CN109198811A - Method for manufacturing waterproof zipper and product thereof - Google Patents
Method for manufacturing waterproof zipper and product thereof Download PDFInfo
- Publication number
- CN109198811A CN109198811A CN201810490020.XA CN201810490020A CN109198811A CN 109198811 A CN109198811 A CN 109198811A CN 201810490020 A CN201810490020 A CN 201810490020A CN 109198811 A CN109198811 A CN 109198811A
- Authority
- CN
- China
- Prior art keywords
- zipper
- melt adhesive
- hot melt
- waterproof
- slide fastener
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
A method for manufacturing water-proof zipper includes such steps as providing a piece of release paper, which has a bright or foggy surface, or pattern, or trademark, or character. Then, a liquid hot melt adhesive is coated on the release side, and a heating procedure is carried out on the liquid hot melt adhesive. And continuously providing a zipper, and carrying out a hot rolling procedure on the zipper, the release paper and the liquid hot melt adhesive, wherein one side of the zipper tape without the zipper teeth is combined with the liquid hot melt adhesive and the release paper in a hot rolling way, and the liquid hot melt adhesive forms a waterproof layer. Finally, the release paper is peeled off to form a bright surface, a matte surface, a pattern, a trademark or characters on the surface of the waterproof layer contacted with the release side, so as to finish the product.
Description
Technical field
The present invention relates to a kind of method for producing slide fastener and products thereof, espespecially a kind of to produce zipper using liquid hot melt adhesive
Waterproof slide fastener manufacturing method and products thereof.
Background technique
It as shown in Figs.1 and 2, is for existing Water-proof zipper structure 10 and its manufacturing equipment 11, the waterproof slide fastener knot
Structure 10 includes that a zipper 100, one is the waterproof layer and a mucigel 102 that solid-state hot melt adhesive 106 is formed.The zipper 100 packet
103 centre of zipper strip is set containing a zipper strip 103 and a row and is located at the zipper teeth 104 of 103 side of zipper strip,
Wherein it is located at the same side of the zipper strip 103 after the zipper teeth 104 engagement.The mucigel 102 is that setting does not have in the zipper strip 103
Have between the side of the zipper teeth 104 and the solid-state hot melt adhesive 106.
The manufacturing equipment 11 includes an apparatus for coating 110, a hot rolling device 111 and a fair lead 112.Thing
One strippable paper 105 for being equipped with the solid-state hot melt adhesive 106 is first provided, is hereafter coated with the mucigel 102 via the apparatus for coating 110
In the solid-state hot melt adhesive 106.Pass through the hot rolling device 111 again for the zipper 100, the mucigel 102, the solid-state hot melt adhesive
106, the strippable paper 105, which carries out heat rolling, binds it mutually, and wherein the mucigel 102 is that setting does not have in the zipper strip 103
Between the side of the zipper teeth 104 and the solid-state hot melt adhesive 106.Finally the strippable paper 105 is removed again to form waterproof drawing
Chain structure 10, and the Water-proof zipper structure 10 is furled by fair lead 112.
Since the conjugation between the solid-state hot melt adhesive 106 and the zipper strip 103 is bad, lead to the solid-state hot melt adhesive 106
It is not easy gluing between the zipper strip 103, it is therefore necessary to which setting should between the solid-state hot melt adhesive 106 and the zipper strip 103
Mucigel 102 can just make the solid-state hot melt adhesive 106 is preferably glutinous to be located on the zipper strip 103.
However after the mucigel 102 cooling and solidifying, the Water-proof zipper structure 10 can be made harder.Once the waterproof is drawn
Chain structure 10 is assembled in such as clothes, housing dress ornament, and user can reduce comfort after putting on.
In addition, the existing Water-proof zipper structure 10 is also because only have a little colloid osmotic after the solid-state hot melt adhesive 106 heating
Into the fibr tissue of the zipper strip 103, cause the waterproof effect of the existing Water-proof zipper structure 10 bad.In this regard, existing anti-
Water zipper has the necessity improved again.
Summary of the invention
It is an object of the invention to propose that it is good comfortable with relatively softening that a kind of utilization liquid hot melt adhesive produces waterproof effect
Waterproof slide fastener manufacturing method and products thereof.
According to above-mentioned purpose, the present invention proposes a kind of waterproof slide fastener manufacturing method, and it includes have following steps:
Step A: providing a strippable paper, the strippable paper upward from shape side, and be formed with bright face or cloudy surface from shape side, or
It is suppressed with the figure or decorative pattern or trade mark or text of dent or convex epirelief;
Step B: by a liquid hot melt adhesive be applied to the strippable paper from shape side;
Step C: a heating schedule is carried out to the liquid hot melt adhesive, activates the liquid hot melt adhesive;
Step D: providing a zipper, which is espespecially the zipper for being located at zipper strip the same side after zipper tooth engagement;
Step E: the zipper, the strippable paper and the liquid hot melt adhesive are subjected to a heat rolling program, which is equipped with should
The side of zipper teeth upward, the zipper strip not the zipper teeth side downwards and with the liquid hot melt adhesive heat rolling combined, and
The liquid hot melt adhesive is formed as a waterproof layer;And
Step F: the strippable paper is removed, make the waterproof layer and surface from shape side contacts be formed with bright face or cloudy surface or
Figure or decorative pattern or trade mark or text.
Further, which is set as nylon tooth or metal-toothed or plastic-steel tooth.
Further, which is set as low temperature liquid polyurethane (Polyurethane, PU) glue.
Further, which is provided with six heater boxes, and heating temperature is set to 55 DEG C, 55 DEG C, 60 DEG C, 85
℃、60℃、55℃。
Further, the heat rolling program among step E is rolled by one first hot rolling device and one second heat
Pressure device carries out hot rolling, and first hot rolling device and second heat to the zipper, the strippable paper and the liquid hot melt adhesive
The zipper and the strippable paper will be first overturn between rolling device, make side of the zipper strip equipped with the zipper teeth downward, the zipper
Band without the zipper teeth side and the strippable paper, the waterproof layer upward.
Further, also include a step G after step F: one being carried out to the zipper and dials aqua program, makes the drawing
Chain increases waterproof effect.
Further, this in step G dial aqua program be to provide a leaching dryingagent device and one spray dryingagent dress
It sets and a water repellent oxidant layer is added to the zipper.
It further, also include a step H after step G: in the waterproof layer axial direction formed to the liquid hot melt adhesive
A cutting process is carried out at centre, and cut place is in alignment at the bridle joint of zipper teeth.
Furthermore the present invention proposes a kind of waterproof slide fastener, and it includes the waterproof layers and one that have one to be formed by liquid hot melt adhesive to draw
Chain.The zipper includes a zipper strip and a row is connected to the zipper strip side and is located at the zipper of the zipper strip axial direction centre
Tooth, wherein after the zipper tooth engagement be located at the zipper strip the same side, and the zipper strip not the zipper teeth side be equipped with should
Waterproof layer, the surface of the waterproof layer via be formed with after the rolling of strippable paper heat from the bright face on the strippable paper surface or mist
Face or figure or decorative pattern or trade mark or text.
Further, the waterproof layer which forms is set as low temperature liquid polyurethane (Polyurethane, PU)
Glue.
Further, which is set as nylon tooth or metal-toothed or plastic-steel tooth.
It further, also include the water repellent oxidant layer of the cladding zipper, the water repellent oxidant layer is for increasing the waterproof of the zipper
Effect.
Further, the waterproof layer axial direction centre which forms is equipped with a cut place, and the cut place pair
At the bridle joint of the quasi- zipper teeth.
Present invention is characterized in that
1. due to there is the more colloid readily permeable fibr tissue to the zipper strip when liquid hot melt adhesive activated by heat
In, the waterproof layer for enabling the liquid hot melt adhesive to be formed promotes gluing effect and waterproof effect between the zipper strip.
2. user puts on configured with the product in addition, making the product softer due to the unused mucigel of the present invention
It can be relatively comfortable when dress ornament.
Detailed description of the invention
Fig. 1: for the stereogram exploded view of existing Water-proof zipper structure.
Fig. 2: for the schematic diagram of existing Water-proof zipper structure manufacturing equipment.
Fig. 3: for the flow chart (one) of waterproof slide fastener manufacturing method of the present invention.
Fig. 4: for the equipment schematic diagram (one) of waterproof slide fastener manufacturing method of the present invention.
Fig. 5: for the stereogram exploded view of waterproof slide fastener product of the present invention.
Fig. 6: for the three-dimensional combination figure of waterproof slide fastener product of the present invention.
Fig. 7: for the flow chart (two) of waterproof slide fastener manufacturing method of the present invention.
Fig. 8: for the flow chart (three) of waterproof slide fastener manufacturing method of the present invention.
Fig. 9: for the equipment schematic diagram (two) of waterproof slide fastener manufacturing method of the present invention.
Figure 10: for the plan view of waterproof slide fastener product of the present invention.
Wherein appended drawing reference are as follows:
10 zipper 100 of Water-proof zipper structure
102 zipper strip 103 of mucigel
104 strippable paper 105 of zipper teeth
106 manufacturing equipment 11 of solid-state hot melt adhesive
110 hot rolling device 111 of apparatus for coating
Fair lead 112
﹝ this Fa Ming ﹞
2 product 3 of waterproof slide fastener manufacturing method
Strippable paper 30 is from shape side 300
31 surface 310 of liquid hot melt adhesive
32 zipper teeth 320 of zipper
321 water repellent oxidant layer 33 of zipper strip
34 waterproof slide fastener manufacturing equipment 4 of cut place
Rotate 40 apparatus for coating 41 of frame body
42 heater box 420 of heating device
First fair lead, 43 first hot rolling device 44
Second hot rolling device 45 soaks dryingagent device 46
Spray 47 cutter device 48 of dryingagent device
480 second fair lead 49 of blade
Step A, B, C, D, E, F, G, H
Specific embodiment
It please refers to shown in Fig. 3, Fig. 5, Fig. 6 and Figure 10, is a kind of waterproof slide fastener manufacturing method 2 of the invention and products thereof 3,
Wherein the waterproof slide fastener manufacturing method 2 includes following steps, and together refering to waterproof slide fastener manufacturing equipment 4 shown in Fig. 4:
Step A: providing a strippable paper 30, the strippable paper 30 upward from shape side 300, and should be from being formed on shape side 300
Bright face or cloudy surface, or it is suppressed with the figure or decorative pattern or trade mark or text of dent or convex epirelief;The strippable paper 30 refers in rolls
Strippable paper, and the strippable paper 30 setting one rotation frame body 40 on, one end of the coiled strippable paper 30 is drawn in advance
On one first fair lead 43, can persistently coiled be somebody's turn to do by drawing the strippable paper 30 just thereafter through first fair lead 43
Strippable paper 30 is processed.
Step B: by an apparatus for coating 41 by a liquid hot melt adhesive 31 be applied to the strippable paper 30 from shape side 300;
Step C: a heating schedule is carried out to the liquid hot melt adhesive 31 by a heating device 42, makes the liquid hot melt adhesive 31
Activation;
Step D: providing a zipper 32, which is espespecially to be located at 321 the same side of zipper strip after zipper teeth 320 engages
Zipper;
Step E: the zipper 32, the strippable paper 30 and the liquid hot melt adhesive 31 are subjected to a heat rolling program, the zipper strip
321 be equipped with the zipper teeth 320 sides upward, the zipper strip 321 not the zipper teeth 320 side downwards and with the liquid heat
31 heat rolling of melten gel combines, and the liquid hot melt adhesive 31 is formed as a waterproof layer;And
Step F: the strippable paper 30 is removed, and be formed with the waterproof layer from the surface 310 that shape side 300 contacts with this bright
Face or cloudy surface or figure or decorative pattern or trade mark or text.Hereafter by the strippable paper 30 and the production of the strippable paper 30 is removed
The retracting of product 3 is collected in favor of subsequent processing.
By include in the product 3 made by step A to step F the liquid hot melt adhesive 31 formed the waterproof layer,
And the zipper 32.The zipper 32 includes a zipper strip 321 and a row is connected to 321 side of zipper strip and is located at the zipper
Zipper teeth 320 with 321 axial centres is wherein located at the same side of the zipper strip 321 after the zipper teeth 320 engagement, and should
The side of the not no zipper teeth 320 of zipper strip 321 is equipped with the waterproof layer, the surface 310 of the waterproof layer via with 30 heat of strippable paper
It is formed with after rolling from the bright face on 30 surface of strippable paper or cloudy surface or figure or decorative pattern or trade mark or text.?
In embodiment of this case, which is set as nylon tooth or metal-toothed or plastic-steel tooth, and but not limited to this.
It illustrates, first by the bright face of client demand or cloudy surface or figure or decorative pattern or trade mark or text etc.
Pattern this from being formed on shape side 300.Hereafter the strippable paper 30 is arranged with the liquid hot melt adhesive 31 to the zipper strip 321 does not have
The side of the zipper teeth 320 connects and allows the liquid hot melt adhesive 31 liquid hot melt adhesive 31 to activate by the heating schedule, and
The strippable paper 30 is removed after waiting the liquid hot melt adhesive 31 cooling, allows the liquid hot melt adhesive 31 and the table that contacted from shape side 300
Face 310 is formed with the patterns such as bright face or cloudy surface or figure or decorative pattern or trade mark or text.
On continuous, due to there is more colloid readily permeable to the zipper strip 321 when 31 activated by heat of liquid hot melt adhesive
In fibr tissue, the waterproof layer for enabling the liquid hot melt adhesive 31 to be formed promoted gluing effect between the zipper strip 321 with
Waterproof effect.In addition, also keeping the product 3 softer because of the unused mucigel of the present invention, user is put on configured with the product 3
It can be relatively comfortable when dress ornament.
It please read shown in Fig. 4 and Figure 10 again, the heat rolling program among step E is by one first hot rolling device 44
Hot rolling carried out to the zipper 32, the strippable paper 30 and the liquid hot melt adhesive 31 with one second hot rolling device 45, and this first
The zipper 32 and the strippable paper 30 will be first overturn between hot rolling device 44 and second hot rolling device 45, make the zipper strip
321 are equipped with the sides of the zipper teeth 320 downward, the zipper strip 321 not the side of the zipper teeth 320 and the strippable paper 30, should
Waterproof layer is upward.Wherein, when pasting in order to avoid the liquid hot melt adhesive 31 to the zipper strip 321 generate displacement and have gauffer or
Unsturdy defect, hereby sequentially by first hot rolling device 44, roll-over procedure and second hot rolling device 45 to this
Liquid hot melt adhesive 31 and the zipper 32 carry out heat twice and roll.
Referring again to shown in Fig. 7, Fig. 9 and Figure 10, also includes a step G after step F: one is carried out to the zipper 32
Aqua program is dialed, increases the zipper 32 by waterproof effect.This in step G dials aqua program and is to provide a leaching dryingagent
Device 46 and a spray dryingagent device 47 are to the zipper 32 plus a water repellent oxidant layer 33.Wherein, it is compareed in the product 3 in step G,
The product 3 also includes the water repellent oxidant layer 33 of the cladding zipper 32, which imitates for increasing the waterproof of the zipper 32
Fruit.
It please refers to shown in Fig. 8 to Figure 10, also includes a step H after step G: by a cutter device 48 to the liquid
The waterproof layer axial direction centre that state hot melt adhesive 31 is formed carries out a cutting process, and cut place 34 is in alignment with the zipper teeth 320
At bridle joint, the product 3 is towed thereafter through one second fair lead 49 and furls collection.Due to before carrying out the cutting process
It has first passed through that the roll-over procedure overturns the zipper 32 and the liquid hot melt adhesive 31 makes the zipper strip 321 upward, therefore has carried out
When the cutting process, it can facilitate and the zipper strip 321 is cut with the cutter device 48 directed downwardly of blade 480.Wherein, it walks
Rapid H is compareed in the product 3, and the waterproof layer axial direction centre which forms is equipped with the cut place 34, and should
Cut place 34 is aligned at the bridle joint of each zipper teeth 320.
Further, it please read shown in Fig. 4 and Fig. 9 again, in embodiment of this case, when the liquid hot melt adhesive 31 is set as Low Temperature Liquid
When state polyurethane (Polyurethane, PU) glue, which is provided with six heater boxes 420, and heating temperature is set respectively
It is 55 DEG C, 55 DEG C, 60 DEG C, 85 DEG C, 60 DEG C and 55 DEG C.In order to avoid heating temperature significantly changes suddenly and influences activation knot
Fruit, the present invention especially heat the liquid hot melt adhesive 31 using the progressive heating temperature slowly activated.
In conclusion present invention is characterized in that
1. due to there is the more colloid readily permeable fiber to the zipper strip 321 when 31 activated by heat of liquid hot melt adhesive
In tissue, the waterproof layer for enabling the liquid hot melt adhesive 31 to be formed promotes gluing effect and waterproof between the zipper strip 321
Effect.
2. user puts on configured with the product 3 in addition, keeping the product 3 softer due to the unused mucigel of the present invention
It can be relatively comfortable when dress ornament.
Claims (13)
1. a kind of waterproof slide fastener manufacturing method, which is characterized in that the waterproof slide fastener manufacturing method includes following steps:
Step A: providing a strippable paper, the strippable paper upward from shape side, and be formed with bright face or cloudy surface from shape side, or compacting
There are the figure or decorative pattern or trade mark or text of dent or convex epirelief;
Step B: by a liquid hot melt adhesive be applied to the strippable paper from shape side;
Step C: a heating schedule is carried out to the liquid hot melt adhesive, activates the liquid hot melt adhesive;
Step D: providing a zipper, which is espespecially the zipper for being located at zipper strip the same side after zipper tooth engagement;
Step E: the zipper, the strippable paper and the liquid hot melt adhesive are subjected to a heat rolling program, which is equipped with the zipper
Upward, the side of the not no zipper teeth of the zipper strip is combined downwards and with liquid hot melt adhesive heat rolling, and the liquid for the side of tooth
State hot melt adhesive is formed as a waterproof layer;And
Step F: the strippable paper is removed, and the surface for making the waterproof layer and being somebody's turn to do from shape side contacts is formed with bright face or cloudy surface or figure
Shape or decorative pattern or trade mark or text.
2. waterproof slide fastener manufacturing method according to claim 1, which is characterized in that the zipper teeth is set as nylon tooth or gold
Belong to tooth or plastic-steel tooth.
3. waterproof slide fastener manufacturing method according to claim 1, which is characterized in that the liquid hot melt adhesive is set as low temperature liquid
Polyurethane (Polyurethane, PU) glue.
4. waterproof slide fastener manufacturing method according to claim 3, which is characterized in that the heating schedule is provided with six heating
Case, heating temperature are set to 55 DEG C, 55 DEG C, 60 DEG C, 85 DEG C, 60 DEG C, 55 DEG C.
5. waterproof slide fastener manufacturing method according to claim 1, which is characterized in that the heat among step E rolls journey
Sequence is to be carried out by one first hot rolling device and one second hot rolling device to the zipper, the strippable paper and the liquid hot melt adhesive
Heat rolling, and the zipper and the strippable paper are first overturn between first hot rolling device and second hot rolling device, make the drawing
Chain belt is equipped with the side of the zipper teeth downward, and the side of the zipper teeth and the strippable paper, the waterproof layer be not upward for the zipper strip.
6. waterproof slide fastener manufacturing method according to claim 5, which is characterized in that after the step F also include a step
Rapid G: one is carried out to the zipper and dials aqua program, increases the zipper by waterproof effect.
7. waterproof slide fastener manufacturing method according to claim 6, which is characterized in that this in step G dials aqua journey
Sequence is to provide a leaching dryingagent device and a spray dryingagent device adds a water repellent oxidant layer to the zipper.
8. waterproof slide fastener manufacturing method according to claim 6, which is characterized in that after the step G also include a step
Rapid H: a cutting process is carried out to the waterproof layer axial direction centre that the liquid hot melt adhesive is formed, and cut place is in alignment with zipper teeth
Bridle joint at.
9. a kind of waterproof slide fastener, which is characterized in that the waterproof slide fastener includes:
One waterproof layer, the waterproof layer are formed by liquid hot melt adhesive;And
One zipper, which includes a zipper strip and a row is connected to the zipper strip side and is located at the axial center of the zipper strip
The zipper teeth at place, wherein after the zipper tooth engagement be located at the zipper strip the same side, and the zipper strip not the zipper teeth one
Side is equipped with the waterproof layer, the surface of the waterproof layer via be formed with after the rolling of strippable paper heat from the bright of the strippable paper surface
Face or cloudy surface or figure or decorative pattern or trade mark or text.
10. product according to claim 9, which is characterized in that the zipper teeth is set as nylon tooth or metal-toothed or plastic-steel
Tooth.
11. product according to claim 9, which is characterized in that the liquid hot melt adhesive is set as low temperature liquid polyurethane
(Polyurethane, PU) glue.
12. product according to claim 9, which is characterized in that also include the water repellent oxidant layer of the cladding zipper, this group
Aqua layer is for increasing the waterproof effect of the zipper.
13. product according to claim 12, which is characterized in that the axial center of the waterproof layer that the liquid hot melt adhesive is formed
Place is equipped with a cut place, and the cut place is aligned at the bridle joint of the zipper teeth.