CN1094016A - 一种净水剂的生产方法 - Google Patents
一种净水剂的生产方法 Download PDFInfo
- Publication number
- CN1094016A CN1094016A CN 93107677 CN93107677A CN1094016A CN 1094016 A CN1094016 A CN 1094016A CN 93107677 CN93107677 CN 93107677 CN 93107677 A CN93107677 A CN 93107677A CN 1094016 A CN1094016 A CN 1094016A
- Authority
- CN
- China
- Prior art keywords
- water
- purification agent
- water purification
- production method
- waste water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
本发明涉及一种净水剂的生产方法,将铁屑、硫
酸加入线路板废液中,可得七水硫酸亚铁;硅砂加入
氢氧化钠在反射炉中焙烧,可得硅酸钠;将两者按一
定比例混合即可得到净水剂。本发明对印染废水、电
镀废水有较好的治理效果,处理后废水的透明度,水
中含铬达到排放标准,具有使用方便、制作简便、成本
低廉的特点。
Description
本发明涉及一种净水剂的生产方法,尤其是适用于印染废水、电镀废水的净水剂。
现有的净水剂是以聚铝、硫酸亚铁为主,前者因为不具有还原性,故使废水不能脱色,后者只能处理电镀废水,不能处理印染废水,且褪色率只有50%。
本发明的目的就是解决现有技术的不足,而提供一种处理印染废水、电镀废水效果好的净水剂。
本发明的生产方法如下:
①用铁屑、硫酸加入线路板废液中,加温至60~70℃,24小时后,即析出铜,用离心分离机使铜粉与硫酸亚铁分离出来,在溶液中的是硫酸亚铁,当温度冷却至室温时,即析出七水硫酸亚铁(FeSO4·7H2O)。
②把硅砂按比例与氢氧化钠混和好,放进生铁锅内在反射炉中焙烧,以免流失,温度用热电偶丝控制,连接自动温度计,温度达到650~700℃时,恒温30分钟,即可溶解,生成硅酸钠。
③将七水硫酸亚铁和硅酸钠按3∶1混和均匀,即得净水剂。
本发明对印染废水、电镀废水有较好的治理效果,处理后,废水的透明度,水中含铬达到排放标准,具有使用方便,制作简便,成本低廉的特点。
实施例:
取线路板腐蚀液10升(含铜量约10%)加浓硫酸1.54kg、铁屑0.88kg,加温至68℃,24小时后反应完全,析出铜粉1.0kg,分离铜粉后,把溶液冷却至25℃,可得七水硫酸亚铁4.28kg。称取硅砂(含量95%)1.0kg,加过量硫酸亚铁1.67kg,混和,放入生铁锅内,在反射炉中焙烧,加温至680℃时,恒温30分钟,即可得硅酸钠2.54kg。取七水硫酸亚铁4.28kg,加入1.43kg硅酸钠,混合均匀,得到5.71kg净水剂。
当处理印染废水时,在PH为9~10时,加入2‰的净水剂,对色度为300~400,稀释倍数法废水去除率大于90%,对COD为300~400mg/L的废水去除率大于90%,对浊度为200的废水去除率大于90%。
当处理电镀废水时,每升废水中加入2克的净水剂,将废水的PH值调至8~9,水质才能达到标准,透明度达90%以上,水中含铬离子达到排放标准。
Claims (1)
1、一种净水剂的生产方法,其特征在于:
①将铁屑、硫酸加入线路板废液,加温至60~70℃,24小时后,析出铜粉,先分离铜粉,把溶液冷至室温可得七水硫酸亚铁;
②将硅砂加入氢氧化纳中,在反射炉中加温至650~700℃,恒温30分钟,可得硅酸钠;
③将七水硫酸钠与硅酸钠按3∶1混后。