CN110126011A - A kind of punching cutting process of bright enhancement film - Google Patents

A kind of punching cutting process of bright enhancement film Download PDF

Info

Publication number
CN110126011A
CN110126011A CN201910260072.2A CN201910260072A CN110126011A CN 110126011 A CN110126011 A CN 110126011A CN 201910260072 A CN201910260072 A CN 201910260072A CN 110126011 A CN110126011 A CN 110126011A
Authority
CN
China
Prior art keywords
enhancement film
bright enhancement
aperture
cutting process
film
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201910260072.2A
Other languages
Chinese (zh)
Inventor
傅丽丽
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHENZHEN SANBUM OPTOELECTRONICS CO Ltd
Original Assignee
SHENZHEN SANBUM OPTOELECTRONICS CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHENZHEN SANBUM OPTOELECTRONICS CO Ltd filed Critical SHENZHEN SANBUM OPTOELECTRONICS CO Ltd
Priority to CN201910260072.2A priority Critical patent/CN110126011A/en
Publication of CN110126011A publication Critical patent/CN110126011A/en
Pending legal-status Critical Current

Abstract

The present invention relates to a kind of punching cutting process of bright enhancement film, there is following steps: S10, cross cutting rushes aperture and shape on the bright enhancement film;S20, row aperture at and side edge bright enhancement film waste material;S30, patch third protective film;S40, winding cut after the completion of bright enhancement film.The present invention directly cuts out the shape of aperture and bright enhancement film, and the bright enhancement film waste material at aperture and at frame is disposably excluded by cross cutting one-step shaping, and the whole concise in technology that cuts is efficient, can fast implement the processing of the bright enhancement film with front camera hole.

Description

A kind of punching cutting process of bright enhancement film
Technical field
The present invention relates to optical element processing technique field more particularly to a kind of punching cutting process of bright enhancement film.
Background technique
Die-cutting machine (Die Cutting Machine), is called hydraulic cutting presser, guillotine and numerical control stamping machine, is mainly used for corresponding Some nonmetallic materials, adhesive sticker, EVA, double-sided adhesive, electronics and mobile phone rubber mat etc. cross cutting (complete disconnected, half disconnected), impression, scald Gold, fitting and automatic waste discharge, die-cutting machine pass through coining using steel knife, hardware dies and steel wire (or steel engraving at template) Version applies certain pressure, and printing or cardboard are rolled and are cut into certain shapes.
Bright enhancement film is also referred to as brightness enhancement film, condensing film or BEF, is widely used in opto-electronics, is issued for converging light source Light.Bright enhancement film is mounted on the light-emitting surface of backlight, the light that backlight issues will be assembled towards user direction, thus can mention The positive emitting brightness of high backlight, also, unemployed light outside visual angle are recycled according to the reflection effect again of light, And assembled with optimal angle towards user.Bright enhancement film is usually to be arranged to make up by many a prism bars according to a direction , form a prism array.
In order to realize the comprehensive screenization of display screen for the mobile phone for having front camera, (95% or more screen occupies Rate), it is required that the backlight module aperture as light source, to place front camera, wherein the important composition as backlight module One of bright enhancement film also need to punch, for this reason, it may be necessary to which the punching cutting process to bright enhancement film carries out design of making rational planning for.
Summary of the invention
The technical problems to be solved by the invention are how to realize quickly having for the bright enhancement film with front camera hole Effect processing.
The technical proposal adopted by the invention to solve the above technical problems is that:
A kind of punching cutting process of bright enhancement film, comprising the following steps: S10, on the bright enhancement film cross cutting rush aperture and Shape;S20, row aperture at and side edge bright enhancement film waste material;S30, patch third protective film.
In a preferred embodiment, in step slo, it is punched since the prism surface side of the bright enhancement film.
In a preferred embodiment, it in step S20, is removed by having sticking OPP adhesive tape bonding on one side At aperture and the bright enhancement film waste material of side edge.
In a preferred embodiment, the OPP adhesive tape passes through adjacent two rubber rollers and the film compacting that adds lustre to Fitting, to be bonded waste material waste discharge.
In a preferred embodiment, in step slo, the punching of bright enhancement film is realized by single seat die-cutting machine.
The beneficial effects of the present invention are:
The present invention directly cuts out the shape of aperture and bright enhancement film by cross cutting one-step shaping, and will be at aperture and frame The bright enhancement film waste material at place disposably excludes, and the whole concise in technology that cuts is efficient, can fast implement the increasing with front camera hole The processing of light film.
Detailed description of the invention
The present invention will be further described with reference to the accompanying drawings and examples.
Fig. 1 is the flow chart of the punching cutting process of the bright enhancement film of one embodiment of the invention;
Fig. 2 is the cross-sectional view before the punching of the bright enhancement film of one embodiment of the invention;
Fig. 3 is facing at row's aperture of the bright enhancement film of one embodiment of the invention and after the bright enhancement film waste material of side edge Figure;
Fig. 4 is the cross-sectional view at row's aperture of the bright enhancement film of one embodiment of the invention and after the bright enhancement film waste material of side edge A-A;
Fig. 5 is the schematic diagram of the one embodiment for the waste discharge that the present invention has sticking OPP adhesive tape and bright enhancement film on one side;
Fig. 6 is the cross-sectional view after the patch third protective film of the bright enhancement film of one embodiment of the invention.
Specific embodiment
It is carried out below with reference to technical effect of the embodiment and attached drawing to design of the invention, specific structure and generation clear Chu, complete description, to be completely understood by the purpose of the present invention, scheme and effect.It should be noted that the case where not conflicting Under, the features in the embodiments and the embodiments of the present application can be combined with each other.
It should be noted that unless otherwise specified, when a certain feature referred to as " fixation ", " connection " are in another feature, It can directly fix, be connected to another feature, and can also fix, be connected to another feature indirectly.In addition, this The descriptions such as upper and lower, left and right used in invention are only the mutual alignment pass relative to each component part of the present invention in attached drawing For system.
In addition, unless otherwise defined, the technology of all technical and scientific terms used herein and the art The normally understood meaning of personnel is identical.Term used in the description is intended merely to description specific embodiment herein, without It is to limit the present invention.Term " and or " used herein includes the arbitrary of one or more relevant listed items Combination.
Referring to Fig.1, Fig. 1 is the flow chart of the punching cutting process of the bright enhancement film of one embodiment of the invention, in the process In, include following steps: S00, the film raw material that will add lustre to are posted on carrier film;S10, cross cutting rushes aperture on the bright enhancement film And shape;S20, row aperture at and side edge bright enhancement film waste material;S30, patch third protective film;After the completion of S40, winding are cut Bright enhancement film.
Referring to Fig. 2, Fig. 2 is the cross-sectional view before the punching of the bright enhancement film of one embodiment of the invention.In the present embodiment, make Bright enhancement film for raw material includes the first protective film 1, add lustre to membrane body 2 and the second protective film 3, wherein the rib for the membrane body 2 that adds lustre to Mirror surface the first protective film 1 of direction.
Referring to Fig. 3 and Fig. 4, Fig. 3 is at row's aperture of the bright enhancement film of one embodiment of the invention and the bright enhancement film of side edge Front view after waste material, Fig. 4 are at row's aperture of the bright enhancement film of one embodiment of the invention and after the bright enhancement film waste material of side edge Cross-sectional view A-A.In Fig. 3, the aperture and border area for beating hacures are the region for needing to cut off, and in cutting process In, it is punched since the prism facets (namely the upper side for the membrane body 2 that adds lustre in Fig. 4) for the membrane body 2 that adds lustre to, hemisection when punching, only The first protective film 1 and the membrane body 2 that adds lustre to are cut off, and the second protective film 3 is not punched.Wherein, carrier film 4 is used for secondary process, and The second protective film 3 is protected, the second protective film 3 is prevented to be scratched or be stained in process foreign matter.
Fig. 5 is the schematic diagram of the one embodiment for the waste discharge that the present invention has sticking OPP adhesive tape and bright enhancement film on one side;Its In, what the spline curve of dotted line shape represented is to have sticking OPP adhesive tape on one side, and what upper and lower two circles represented is rubber roller, is located at What the straight line between two adjacent rubber rollers represented is bright enhancement film, and OPP adhesive tape is bonded with bright enhancement film by adjacent rubber roller compression, And OPP adhesive tape is towards the one side band toughness of bright enhancement film, thus by gluing in the bright enhancement film waste material of unfettered state.
Referring to Fig. 6, Fig. 6 is the cross-sectional view after the patch third protective film 5 of the bright enhancement film of one embodiment of the invention.To prevent Bright enhancement film after processing is completed is mixed into dust and magazine in winding and transfer process, attaches in the upper side for the membrane body 2 that adds lustre to One layer of third protective film 5, attaching mode is similar with film compacting waste discharge mode of adding lustre to OPP adhesive tape, and passes through multiple rows of rubber roller Third protective film 5 is compressed and is fitted in 2 upside of membrane body of adding lustre to.
It is to be illustrated to preferable implementation of the invention, but the invention is not limited to the implementation above Example, those skilled in the art can also make various equivalent variations on the premise of without prejudice to spirit of the invention or replace It changes, these equivalent deformations or replacement are all included in the scope defined by the claims of the present application.

Claims (5)

1. a kind of punching cutting process of bright enhancement film, which is characterized in that include the following steps,
S10 is die cut on the bright enhancement film and rushes aperture and shape;
S20 is arranged at aperture and the bright enhancement film waste material of side edge;
S30 pastes third protective film.
2. the punching cutting process of bright enhancement film according to claim 1, which is characterized in that in step slo, from the increasing The prism surface side of light film starts to be punched.
3. the punching cutting process of bright enhancement film according to claim 1, which is characterized in that in step S20, pass through one side Have at sticking OPP adhesive tape bonding removal aperture and the bright enhancement film waste material of side edge.
4. the punching cutting process of bright enhancement film according to claim 3, which is characterized in that the OPP adhesive tape passes through adjacent Two rubber rollers be bonded with the film compacting that adds lustre to, to be bonded waste material waste discharge.
5. the punching cutting process of bright enhancement film according to claim 1, which is characterized in that in step slo, pass through single seat The punching of die-cutting machine realization bright enhancement film.
CN201910260072.2A 2019-04-02 2019-04-02 A kind of punching cutting process of bright enhancement film Pending CN110126011A (en)