CN109176785A - A kind of wood skin dyeing of reserve flesh side muscle - Google Patents
A kind of wood skin dyeing of reserve flesh side muscle Download PDFInfo
- Publication number
- CN109176785A CN109176785A CN201810998800.5A CN201810998800A CN109176785A CN 109176785 A CN109176785 A CN 109176785A CN 201810998800 A CN201810998800 A CN 201810998800A CN 109176785 A CN109176785 A CN 109176785A
- Authority
- CN
- China
- Prior art keywords
- wood skin
- reserve
- dyeing
- wood
- side muscle
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to wood skin staining technique fields, and disclose a kind of wood skin dyeing of reserve flesh side muscle, comprising the following steps: sorting: the trees kind that fast growth, morning of becoming a useful person, the period of felling in turn are short are selected, to reduce cost;Log is into after factory, and first, in accordance with required length cutting into lengths, then when cuing open juggle processed, using the cutting method of quarter sawing, i.e., the annual ring of vertical tangential log produces the wood skin that straight grain is presented, and reserve flesh side muscle;By the manual block pattern row pattern of the wood skin being cut into hanging basket.The wood skin dyeing of the reserve flesh side muscle, the texture and color of various rare precious timbers can be copied, meet people to rare rare timber like and demand, and by the dyeing wood skin after processing, surface is smooth, there is no worm channel, white edge etc., not only color more horn of plenty, but also can be very good to meet and like in the requirement in different finishing places and the vast respective texture of people of choosing.
Description
Technical field
The present invention relates to wood skin staining technique field, specially a kind of wood skin dyeing of reserve flesh side muscle.
Background technique
Wood skin and its faced deorative industry are started in the fifties in last century, through semicentennial development, have been equipped with comparable
Scale, especially in the latest 20 years, as China's furniture manufacturing industry and the great-jump-forward of decorations industry increase, development is more
It is to advance by leaps and bounds, has emerged in large numbers a large amount of industry expert, natural veneer is to be formed completely with log slicing, without any people
Work modification, remains natural texture and texture, and raw material are all from pure natural, and grain can not be changed, and have unique
Property, more naturally beautiful property, and have the characteristics that indeformable, not warpage, but natural veneer also has its defect, such as wood
Mineral line, fast knot, the slip-knot in epidermis face, worm channel, white edge etc., these are all the distinctive features of natural veneer, in addition, natural wood
Color of the leather lathe work reason naturally, but it is difficult harmonious, and in recent years, more and more log exporting countries start the money that conserves forests
Source limits the felling of precious log, so that rare rare natural veneer kind is fewer and fewer, it is therefore desirable to it is a kind of to it is cheap,
The period of felling in turn short trees are processed, and can replace the dyeing of natural veneer, so that no matter dyeing wood skin is from class, product
In terms of matter or color, decorative pattern, finish, consumer demand can be met.
Summary of the invention
(1) the technical issues of solving
In view of the deficiencies of the prior art, the present invention provides a kind of wood skin dyeing of reserve flesh side muscle, has table
The advantages that face is smooth, uniform in color, cheap opposite natural veneer, solving the problems, such as natural veneer, there are natural defects.
(2) technical solution
To realize smooth above-mentioned dyeing veneer surface, uniform in color, the opposite cheap purpose of natural veneer, this hair
It is bright to provide the following technical solutions: a kind of wood skin dyeing of reserve flesh side muscle, comprising the following steps:
S1. sorting: the trees kind that fast growth, morning of becoming a useful person, the period of felling in turn are short is selected, to reduce cost;
S2. log is into after factory, first, in accordance with required length cutting into lengths, then when cuing open juggle processed, uses the cutting side of quarter sawing
Method, i.e., the annual ring of vertical tangential log, produces the wood skin that straight grain is presented, and reserve flesh side muscle;
S3. by the manual block pattern row pattern of the wood skin being cut into hanging basket, and using loop wheel machine by hanging basket be put into boiling pond into
Row bleaching, boiling pond is interior to be put into ethyl alcohol, hydrogen peroxide and piece alkali in the ratio of 1:2:2, and water temperature remains often first in boiling pond
Then temperature is to slowly warm up to 70-80 degrees Celsius, and keep this temperature boiling 3-5 hours, in order to avoid because thermal stress causes wood skin to be opened
It splits;
S4. well-done wood skin is put into color pond using loop wheel machine, dyestuff, dyestuff and water is added in color pond
Ratio be 1:1000, water temperature is 80-90 degrees Celsius in color pond, and wood skin is dyed 6-10 hours, and obtained moisture content is
The dyeing wood skin of 94%-96%;
S5. wood skin is sling by loop wheel machine after the completion of dyeing, and is drained at normal temperature, until wood skin moisture content drops to 40%-
After 50%, wood skin is placed in drying machine and is dried, the wood skin moisture control after drying is in 8%-12%;
S6. the wood skin after will be dried carries out hot pressing using hot press, and hot pressing temperature is 100-110 degrees Celsius, hot pressing pressure
Power is 2 megapascal, and smooth wood skin is made;
S7. it is sliced after wood skin is cooling, finished product wood skin, and puts packaging in order.
Preferably, the wood skin being cut into the step S2 is with a thickness of 0.2-0.8mm.
Preferably, replacements in boiling liquid 2-3 days in the step S3 are primary, and clear up the resin deposited in boiling pond,
Bark, silt, to reduce the pollution to wood skin.
Preferably, the boiling pond in the step S3 is provided with multiple, according to different tree species and chip dimensions, respectively
Wood chip is placed in different boiling ponds.
Preferably, the dyestuff of the step S4 is acid dyes or uses disperse dyes, has preferable permeability,
It is suitable for wood staining, and color fastness is high.
Preferably, it after a collection of wood skin of the every processing of color pond in the step S4, needs to supplement equal proportion into color pond
Water and dyestuff, it is full that water adds to color pond.
Preferably, the drying machine of the step S5 uses band drier, and drying effect is good, and is not easy to make wood chip
At damage.
(3) beneficial effect
Compared with prior art, the present invention provides a kind of wood skin dyeing of reserve flesh side muscle, having following has
Beneficial effect:
The wood skin dyeing of the reserve flesh side muscle, by selecting growth fast, morning of becoming a useful person, the period of felling in turn short trees product
Kind, to reduce cost, and it is cut to wood chip, the wood chip of well cutting, which is placed in boiling pond, carries out bleaching discoloration, then puts
Enter in color pond and dyed, wood skin finished product must be dyed finally by dry and hot pressing, due to using cheap timber former
Material, and processed by technique, allow dyeing wood skin to copy the texture and color of various rare precious timbers, meets people
To rare rare timber like and demand, and by processing after dyeing wood skin, surface is smooth, without worm channel, white edge
Deng, not only color more horn of plenty, and can be very good to meet different finishing places requirements and vast choose people respectively
Texture hobby.
Specific embodiment
The technical scheme in the embodiments of the invention will be clearly and completely described below, it is clear that described reality
Applying example is only a part of the embodiment of the present invention, instead of all the embodiments.Based on the embodiments of the present invention, this field
Those of ordinary skill's every other embodiment obtained without making creative work, belongs to guarantor of the present invention
The range of shield.
Embodiment 1
A kind of wood skin dyeing of reserve flesh side muscle, comprising the following steps:
S1. sorting: the trees kind that fast growth, morning of becoming a useful person, the period of felling in turn are short is selected, to reduce cost;
S2. log is into after factory, first, in accordance with required length cutting into lengths, then when cuing open juggle processed, uses the cutting side of quarter sawing
Method, i.e., the annual ring of vertical tangential log, produces the wood skin that straight grain is presented, and reserve flesh side muscle;
S3. by the manual block pattern row pattern of the wood skin being cut into hanging basket, and using loop wheel machine by hanging basket be put into boiling pond into
Row bleaching, boiling pond is interior to be put into ethyl alcohol, hydrogen peroxide and piece alkali in the ratio of 1:2:2, and water temperature remains often first in boiling pond
Then temperature is to slowly warm up to 70 degrees Celsius, and keep this temperature boiling 3-5 hours, in order to avoid because thermal stress causes wood skin to crack;
S4. well-done wood skin is put into color pond using loop wheel machine, dyestuff, dyestuff and water is added in color pond
Ratio be 1:1000, water temperature is 80 degrees Celsius in color pond, and wood skin is dyed 6 hours, and the dye that moisture content is 94% is made
Color wood skin;
S5. wood skin is sling by loop wheel machine after the completion of dyeing, and is drained at normal temperature, until wood skin moisture content drops to 40%
Afterwards, wood skin is placed in drying machine and is dried, the wood skin moisture control after drying is 8%;
S6. the wood skin after will be dried carries out hot pressing using hot press, and hot pressing temperature is 100 degrees Celsius, and hot pressing pressure is
Smooth wood skin is made in 2 megapascal;
S7. it is sliced after wood skin is cooling, finished product wood skin, and puts packaging in order.
The wood skin being cut into step S2 is with a thickness of 0.3mm.
Replacements in boiling liquid 2 days in step S3 are primary, and clear up the resin deposited in boiling pond, bark, silt, with
Reduce the pollution to wood skin.
Boiling pond in step S3 is provided with multiple, according to different tree species and chip dimensions, is respectively placed on wood chip
In different boiling ponds.
The dyestuff of step S4 is acid dyes or uses disperse dyes, has preferable permeability, is suitable for timber dye
Color, and color fastness is high.
After a collection of wood skin of the every processing of color pond in step S4, need to supplement the water and dyestuff of equal proportion into color pond,
It is full that water adds to color pond.
The drying machine of step S5 uses band drier, and drying effect is good, and is not easy to cause to damage to wood chip.
Embodiment 2
A kind of wood skin dyeing of reserve flesh side muscle, comprising the following steps:
S1. sorting: the trees kind that fast growth, morning of becoming a useful person, the period of felling in turn are short is selected, to reduce cost;
S2. log is into after factory, first, in accordance with required length cutting into lengths, then when cuing open juggle processed, uses the cutting side of quarter sawing
Method, i.e., the annual ring of vertical tangential log, produces the wood skin that straight grain is presented, and reserve flesh side muscle;
S3. by the manual block pattern row pattern of the wood skin being cut into hanging basket, and using loop wheel machine by hanging basket be put into boiling pond into
Row bleaching, boiling pond is interior to be put into ethyl alcohol, hydrogen peroxide and piece alkali in the ratio of 1:1:1, and water temperature remains often first in boiling pond
Then temperature is to slowly warm up to 75 degrees Celsius, and keep this temperature boiling 4 hours, in order to avoid because thermal stress causes wood skin to crack;
S4. well-done wood skin is put into color pond using loop wheel machine, dyestuff, dyestuff and water is added in color pond
Ratio be 1:900, water temperature is 85 degrees Celsius in color pond, and wood skin is dyed 8 hours, and the dye that moisture content is 95% is made
Color wood skin;
S5. wood skin is sling by loop wheel machine after the completion of dyeing, and is drained at normal temperature, until wood skin moisture content drops to 45%
Afterwards, wood skin is placed in drying machine and is dried, the wood skin moisture control after drying is 10%;
S6. the wood skin after will be dried carries out hot pressing using hot press, and hot pressing temperature is 105 degrees Celsius, and hot pressing pressure is
Smooth wood skin is made in 2 megapascal;
S7. it is sliced after wood skin is cooling, finished product wood skin, and puts packaging in order.
The wood skin being cut into step S2 is with a thickness of 0.5mm.
Replacements in boiling liquid 3 days in step S3 are primary, and clear up the resin deposited in boiling pond, bark, silt, with
Reduce the pollution to wood skin.
Boiling pond in step S3 is provided with multiple, according to different tree species and chip dimensions, is respectively placed on wood chip
In different boiling ponds.
The dyestuff of step S4 is acid dyes or uses disperse dyes, has preferable permeability, is suitable for timber dye
Color, and color fastness is high.
After a collection of wood skin of the every processing of color pond in step S4, need to supplement the water and dyestuff of equal proportion into color pond,
It is full that water adds to color pond.
The drying machine of step S5 uses band drier, and drying effect is good, and is not easy to cause to damage to wood chip.
In conclusion the wood skin dyeing of the reserve flesh side muscle, by selecting fast growth, morning of becoming a useful person, the period of felling in turn short
Trees kind, to reduce cost, and be cut to wood chip, the wood chip of well cutting be placed in boiling pond carries out bleaching go
Color is then placed in color pond and is dyed, and must dye wood skin finished product finally by dry and hot pressing, cheap due to using
Wood raw material, and processed by technique, dyeing wood skin allowed to copy the texture and color of various rare precious timbers,
Meet people to rare rare timber like and demand, and by processing after dyeing wood skin, surface is smooth, does not have
Worm channel, white edge etc., not only color more horn of plenty, but also can be very good to meet the requirements and vast choosing in different finishing places
Purchase the respective texture hobby of people.
It should be noted that the terms "include", "comprise" or its any other variant are intended to the packet of nonexcludability
Contain, so that the process, method, article or equipment for including a series of elements not only includes those elements, but also including
Other elements that are not explicitly listed, or further include for elements inherent to such a process, method, article, or device.
In the absence of more restrictions, the element limited by sentence "including a ...", it is not excluded that including the element
Process, method, article or equipment in there is also other identical elements.
It although an embodiment of the present invention has been shown and described, for the ordinary skill in the art, can be with
A variety of variations, modification, replacement can be carried out to these embodiments without departing from the principles and spirit of the present invention by understanding
And modification, the scope of the present invention is defined by the appended.
Claims (7)
1. a kind of wood skin dyeing of reserve flesh side muscle, which comprises the following steps:
S1. sorting: the trees kind that fast growth, morning of becoming a useful person, the period of felling in turn are short is selected, to reduce cost;
S2. log is into after factory, first, in accordance with required length cutting into lengths, then when cuing open juggle processed, using the cutting method of quarter sawing, i.e.,
The annual ring of vertical tangential log, produces the wood skin that straight grain is presented, and reserve flesh side muscle;
S3. by the manual block pattern row pattern of the wood skin being cut into hanging basket, and hanging basket is put into boiling pond using loop wheel machine and is floated
It is white, it is put into ethyl alcohol, hydrogen peroxide and piece alkali in the ratio of 1:2:2 in boiling pond, water temperature remains room temperature first in boiling pond, then
It is to slowly warm up to 70-80 degrees Celsius, and keeps this temperature boiling 3-5 hours, in order to avoid because thermal stress causes wood skin to crack;
S4. well-done wood skin is put into color pond using loop wheel machine, dyestuff, the ratio of dyestuff and water is added in color pond
For 1:1000, in color pond, water temperature is 80-90 degrees Celsius, and wood skin is dyed 6-10 hour, and it is 94%-96% that moisture content, which is made,
Dyeing wood skin;
S5. wood skin is sling by loop wheel machine after the completion of dyeing, and is drained at normal temperature, until wood skin moisture content drops to 40%-50%
Afterwards, wood skin is placed in drying machine and is dried, the wood skin moisture control after drying is in 8%-12%;
S6. the wood skin after will be dried carries out hot pressing using hot press, and hot pressing temperature is 100-110 degrees Celsius, hot pressing pressure 2
Smooth wood skin is made in megapascal;
S7. it is sliced after wood skin is cooling, finished product wood skin, and puts packaging in order.
2. a kind of wood skin dyeing of reserve flesh side muscle according to claim 1, it is characterised in that: the step S2
In the wood skin that is cut into a thickness of 0.2-0.8mm.
3. a kind of wood skin dyeing of reserve flesh side muscle according to claim 1, it is characterised in that: the step S3
In replacements in boiling liquid 2-3 days it is primary, and the resin deposited in boiling pond, bark, silt are cleared up, to reduce the dirt to wood skin
Dye.
4. a kind of wood skin dyeing of reserve flesh side muscle according to claim 1, it is characterised in that: the step S3
In boiling pond be provided with multiple, according to different tree species and chip dimensions, wood chip is placed in different boiling ponds respectively.
5. a kind of wood skin dyeing of reserve flesh side muscle according to claim 1, it is characterised in that: the step S4
Dyestuff be acid dyes or use disperse dyes that there is preferable permeability, be suitable for wood staining, and color fastness is high.
6. a kind of wood skin dyeing of reserve flesh side muscle according to claim 1, it is characterised in that: the step S4
In a collection of wood skin of the every processing of color pond after, need to supplement the water and dyestuff of equal proportion into color pond, water adds to color pond
It is full.
7. a kind of wood skin dyeing of reserve flesh side muscle according to claim 1, it is characterised in that: the step S5
Drying machine use band drier, drying effect is good, and is not easy to cause to damage to wood chip.