CN108970929A - A kind of method of paint spraying - Google Patents

A kind of method of paint spraying Download PDF

Info

Publication number
CN108970929A
CN108970929A CN201810923716.7A CN201810923716A CN108970929A CN 108970929 A CN108970929 A CN 108970929A CN 201810923716 A CN201810923716 A CN 201810923716A CN 108970929 A CN108970929 A CN 108970929A
Authority
CN
China
Prior art keywords
finishing coat
paint
drying
layer finishing
layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201810923716.7A
Other languages
Chinese (zh)
Inventor
董春艳
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hefei You Heng Wang Mdt Infotech Ltd
Original Assignee
Hefei You Heng Wang Mdt Infotech Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hefei You Heng Wang Mdt Infotech Ltd filed Critical Hefei You Heng Wang Mdt Infotech Ltd
Priority to CN201810923716.7A priority Critical patent/CN108970929A/en
Publication of CN108970929A publication Critical patent/CN108970929A/en
Withdrawn legal-status Critical Current

Abstract

The present invention relates to a kind of methods of paint spraying, comprising the following steps: (1) primes;(2) first layer finishing coat is applied, second layer finishing coat will be sprayed again after the drying of first layer finishing coat;(3) at least layer of transparent paint transparent painting: is sprayed on the surface of the second layer finishing coat;It is characterized by: the first layer finishing coat is dried by the way of drying, and the temperature of the drying is 140-160 degrees Celsius, to accelerate the solvent in the first layer finishing coat to volatilize, so as to avoid point phenomenon, the workpiece temperature by drying also makes the second layer finishing coat be more easier to adhere to simultaneously, to avoid the phenomenon that whitening and flow paint.Due to the method in the method for paint spraying in the present invention in the drying of first layer finishing coat using drying, the volatilization of solvent is accelerated, thus the defect for successfully avoiding point, whitening and flowing paint.

Description

A kind of method of paint spraying
Technical field
The present invention relates to industrial technical fields, and in particular to a kind of method of paint spraying.
Background technique
Spray painting and the main path that plastic-spraying is that current industrial surface is decorated, spray painting is compared with plastic-spraying with levelling is good, can repair The advantages of benefit, flexibility are good, decorative abundant, hardness is high, high-efficient, easily against ground defect, thus obtained increasingly It is widely applied.The method that usually spray painting uses is: successively by spray-applied primer, first of finishing coat, second finishing coat, transparent Paint, wherein what first of finishing coat took is surface drying, i.e., it is dry in the environment of 70 DEG C or so.
However, during spray painting the problem of painting environment, since environment is unholiness, many dusts be mingled with wherein, because And point is formed after will lead to spray painting, it is generally the case that since the defect of point causes spray painting qualification rate less than 10%, how to prevent Only occur in painting process point be this field directly facing a technical problem.Since point is really fine dust attachment Caused by, therefore to eliminate point and need to increase substantially painting environment cleannes, but this can make spray painting cost be enhanced several times.
In addition, the reason of causing the defect of the point be not it is unique, in addition to dirt, it is also possible to cross spray or The reasons such as the other reason of person, such as levelling is insufficient, drying temperature is excessively high, coating quality;The selection for spraying tool is also important, matter The flow that bad spray tool has been unable to control spray gun rifle mouth is measured, thus the problems such as also resulting in point;In addition, the paint layer mistake of spraying Exclusion that is thick and being unfavorable for bubble, it is also possible to cause point.
Spray painting is other than can have the defects that point, and there are also white point problems, if overspray can also flow the defect of paint.
Summary of the invention
It can prevent from occurring point and/or stream paint in painting process the object of the present invention is to provide one kind and/or white point lacks Sunken, easy to operate, at low cost method for paint spraying.
In order to solve the above technical problems, the present invention takes following technical scheme: a kind of method of paint spraying, including it is following Step: (1) it primes;(2) first layer finishing coat is applied, second layer finishing coat will be sprayed again after the drying of first layer finishing coat;(3) transparent painting: At least layer of transparent paint is sprayed on the surface of the second layer finishing coat;It is characterized by: the first layer finishing coat is using drying Mode be dried, and the temperature of the drying be 140-160 degrees Celsius, to accelerate the solvent in the first layer finishing coat to wave Hair, so as to avoid point phenomenon, while the workpiece temperature by drying also makes the second layer finishing coat be more easier to adhere to, To avoid the phenomenon that whitening and flow paint.
Due in the method for the paint spraying in the present invention in the drying of first layer finishing coat using the method for drying, because This accelerates the volatilization of solvent, thus the defect for successfully avoiding point, whitening and flowing paint.
Specific embodiment
Technical solution of the present invention is described in detail below.
The method of paint spraying in the present invention the following steps are included:
(1) it derusts: if workpiece surface has iron mold, carrying out manual removal with scraper, emery cloth and steel brush class tool, when necessary Chemicals (such as pickling, formula are sulfuric acid, peregal, hexamethylenetetramine, water) cleaning can be used, in addition, gas also can be used Dynamic steel needle pistol for rust removal.Preferably, using best selection office moat type pipette tips when the rifle.
(2) paint if workpiece surface is had been friends in the past, carries out depainting: being all de- according to the determination of the situation of piece surface when operation Paint or local depainting.Preferably, the method that depainting uses sandblasting depainting, paint stripper depainting.After old paint film is removed completely, use Warm water cleans up piece surface.And remaining paint stripper is cleaned with gasoline or kerosene, in order to avoid influence the gloss of new lacquer painting, Dry and adhesive force.
(3) position for not needing spraying block being protected with adhesive plaster, paper or lubricating grease etc..
(4) it primes.
(5) the defects of filling out Puttying to eliminate the pit of piece surface, stomata, pitted skin, scratch, makes its uniform ground.Such as When fruit piece surface recess too depth or excessive area, it can be touched at this with rubber hammer, it is made to be full of reinstatement.
(6) polish: dry grinding or water mill can be used in polishing, no matter which kind of uses, and removes floating dust, scale after having polished and does Only, and it is completely dried surface for use.
(7) apply base coat: the putty after polishing can not all be smooth, it sometimes appear that many holes are big Small sand holes are formed in situ bubble if do not repaired, and influence the total quality and appearance of finishing coat.So at this moment must apply Second priming paint, it is therefore an objective to fill up pin hole sand holes, while be also to increase binding force for the finishing coat of later process.
(8) paint: looked into piece surface really without sand holes after can spray paint.Finishing coat first uses spray gun when spraying Thin one layer of spray, sprays the second layer, third layer again after parching, cannot act with undue haste when desired light tone, spraying, primary to spray It is thick to be easy to spray, causes uneven shade or water droplet phenomenon.
Preferably, first layer finishing coat being dried by the way of drying, it is preferable that the temperature of the drying is 150 DEG C or so, due to workpiece, such as wheel hub, the solvent in first layer finishing coat can be accelerated to volatilize by drying, so as to keep away Exempt from point phenomenon, while the wheel hub temperature by drying also makes second layer finishing coat be more easier to adhere to, avoids whitening and flowing paint Phenomenon.
(9) transparent painting: one layer or several layers of colored varnishes, i.e. varnish are sprayed, on finishing coat surface to improve surface quality.
(10) it polishes: for further smooth surface of the paint film, being allowed to bright beautiful.
Due to the method in the method in the present invention in the drying of first layer finishing coat using drying, accelerate molten The volatilization of agent, thus the defect for successfully avoiding point, whitening and flowing paint.

Claims (8)

1. a kind of method of paint spraying, comprising the following steps:
(1) it primes;
(2) first layer finishing coat is applied, second layer finishing coat will be sprayed again after the drying of first layer finishing coat;
(3) at least layer of transparent paint transparent painting: is sprayed on the surface of the second layer finishing coat;
It is characterized by: the first layer finishing coat is dried by the way of drying, and the temperature of the drying is 140-160 Degree Celsius, to accelerate the solvent in the first layer finishing coat to volatilize, so as to avoid point phenomenon, while by the work of drying Part temperature also makes the second layer finishing coat be more easier to adhere to, to avoid the phenomenon that whitening and flow paint.
2. according to the method described in claim 1, it is characterized by:
Further include the steps that derusting before the step (1), the derusting is using chemicals cleaning or pneumatic steel needle derusting Rifle derusts.
3. according to the method described in claim 2, it is characterized by: if workpiece surface is had been friends in the past paint, in the descaling step The step of being additionally provided with depainting between the step (1).
4. according to the method described in claim 3, it is characterized by: de- using sandblasting depainting or paint stripper the step of the depainting The method of paint.
5. method according to claim 1-4, it is characterised in that: be additionally provided with throwing after the step (3) The step of light.
6. method according to claim 1-4, it is characterised in that: the temperature of the drying is 150 degrees Celsius.
7. according to the method described in claim 6, it is characterized by: applying twice priming paint in the step (1).
8. according to the method described in claim 7, it is characterized by: the step of painting twice priming paint among the step (1) Between be additionally provided with the step of filling out Puttying.
CN201810923716.7A 2018-08-11 2018-08-11 A kind of method of paint spraying Withdrawn CN108970929A (en)