CN108931455A - 电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置 - Google Patents
电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置 Download PDFInfo
- Publication number
- CN108931455A CN108931455A CN201810319478.9A CN201810319478A CN108931455A CN 108931455 A CN108931455 A CN 108931455A CN 201810319478 A CN201810319478 A CN 201810319478A CN 108931455 A CN108931455 A CN 108931455A
- Authority
- CN
- China
- Prior art keywords
- electrode
- silicone grease
- silicon rubber
- drying chamber
- heat
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,包括恒温干燥箱,所述恒温干燥箱内底部放置有绝缘台,绝缘台表面中心安装有接地电极,接地电极上方设有高压电极,高压电极顶面通过连接柱与恒温干燥箱内顶面固定连接,所述高压电极与接地电极之间设有夹持装置,夹持装置通过连接杆与恒温干燥箱侧壁固定连接,所述恒温干燥箱内还设有电源,电源的正极通过导线与高压电极连接,电源的负极通过导线与接地电极连接。本发明可实现温度、电场和机械拉应力可调,保证了实验环境的稳定性和实验数据的精确性,且适于其他有机绝缘材料的吸收硅脂实验。
Description
技术领域
本发明属于有机绝缘材料试验技术领域,具体涉及一种电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置。
背景技术
电力电缆是用于传输和分配电能的电缆,在电力线路中,电缆所占比重正逐渐增加。电缆按绝缘材料分为油浸纸绝缘电力电缆、塑料绝缘电力电缆和橡皮绝缘电力电缆。在电力电缆实际运行时硅橡胶冷缩管始终处于高温、电场和扩张应力共存的外部环境中。为了真实模拟硅橡胶冷缩管实际运行时它对硅橡胶-交联聚乙烯界面处涂覆硅脂的吸收,设计电场-热-扩张应力共存环境下硅橡胶吸收硅脂特性的实验装置。
发明内容
本发明所要解决的技术问题便是针对上述现有技术的不足,提供一种电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置。
本发明所采用的技术方案是:一种电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,包括恒温干燥箱,所述恒温干燥箱内底部放置有绝缘台,绝缘台表面中心安装有接地电极,接地电极上方设有高压电极,高压电极顶面通过连接柱与恒温干燥箱内顶面固定连接,所述高压电极与接地电极之间设有夹持装置,夹持装置通过连接杆与恒温干燥箱侧壁固定连接,所述恒温干燥箱内还设有电源,电源的正极通过导线与高压电极连接,电源的负极通过导线与接地电极连接。
作为优选,所述高压电极与接地电极大小一致,均均为圆形平板状。
作为优选,所述高压电极与接地电极上下对应设置。
作为优选,所述连接柱为环氧芯棒,连接柱底端与高压电极螺纹连接,连接柱顶端与恒温干燥箱内顶面螺纹连接。
作为优选,所述夹持装置包括两个对称设置的卡爪,卡爪通过液压伸缩杆与恒温干燥箱侧壁固定。
作为优选,所述两个卡爪位于高压电极与接地电极连线的中线上。
作为优选,所述两个卡爪之间连线的中线与连接柱的轴线重合。
作为优选,所述恒温干燥箱侧壁上与高压电极和接地电极对应处分别设有用于导线穿过的套管。
本发明可实现电力电缆附件硅橡胶在电场、热、扩张应力三种环境因素共同作用下的吸收硅脂实验,可实现温度、电场和机械拉应力三个环境参数的独立调节,保证了实验环境的稳定性和实验数据的精确性,更符合附件硅橡胶的实际运行环境,且适于其他有机绝缘材料的吸收硅脂实验。
附图说明
图1为本发明的结构示意图;
图2为本发明硅橡胶的增重率-吸收时间曲线图。
图中:1、恒温干燥箱;2、绝缘台;3、接地电极;4、高压电极;5、连接柱;6、夹持装置;7、电源;8、套管;61、卡爪;62、液压伸缩杆。
具体实施方式
下面将结合附图及具体实施例对本发明作进一步详细说明。
实施例1
如图1所示,本实施例提供的电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置包括恒温干燥箱1,所述恒温干燥箱1内底部放置有绝缘台2,绝缘台2表面中心安装有接地电极3,接地电极3上方对应设有与其大小一致,均为圆形平板状的高压电极4,高压电极4顶面通过连接柱5与恒温干燥箱1 内顶面固定连接,所述连接柱5为环氧芯棒,环氧芯棒的底端与高压电极4螺纹连接,环氧芯棒的顶端与恒温干燥箱1内顶面螺纹连接,所述高压电极4与接地电极3之间设有夹持装置6,所述夹持装置6包括两个对称设置的卡爪61,每个卡爪61分别通过连接杆与恒温干燥箱1侧壁固定连接,所述两个卡爪61 位于高压电极4与接地电极3连线的中线上,且两个卡爪61之间连线的中线与连接柱5的轴线重合,所述连接杆为液压伸缩杆62,所述恒温干燥箱1内还设有电源7,电源7的正极通过导线与高压电极4连接,电源7的负极通过导线与接地电极3连接。
实施例2
本实施例与实施例1基本相同,仅是对恒温干燥箱1作出了改变,所述恒温干燥箱1侧壁上与高压电极4和接地电极3对应处分别设有用于导线穿过的套管8。
浸渍-增重法的步骤:制备硅橡胶样品、用去离子水和无水乙醇清洗样品,干燥后测其初始质量,而后浸渍于硅脂内,每隔一段时间取出样品并用汽油清洗去除样品表面的硅脂,待汽油挥发完后利用电子分析天平(G&G JJ224BC 320g 0.1mg)测量样品质量,直至天平读数稳定后记录质量数据,重新将该样品浸渍于硅脂内,每隔一段时间重复上述程序,就可获得硅橡胶样品的增重率-吸收时间曲线(典型曲线如图2所示),增重率即为吸收硅脂率。在给定温度、电场和扩张应力的情况下,利用浸渍-增重法研究硅橡胶样品在该环境下不同吸收时间时的吸收硅脂率或饱和吸收硅脂率。更改温度、电场或扩张应力的任何一个参数并更换硅橡胶样品,重复上述过程,就可获得这三个因素的不同组合作用下硅橡胶的(饱和)吸收硅脂率。从而可实现电力电缆附件硅橡胶在电场、热、扩张应力三种环境因素共同作用下吸收硅脂特性的研究。
Claims (8)
1.一种电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,其特征在于:包括恒温干燥箱(1),所述恒温干燥箱(1)内底部放置有绝缘台(2),绝缘台(2)表面中心安装有接地电极(3),接地电极(3)上方设有高压电极(4),高压电极(4)顶面通过连接柱(5)与恒温干燥箱(1)内顶面固定连接,所述高压电极(4)与接地电极(3)之间设有夹持装置(6),夹持装置(6)通过连接杆与恒温干燥箱(1)侧壁固定连接,所述恒温干燥箱(1)内还设有电源(7),电源(7)的正极通过导线与高压电极(4)连接,电源(7)的负极通过导线与接地电极(3)连接。
2.根据权利要求1所述的电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,其特征在于:所述高压电极(4)与接地电极(3)大小一致,均均为圆形平板状。
3.根据权利要求1所述的电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,其特征在于:所述高压电极(4)与接地电极(3)上下对应设置。
4.根据权利要求1所述的电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,其特征在于:所述连接柱(5)为环氧芯棒,连接柱(5)底端与高压电极(4)螺纹连接,连接柱(5)顶端与恒温干燥箱(1)内顶面螺纹连接。
5.根据权利要求1所述的电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,其特征在于:所述夹持装置(6)包括两个对称设置的卡爪(61),卡爪(61)通过液压伸缩杆(62)与恒温干燥箱(1)侧壁固定。
6.根据权利要求1所述的电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,其特征在于:所述两个卡爪(61)位于高压电极(4)与接地电极(3)连线的中线上。
7.根据权利要求1所述的电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,其特征在于:所述两个卡爪(61)之间连线的中线与连接柱(5)的轴线重合。
8.根据权利要求1所述的电场、热、扩张应力共存环境下硅橡胶吸收硅脂实验装置,其特征在于:所述恒温干燥箱(1)侧壁上与高压电极(4)和接地电极(3)对应处分别设有用于导线穿过的套管(8)。