CN108907512A - 碳化硅颗粒增强铝基复合材料用镓基钎料制备和使用方法 - Google Patents
碳化硅颗粒增强铝基复合材料用镓基钎料制备和使用方法 Download PDFInfo
- Publication number
- CN108907512A CN108907512A CN201811000847.4A CN201811000847A CN108907512A CN 108907512 A CN108907512 A CN 108907512A CN 201811000847 A CN201811000847 A CN 201811000847A CN 108907512 A CN108907512 A CN 108907512A
- Authority
- CN
- China
- Prior art keywords
- gallium
- composite material
- silicon carbide
- base
- carbide particles
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
Claims (8)