CN109103450A - A kind of control method for air door for extending lead plaster high temperature and holding time - Google Patents

A kind of control method for air door for extending lead plaster high temperature and holding time Download PDF

Info

Publication number
CN109103450A
CN109103450A CN201810861855.1A CN201810861855A CN109103450A CN 109103450 A CN109103450 A CN 109103450A CN 201810861855 A CN201810861855 A CN 201810861855A CN 109103450 A CN109103450 A CN 109103450A
Authority
CN
China
Prior art keywords
temperature
air door
lead plaster
maximum temperature
paste
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810861855.1A
Other languages
Chinese (zh)
Inventor
钦晓峰
陈林
龙洋洋
陆毅
汪章杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tianneng Battery Wuhu Co Ltd
Original Assignee
Tianneng Battery Wuhu Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tianneng Battery Wuhu Co Ltd filed Critical Tianneng Battery Wuhu Co Ltd
Priority to CN201810861855.1A priority Critical patent/CN109103450A/en
Publication of CN109103450A publication Critical patent/CN109103450A/en
Pending legal-status Critical Current

Abstract

The object of the present invention is to provide a kind of control method for air door that extension lead plaster high temperature is held time, and set the deviation up and down of maximum temperature and maximum temperature first, acid adding heating is carried out later, after being raised to maximum temperature, obtains actual temperature, if being higher than upper deviation value, air door is then opened, if being lower than lower deviation value, closes air door, this course location 300s, it can be very good extension lead plaster high temperature in this way to hold time, so that lead plaster sufficiently reacts, suitable for production.

Description

A kind of control method for air door for extending lead plaster high temperature and holding time
Technical field
The present invention relates to battery lead plaster mixing paste field more particularly to a kind of air door controls for extending lead plaster high temperature and holding time Method processed.
Background technique
Battery includes pole plate, and pole plate needs to carry out it during the manufacturing coated plate, and coated plate needs use Lead plaster, lead plaster needs use paste mixing machine acid adding mixing paste.At present for the mixing paste of lead plaster paste mixing machine, acid adding heating reaches After maximum temperature, air door blower, which is just opened, carries out hydrofuge cooling, and high temperature is held time too short, and lead plaster fails sufficiently to react.In this way It cannot meet the needs of production, therefore solve the problems, such as that this is just seemed very necessary.
Summary of the invention
To solve the above problems, the present invention provides a kind of control method for air door that extension lead plaster high temperature is held time, first The deviation up and down of maximum temperature and maximum temperature is set, carries out acid adding heating later, after being raised to maximum temperature, is obtained Actual temperature opens air door if being higher than upper deviation value, if being lower than lower deviation value, closes air door, this course location 300s, It can be very good to extend lead plaster high temperature in this way and hold time, so that lead plaster sufficiently reacts, solve asking of occurring in background technique Topic.
The object of the present invention is to provide a kind of control method for air door that extension lead plaster high temperature is held time, and include following step It is rapid:
Step 1: the maximum temperature of setting lead plaster mixing paste, and set the deviation up and down of maximum temperature;
Step 2: carrying out acid adding to lead plaster paste mixing machine, carry out heating stirring later, obtains the temperature in paste mixing machine at any time;
Step 3: lead plaster paste mixing machine temperature being raised at maximum temperature value, the temperature of paste mixing machine is obtained, when paste mixing machine temperature is higher than When maximum temperature upper deviation value, air door cooling is opened, when paste mixing machine temperature is lower than maximum temperature lower deviation value, air door is closed, This process maintains 300s;
Step 4: after highest high temperature maintains 300s, air door is normally opened, starts fast cooling, until mixing paste terminates.
Further improvement lies in that: the maximum temperature of the lead plaster mixing paste is 66-68 DEG C.
Further improvement lies in that: the deviation up and down for setting maximum temperature is ± 0.2 DEG C.
Beneficial effects of the present invention: the present invention sets the deviation up and down of maximum temperature and maximum temperature first, it Acid adding heating is carried out afterwards, after being raised to maximum temperature, is obtained actual temperature, if being higher than upper deviation value, air door is opened, if under being lower than Deviation then closes air door, this course location 300s, can be very good extension lead plaster high temperature in this way and holds time, so that lead plaster Sufficiently reaction, suitable for production.
Specific embodiment
In order to deepen the understanding of the present invention, the present invention will be described in further detail with reference to the examples below, the embodiment For explaining only the invention, it is not intended to limit the scope of the present invention..
The present embodiment provides a kind of control method for air door that extension lead plaster high temperature is held time, and include following steps:
Step 1: the maximum temperature of setting lead plaster mixing paste, and set the deviation up and down of maximum temperature;
Step 2: carrying out acid adding to lead plaster paste mixing machine, carry out heating stirring later, obtains the temperature in paste mixing machine at any time;
Step 3: lead plaster paste mixing machine temperature being raised at maximum temperature value, the temperature of paste mixing machine is obtained, when paste mixing machine temperature is higher than When maximum temperature upper deviation value, air door cooling is opened, when paste mixing machine temperature is lower than maximum temperature lower deviation value, air door is closed, This process maintains 300s;
Step 4: after highest high temperature maintains 300s, air door is normally opened, starts fast cooling, until mixing paste terminates.
The maximum temperature of the lead plaster mixing paste is 66.8 DEG C.The deviation up and down for setting maximum temperature is ± 0.2 DEG C.
The deviation up and down of maximum temperature and maximum temperature is set first, is carried out acid adding heating later, is raised to highest After temperature, actual temperature is obtained, if being higher than upper deviation value, opens air door, if being lower than lower deviation value, closes air door, this mistake Journey position 300s can be very good extension lead plaster high temperature in this way and hold time, so that lead plaster sufficiently reacts, suitable for production.

Claims (3)

1. a kind of control method for air door for extending lead plaster high temperature and holding time, it is characterised in that: include following steps:
Step 1: the maximum temperature of setting lead plaster mixing paste, and set the deviation up and down of maximum temperature;
Step 2: carrying out acid adding to lead plaster paste mixing machine, carry out heating stirring later, obtains the temperature in paste mixing machine at any time;
Step 3: lead plaster paste mixing machine temperature being raised at maximum temperature value, the temperature of paste mixing machine is obtained, when paste mixing machine temperature is higher than When maximum temperature upper deviation value, air door cooling is opened, when paste mixing machine temperature is lower than maximum temperature lower deviation value, air door is closed, This process maintains 300s;
Step 4: after highest high temperature maintains 300s, air door is normally opened, starts fast cooling, until mixing paste terminates.
2. a kind of control method for air door for extending lead plaster high temperature and holding time as described in claim 1, it is characterised in that: the lead The maximum temperature of cream mixing paste is 66-68 DEG C.
3. a kind of control method for air door for extending lead plaster high temperature and holding time as claimed in claim 1 or 2, it is characterised in that: institute The deviation up and down for setting maximum temperature is stated as ± 0.2 DEG C.
CN201810861855.1A 2018-08-01 2018-08-01 A kind of control method for air door for extending lead plaster high temperature and holding time Pending CN109103450A (en)