CN108831746A - A method of improving aluminium electrolutic capacitor Waste Acid From Hua Cheng Foil aberrations in property - Google Patents
A method of improving aluminium electrolutic capacitor Waste Acid From Hua Cheng Foil aberrations in property Download PDFInfo
- Publication number
- CN108831746A CN108831746A CN201810619241.2A CN201810619241A CN108831746A CN 108831746 A CN108831746 A CN 108831746A CN 201810619241 A CN201810619241 A CN 201810619241A CN 108831746 A CN108831746 A CN 108831746A
- Authority
- CN
- China
- Prior art keywords
- floating ball
- tank liquor
- electrolutic capacitor
- aluminium electrolutic
- waste acid
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of improvement aluminium electrolutic capacitor methods of Waste Acid From Hua Cheng Foil aberrations in property, and steps are as follows:Use the PPH floating ball of two or more diameters, it is evenly distributed on aluminium electrolutic capacitor chemical conversion tank liquor liquid level, small diameter floating ball fills the gap between larger diameter floating ball, guarantee that 90% or more of liquid level is covered by floating ball, inhibit the evaporation of chemical conversion tank liquor at high temperature, chemical conversion tank liquor temperature and ingredient stability are improved, aluminium electrolutic capacitor Waste Acid From Hua Cheng Foil head and the tail deviation is improved.It is an advantage of the invention that:Using two or more diameters PPH floating ball, uniformly dispersing inhibits the evaporation of chemical conversion tank liquor on tank liquor surface.Improve Waste Acid From Hua Cheng Foil aberrations in property, while reducing the waste of chemicals and the energy.
Description
Technical field
The invention belongs to the manufacturing methods of low-voltage anodic foil for aluminum electrolytic capacitor, and in particular to aluminium electrolutic capacitor low pressure
The chemical conversion manufacturing process of anode foils.
Background technique
Currently, low-voltage anodic foil for aluminum electrolytic capacitor, in formation process, chemical conversion tank liquor is exposed in air, electrolytic bath
Liquid temperature causes tank liquor surface liquid to be easy to volatilize between 70-90 DEG C, takes away a large amount of tank liquors and heat, leads to tank liquor surface
There is deviations inside temperature and ingredient and tank liquor, and fluctuate at any time, lead to the inhomogeneities of chemical conversion treatment, are embodied in production
Moral character can go up the use that subsequent capacitance device producer is influenced as front and back aberrations in property.Meanwhile ammonium adipate has been taken away in tank liquor evaporation
And amount of heat, also result in the waste of chemicals and the energy.
Summary of the invention
It is an object of the invention to overcome the above shortcoming, the evaporation situation of chemical conversion tank liquor is improved, is used
Two or more diameters PPH floating ball, uniformly dispersing inhibit the evaporation of chemical conversion tank liquor on tank liquor surface.It is inclined to improve Waste Acid From Hua Cheng Foil performance
Difference, while reducing the waste of chemicals and the energy.
The purpose of the present invention is achieved through the following technical solutions:A kind of improvement aluminium electrolutic capacitor is inclined with Waste Acid From Hua Cheng Foil performance
The method of difference, steps are as follows:Using the PPH floating ball of two or more diameters, it is evenly distributed in aluminium electrolutic capacitor electrolytic bath
On liquid liquid level, small diameter floating ball fills the gap between larger diameter floating ball, guarantees that 90% of liquid level or more is covered by floating ball,
Inhibit the evaporation of chemical conversion tank liquor at high temperature, improves chemical conversion tank liquor temperature and ingredient stability, improve aluminium electrolutic capacitor
At foil head and the tail deviation.
Preferably, floating ball has eccentric structure, and the deviation of gravity center centre of sphere generates phase when electrode foil is in contact with floating ball
To rolling, guarantee that floating ball will not generate scratch to aluminium foil, while floating ball will not overturn rolling, the tank liquor that will not will be adhered under floating ball
It is exposed in upper air, inhibits tank liquor evaporation.
Preferably, floating ball diameter is two kinds, respectively 10 cm and φ 2cm of φ.
Preferably, floating ball diameter is three kinds, respectively 10 4 cm and φ 1cm of cm, φ of φ.
In conclusion the present invention has the following advantages that:Using two or more diameters PPH floating ball, uniformly dispersing is in tank liquor
Surface inhibits the evaporation of chemical conversion tank liquor.Improve Waste Acid From Hua Cheng Foil aberrations in property, while reducing the waste of chemicals and the energy.
Specific embodiment
In order to deepen the understanding of the present invention, the present invention will be described in further detail with reference to the examples below, the embodiment
For explaining only the invention, it is not intended to limit the scope of the present invention..
The present invention provides a kind of improvement aluminium electrolutic capacitor methods of Waste Acid From Hua Cheng Foil aberrations in property, and steps are as follows:It uses
The PPH of two or more diameters(Homopolypropylene)Floating ball, can bear the chemical conversion acidity of tank liquor, hot environment and it is indeformable.?
Even is dispersed on aluminium electrolutic capacitor chemical conversion tank liquor liquid level, and small diameter floating ball fills the gap between larger diameter floating ball,
Guarantee that 90% or more of liquid level is covered by floating ball, inhibits the evaporation of chemical conversion tank liquor at high temperature, improve chemical conversion tank liquor temperature and ingredient
Stability improves aluminium electrolutic capacitor Waste Acid From Hua Cheng Foil head and the tail deviation.
Floating ball has eccentric structure, and the deviation of gravity center centre of sphere floats on chemical conversion tank liquor liquid level similar to tumbler, works as electrode
When foil is in contact with floating ball, relative rolling is generated, guarantees that floating ball will not generate scratch to aluminium foil, while floating ball will not overturn rolling
It is dynamic, the tank liquor adhered under floating ball will not be exposed in upper air, inhibit tank liquor evaporation.
Embodiment 1:Floating ball diameter is two kinds, and respectively 10 cm and φ 2cm of φ is evenly distributed in aluminium electrolutic capacitor
It is melted on tank liquor liquid level, carries out the chemical conversion of ammonium adipate system, chemical synthesis technology remains unchanged.
Embodiment 2:Floating ball diameter is three kinds, respectively 10 4 cm and φ 1cm of cm, φ of φ, is evenly distributed in aluminium electroloysis
Capacitor is melted on tank liquor liquid level, carries out the chemical conversion of ammonium adipate system, and chemical synthesis technology remains unchanged.
6 capacity scattered error correlation data results of chemical conversion electrode foil head and the tail of present invention chemical conversion electrode foil and prior art are such as
Under:
As can be seen from the comparison result, significant using chemical conversion electrode foil 6 capacity tolerances of head and the tail of chemical synthesis technology output of the present invention
Improve, by original 5% or so, is improved to 3.5% or so.
Claims (4)
1. a kind of method for improving aluminium electrolutic capacitor Waste Acid From Hua Cheng Foil aberrations in property, it is characterised in that:Steps are as follows:Use two kinds
Or the PPH floating ball of multiple diameter, be evenly distributed in aluminium electrolutic capacitor chemical conversion tank liquor liquid level on, small diameter floating ball filling compared with
Gap between major diameter floating ball guarantees that 90% of liquid level or more is covered by floating ball, inhibits the evaporation of chemical conversion tank liquor at high temperature,
Chemical conversion tank liquor temperature and ingredient stability are improved, aluminium electrolutic capacitor Waste Acid From Hua Cheng Foil head and the tail deviation is improved.
2. a kind of method for improving aluminium electrolutic capacitor Waste Acid From Hua Cheng Foil aberrations in property according to claim 1, feature exist
In:The floating ball has eccentric structure, and the deviation of gravity center centre of sphere generates relative rolling when electrode foil is in contact with floating ball, guarantees
Floating ball will not generate scratch to aluminium foil, while floating ball will not overturn rolling, the tank liquor that adhered under floating ball will not be exposed to top
In air, inhibit tank liquor evaporation.
3. a kind of method for improving aluminium electrolutic capacitor Waste Acid From Hua Cheng Foil aberrations in property according to claim 2, feature exist
In:The floating ball diameter is two kinds, respectively 10 cm and φ 2cm of φ.
4. a kind of method for improving aluminium electrolutic capacitor Waste Acid From Hua Cheng Foil aberrations in property according to claim 2, feature exist
In:The floating ball diameter is three kinds, respectively 10 4 cm and φ 1cm of cm, φ of φ.