CN108972753A - Prevent the solid wood door manufacture method of deformation - Google Patents
Prevent the solid wood door manufacture method of deformation Download PDFInfo
- Publication number
- CN108972753A CN108972753A CN201811043411.3A CN201811043411A CN108972753A CN 108972753 A CN108972753 A CN 108972753A CN 201811043411 A CN201811043411 A CN 201811043411A CN 108972753 A CN108972753 A CN 108972753A
- Authority
- CN
- China
- Prior art keywords
- plate
- door
- rectangular slab
- steelframe
- veneer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
The invention discloses the solid wood door manufacture methods for preventing deformation, veneer is cut into when passing through processing logs, removal corner is maximized according to veneer, so that log maximizes the use, large plate is spliced by rectangular slab, small section timber is become to the plate of large-scale suitable production door, it is pressed together again by two layers of rectangular slab viscose glue, form the double-deck large plate, a core substrate is cut into using doubling plate, steelframe is filled between the substrates, the form of door core is kept using steelframe, wooden dilation when steel plate stress prevent plate deformation power, keep door core indeformable.
Description
Technical field
The present invention relates to a kind of timber processing methods, and in particular to prevents the solid wood door manufacture method of deformation.
Background technique
Solid Door is constantly subjected to masses and likes, Solid Door in use due to Changes in weather, lead by air humidity variation
Wood dilation is caused, so that the tension on door panel is uneven, thus the problem of the deformation of generation.
Summary of the invention
The present invention provides the solid wood door manufacture methods for preventing deformation solved the problems, such as in above-mentioned background technique.
The present invention is achieved through the following technical solutions:
Prevent the solid wood door manufacture method of deformation, comprising the following steps:
S1, veneer is cut log into, the surrounding of veneer is cut into rectangular slab according to veneer maximization;
S2, rectangular slab is spliced into a big template, the gluing in large plate, then is bonded in large plate with rectangular slab splicing
On, pressing drying forms the double-deck force fit plate;
S3, the double-deck force fit plate is cut into gate, as door panel substrate;
S4, it is overlapped setting using at least two door core substrates as core plate, the steelframe of " day " shape is set between door core substrate,
Place compacting and the matched groove of steelframe of steelframe are set on door core substrate, and in groove and door core substrate adhesive surface applies
Glue, then pressing drying;
S5, the two sides that core plate is bonded in using wood panel planish to corner using compacting drying after panel bonding
Processing;
S6, edge sealing processing is carried out to the corner after planing.
It is cut into veneer when passing through processing logs, removal corner is maximized according to veneer, so that log obtains maximumlly
It utilizes, large plate is spliced by rectangular slab, small section timber is become to the plate of large-scale suitable production door, then pass through two layers of square
Shape plate viscose glue is pressed together, and is formed the double-deck large plate, is cut into a core substrate using doubling plate, fills steelframe between the substrates,
Using steelframe keep door core form, wooden dilation when steel plate stress prevent plate deformation power, keep Men Xin not
Deformation.
Further, veneer with a thickness of 0.5-1cm.The thickness of veneer determines the efficiency of multi-layer board production, and veneer is thicker,
Multi-layer board producing efficiency is higher, and the thinner manufacture craft difficulty of veneer is high, but the effect of cracking-proof is better, therefore, in view of solid wood
The thickness of door is between 3-5cm, using veneer with a thickness of 0.5-1cm, so that three to five layers of production, guarantees effect of anti-cracking
Meanwhile guaranteeing manufacture efficiency.
Further, the thickness of the steelframe is less than the thickness of doubling plate, and the length and width of steelframe are less than door core substrate
Length and width but be greater than a half for core substrate length and width.The thickness of steelframe be less than doubling plate thickness be in order to
The groove of steel plate is set not press to wear substrate, the length and width of steelframe are less than the length of door core substrate and width but are greater than a core
Substrate length and the half of width guarantee steel frame construction suitable size.
Further, edge sealing processing is pressed using viscose glue, then firm with text nail.Edge sealing only uses viscose glue since area is small
Therefore easy degumming reuses text nail and fixes, keep it more durable, the hidden effect of text nail is good, guarantees the smooth of edge sealing surface
Property.
Further, the carving of panel, whole japanning processing are carried out after step S6 again.
Further, when increasing by one layer of rectangular slab in step S2, each independent four side of rectangular slab and upper one layer of large plate
In four side of rectangular slab be not overlapped, formed adjacent two layers large plate between rectangular slab bonding straggly.Japanning is finally carried out, so that
Lacquer painting can fill up scratch small in manufacturing process.
The present invention has the advantage that and the utility model has the advantages that
1, it is cut into veneer when the present invention passes through processing logs, removal corner is maximized according to veneer, so that log obtains
It is maximized to utilize, large plate is spliced by rectangular slab, small section timber is become to the plate of large-scale suitable production door, then is led to
It crosses two layers of rectangular slab viscose glue to be pressed together, forms the double-deck large plate, a core substrate is cut into using doubling plate, is filled out between the substrates
Fill steelframe, using steelframe keep door core form, wooden dilation when steel plate stress prevent plate deformation power, keep
Door core is indeformable;
2, the present invention, so that making three to five layers, guarantees the same of effect of anti-cracking using veneer with a thickness of 0.5-1cm
When, guarantee manufacture efficiency;
3, edge sealing of the present invention due to area it is small, only use viscose glue be easy degumming, therefore, reuse text nail fix, make it more
Add durable, text follows closely that hidden effect is good, guarantees the planarization on edge sealing surface.
Specific embodiment
To make the objectives, technical solutions, and advantages of the present invention clearer, below with reference to embodiment, the present invention is made
Further to be described in detail, exemplary embodiment of the invention and its explanation for explaining only the invention, are not intended as to this
The restriction of invention.
Embodiment 1
Prevent the solid wood door manufacture method of deformation, comprising the following steps:
S1, veneer is cut log into, the surrounding of veneer is cut into rectangular slab according to veneer maximization;
S2, rectangular slab is spliced into a big template, the gluing in large plate, then is bonded in large plate with rectangular slab splicing
On, pressing drying forms the double-deck force fit plate;
S3, the double-deck force fit plate is cut into gate, as door panel substrate;
S4, it is overlapped setting using at least two door core substrates as core plate, the steelframe of " day " shape is set between door core substrate,
Place compacting and the matched groove of steelframe of steelframe are set on door core substrate, and in groove and door core substrate adhesive surface applies
Glue, then pressing drying;
S5, the two sides that core plate is bonded in using wood panel planish to corner using compacting drying after panel bonding
Processing;
S6, edge sealing processing is carried out to the corner after planing.
When implementation, veneer with a thickness of 0.5-1cm;The thickness of the steelframe is less than the thickness of doubling plate, the length of steelframe
It is less than the length of door core substrate with width and width but is greater than a half for core substrate length and width;Edge sealing processing uses viscous
Glue laminated is closed, then firm with text nail;The carving of panel, whole japanning processing are carried out after step S6 again;Increase by one layer in step S2
When rectangular slab, each independent rectangular slab four is not overlapped while with the rectangular slab four in upper one layer of large plate, forms adjacent two layers
Rectangular slab bonding straggly between large plate.When the corner cutting of veneer, corner guarantees to become regular at 90 degree when should be as far as possible
Rectangular slab, when splicing when facilitate splicing to be not easy to stay seam, when processing logs, by log wire cutting at identical section of material of length,
Length is identical when guarantee is cut into veneer, and large plate is spliced into after convenient.
Above-described specific embodiment has carried out further the purpose of the present invention, technical scheme and beneficial effects
It is described in detail, it should be understood that being not intended to limit the present invention the foregoing is merely a specific embodiment of the invention
Protection scope, all within the spirits and principles of the present invention, any modification, equivalent substitution, improvement and etc. done should all include
Within protection scope of the present invention.
Claims (6)
1. preventing the solid wood door manufacture method of deformation, which comprises the following steps:
S1, veneer is cut log into, the surrounding of veneer is cut into rectangular slab according to veneer maximization;
S2, rectangular slab is spliced into a big template, the gluing in large plate, then is bonded in large plate with rectangular slab splicing,
Pressing drying forms the double-deck force fit plate;
S3, the double-deck force fit plate is cut into gate, as door panel substrate;
S4, it is overlapped setting using at least two door core substrates as core plate, the steelframe of " day " shape is set between door core substrate, in door
Place compacting and the steelframe matched groove of steelframe are set on core substrate, in groove and door core substrate adhesive surface gluing, so
Pressing drying afterwards;
S5, the two sides that core plate is bonded in using wood panel carry out at planing corner using compacting drying after panel bonding
Reason;
S6, edge sealing processing is carried out to the corner after planing.
2. it is according to claim 1 prevent deformation solid wood door manufacture method, which is characterized in that the veneer with a thickness of
0.5-1cm。
3. the solid wood door manufacture method according to claim 1 for preventing deformation, which is characterized in that the thickness of the steelframe is small
In the thickness of doubling plate, the length and width of steelframe be less than door core substrate length and width but be greater than core substrate length with
The half of width.
4. the solid wood door manufacture method according to claim 1 for preventing deformation, which is characterized in that the edge sealing processing uses
Viscose glue pressing, then it is firm with text nail.
5. the solid wood door manufacture method according to claim 1 for preventing deformation, which is characterized in that carried out again after step S6
The carving of panel, whole japanning processing.
6. the solid wood door manufacture method according to claim 1 for preventing deformation, which is characterized in that increase by one layer in step S2
When rectangular slab, each independent rectangular slab four is not overlapped while with the rectangular slab four in upper one layer of large plate, forms adjacent two layers
Rectangular slab bonding straggly between large plate.