CN108715691A - Environmental-friendly construction material - Google Patents
Environmental-friendly construction material Download PDFInfo
- Publication number
- CN108715691A CN108715691A CN201810623780.3A CN201810623780A CN108715691A CN 108715691 A CN108715691 A CN 108715691A CN 201810623780 A CN201810623780 A CN 201810623780A CN 108715691 A CN108715691 A CN 108715691A
- Authority
- CN
- China
- Prior art keywords
- parts
- construction material
- environmental
- water
- friendly construction
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
The invention discloses a kind of environmental-friendly construction materials.The environmental-friendly construction material is made of following components:Rubber grain, coal ash powder, quick lime, zirconium dioxide, xanthans, peppermint, dimethyl ester, foam;Remaining is water.The parts by weight of said components are:10-15 parts of rubber grain, 20-22 parts of coal ash powder, 8-10 parts of quick lime, 10-12 parts of zirconium dioxide, 7-16 parts of xanthans, 18-25 parts of peppermint, 6-12 parts of dimethyl ester, 5-8 parts of foam;Remaining is water.The object of the present invention is to provide a kind of extension construction material service lifes, environmentally protective construction material, and not only water absorption rate is high, fire-retardant rate is high, intensity is high, but also it also has the function of stronger insulation.
Description
Technical field
The present invention relates to building material field, more particularly to a kind of environmental-friendly construction material.
Background technology
Currently, the material used in building often uses cement, concrete, these are easy to pollute the environment, and it
Water absorption rate, intensity, fire-retardant rate all be not so good as ideal, influence monolithic architecture quality.Present various countries, area all advocating environment protection sections
Can, in terms of building, it is desirable to be able to develop a kind of more preferable effect, more preferably quality, environmentally friendly construction material.
Invention content
The technical solution adopted by the present invention to solve the technical problems is:A kind of environmental-friendly construction material, it is characterized in that:The ring
Construction material is protected to be made of following components:Rubber grain, coal ash powder, quick lime, zirconium dioxide, xanthans, peppermint, fumaric acid two
Ester, foam;Remaining is water.The parts by weight of said components are:10-15 parts of rubber grain, 20-22 parts of coal ash powder, quick lime 8-
10 parts, 10-12 parts of zirconium dioxide, 7-16 parts of xanthans, 18-25 parts of peppermint, 6-12 parts of dimethyl ester, 5-8 parts of foam;Remaining
For water.
The beneficial effects of the invention are as follows:The object of the present invention is to provide a kind of extension construction material service life, green rings
The construction material of guarantor, not only water absorption rate is high, fire-retardant rate is high, intensity is high, but also it also has the function of stronger insulation.
Specific implementation mode
Specific embodiment:A kind of environmental-friendly construction material, it is characterized in that:The environmental-friendly construction material is made of following components:Rubber
Glue particle, coal ash powder, quick lime, zirconium dioxide, xanthans, peppermint, dimethyl ester, foam;Remaining is water.Said components
Parts by weight are:10-15 parts of rubber grain, 20-22 parts of coal ash powder, 8-10 parts of quick lime, 10-12 parts of zirconium dioxide, xanthans
7-16 parts, 18-25 parts of peppermint, 6-12 parts of dimethyl ester, 5-8 parts of foam;Remaining is water.
The beneficial effects of the invention are as follows:The object of the present invention is to provide a kind of extension construction material service life, green rings
The construction material of guarantor, not only water absorption rate is high, fire-retardant rate is high, intensity is high, but also it also has the function of stronger insulation.
Obviously, the above embodiments are merely examples for clarifying the description, and does not limit the embodiments.It is right
For those of ordinary skill in the art, can also make on the basis of the above description it is other it is various forms of variation or
It changes.There is no necessity and possibility to exhaust all the enbodiments.And it is extended from this it is obvious variation or
It changes still within the protection scope of the invention.
Claims (1)
1. a kind of environmental-friendly construction material, it is characterized in that:The environmental-friendly construction material is made of following components:Rubber grain, coal ash powder,
Quick lime, zirconium dioxide, xanthans, peppermint, dimethyl ester, foam;Remaining is water.The parts by weight of said components are:Rubber
10-15 parts of glue particle, 20-22 parts of coal ash powder, 8-10 parts of quick lime, 10-12 parts of zirconium dioxide, 7-16 parts of xanthans, peppermint 18-
25 parts, 6-12 parts of dimethyl ester, 5-8 parts of foam;Remaining is water.