CN108995459A - A kind of production method of 3D color ink relief wall painting - Google Patents

A kind of production method of 3D color ink relief wall painting Download PDF

Info

Publication number
CN108995459A
CN108995459A CN201811041443.XA CN201811041443A CN108995459A CN 108995459 A CN108995459 A CN 108995459A CN 201811041443 A CN201811041443 A CN 201811041443A CN 108995459 A CN108995459 A CN 108995459A
Authority
CN
China
Prior art keywords
embossment
color ink
production method
wall painting
relief wall
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201811041443.XA
Other languages
Chinese (zh)
Inventor
崔峰涛
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201811041443.XA priority Critical patent/CN108995459A/en
Publication of CN108995459A publication Critical patent/CN108995459A/en
Pending legal-status Critical Current

Abstract

The present invention relates to a kind of production methods of 3D color ink relief wall painting, specifically includes the following steps: 1) raw material and tool prepare, 2) bottoming, 3) condiment, 4) sketch the contours, 5) roughhew, 6) finishing impression, 7) polishing, 8) paint.The invention has the advantages that: the diatom ooze using health environment-friendly is that raw material combine embossment and mural painting, compared with traditional mural painting, there is true tangibly three-dimensional sense, departing from the confinement of two-dimentional metope, is mutually set off by contrast with exquisite sculpture with color, strengthen the spatial impression of picture, it is allowed to more lively, like on the spot in person, more there is visual impact, subject matter is unrestricted arbitrarily to be customized, and the friendly process of pure manual drawing is belonged to.

Description

A kind of production method of 3D color ink relief wall painting
Technical field
The present invention relates to a kind of production methods of 3D color ink relief wall painting.
Background technique
Increasingly improved with social progress, people's living standard with the development of economy, demand of the people to ornament and It is required that mural painting makes people pleasant as a kind of art effect, beauty, and existing mural painting is mostly planar design being continuously improved, Lack fluctuating sense, three-dimensional sense and spatial impression.
Summary of the invention
The purpose of the present invention is to provide to solve the problems mentioned in the above background technology.
In order to solve the above technical problems, technical solution provided by the invention are as follows: a kind of production side of 3D color ink relief wall painting Method, specifically includes the following steps:
1) raw material and tool prepare: preparing diatom ooze, quartz sand, acrylic paints, bucket, perching knife, cleaver, broach knife, essence Icking tool, sand paper, rough draft pen and paintbrush;
2) bottoming: uniform three times diatom oozes of roller coating on metope, to dry;
3) condiment: being sequentially added clear water, diatom ooze and quartz sand in bucket, and immersion stirs into pug after five minutes;
4) it sketches the contours: after the metope to the good diatom ooze of roller coating air-dries, the pattern rough draft of desired picture is sketched the contours of using rough draft pen;
5) roughhew: being stacked to the pug mixed up in step 3) on pattern rough draft using perching knife and cleaver, using broaching knife Crude embossment is depicted, according to hierarchical relationship, between crude embossment protrusion metope 1cm~5cm;
6) finishing impression: doing very likely to pug, is worked with great care using finishing impression knife to crude embossment, keeps embossment more smart Carefully, vividly;
7) it polishes: being polished after pug is completely dry using sand paper, embossment is partially completed;
8) it paints: dipping acrylic paints using paintbrush and paint one by one to embossment scenery.
As a preferred embodiment, the plasticity that the step 5) roughhew can use diatom ooze make corresponding massif, Rivers and creeks, trees, grassland, house, bridge, personage, animal shape, can according to need and be fabricated to engraved structure.
As a preferred embodiment, when the step 8) is painted, acrylic paints can be not added to the direct thickness of water and be coated in embossment scape On object, the thick and heavy effect of oil painting is made.
As a preferred embodiment, when the step 8) is painted, acrylic paints can be added water be coated on embossment scenery, Make the rendering effect of traditional Chinese Painting.
As a preferred embodiment, the rough draft pen is one of pencil and chalk.
The invention has the advantages that: the diatom ooze using health environment-friendly is that raw material combine embossment and mural painting, with tradition Mural painting is compared, and has true tangibly three-dimensional sense, departing from the confinement of two-dimentional metope, is mutually dried with exquisite sculpture with color Support, strengthens the spatial impression of picture, is allowed to more lively, like on the spot in person, more has visual impact, subject matter is unrestricted can Arbitrarily customization, belongs to the friendly process of pure manual drawing.
Specific embodiment
Illustrate the present invention with specific embodiment below, is not limitation of the present invention.
Embodiment 1
A kind of production method of 3D color ink relief wall painting, specifically includes the following steps:
1) raw material and tool prepare: preparing diatom ooze, quartz sand, acrylic paints, bucket, perching knife, cleaver, broach knife, essence Icking tool, sand paper, rough draft pen and paintbrush;
2) bottoming: uniform three times diatom oozes of roller coating on metope, to dry;
3) condiment: being sequentially added clear water, diatom ooze and quartz sand in bucket, and immersion stirs into pug after five minutes;
4) it sketches the contours: after the metope to the good diatom ooze of roller coating air-dries, the pattern rough draft of desired picture is sketched the contours of using rough draft pen;
5) roughhew: being stacked to the pug mixed up in step 3) on pattern rough draft using perching knife and cleaver, using broaching knife Crude embossment is depicted, according to hierarchical relationship, between crude embossment protrusion metope 1cm~5cm;
6) finishing impression: doing very likely to pug, is worked with great care using finishing impression knife to crude embossment, keeps embossment more smart Carefully, vividly;
7) it polishes: being polished after pug is completely dry using sand paper, embossment is partially completed;
8) it paints: dipping acrylic paints using paintbrush and paint one by one to embossment scenery.
The plasticity that the step 5) roughhew can use diatom ooze makes corresponding massif, rivers and creeks, trees, grassland, room The shapes such as room, bridge, personage animal, can according to need and be fabricated to engraved structure.
When the step 8) is painted, acrylic paints can be not added to the direct thickness of water and be coated on embossment scenery, oil painting can be made Thick and heavy effect.
Embodiment 2
A kind of production method of 3D color ink relief wall painting, specifically includes the following steps:
1) raw material and tool prepare: preparing diatom ooze, quartz sand, acrylic paints, bucket, perching knife, cleaver, broach knife, essence Icking tool, sand paper, rough draft pen and paintbrush;
2) bottoming: uniform three times diatom oozes of roller coating on metope, to dry;
3) condiment: being sequentially added clear water, diatom ooze and quartz sand in bucket, and immersion stirs into pug after five minutes;
4) it sketches the contours: after the metope to the good diatom ooze of roller coating air-dries, the pattern rough draft of desired picture is sketched the contours of using rough draft pen;
5) roughhew: being stacked to the pug mixed up in step 3) on pattern rough draft using perching knife and cleaver, using broaching knife Crude embossment is depicted, according to hierarchical relationship, between crude embossment protrusion metope 1cm~5cm;
6) finishing impression: doing very likely to pug, is worked with great care using finishing impression knife to crude embossment, keeps embossment more smart Carefully, vividly;
7) it polishes: being polished after pug is completely dry using sand paper, embossment is partially completed;
8) it paints: dipping acrylic paints using paintbrush and paint one by one to embossment scenery.
The plasticity that the step 5) roughhew can use diatom ooze makes corresponding massif, rivers and creeks, trees, grassland, room The shapes such as room, bridge, personage animal, can according to need and be fabricated to engraved structure.
When the step 8) is painted, acrylic paints can be added water be coated on embossment scenery, utilize the water suction of diatom ooze Property can imitate rice paper and make traditional Chinese Painting effect, paint one by one to embossment scenery.
The foregoing is only a preferred embodiment of the present invention, but scope of protection of the present invention is not limited thereto, Anyone skilled in the art in the technical scope disclosed by the present invention, according to the technique and scheme of the present invention and its Inventive concept is subject to equivalent substitution or change, should be covered by the protection scope of the present invention.

Claims (5)

1. a kind of production method of 3D color ink relief wall painting, which is characterized in that specifically includes the following steps:
1) raw material and tool prepare: prepare diatom ooze, quartz sand, acrylic paints, bucket, perching knife, cleaver, broach knife, finishing impression knife, Sand paper, rough draft pen and paintbrush;
2) bottoming: uniform three times diatom oozes of roller coating on metope, to dry;
3) condiment: being sequentially added clear water, diatom ooze and quartz sand in bucket, and immersion stirs into pug after five minutes;
4) it sketches the contours: after the metope to the good diatom ooze of roller coating air-dries, the pattern rough draft of desired picture is sketched the contours of using rough draft pen;
5) roughhew: being stacked to the pug mixed up in step 3) on pattern rough draft using perching knife and cleaver, is drawn using graduating with cutter is broached Crude embossment out, according to hierarchical relationship, between crude embossment protrusion metope 1cm~5cm;
6) finishing impression: doing very likely to pug, is worked with great care using finishing impression knife to crude embossment, make embossment it is more fine, Vividly;
7) it polishes: being polished after pug is completely dry using sand paper, embossment is partially completed;
8) it paints: dipping acrylic paints using paintbrush and paint one by one to embossment scenery.
2. a kind of production method of 3D color ink relief wall painting according to claim 1, it is characterised in that: the step 5) is thick Carving can use diatom ooze plasticity make corresponding massif, rivers and creeks, trees, grassland, house, bridge, personage, animal shape Shape can according to need and be fabricated to engraved structure.
3. a kind of production method of 3D color ink relief wall painting according to claim 1, it is characterised in that: in the step 8) When color, acrylic paints can be not added to the direct thickness of water and be coated on embossment scenery.
4. a kind of production method of 3D color ink relief wall painting according to claim 1, it is characterised in that: in the step 8) When color, acrylic paints can be added water be coated on embossment scenery.
5. a kind of production method of 3D color ink relief wall painting according to claim 1, it is characterised in that: the rough draft pen For one of pencil and chalk.
CN201811041443.XA 2018-09-07 2018-09-07 A kind of production method of 3D color ink relief wall painting Pending CN108995459A (en)