CN108676415A - A kind of water-fast indoor wall alignment material thick with quick-drying heap, neutral - Google Patents
A kind of water-fast indoor wall alignment material thick with quick-drying heap, neutral Download PDFInfo
- Publication number
- CN108676415A CN108676415A CN201810914042.4A CN201810914042A CN108676415A CN 108676415 A CN108676415 A CN 108676415A CN 201810914042 A CN201810914042 A CN 201810914042A CN 108676415 A CN108676415 A CN 108676415A
- Authority
- CN
- China
- Prior art keywords
- water
- kilograms
- quick
- alignment material
- heap
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of indoor wall alignment material thick with quick-drying heap, neutrality is water-fast, required raw material includes:0.4 kilogram of 2200 kilograms of tap water, 400 kilograms of gypsum, 600 kilograms of coarse whiting, 3.5 kilograms of cellulose, 3 kilograms of latex powder and retarder;Wherein, the gypsum is semi-hydrated gypsum, desulfurated plaster and ardealite.Compared with prior art, the present invention, which discloses, is beneficial in that:It solves the phenomenon that existing wall alignment material accumulation of salt in the surface soil, nose of choking, polishing dust easily cause skin allergy, solves existing wall alignment material batch and scrape the disadvantage for being difficult to that heap is thick, the dry and hard time is long, not water-fast;The characteristics of heat-insulated, fire-retardant, lightweight, heat preservation, meets environmentally friendly, the energy-efficient policy of country's promotion and solves the problems, such as building load-bearing and fire-proof and thermal-insulation problem, neutrality, heap thickness, quick-drying, the advantages of allow worker is easy for construction, saves the time, effectively shorten the construction period.
Description
Technical field
The present invention relates to structure material technical fields, more particularly to a kind of to have quick-drying heap thick, neutral resistance to
The indoor wall alignment material of water.
Background technology
Existing indoor decoration wall body leveling putty has neutral " 821 putty " than more typical, the putty batch scrape to fill thick cracking,
Drying time is slow, remitted its fury occurs for easy and basic products and batch scrapes difficult reaction, and has insufficient strength, not water-fast etc.
Disadvantage, should be the disadvantage is that because packing material main component be coarse whiting, and additive is HPMC, CMC and@starch, and HPMC and CMC are main
Play water conservation, thickening power, it is ensured that performance is scraped in criticizing for putty, but drying time is slow;@starch plays adhesion strength or so, but strong
Degree is weaker and not water-fast.
Another alkalinity putty is also water proof putty, this product pH value=14 reaches highly basic range, does emulsion paint and do not do
The alkali-resistant primer meeting accumulation of salt in the surface soil, easy to shell of constructing on woodwork and Etta's plate, polishing dust be easy to cause skin allergy.Alkalinity is greasy
It is coarse whiting 75%, grey calcium 25% that sub- disadvantage, which is filled primarily with ingredient, and coarse whiting does not have intensity, grey calcium to have certain water resistance and intensity, still
The characteristic of highly basic causes the phenomenon that emulsion paint accumulation of salt in the surface soil and skin allergy.
Therefore, how to provide one kind having environmentally friendly, heat-insulated, fire-retardant, lightweight, water-fast, heat preservation, neutrality, heap thickness, quick-drying, applies
It is those skilled in the art that work is convenient, saves the water-fast indoor wall alignment material thick with quick-drying heap, neutral of time feature
The problem of urgent need to resolve.
Invention content
In view of this, the present invention provides one kind have environmentally friendly, heat-insulated, fire-retardant, lightweight, water-fast, heat preservation, neutral, heap thickness,
Quick-drying, water-fast indoor wall alignment material thick with quick-drying heap, neutral easy for construction, saving time feature.
To achieve the above object, the present invention provides the following technical solutions:
A kind of water-fast indoor wall alignment material thick with quick-drying heap, neutral, required raw material include:Tap water, gypsum, again
Calcium, cellulose, latex powder and retarder;Wherein, the gypsum is semi-hydrated gypsum, desulfurated plaster and ardealite.
Preferably, in a kind of above-mentioned water-fast indoor wall alignment material thick with quick-drying heap, neutral, required raw material is pressed
It is formed according to following proportioning:2200 kilograms of tap water, 400 kilograms of gypsum, 600 kilograms of coarse whiting, 3.5 kilograms of cellulose, latex powder 3 are public
Jin, 0.4 kilogram of retarder.
Preferably, in a kind of above-mentioned water-fast indoor wall alignment material thick with quick-drying heap, neutral, construction equipment packet
It includes:Stainless scraper plate, grey knife, charging basket, stirring rod, electric blender, levelling ruler.
Preferably, in a kind of above-mentioned water-fast indoor wall alignment material thick with quick-drying heap, neutral, Specific construction side
Method is:1, check that formation level must be firm;2, bucket is packed into tap water;3, it is slowly added into fast painting powder stirring 10 minutes
(Tap water:Powder=1:2.5);4, paste is stirred into can be used.
It can be seen via above technical scheme that compared with prior art, the present invention, which discloses, to be beneficial in that:
It solves the phenomenon that existing wall alignment material accumulation of salt in the surface soil, nose of choking, polishing dust easily cause skin allergy, solves existing
Have the shortcomings that wall alignment material batch is scraped and is difficult to that heap is thick, the dry and hard time is not long, water-fast;The characteristics of heat-insulated, fire-retardant, lightweight, heat preservation
Meet environmentally friendly, the energy-efficient policy of country's promotion and solves the problems, such as building load-bearing and fire-proof and thermal-insulation problem, neutral, heap thickness,
Quick-drying, the advantages of allow worker is easy for construction, saves the time, effectively shorten the construction period.
Specific implementation mode
Below in conjunction with the embodiment of the present invention, technical scheme in the embodiment of the invention is clearly and completely described,
Obviously, described embodiments are only a part of the embodiments of the present invention, instead of all the embodiments.Based in the present invention
Embodiment, every other embodiment obtained by those of ordinary skill in the art without making creative efforts, all
Belong to the scope of protection of the invention.
The embodiment of the invention discloses one kind to have environmentally friendly, heat-insulated, fire-retardant, lightweight, water-fast, heat preservation, neutrality, heap thick, fast
Water-fast indoor wall alignment material thick with quick-drying heap, neutral that is dry, easy for construction, saving time feature.
A kind of water-fast indoor wall alignment material thick with quick-drying heap, neutral disclosed by the invention is please referred to, it is specific to wrap
It includes:
A kind of water-fast indoor wall alignment material thick with quick-drying heap, neutral, required raw material include:Tap water, gypsum, again
Calcium, cellulose, latex powder and retarder;Wherein, the gypsum is semi-hydrated gypsum, desulfurated plaster and ardealite.
In order to advanced optimize above-mentioned technical proposal, required raw material is formed according to following proportioning:2200 kilograms of tap water, stone
400 kilograms of cream, 600 kilograms of coarse whiting, 3.5 kilograms of cellulose, 3 kilograms of latex powder, 0.4 kilogram of retarder.
In order to advanced optimize above-mentioned technical proposal, construction equipment includes:Stainless scraper plate, grey knife, charging basket, stirring rod, electricity
Dynamic blender, levelling ruler.
In order to advanced optimize above-mentioned technical proposal, concrete construction method is:1, check that formation level must be firm;2, it contains
Charging basket is packed into tap water;3, it is slowly added into fast painting powder stirring 10 minutes(Tap water:Powder=1:2.5);4, paste is stirred into i.e.
It can be used.
Each embodiment is described by the way of progressive in this specification, the highlights of each of the examples are with other
The difference of embodiment, just to refer each other for identical similar portion between each embodiment.For device disclosed in embodiment
For, since it is corresponded to the methods disclosed in the examples, so description is fairly simple, related place is said referring to method part
It is bright.
The foregoing description of the disclosed embodiments enables those skilled in the art to implement or use the present invention.
Various modifications to these embodiments will be apparent to those skilled in the art, as defined herein
General Principle can be realized in other embodiments without departing from the spirit or scope of the present invention.Therefore, of the invention
It is not intended to be limited to the embodiments shown herein, and is to fit to and the principles and novel features disclosed herein phase one
The widest range caused.
Claims (4)
1. a kind of water-fast indoor wall alignment material thick with quick-drying heap, neutral, required raw material include:Tap water, gypsum, again
Calcium, cellulose, latex powder and retarder;Wherein, the gypsum is semi-hydrated gypsum, desulfurated plaster and ardealite.
2. a kind of water-fast indoor wall alignment material thick with quick-drying heap, neutral according to claim 1, feature exist
In required raw material is formed according to following proportioning:2200 kilograms of tap water, 400 kilograms of gypsum, 600 kilograms of coarse whiting, cellulose 3.5
Kilogram, 3 kilograms of latex powder, 0.4 kilogram of retarder.
3. a kind of water-fast indoor wall alignment material thick with quick-drying heap, neutral according to claim 1, feature exist
In construction equipment includes:Stainless scraper plate, grey knife, charging basket, stirring rod, electric blender, levelling ruler.
4. a kind of water-fast indoor wall alignment material thick with quick-drying heap, neutral according to claim 1, feature exist
In concrete construction method is:1, check that formation level must be firm;2, bucket is packed into tap water;3, it is slowly added into fast dusting
Material stirring 10 minutes(Tap water:Powder=1:2.5);4, paste is stirred into can be used.