CN109776029A - A kind of aqueous energy conservation and environmental protection decorating integrative coating and its production method - Google Patents
A kind of aqueous energy conservation and environmental protection decorating integrative coating and its production method Download PDFInfo
- Publication number
- CN109776029A CN109776029A CN201711128034.9A CN201711128034A CN109776029A CN 109776029 A CN109776029 A CN 109776029A CN 201711128034 A CN201711128034 A CN 201711128034A CN 109776029 A CN109776029 A CN 109776029A
- Authority
- CN
- China
- Prior art keywords
- powder
- glue
- environmental protection
- energy conservation
- aggregate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention is a kind of aqueous energy conservation and environmental protection decorating integrative coating and its production method.The aqueous energy conservation and environmental protection decorating integrative coating includes industrial water 40~80%, alcohol ester 12~2.5%, dry glue powder 1.0~3.0%, organosilicon modifier 2.0~5.0%, retarder 0.1~0.6%;Coloring earth joins reinforcing agent class lotion 10~40% by design and user's requirement allotment and additive amount, glue;Aggregate silicon dioxide hollow microballon, aluminium oxide cenosphere, fly ash float, ceramic hollow microballon, flyash, sepiolite powder, straw powder, corn core powder, plant shell powder, sawdust powder, glass bead, expanded perlite granule 10~50%, glue connection frame material land plaster 50~90% are through in substep investment mixing agitator; agitated 2~10 minutes and uniformly,.The coating has reached a material molding multi-functional, the multipurpose purpose that integrates energy conservation and environmental protection, heat preservation, heat-insulated, fire prevention, waterproof, one material of decoration.
Description
Technical field
A kind of aqueous energy conservation and environmental protection decorating integrative coating and its production method, the present invention relates to building energy conservation environmental protection, decoration
Material Field, is a kind of collection energy-saving and environmental protection, heat preservation, heat-insulated, fire prevention, water-proof decorative one coating and its production method, especially
A kind of flyash generated using the lower lightweight of thermal coefficient, the preferable agricultural wastes of hollow and insulation effect and industry
Floating bead, flyash, expanded perlite, coloring earth and glue join the frame materials such as the land plaster of toughness and high stability and tool
There are glue connection enhancement and the preferable chemical industry organosilicon materials of waterproof performance to combine together together, reaches various composition materials and carry out
Superiority and inferiority complementation is modified, mutually increases performance, a kind of energy conservation and environmental protection dress with larger application value that final function normalizing produces
Adorn integrated coating and its production method, the coating be especially suitable for making construction wall and flooring, roof and various industry it is cold,
The energy conservation insulation and decoration such as heated conveying pipeline is used.
Background technique
Conventional thermal insulation mortar, as building heat-insulating mortar mainly uses cement, sand, granules of polystyrene, expanded perlite
Addition water mixes, and that there are heat insulation effects is poor, intensity is low, without waterproof performance, spy for construction wall heat preservation for the thermal insulation mortar
It is not that auxiliary material must be safeguarded, repeatedly at many levels when not having decorative effect, number of drawbacks as existing for it, being used for wall
Construction operation, difficulty of construction be larger, following example: construction technology process is: smoothing out wall → smear interface with cement mortar first
Mortar → smear building heat-insulating mortar → paving pressure grid cloth → bolt anchor studs are beaten in drilling → is smeared anticracking grout → alkali-resistant primer → and is smeared greasy
Son → decorative paint.It can be seen that its cost source effect is big from its composition material and construction technology process, and there are each layer compositions
The physical and mechanical property technical indicator and shrinking percentage of material be inconsistent and layers of material there are aging and service life are inconsistent
The disadvantages of, especially its without globality as the mutation of climate change its layers of material is larger, cause crack, layering, hollowing,
Peel off, repaired after damage it is difficult, and due to its poor mechanical property, for that must be bored on construction wall when construction wall construction
The defects of hole beats bolt anchor studs and destroys main body brick, causes to seep water at wall damage, and service life is short.
Summary of the invention
The purpose of the present invention is to improve energy-saving and environmental protection, economize on resources, create a kind of multi-functional, multipurpose product.It is carrying on the back
In scape technical foundation, by adjusting its composition material and construction technology, is reached with this and improve energy-saving and environmental protection, with material collection building
Heat preservation, heat-insulated, fire prevention, waterproof, decoration are integrated purpose, and improve anti-radiation, shock resistance and cracking resistance, enhance building
Energy conservation and environmental protection and decoration, the globality of finishing material and stability, so as to improve safety and practicability, thus reach saving money
The purpose of source raising Social benefit and economic benefit.Therefore, the present invention especially use the lower lightweight of thermal coefficient, it is hollow and
The preferable agricultural wastes of insulation effect and industry generate fly ash float, flyash, coloring earth and glue connection toughness and
The materials such as the land plaster of high stability mix together with having glue connection enhancement and the preferable chemical industry organosilicon materials of waterproof performance
Conjunction combines together, reaches various composition materials and carries out superiority and inferiority complementation modification, mutually increases performance, a kind of tool that function normalizing produces
There is a kind of aqueous energy conservation and environmental protection decorating integrative coating of larger application value, background technique building is made up with the coating to realize
Thermal insulation mortar without globality, without waterproof performance, constructional difficulties and its repeatedly security risk existing for construction operation the defects of.
The present invention uses material blending and modifying, makes the function of composition material that reason be normalized, and is finally filled with a kind of aqueous energy conservation and environmental protection
It adorns integrated coating and solves the problems, such as various disadvantages present in background technique, and reach the environmental protection of collection building energy conservation, keep the temperature, is heat-insulated, anti-
Fire, waterproof, decoration are integration, which has reached multi-functional one material of building field long-sought, versatility, raising are applied
Work progress, the purpose for the requirements such as prolong the service life.
Solution of the invention is the material and on the basis of production technology in adjusting background technique, is changed using organosilicon
Property raw material and the lower light thermal insulation aggregate silicon dioxide hollow microballon of thermal coefficient, aluminium oxide cenosphere, fly ash float,
Ceramic hollow microballon, flyash, glass bead, expanded perlite granule, sepiolite powder, straw powder, corn core powder, sawdust powder,
Plant shell powder, coloring earth, glue join frame material land plaster, to realize its purpose.Therefore, the technology of the present invention produces a kind of aqueous
Energy conservation and environmental protection decorating integrative coating includes water, auxiliary agent, coloring earth, aggregate and principal component organosilicon modifier, organic silicon water-proofing
Lotion, silicon Acrylote acrylic emulsion, styrene-acrylic emulsion, dry glue powder, auxiliary agent include film forming agent alcohol ester 12, and retarder, aggregate includes two
Silica cenosphere, aluminium oxide cenosphere, fly ash float, ceramic hollow microballon, flyash, glass bead, expansion are precious
Pearl rock particle or/and sepiolite powder, straw powder, corn core powder, plant shell powder, sawdust powder, glue sign frame material land plaster, key exist
It include that organosilicon modifier or/and glue connection reinforcing agent organosilicon water-proof emulsion, silicon Acrylote acrylic emulsion, phenylpropyl alcohol are newborn in its principal component
Liquid, dry glue powder;Above-mentioned each ingredient is based on dry aggregate weight percent: clear water 40~80%, alcohol ester 12~2.5% are done
Rubber powder 1.0~3.0%, organosilicon modifier 2.0~5.0%, retarder 0.1~0.6%;Coloring earth is wanted by design and user
Allotment and additive amount are asked, glue joins reinforcing agent class lotion 10~40%;Aggregate silicon dioxide hollow microballon, aluminium oxide cenosphere,
Fly ash float, ceramic hollow microballon, flyash, sepiolite powder, straw powder, corn core powder, plant shell powder, sawdust powder, vitreous
Microballon, expanded perlite granule 10~50%, glue join frame material land plaster 50~90% through stirring in substep investment mixing agitator
It mixes 2~10 minutes and uniform,.
A kind of above-mentioned aqueous energy conservation and environmental protection decorating integrative coating and its production method:
A, modified solution aqua is prepared first: first by clear water 40~80%, alcohol ester 12~2.0%, dry glue powder 1.0
~1.5%, retarder 0.1~0.3%, coloring earth is according to design and requires metering addition, principal component organosilicon modifier 2.0
~5.0%, glue connection reinforcing agent class lotion 10~20% is put into blender be mixed evenly after, i.e., as producing aqueous energy conservation
The modified solution aqua of environmental-protection decoration one coating waits for mixing with B component,.
B, aggregate silicon dioxide hollow microballon, aluminium oxide cenosphere, fly ash float, ceramic hollow microballon, flyash,
Sepiolite powder, straw powder, corn core powder, plant shell powder, sawdust powder, glass bead, expanded perlite granule 10~50%, glue connection
Frame material land plaster 50~90% put into low speed drum-type container in be mixed evenly after addition A prepare modified solutions after
It is continuous to be mixed evenly,.
Above-mentioned content is the weight percent content of gained final products.
The aggregate silicon dioxide hollow microballon, aluminium oxide cenosphere, fly ash float, ceramic hollow microballon, fine coal
Ash, glass bead, expanded perlite, sepiolite powder, straw powder, plant shell powder, sawdust powder, its granularity of corn core powder be 0.1~
0.6mm, plant aggregate pass through (anti-corrosion, mould proof processing).
The present invention is due to micro- using silicon dioxide hollow microballon, aluminium oxide cenosphere, fly ash float, ceramic hollow
Pearl, flyash, glass bead, expanded perlite, straw powder, plant shell powder, land plaster, sepiolite powder etc. are used as main aggregate,
And accordingly adjust its composition material and production technology, and using a large amount of fireproof inorganic material and coloring earth and crosslinking and
Generation multilayer is intersected after the higher land plaster of stability merges together, calcium plaster is made to penetrate into particulate interspaces, its solidification naturally
Framework film modeling web frame, the structure play anti-aging stability action, and for straw powder, corn core powder, plant shell powder,
The materials such as sawdust powder have achieved the purpose that separate environmental sealing, so that making the coating not only has preferable energy conservation and environmental protection and fire prevention
Performance, and cracking resistance, anti-radiation, compression strength is high, and has reached a material and integrated heat preservation, heat-insulated, fire prevention, waterproof, decoration
One material is molding multi-functional, multiduty purpose, does not smear cement mortar for wall, interfacial agents, anticracking grout, does not have to grid
Cloth, the nailing that do not drill, wall body structure without the construction speed for destroying, being not required to architectural surface, improving 5 times or more compared with background technique and
It smears, spray with various colors and preferable exterior decorative effect, its easy construction, construction method, compression strength is high, steady
It is qualitative good, the features such as service life improves 10 times or more compared with background technique.
Embodiment one
The present embodiment is for producing coating finished product dry density 1000kg:
A, modified solution is prepared first: first by clear water 400kg, 12 15kg of alcohol ester, dry glue powder 10kg, slow coagulator
1.5kg, principal component organosilicon modifier 30kg, organosilicon water-proof emulsion 100kg, silicon Acrylote acrylic emulsion 50kg, styrene-acrylic emulsion
100kg, coloring earth by design and requirements color in right amount modulate add put into blender in be mixed evenly to B component
Mixing,.
B, aggregate silicon dioxide hollow microballon 10kg, aluminium oxide cenosphere 10kg, fly ash float 100kg, ceramics are empty
Heart microballon 10kg, flyash 150kg, glass bead 10kg, expanded perlite granule 20kg, straw powder 10kg, corn core powder
10kg, plant shell powder 10, sawdust powder 10kg, land plaster 600kg, sepiolite powder 50kg put into low speed drum-type container to mix and stir
After mixing uniformly, the modified solution for adding A preparations, which continuess to mix, to be stirred evenly,.
Embodiment two
The present embodiment is still for producing coating finished product dry density 1000kg:
A, modified solution is prepared first: by clear water 500kg, 12 13kg of alcohol ester, slow coagulator 2kg, principal component organosilicon
Modifying agent 35kg, dry glue powder 20kg, organosilicon water-proof emulsion 50kg, styrene-acrylic emulsion 150kg, coloring earth according to design and require
Color add in right amount investment blender in be mixed evenly to be mixed with B component,.
B, straw powder 50kg, corn core powder 50kg, plant shell powder 50, sawdust powder 50kg, fly ash float 100kg, gypsum
After being mixed evenly in powder 650kg, sepiolite powder 50kg investment low speed drum-type container, A modified solutions of addition continue to mix
Conjunction stirs evenly,.
Embodiment three
The present embodiment is still for producing coating finished product dry density 1000kg:
A, prepare modified solution first: first by clear water 750kg, alcohol ester 12 10kg, dry glue powder 10kg, slow coagulator 2kg,
Principal component organosilicon modifier 33kg, silicon Acrylote acrylic emulsion 150kg, coloring earth add in right amount according to design and desired color
Add and is mixed evenly in investment blender to be mixed with B component,.
B, aggregate fly ash float 50kg, flyash 150kg, glass bead 50kg, expanded perlite granule 100kg, stone
A modified solutions of addition, which continues to mix, after being mixed evenly in cream powder 650kg investment low speed drum-type container stirs evenly, i.e.,
At.
Example IV
The present embodiment is still for producing coating finished product dry density 1000kg:
A, modified solution is prepared first: first by clear water 800kg, dry glue powder 30kg, 12 15kg of alcohol ester, retarder 2.5kg,
It is mixed evenly in main composition organosilicon modifier 35kg, styrene-acrylic emulsion 150kg investment blender to be mixed with B component
It is even,.
B, straw powder 50kg, corn flour 50kg, plant shell powder 50kg, land plaster 700kg, expanded perlite granule 150kg
After investment low speed drum-type container is mixed evenly, A modified solutions of addition, which continues to mix, to be stirred evenly,.
Claims (3)
1. a kind of aqueous energy conservation and environmental protection decorating integrative coating and its production method include that water, auxiliary agent, aggregate and principal component include
Machine silica modifier, glue connection reinforcing agent include organosilicon water-proof emulsion, silicon Acrylote acrylic emulsion, styrene-acrylic emulsion, dry glue powder, its feature
It is above-mentioned main composition organosilicon modifier and glue connection reinforcing agent series emulsion and dry glue powder, auxiliary agent includes film forming agent alcohol ester ten
Two, delaying coagulator, coloring earth, aggregate then includes silicon dioxide hollow microballon, aluminium oxide cenosphere, fly ash float, pottery
Porcelain cenosphere, flyash, glass bead, expanded perlite granule or/and sepiolite powder, straw powder, Wang meter Xin powder, plant shell
Powder, sawdust powder, land plaster, above-mentioned each ingredient is based on dry aggregate weight percent, the aqueous energy conservation and environmental protection decorating integrative coating
And its production method includes water 40~80%, alcohol ester 12~2.5%, dry glue powder 1.0~3.0%, organosilicon modifier
2.0~5.0%, delay coagulator 0.1~0.6%, coloring earth joins reinforcing agent by design and user's requirement allotment and additive amount, glue
Class lotion 10~40%;Aggregate silicon dioxide hollow microballon, aluminium oxide cenosphere, fly ash float, ceramic hollow microballon, powder
Coal ash, sepiolite powder, straw powder, corn core powder, plant shell powder, sawdust powder, glass bead, expanded perlite granule 10~
50%, glue connection frame material land plaster 50~90% stir 2~10 minutes and uniform in substep investment mixing agitator,
Final products dry density should be in 200~650kg/m3In range.
2. a kind of aqueous energy conservation and environmental protection decorating integrative coating according to claim 1 and its production method, it is characterised in that should
Method includes:
A, modified solution aqua is prepared first: first by clear water 40~80%, alcohol ester 12~2.0%, dry glue powder 1.0~
1.5%, retarder 0.1~0.3%, coloring earth is according to design and requires metering addition, and principal component organosilicon modifier 2.0~
5.0%, glue connection reinforcing agent class lotion 10~40% is put into blender be mixed evenly after, i.e., as producing aqueous energy-saving ring
The modified solution aqua for protecting decorating integrative coating waits for mixing with B component,;
B, aggregate silicon dioxide hollow microballon, aluminium oxide cenosphere, fly ash float, ceramic hollow microballon, flyash, Hai Pao
Mountain flour, straw powder, corn core powder, plant shell powder, sawdust powder, glass bead, expanded perlite granule 10~50%, glue join skeleton
The modified solutions of A preparations of addition continue to mix after being mixed evenly in the material investment low speed drum-type container of land plaster 50~90%
Conjunction stirs evenly,;
Its final products dry density should be in 200~650kg/m3In range;
Above-mentioned content is the weight percent content of gained final products.
3. by a kind of aqueous energy conservation and environmental protection decorating integrative coating and its production method described in claim 2, it is characterised in that including
Its partial size of the aggregate, silicon dioxide hollow microballon, fly ash float, straw powder, corn core powder, are planted at aluminium oxide cenosphere
Object shell powder, sawdust powder, ceramic hollow microballon, flyash, glass bead, 0.1~0.6mm of expanded perlite.