CN109203527A - A kind of preparation method of corrosion-resistant water pipe - Google Patents

A kind of preparation method of corrosion-resistant water pipe Download PDF

Info

Publication number
CN109203527A
CN109203527A CN201811230956.5A CN201811230956A CN109203527A CN 109203527 A CN109203527 A CN 109203527A CN 201811230956 A CN201811230956 A CN 201811230956A CN 109203527 A CN109203527 A CN 109203527A
Authority
CN
China
Prior art keywords
water pipe
heating
corrosion
preparation
molding
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811230956.5A
Other languages
Chinese (zh)
Inventor
陈建定
韩国平
杨学青
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Qingrun Precision Technology Co Ltd
Original Assignee
Anhui Qingrun Precision Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Qingrun Precision Technology Co Ltd filed Critical Anhui Qingrun Precision Technology Co Ltd
Priority to CN201811230956.5A priority Critical patent/CN109203527A/en
Publication of CN109203527A publication Critical patent/CN109203527A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of preparation methods of corrosion-resistant water pipe, and specific step is as follows for the preparation method of the corrosion-resistant water pipe: S1: coagulation, S2: stirring, S3: fill mould, S4: heating, S5: depanning, S6: polishing, S7: S8: coating is collected.The present invention passes through addition waterproof, anti-oxidation and curing materials, water pipe is set to be less prone to slight crack, it causes to corrode in the inside that wet air will not be made to enter water pipe, influence the use of water pipe, and, waterproof and anti-oxidation materials are added with by water pipe itself, the outer surface of water pipe will not be made by the damage of a little, it just will affect the use of water pipe, by smearing one layer of anti-oxidation and waterproof material in the outer surface of water pipe, making the outer surface of water pipe more has rotproofness, the present invention is also by way of heating, to waterproof material, anti-oxidation materials and curing materials solidify faster, make coagulation result more preferably, it is easy to operate, it is convenient.

Description

A kind of preparation method of corrosion-resistant water pipe
Technical field
The present invention relates to the preparation method technical field of corrosion water pipe, specially a kind of preparation methods of corrosion-resistant water pipe.
Background technique
Water pipe of today is all to be imbedded in underground, but since underground air humidity is big, moisture is big, is easy to keep water pipe long-term Corroded in underground, influences the service life of water pipe, and traditional water pipe cracky, cannot use well, so, I Propose the preparation method of corrosion-resistant water pipe a kind of, to solve the above problems.
Summary of the invention
The purpose of the present invention is to provide a kind of preparation methods of corrosion-resistant water pipe, to solve to propose in above-mentioned background technique The problem of.
To achieve the above object, the invention provides the following technical scheme: a kind of preparation method of corrosion-resistant water pipe, specific to walk It is rapid as follows:
S1, coagulation: thickener, waterproofing agent, antioxidant, polyester and fixing agent are added to according to the ratio of 1:3:2:2:3 In agitator tank, mixed raw material is obtained;
S2, stirring: the mixed raw material in S1 being placed in agitator tank and is stirred, and the revolving speed of agitator tank is set as 500r/min, is stirred Mixing the time is set as 10min, every 5min during stirring, adds 100ml water, addition number is 2-3 times;
S3, it fills mould: the mixed raw material being stirred being taken out, is encased in water pipe mold, clean in water pipe mold, free from admixture;
S4, heating: the water pipe mold equipped with mixed raw material is passed into heating machine, and heating process is set as being segmented, sliding The time of heating, every section of heating is set as 10min, and the heating temperature of heating machine is set as 40 DEG C -50 DEG C, obtains molding water Pipe;
S5, depanning: by the water pipe mold cold-zone heated to room temperature, then to molding water pipe depanning, when depanning, by water pipe mold Outer layer open, is divided into two, extraction molding water pipe;
S6, polishing: the outer surface of the molding water pipe in S5 is polished with sanding machine, by protrusion part polish flat, and at The both ends of type water pipe polish flat;
S7, coating: waterproofing agent and antioxidant are smeared in the outer surface of the molding water pipe after having polished, and place at dry and ventilated It dries, obtains finished product;
S8, collection: finally by the finished product in S7, putting on one layer of the modern designs of plastics, is placed on warehouse collection, and molding water pipe is placed on placement On frame.
Preferably, waterproofing agent in the S1 and S7 select one of waterproofing agent of organosilicon, nanometer infiltration waterproofing agent or It is a variety of.
Preferably, the antioxidant in the S1 and S7 selects alkenyl bis-phenol, alkyl phenol, di-tert-butyl p-cresol, front three One of base triphen is a variety of.
Preferably, the thickener in the S1 selects xanthan gum, gelatin, hydroxyalkyl starch, methylcellulose, cellulose ether One of or it is a variety of.
Preferably, the curing agent in the S1 selects one of four ammonia of triethylene, m-xylene diamine, diamino cyclohexane Or it is a variety of.
Compared with prior art, the beneficial effects of the present invention are: the present invention passes through addition waterproof, anti-oxidation and solidification material Material, makes water pipe be less prone to slight crack, and the inside that wet air will not be made to enter water pipe causes to corrode, and influences the use of water pipe, Moreover, being added with waterproof and anti-oxidation materials by water pipe itself, the outer surface of water pipe will not be made by the damage of a little, just The use that will affect water pipe makes the outer surface of water pipe by smearing one layer of anti-oxidation and waterproof material in the outer surface of water pipe More there is rotproofness, the present invention is faster to waterproof material, anti-oxidation materials and curing materials also by way of heating Solidification, makes coagulation result more preferably, and the present invention can prevent the moisture water leaking-in in soil by smearing waterproof material in extexine In pipe, by the way that waterproofing agent is added in water pipe, can water exudation water pipe in anti-antipriming pipe outside, influence to use, operation letter It is single, it is convenient.
Specific embodiment
In order to make the objectives, technical solutions, and advantages of the present invention clearer, below in conjunction with specific embodiment, to this Invention is further elaborated.It should be appreciated that the specific embodiments described herein are merely illustrative of the present invention, not For limiting the present invention.
A kind of preparation method of corrosion-resistant water pipe, the specific steps are as follows:
S1, coagulation: thickener, waterproofing agent, antioxidant, polyester and fixing agent are added to according to the ratio of 1:3:2:2:3 In agitator tank, mixed raw material is obtained;
S2, stirring: the mixed raw material in S1 being placed in agitator tank and is stirred, and the revolving speed of agitator tank is set as 500r/min, is stirred Mixing the time is set as 10min, every 5min during stirring, adds 100ml water, addition number is 2-3 times;
S3, it fills mould: the mixed raw material being stirred being taken out, is encased in water pipe mold, clean in water pipe mold, free from admixture;
S4, heating: the water pipe mold equipped with mixed raw material is passed into heating machine, and heating process is set as being segmented, sliding The time of heating, every section of heating is set as 10min, and the heating temperature of heating machine is set as 40 DEG C -50 DEG C, obtains molding water Pipe;
S5, depanning: by the water pipe mold cold-zone heated to room temperature, then to molding water pipe depanning, when depanning, by water pipe mold Outer layer open, is divided into two, extraction molding water pipe;
S6, polishing: the outer surface of the molding water pipe in S5 is polished with sanding machine, by protrusion part polish flat, and at The both ends of type water pipe polish flat;
S7, coating: waterproofing agent and antioxidant are smeared in the outer surface of the molding water pipe after having polished, and place at dry and ventilated It dries, obtains finished product;
S8, collection: finally by the finished product in S7, putting on one layer of the modern designs of plastics, is placed on warehouse collection, and molding water pipe is placed on placement On frame.
Specifically, waterproofing agent in the S1 and S7 select one of waterproofing agent of organosilicon, nanometer infiltration waterproofing agent or It is a variety of.
Specifically, the antioxidant in the S1 and S7 selects alkenyl bis-phenol, alkyl phenol, di-tert-butyl p-cresol, front three One of base triphen is a variety of.
Specifically, the thickener in the S1 selects xanthan gum, gelatin, hydroxyalkyl starch, methylcellulose, cellulose ether One of or it is a variety of.
Specifically, the curing agent in the S1 selects one of four ammonia of triethylene, m-xylene diamine, diamino cyclohexane Or it is a variety of.
The present invention makes water pipe be less prone to slight crack by addition waterproof, anti-oxidation and curing materials, will not make moist sky The inside that gas enters water pipe causes to corrode, and influences the use of water pipe, moreover, being added with waterproof and anti-oxidation material by water pipe itself Material, will not make the outer surface of water pipe by the damage of a little, just will affect the use of water pipe, by applying in the outer surface of water pipe One layer of anti-oxidation and waterproof material is smeared, makes the outer surface of water pipe that more there is rotproofness, the present invention also passes through the side of heating Formula solidifies waterproof material, anti-oxidation materials and curing materials faster, makes coagulation result more preferably, and the present invention can be effective Corrosion reaction occurs for anti-antipriming pipe, keeps it longer using the time, easy to operate, convenient.
The foregoing is only a preferred embodiment of the present invention, but scope of protection of the present invention is not limited thereto, Anyone skilled in the art in the technical scope disclosed by the present invention, according to the technique and scheme of the present invention and its Inventive concept is subject to equivalent substitution or change, should be covered by the protection scope of the present invention.

Claims (5)

1. a kind of preparation method of corrosion-resistant water pipe, which is characterized in that specific step is as follows:
S1, coagulation: thickener, waterproofing agent, antioxidant, polyester and fixing agent are added to according to the ratio of 1:3:2:2:3 In agitator tank, mixed raw material is obtained;
S2, stirring: the mixed raw material in S1 being placed in agitator tank and is stirred, and the revolving speed of agitator tank is set as 500r/min, is stirred Mixing the time is set as 10min, every 5min during stirring, adds 100ml water, addition number is 2-3 times;
S3, it fills mould: the mixed raw material being stirred being taken out, is encased in water pipe mold, clean in water pipe mold, free from admixture;
S4, heating: the water pipe mold equipped with mixed raw material is passed into heating machine, and heating process is set as being segmented, sliding The time of heating, every section of heating is set as 10min, and the heating temperature of heating machine is set as 40 DEG C -50 DEG C, obtains molding water Pipe;
S5, depanning: by the water pipe mold cold-zone heated to room temperature, then to molding water pipe depanning, when depanning, by water pipe mold Outer layer open, is divided into two, extraction molding water pipe;
S6, polishing: the outer surface of the molding water pipe in S5 is polished with sanding machine, by protrusion part polish flat, and at The both ends of type water pipe polish flat;
S7, coating: waterproofing agent and antioxidant are smeared in the outer surface of the molding water pipe after having polished, and place at dry and ventilated It dries, obtains finished product;
S8, collection: finally by the finished product in S7, putting on one layer of the modern designs of plastics, is placed on warehouse collection, and molding water pipe is placed on placement On frame.
2. a kind of preparation method of corrosion-resistant water pipe according to claim 1, it is characterised in that: anti-in the S1 and S7 Aqua selects one of waterproofing agent of organosilicon, nanometer infiltration waterproofing agent or a variety of.
3. a kind of preparation method of corrosion-resistant water pipe according to claim 1, it is characterised in that: anti-in the S1 and S7 Oxidant selects one of alkenyl bis-phenol, alkyl phenol, di-tert-butyl p-cresol, trimethyl triphen or a variety of.
4. a kind of preparation method of corrosion-resistant water pipe according to claim 1, it is characterised in that: the thickener in the S1 Select one of xanthan gum, gelatin, hydroxyalkyl starch, methylcellulose, cellulose ether or a variety of.
5. a kind of preparation method of corrosion-resistant water pipe according to claim 1, it is characterised in that: the curing agent in the S1 Select one of four ammonia of triethylene, m-xylene diamine, diamino cyclohexane or a variety of.
CN201811230956.5A 2018-10-22 2018-10-22 A kind of preparation method of corrosion-resistant water pipe Pending CN109203527A (en)