CN1096277A - 超轻特异水泥 - Google Patents
超轻特异水泥 Download PDFInfo
- Publication number
- CN1096277A CN1096277A CN93112006A CN93112006A CN1096277A CN 1096277 A CN1096277 A CN 1096277A CN 93112006 A CN93112006 A CN 93112006A CN 93112006 A CN93112006 A CN 93112006A CN 1096277 A CN1096277 A CN 1096277A
- Authority
- CN
- China
- Prior art keywords
- parts
- cement
- microballon
- ultra
- flyash
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及建筑材料,具体地说是水泥成分和性
能的改进。它是以100份硅酸盐水泥熟料为基料,
加5~20份明矾石、5~25份石膏混合粉磨至水泥细
度,再加入10~45份粉煤灰提取物的漂珠和微珠,
经均化处理制成。本发明与普通水泥相比,具有耐高
温、隔热、防火、吸音、抗渗、抗冻、耐磨收缩系数小等
优点。其容重小仅为750~800kg/M3,比重轻仅为
1.9~2.1,性能优于普通水泥。
Description
本发明涉及建筑材料,具体地说是水泥成分和性能的改进。
目前,在建筑行业、水泥造船业、大型高架桥涵等各类需要水泥的场合,常用的水泥为普通硅酸盐水泥、矿渣水泥、粉煤灰水泥等。这些作为水泥构筑物的胶凝材料容重一般为1000~1600kg/M3,比重一般为2.8~3.15。因此存在容重大、收缩性系数大等缺点。
本发明的目的是针对上述存在的缺点,提供一种容重轻,比重少,并具有抗渗、抗冻等功能的水泥。
本发明的目的是这样实现的:它是以100份硅酸盐水泥熟料为基料,加5~20份明矾石、5~25份石膏混合粉磨至水泥细度,入10~45份粉煤灰提取物的漂珠和微珠,经均化处理制成。以100份硅酸盐水泥为基料,加5~20份膨胀剂、10~45份粉煤灰提取物漂珠和微珠,经均化处理制成。
本发明与普通水泥相比,具有耐高温、隔热、防火、吸音、抗渗、抗冻、耐磨收缩系数小等优点。其容重小仅为750~800kg/M3,比重轻仅为1.9~2.1,性能优于普通水泥。
本发明所说的粉煤灰提取物的漂珠和微珠经烘干应达到含水量<2%,粒度筛选至水泥细度要求;其物理性能为体轻、耐高温、绝缘、隔热、吸音、耐磨,筒压强度1000kg~7000kg/cm2;粉煤灰提取物的来源为火电厂或大型沸腾炉。所说的膨胀剂为EA-L型和U型。
实施例
1.按重量取硅酸盐水泥熟料100份,明矾石10份,石膏10
份混合入水泥磨磨制为水泥细度,加烘干、过0.08~0.2mm筛筛选后的粉煤灰提取物漂珠和微珠,配料后经均化设备处理后制成包装。
2.按重量取硅酸盐水泥100份,加5份EA-L型膨胀剂,10份经烘干过0.2筛的粉煤灰提取物漂珠和微珠,配料后经均化处理后制成包装。
Claims (4)
1、一种超轻特异水泥,其特征是以100份硅酸盐水泥熟料为基料,加5~20份明矾石、5~25份石膏混合粉磨水泥细度,入10~45份粉煤灰提取物的漂珠和微珠,经均化处理制成。
2、一种超轻特异水泥,其特征是以100份硅配盐水泥为基料,加5~20份膨胀剂、10~45份粉煤灰提取物漂珠和微珠,经均化处理制成。
3、按照权利要求1所述的水泥,其特征是所说的粉煤灰提取物的漂珠和微珠经烘干应达到含水量<2%,粒度筛选至水泥细度要求。
4、按照权利要求2所述的水泥,其特征是所说的膨胀剂为EA-L型和U型。