorption and environmental protection.
2. The compression resistance, the tensile resistance, the water resistance and the acid resistance all accord with the national standard.
3. The anti-skid rubber is anti-skid, not easy to break, not easy to fall off, environment-friendly and safe.
Detailed Description
In order that the present invention may be more readily understood, embodiments of the present invention are described in detail below with reference to specific examples.
The environment-friendly wood grain waterproof mosaic and the manufacturing process thereof are as follows: flatly placing the aluminum-plastic plate on a compound machine platform, covering the hot melt adhesive film on the aluminum-plastic plate, and cutting off the redundant hot melt adhesive film to enable the size of the hot melt adhesive film to be the same as that of the aluminum-plastic plate; flatly covering a wood veneer on a hot-melt adhesive film, then covering a silk screen and a plastic bag, and pressing four edges of the plastic bag to enable the compound machine platform to be in a sealing state; putting the sealed adhesive bag on a platform of the compound machine, starting the compound machine, opening an air extraction switch, checking whether the adhesive bag leaks air, pushing the platform into the compound machine after confirming that the adhesive bag does not leak air, closing a machine door, heating to the temperature of 100 plus 130 ℃, and preserving the heat for 40-70 minutes; after the heat preservation time is over, pushing the whole plastic bag out of the compound machine platform, cooling for 30 minutes, opening the plastic bag, taking out the formed veneer aluminum-plastic plate, brushing the mixed pigment on the surface of the veneer, and waiting for 24 hours until the pigment is completely dried; and conveying the formed veneer aluminum-plastic panel dyed with the pigment to a paint spraying workshop, putting the panel in order, conveying the panel into a paint spraying track, spraying a protective environment-friendly paint layer, conveying the panel into the paint spraying track again after the formed veneer aluminum-plastic panel is dried completely, spraying a waterproof agent layer, performing quality inspection after the waterproof agent is dried completely, and checking the quality to obtain a finished wood grain mosaic product.
In summary, the contents and specific embodiments of the manufacturing process of the environment-friendly wood-grain waterproof mosaic are only for illustrating the essence and the content of the present invention clearly, and are not limited to the changes based on the concept of the present invention in a limiting way, and the inventor in the art can arbitrarily change the concept of the present invention, but still fall into the protection scope of the present invention by combining the common general knowledge and the conventional means in the art based on the concept of the present invention.

Claims (9)

1. The environment-friendly wood grain waterproof mosaic is mainly characterized in that: the hot-melt adhesive film is compounded on one aluminum-plastic plate, and a veneer is compounded on one hot-melt adhesive film.
2. The manufacturing process of the environment-friendly wood grain waterproof mosaic is mainly characterized by comprising the following steps of:
flatly placing an aluminum-plastic plate on a compound machine platform, covering a hot melt adhesive film on the aluminum-plastic plate, and cutting off redundant hot melt adhesive films to enable the hot melt adhesive films to be the same as the aluminum-plastic plate in size;
flatly covering the wood veneer on the hot melt adhesive film, then covering the hot melt adhesive film with a silk screen and a plastic bag, and pressing four edges of the plastic bag to enable the compound machine platform to be in a sealed state;
putting the sealed adhesive bag on a platform of the compound machine, starting the compound machine, opening an air extraction switch, checking whether the adhesive bag leaks air, pushing the platform into the compound machine after confirming that the adhesive bag does not leak air, closing a machine door, heating to the temperature of 100-;
fourthly, after the heat preservation time is over, pushing the whole plastic bag out of the compound machine platform, cooling the plastic bag for 30 minutes at normal temperature, opening the plastic bag, taking out the formed veneer aluminum-plastic plate, brushing the mixed pigment on the surface of the veneer, and waiting for 24 hours until the pigment is completely dried;
and fifthly, conveying the formed veneer aluminum-plastic plate dyed with the pigment to a paint spraying workshop, neatly placing the formed veneer aluminum-plastic plate and conveying the formed veneer aluminum-plastic plate to a paint spraying track, spraying a layer of protective environment-friendly paint, conveying the formed veneer aluminum-plastic plate to the paint spraying track again after the formed veneer aluminum-plastic plate is dried completely, spraying a layer of waterproof agent, performing quality inspection after the waterproof agent is dried completely, and checking the quality to be qualified to obtain the finished product of the environment-friendly wood grain waterproof mosaic.
3. The manufacturing process of the environment-friendly wood grain waterproof mosaic as claimed in claim 2, wherein the main characteristics are as follows: and secondly, covering the plastic-aluminum plate hot-melt adhesive film wood veneer with a plastic bag to form a sealing body, and vacuumizing the sealing body.
4. The manufacturing process of the environment-friendly wood grain waterproof mosaic as claimed in claim 2, wherein the main characteristics are as follows: and step three, heating the pumped-out sealing body at the temperature of 100-130 ℃.
5. The manufacturing process of the environment-friendly wood grain waterproof mosaic as claimed in claim 2, wherein the main characteristics are as follows: and step three, after the heating operation of the sealing body is finished, heat preservation is needed for 40-70 minutes.
6. The manufacturing process of the environment-friendly wood grain waterproof mosaic as claimed in claim 2, wherein the main characteristics are as follows: and fourthly, cooling at normal temperature after the heat preservation time of the sealing body is finished, wherein the cooling time is 30 minutes.
7. The manufacturing process of the environment-friendly wood grain waterproof mosaic as claimed in claim 2, wherein the main characteristics are as follows: and fourthly, after the sealing body is cooled at normal temperature, opening the rubber bag to take out a finished veneer aluminum-plastic plate, processing the pigment on the surface of the veneer, and waiting for the pigment to dry out for 24 hours.
8. The manufacturing process of the environment-friendly wood grain waterproof mosaic as claimed in claim 2, wherein the main characteristics are as follows: and in the fifth step, after the pigment of the finished veneer aluminum-plastic panel is dried completely, carrying out environment-friendly paint spraying treatment on the surface of the veneer.
9. The manufacturing process of the environment-friendly wood grain waterproof mosaic as claimed in claim 2, wherein the main characteristics are as follows: and fifthly, spraying a waterproof agent after the finished veneer aluminum-plastic plate is completely painted.
CN201810855635.8A 2018-07-31 2018-07-31 Environment-friendly wood grain waterproof mosaic and manufacturing process thereof Pending CN110616866A (en)