- gangue
- mould material
- retinal
- raw material
- attapulgite clay
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C04—CEMENTS; CONCRETE; ARTIFICIAL STONE; CERAMICS; REFRACTORIES
- C04B—LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE; CERAMICS; REFRACTORIES; TREATMENT OF NATURAL STONE
- C04B26/00—Compositions of mortars, concrete or artificial stone, containing only organic binders, e.g. polymer or resin concrete
- C04B26/02—Macromolecular compounds
- C04B26/22—Natural resins, e.g. rosin
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Ceramic Engineering (AREA)
- Materials Engineering (AREA)
- Structural Engineering (AREA)
- Organic Chemistry (AREA)
- Paper (AREA)
Abstract
本发明是一种用于模具成型的材料,包含添加剂和载体,配方中的原料按重量百分比组成分别是:0.5~6%凹凸棒粘土,10~35%石英砂,1~10%松香油,0~3%纸板纤维,0~2.5%煤矸石,5~20%石灰粉,10~20%浸泡液,30~60%防老剂,通过本方法制备的产品,除去存在的甲醛等致癌物质,在拥有较好的强度同时,不会对环境造成伤害。
Description
技术领域
本发明公开了一种用于模具成型的材料。
背景技术
模具成型材料是指低毒、低排放型,经过加工、合成等技术手段来控制有毒、有害物质的积聚和缓慢释放、因其毒性轻微、对人类健康不构成危险的装饰材料,现有的装饰砖块中,存在少量的甲醛等物质,会对人体和环境造成一定程度的伤害。
发明内容
针对上述现有技术存在的问题,本发明提供一种用于模具成型的材料,在拥有较好的强度同时,不会对环境造成伤害。
为了实现上述目的,本发明通过以下技术方案实现:一种用于模具成型的材料,配方中的原料按重量百分比组成分别是:0.5~6%凹凸棒粘土,10~35%石英砂,1~10%松香油, 0~3%纸板纤维,0~2.5%煤矸石,5~20%石灰粉,10~20%浸泡液,30~60%防老剂。
有益效果:通过本方法制备的产品,在拥有较好的强度同时,不会对环境造成伤害。
具体实施方式
实施例1
一种用于模具成型的材料,配方中的原料按重量百分比组成分别是:0.5%凹凸棒粘土,10%石英砂,1%松香油,1%纸板纤维,1%煤矸石,5%石灰粉,10%浸泡液,30%防老剂,此时砖块强度不足。
实施例2
一种用于模具成型的材料,配方中的原料按重量百分比组成分别是:6%凹凸棒粘土,35%石英砂,10%松香油,3%纸板纤维,2.5%煤矸石,20%石灰粉,20%浸泡液,60%防老剂,此时存在甲醛等物质。
实施例3
一种用于模具成型的材料,配方中的原料按重量百分比组成分别是:4%凹凸棒粘土,23%石英砂,5%松香油, 1.5%纸板纤维,1.25%煤矸石,13%石灰粉,15%浸泡液,45%防老剂,此时在拥有较好的强度同时,不会对环境造成伤害。
Claims (4)
1.一种用于模具成型的材料,包含添加剂和载体,其特征在于,配方中的原料按重量百分比组成分别是:0.5~6%凹凸棒粘土,10~35%石英砂,1~10%松香油,0~3%纸板纤维,0~2.5%煤矸石,5~20%石灰粉,10~20%浸泡液,30~60%防老剂。
2.根据权利要求1所述的用于模具成型的材料,其特征在于,配方中的原料按重量百分比组成分别是:0.5%凹凸棒粘土,10%石英砂,1%松香油,1%纸板纤维,1%煤矸石,5%石灰粉,10%浸泡液,30%防老剂。
3.根据权利要求1所述的用于模具成型的材料,其特征在于,配方中的原料按重量百分比组成分别是:6%凹凸棒粘土,35%石英砂,10%松香油,3%纸板纤维,2.5%煤矸石,20%石灰粉,20%浸泡液,60%防老剂。
4.根据权利要求1所述的用于模具成型的材料,其特征在于,配方中的原料按重量百分比组成分别是:4%凹凸棒粘土,23%石英砂,5%松香油,1.5%纸板纤维,1.25%煤矸石,13%石灰粉,15%浸泡液,45%防老剂。
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201811427027.3A CN109265074A (zh) | 2018-11-27 | 2018-11-27 | 一种用于模具成型的材料 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201811427027.3A CN109265074A (zh) | 2018-11-27 | 2018-11-27 | 一种用于模具成型的材料 |
Publications (1)
Publication Number | Publication Date |
---|---|
CN109265074A true CN109265074A (zh) | 2019-01-25 |
Family
ID=65186022
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201811427027.3A Pending CN109265074A (zh) | 2018-11-27 | 2018-11-27 | 一种用于模具成型的材料 |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN109265074A (zh) |
Citations (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4970246A (en) * | 1988-11-01 | 1990-11-13 | Coyne Cylinder Company | Acetylene storage vessel filler and method |
CN1048697A (zh) * | 1989-07-10 | 1991-01-23 | 抚顺辽宁发电厂科技开发服务处 | 粉煤灰浸泡砖的生产方法 |
JP2007269508A (ja) * | 2006-03-30 | 2007-10-18 | Ube Ind Ltd | 水硬性組成物 |
CN101805205A (zh) * | 2010-03-04 | 2010-08-18 | 乐山师范学院 | 用于石材保护的有机硅复配液及其施用方法 |
CN103387404A (zh) * | 2013-07-29 | 2013-11-13 | 北京超塑新技术有限公司 | 用于模具的材料、模具及制备模具方法 |
CN105728636A (zh) * | 2016-03-08 | 2016-07-06 | 安徽省大吕精机有限公司 | 一种耐高温模具及其制造方法 |
CN105819803A (zh) * | 2016-03-18 | 2016-08-03 | 安徽绿风环保节能材料有限公司 | 一种带有柠檬芳香气味的环保装饰砖块 |
CN105819738A (zh) * | 2016-03-08 | 2016-08-03 | 安徽省大吕精机有限公司 | 一种抗氧化模具及其制造方法 |
-
2018
- 2018-11-27 CN CN201811427027.3A patent/CN109265074A/zh active Pending
Patent Citations (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4970246A (en) * | 1988-11-01 | 1990-11-13 | Coyne Cylinder Company | Acetylene storage vessel filler and method |
CN1048697A (zh) * | 1989-07-10 | 1991-01-23 | 抚顺辽宁发电厂科技开发服务处 | 粉煤灰浸泡砖的生产方法 |
JP2007269508A (ja) * | 2006-03-30 | 2007-10-18 | Ube Ind Ltd | 水硬性組成物 |
CN101805205A (zh) * | 2010-03-04 | 2010-08-18 | 乐山师范学院 | 用于石材保护的有机硅复配液及其施用方法 |
CN103387404A (zh) * | 2013-07-29 | 2013-11-13 | 北京超塑新技术有限公司 | 用于模具的材料、模具及制备模具方法 |
CN105728636A (zh) * | 2016-03-08 | 2016-07-06 | 安徽省大吕精机有限公司 | 一种耐高温模具及其制造方法 |
CN105819738A (zh) * | 2016-03-08 | 2016-08-03 | 安徽省大吕精机有限公司 | 一种抗氧化模具及其制造方法 |
CN105819803A (zh) * | 2016-03-18 | 2016-08-03 | 安徽绿风环保节能材料有限公司 | 一种带有柠檬芳香气味的环保装饰砖块 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
MX2007010009A (es) | Preparacion de cuerpos moldeados de materiales de particulas finas a base de lignocelulosa. | |
TW200519106A (en) | Organic compounds | |
GEP20084323B (en) | Paving binders (variants) and manufacturing methods | |
TW200500428A (en) | Composition with non-newtonian behaviour | |
DE502007004582D1 (de) | Verwendung von ölhaltigen weichwachsen als hydrophobierungsmittel in holzwerkstoffen, holzwerkstoffe so hergestellt und verfahren zur einbringung von weichwachsen in die holzwerkstoffe | |
US20200115278A1 (en) | Method for manufacturing articles in the form of a slab or block with a hardening binder, and articles thus obtained | |
KR101747877B1 (ko) | 황토보드의 제조방법 및 이에 의하여 제조된 황토보드 | |
EP1155794A3 (en) | Hydraulically settable mixtures | |
CN109265074A (zh) | 一种用于模具成型的材料 | |
DE60213749D1 (de) | Verfahren und Anlage zum Herstellen keramischer Fliesen und Platten | |
EP3354631B1 (de) | Versatz zur herstellung eines ungeformten feuerfesten keramischen erzeugnisses und verfahren zur herstellung eines ungeformten feuerfesten keramischen erzeugnisses | |
WO2006084670A3 (de) | Bindemittel auf basis von calciumaluminat | |
PL1631403T3 (pl) | Sposób wytwarzania masy rdzeniowej i/lub formierskiej do celów odlewniczych | |
CN102515676B (zh) | 环保艺术砖配方及制作方法 | |
CN104341138A (zh) | 利用废弃瓷砂土制作仿陶瓷器的坯料、釉料配方及制作工艺 | |
MX2021003151A (es) | Acelerador para composiciones aglutinantes minerales. | |
RU2558571C1 (ru) | Керамическая масса | |
KR100908606B1 (ko) | 어구용ㆍ낚시용 추 및 그 제조방법 | |
RU2481307C1 (ru) | Керамическая масса | |
CN107285754A (zh) | 一种能增强人体柔韧性的陶瓷制品及其制备方法 | |
RU2477715C1 (ru) | Керамическая масса для производства пуговиц | |
CN108840715A (zh) | 一种柔性装饰轻质墙材 | |
RU2379265C1 (ru) | Сырьевая смесь для изготовления легкого бетона | |
CN105859235A (zh) | 泥雕刻材料及其制备方法 | |
RU2007104281A (ru) | Сырьевая смесь |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PB01 | Publication | ||
PB01 | Publication | ||
SE01 | Entry into force of request for substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
WD01 | Invention patent application deemed withdrawn after publication |
Application publication date: 20190125 |
|
WD01 | Invention patent application deemed withdrawn after publication |