CN108724453A - A kind of processing method of self-luminous cement shaft tower - Google Patents

A kind of processing method of self-luminous cement shaft tower Download PDF

Info

Publication number
CN108724453A
CN108724453A CN201810394554.2A CN201810394554A CN108724453A CN 108724453 A CN108724453 A CN 108724453A CN 201810394554 A CN201810394554 A CN 201810394554A CN 108724453 A CN108724453 A CN 108724453A
Authority
CN
China
Prior art keywords
parts
chalazie
shaft tower
cement
added
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201810394554.2A
Other languages
Chinese (zh)
Inventor
李光海
赵宏伟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HEFEI HAIYIN TOWER CO Ltd
Original Assignee
HEFEI HAIYIN TOWER CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HEFEI HAIYIN TOWER CO Ltd filed Critical HEFEI HAIYIN TOWER CO Ltd
Priority to CN201810394554.2A priority Critical patent/CN108724453A/en
Publication of CN108724453A publication Critical patent/CN108724453A/en
Pending legal-status Critical Current

Abstract

The present invention relates to electric force pole tower technical fields, specifically disclose a kind of processing method of self-luminous cement shaft tower, include the following steps:Step 1, the manufacture of steel reinforcement cage;Step 2, the preparation of concrete;Step 3, molding;Step 4, drying;Step 5, extexine coating;Step 6, luminescent layer manufacture.The present invention overcomes the deficiencies in the prior art, in existing cement shaft tower outer surface, luminescent layer is set, luminescent layer is combined using luminescent powder and chalazie, it is aided with 191 resins, curing agent, accelerating agent and styrene, daytime, ultraviolet light was radiated at through chalazie on luminescent powder, and radiance are re-emitted out by night luminescent powder through chalazie, brightness is not faint dazzling, both too bright caused light pollution had been avoided, has influenced the ecological balance, and there is good prompting effect.

Description

A kind of processing method of self-luminous cement shaft tower
Technical field
The present invention relates to electric force pole tower technical fields, particularly belong to a kind of processing method of self-luminous cement shaft tower.
Background technology
Shaft tower is one of the basic equipment in overhead distribution, can be divided into rod, cement pole and metal by material used Three kinds of bar.Cement pole has many advantages, such as that service life is long, and maintenance workload is small, and use is relatively broad.Using most in cement pole Be dial tip bar, taper is generally 1/75, is divided into regular reinforcement mixed mud bar and prestressing force steel bar mixed mud bar.
Wherein existing part of cement shaft tower is arranged in the both sides of road, is no street lamp in some remote roads that are less than , there are some potential safety problemss for the vehicle of traveling for the cement shaft tower for being arranged in both sides of the road.
Invention content
The object of the present invention is to provide a kind of processing methods of self-luminous cement shaft tower, overcome the prior art not Luminescent layer is arranged in existing cement shaft tower outer surface in foot, and luminescent layer is combined using luminescent powder and chalazie, is aided with 191 trees Fat, curing agent, accelerating agent and styrene, daytime, ultraviolet light was radiated at through chalazie on luminescent powder, and night luminescent powder is by radiance It re-emitting out through chalazie, brightness is not faint dazzling, has both avoided too bright caused light pollution, has influenced the ecological balance, There is good prompting effect again.
To solve the above problems, the technical solution used in the present invention is as follows:
A kind of processing method of self-luminous cement shaft tower, includes the following steps:
Step 1, the manufacture of steel reinforcement cage:Certain length will be cut into after bar straightening first, by welding manufacture at reinforcing bar Then steel reinforcement cage is put into punching block female die by cage;
Step 2, the preparation of concrete:Concrete is stirred into after sand, rubble, cement and water are mixed, is then poured onto punching block In female die, finally punching block upper mold section is closed on punching block female die;
Step 3, molding:The punching block molded after pouring is placed into centrifugation apparatus, centrifugal forming, finally uses steam Sizing, after demould, obtain semi-finished product cement pole;
Step 4, drying:Semi-finished product cement pole is placed at shady and cool ventilation and is dried;
Step 5, extexine coating:First 191 resins are added in container, luminescent powder is then added, are added after stirring evenly Enter curing agent and chalazie, styrene is added after stirring evenly and is diluted, accelerating agent is added after stirring evenly, after being sufficiently stirred;
Step 6, luminescent layer manufacture:Prepared appearance coating is uniformly applied to the cement rod outer surface dried, is waited for certainly After so solidification is dry, surface grinding and buffing is carried out.
Further, step 5 China and foreign countries surface coating material is made from the following raw materials in parts by weight:191 resins 160~210 Part, 40~100 parts of luminescent powder, 90~120 parts of curing agent, 45~60 parts of accelerating agent, 200~360 parts of chalazie, styrene 90~ 110 parts.
Further, step 5 China and foreign countries surface coating material is made from the following raw materials in parts by weight:191 190 parts of resins, noctilucence 50 parts of powder, 100 parts of curing agent, 50 parts of accelerating agent, 280 parts of chalazie, 100 parts of styrene.
Compared with prior art, implementation result of the invention is as follows by the present invention:
Luminescent layer is arranged in existing cement shaft tower outer surface in a kind of processing method of self-luminous cement shaft tower of the present invention, Luminescent layer is combined using luminescent powder and chalazie, is aided with 191 resins, curing agent, accelerating agent and styrene, daytime, ultraviolet light was saturating Chalazie to be crossed to be radiated on luminescent powder, radiance are re-emitted out by night luminescent powder through chalazie, and brightness is not faint dazzling, Both too bright caused light pollution had been avoided, has influenced the ecological balance, and there is good prompting effect.
Specific implementation mode
With reference to embodiment, the invention will be further described, but the present invention is not limited to these instances, and is being de- Under the premise of from present inventive concept, carried out by it is any improvement be within the scope of the present invention.
A kind of processing method of self-luminous cement shaft tower of the present invention, includes the following steps:
Step 1, the manufacture of steel reinforcement cage:Certain length will be cut into after bar straightening first, by welding manufacture at reinforcing bar Then steel reinforcement cage is put into punching block female die by cage;
Step 2, the preparation of concrete:Concrete is stirred into after sand, rubble, cement and water are mixed, is then poured onto punching block In female die, finally punching block upper mold section is closed on punching block female die;
Step 3, molding:The punching block molded after pouring is placed into centrifugation apparatus, centrifugal forming, finally uses steam Sizing, after demould, obtain semi-finished product cement pole;
Step 4, drying:Semi-finished product cement pole is placed at shady and cool ventilation and is dried;
Step 5, extexine coating:First 191 resins are added in container, luminescent powder is then added, are added after stirring evenly Enter curing agent and chalazie, styrene is added after stirring evenly and is diluted, accelerating agent is added after stirring evenly, after being sufficiently stirred;
Step 6, luminescent layer manufacture:Prepared appearance coating is uniformly applied to the cement rod outer surface dried, is waited for certainly After so solidification is dry, surface grinding and buffing is carried out.
Further, step 5 China and foreign countries surface coating material is made from the following raw materials in parts by weight:191 resins 160~210 Part, 40~100 parts of luminescent powder, 90~120 parts of curing agent, 45~60 parts of accelerating agent, 200~360 parts of chalazie, styrene 90~ 110 parts.
Further, step 5 China and foreign countries surface coating material is made from the following raw materials in parts by weight:191 190 parts of resins, noctilucence 50 parts of powder, 100 parts of curing agent, 50 parts of accelerating agent, 280 parts of chalazie, 100 parts of styrene.
Above content is only to present inventive concept example and explanation, affiliated those skilled in the art couple Described specific embodiment does various modifications or additions or substitutes by a similar method, without departing from invention Conceive or beyond the scope defined by this claim, is within the scope of protection of the invention.

Claims (3)

1. a kind of processing method of self-luminous cement shaft tower, it is characterised in that:Include the following steps:
Step 1, the manufacture of steel reinforcement cage:Certain length will be cut into after bar straightening first, by welding manufacture at reinforcing bar Then steel reinforcement cage is put into punching block female die by cage;
Step 2, the preparation of concrete:Concrete is stirred into after sand, rubble, cement and water are mixed, is then poured onto punching block In female die, finally punching block upper mold section is closed on punching block female die;
Step 3, molding:The punching block molded after pouring is placed into centrifugation apparatus, centrifugal forming, finally uses steam Sizing, after demould, obtain semi-finished product cement pole;
Step 4, drying:Semi-finished product cement pole is placed at shady and cool ventilation and is dried;
Step 5, extexine coating:First 191 resins are added in container, luminescent powder is then added, are added after stirring evenly Enter curing agent and chalazie, styrene is added after stirring evenly and is diluted, accelerating agent is added after stirring evenly, after being sufficiently stirred;
Step 6, luminescent layer manufacture:Prepared appearance coating is uniformly applied to the cement rod outer surface dried, is waited for certainly After so solidification is dry, surface grinding and buffing is carried out.
2. a kind of processing method of self-luminous cement shaft tower according to claim 1, it is characterised in that:In the step 5 Appearance coating is made from the following raw materials in parts by weight:191 160~210 parts of resins, 40~100 parts of luminescent powder, curing agent 90~ 120 parts, 45~60 parts of accelerating agent, 200~360 parts of chalazie, 90~110 parts of styrene.
3. a kind of processing method of self-luminous cement shaft tower according to claim 1, it is characterised in that:In the step 5 Appearance coating is made from the following raw materials in parts by weight:191 190 parts of resins, 50 parts of luminescent powder, 100 parts of curing agent, accelerating agent 50 Part, 280 parts of chalazie, 100 parts of styrene.
CN201810394554.2A 2018-04-27 2018-04-27 A kind of processing method of self-luminous cement shaft tower Pending CN108724453A (en)