CN109749444A - A kind of antistatic illuminating lamp shade - Google Patents

A kind of antistatic illuminating lamp shade Download PDF

Info

Publication number
CN109749444A
CN109749444A CN201711055792.2A CN201711055792A CN109749444A CN 109749444 A CN109749444 A CN 109749444A CN 201711055792 A CN201711055792 A CN 201711055792A CN 109749444 A CN109749444 A CN 109749444A
Authority
CN
China
Prior art keywords
parts
antistatic
illuminating lamp
lamp shade
low speed
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201711055792.2A
Other languages
Chinese (zh)
Inventor
王仙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Danyang Best Intelligent System Co Ltd
Original Assignee
Danyang Best Intelligent System Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Danyang Best Intelligent System Co Ltd filed Critical Danyang Best Intelligent System Co Ltd
Priority to CN201711055792.2A priority Critical patent/CN109749444A/en
Publication of CN109749444A publication Critical patent/CN109749444A/en
Withdrawn legal-status Critical Current

Abstract

The present invention relates to a kind of antistatic illuminating lamp shades, the component of the antistatic illuminating lamp shade is as follows according to parts by weight: 15-25 parts of methyl methacrylate, 20-30 parts of Dimethicone, 15-20 parts of cyclic ethylene urea of dihydroxymethyl dihydroxy, 5-10 parts of calcirm-fluoride, 2-5 parts of toluene di-isocyanate(TDI), 5-10 parts of graphite powder, 2-4 parts of age resister, 1-3 parts of cosolvent, 0.5-1 parts of antistatic agent.Manufacture craft of the present invention is simple, and raw material is easy to buy, and cost of manufacture is cheap, and antistatic property is good, has broad application prospects.

Description

A kind of antistatic illuminating lamp shade
Technical field
The present invention relates to field of illumination lamp technology more particularly to a kind of antistatic illuminating lamp shades.
Background technique
The general reflectivity of energy-saving lamp shade only has 85%.Moreover, with the increase of use time, there is aging yellowing, deformation, And temperature tolerance is gradually lost, cause lampshade easily rupturable, greatly reduces the service life of energy-saving lamp shade.In addition also quiet without resisting Electricity Functional.
Summary of the invention
To solve the above problems, the present invention provides a kind of antistatic illuminating lamp shades.
Technical scheme is as follows:
A kind of antistatic illuminating lamp shade, it is characterised in that: the component of the antistatic illuminating lamp shade is as follows according to parts by weight It is shown: 15-25 parts of methyl methacrylate, 20-30 parts of Dimethicone, 15-20 parts of cyclic ethylene urea of dihydroxymethyl dihydroxy, 5-10 parts of calcirm-fluoride, 2-5 parts of toluene di-isocyanate(TDI), 5-10 parts of graphite powder, 2-4 parts of age resister, 1-3 parts of cosolvent, resist quiet Electric agent 0.5-1 parts.
Further, the age resister is thiobis methylphenol, methyl butylbenzene base butane and thio-2 acid double ten One of eight alcohol esters.
Further, the cosolvent is one of acetamide, citric acid.
Further, the antistatic agent is one of sodium alkyl sulfonate, ethoxylated alkylamine.
Further, a kind of antistatic illuminating lamp shade preparation method, it is characterised in that:
S1: by methyl methacrylate, Dimethicone, dihydroxymethyl dihydroxy cyclic ethylene urea, toluene diisocynate Ester, cosolvent are put into reaction kettle, stir at low speed 30min;
S2: being added calcirm-fluoride and graphite powder in a kettle, after high-speed stirred 30min, low speed after being first warming up to 60-80 DEG C Stir 4h;
S3: addition antistatic agent is cooled to room temperature after addition age resister high-speed stirred 1h in a kettle and is stirred at low speed 15h stands 2h, finished product can be obtained.
According to the above aspect of the present invention, the present invention at least has the advantages that
Manufacture craft of the present invention is simple, and raw material is easy to buy, and cost of manufacture is cheap, and antistatic property is good, has wide Application prospect.
Specific embodiment
Technical solution of the present invention is described in detail as follows below with reference to embodiment.
Embodiment 1
A kind of antistatic illuminating lamp shade, it is characterised in that: the component of the antistatic illuminating lamp shade is as follows according to parts by weight It is shown: 16 parts of methyl methacrylate, 28 parts of Dimethicone, 18 parts of urea of dihydroxymethyl dihydroxy cyclic ethylene, calcirm-fluoride 6 Part, 4 parts of toluene di-isocyanate(TDI), 10 parts of graphite powder, double 4 parts of the octadecyls of thio-2 acid, 3 parts of citric acid, sodium alkyl sulfonate 0.6 part.
Preparation method are as follows:
S1: by methyl methacrylate, Dimethicone, dihydroxymethyl dihydroxy cyclic ethylene urea, toluene diisocynate Ester, cosolvent are put into reaction kettle, stir at low speed 30min;
S2: being added calcirm-fluoride and graphite powder in a kettle, after high-speed stirred 30min, low speed after being first warming up to 60-80 DEG C Stir 4h;
S3: addition antistatic agent is cooled to room temperature after addition age resister high-speed stirred 1h in a kettle and is stirred at low speed 15h stands 2h, finished product can be obtained.
Embodiment 2
A kind of antistatic illuminating lamp shade, it is characterised in that: the component of the antistatic illuminating lamp shade is as follows according to parts by weight It is shown: 21 parts of methyl methacrylate, 23 parts of Dimethicone, 17 parts of urea of dihydroxymethyl dihydroxy cyclic ethylene, calcirm-fluoride 6 Part, 3 parts of toluene di-isocyanate(TDI), 5 parts of graphite powder, 3 parts of thiobis methylphenol, 2 parts of acetamide, ethoxylated alkylamine 0.7 Part.
Preparation method are as follows:
S1: by methyl methacrylate, Dimethicone, dihydroxymethyl dihydroxy cyclic ethylene urea, toluene diisocynate Ester, cosolvent are put into reaction kettle, stir at low speed 30min;
S2: being added calcirm-fluoride and graphite powder in a kettle, after high-speed stirred 30min, low speed after being first warming up to 60-80 DEG C Stir 4h;
S3: addition antistatic agent is cooled to room temperature after addition age resister high-speed stirred 1h in a kettle and is stirred at low speed 15h stands 2h, finished product can be obtained.
Embodiment 3
A kind of antistatic illuminating lamp shade, it is characterised in that: the component of the antistatic illuminating lamp shade is as follows according to parts by weight It is shown: 24 parts of methyl methacrylate, 21 parts of Dimethicone, 18 parts of urea of dihydroxymethyl dihydroxy cyclic ethylene, calcirm-fluoride 6 Part, 2 parts of toluene di-isocyanate(TDI), 8 parts of graphite powder, 3 parts of methyl butylbenzene base butane, 1 part of citric acid, 0.5 part of sodium alkyl sulfonate.
Preparation method are as follows:
S1: by methyl methacrylate, Dimethicone, dihydroxymethyl dihydroxy cyclic ethylene urea, toluene diisocynate Ester, cosolvent are put into reaction kettle, stir at low speed 30min;
S2: being added calcirm-fluoride and graphite powder in a kettle, after high-speed stirred 30min, low speed after being first warming up to 60-80 DEG C Stir 4h;
S3: addition antistatic agent is cooled to room temperature after addition age resister high-speed stirred 1h in a kettle and is stirred at low speed 15h stands 2h, finished product can be obtained.
The above is only a preferred embodiment of the present invention, it is not intended to restrict the invention, it is noted that for this skill For the those of ordinary skill in art field, without departing from the technical principles of the invention, can also make it is several improvement and Modification, these improvements and modifications also should be regarded as protection scope of the present invention.

Claims (5)

1. a kind of antistatic illuminating lamp shade, it is characterised in that: the component of the antistatic illuminating lamp shade is according to the following institute of parts by weight Show: 15-25 parts of methyl methacrylate, 20-30 parts of Dimethicone, 15-20 parts of cyclic ethylene urea of dihydroxymethyl dihydroxy, fluorine Calcium 5-10 parts of change, it is 2-5 parts of toluene di-isocyanate(TDI), 5-10 parts of graphite powder, 2-4 parts of age resister, 1-3 parts of cosolvent, antistatic 0.5-1 parts of agent.
2. a kind of antistatic illuminating lamp shade according to claim 1, it is characterised in that: the age resister is thiobis first One of double octadecyls of base phenol, methyl butylbenzene base butane and thio-2 acid.
3. a kind of antistatic illuminating lamp shade according to claim 1, it is characterised in that: the cosolvent is acetamide, Chinese holly One of rafter acid.
4. a kind of antistatic illuminating lamp shade according to claim 1, it is characterised in that: the antistatic agent is alkyl sulfonic acid One of sodium, ethoxylated alkylamine.
5. a kind of antistatic illuminating lamp shade preparation method according to claim 1, it is characterised in that:
S1: by methyl methacrylate, Dimethicone, dihydroxymethyl dihydroxy cyclic ethylene urea, toluene di-isocyanate(TDI) helped Solvent is put into reaction kettle, stirs at low speed 30min;
S2: being added calcirm-fluoride and graphite powder in a kettle, after high-speed stirred 30min, stirs at low speed after being first warming up to 60-80 DEG C 4h;
S3: being cooled to room temperature addition antistatic agent in a kettle and stir at low speed 15h after addition age resister high-speed stirred 1h, quiet 2h is set, finished product can be obtained.
CN201711055792.2A 2017-11-01 2017-11-01 A kind of antistatic illuminating lamp shade Withdrawn CN109749444A (en)