CN108381055A - 一种便于弯折的焊条 - Google Patents
一种便于弯折的焊条 Download PDFInfo
- Publication number
- CN108381055A CN108381055A CN201810405898.9A CN201810405898A CN108381055A CN 108381055 A CN108381055 A CN 108381055A CN 201810405898 A CN201810405898 A CN 201810405898A CN 108381055 A CN108381055 A CN 108381055A
- Authority
- CN
- China
- Prior art keywords
- bending
- welding rod
- convenient
- welding
- block
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供了一种便于弯折的焊条,其特征在于,所述便于弯折的焊条包括焊芯、包覆于所述焊芯的覆层结构,所述覆层结构由直线排列的覆块组成,所述覆块之间留有间隙,所述间隙的宽度为1~3mm。本发明的有益效果:在弯折的过程中不会掉渣,便于焊工进行多元化的焊接操作。
Description
技术领域
本发明涉及焊接耗材,尤其涉及一种便于弯折的焊条。
背景技术
一般情况下焊条为直的,可以直接拿来进行焊接,但是面对不好触及的拾取,焊工常常会巧妙的将直焊条进行折弯,弯曲的焊条更加便于触及犄角旮旯位置。
焊条在焊接的过程中对其进行弯折能便于焊接死角位置。问题在于,在将焊条折弯的过程中就会在折弯的位置焊条表面包覆的药渣脱落,使得焊条失效,从而影响焊接质量。
发明内容
本发明克服背景技术的不足提供了一种便于弯折的焊条,设计开发本产品的目的是:在焊工进行焊接的过程中能随意对焊条进行弯折操作,在弯折的过程中不会掉渣,便于焊工进行多元化的焊接操作。
本发明提供了下述技术方案:一种便于弯折的焊条,其特征在于,所述便于弯折的焊条包括焊芯1、包覆于所述焊芯1的覆层结构,所述覆层结构由直线排列的覆块2组成,所述覆块2之间留有间隙3,所述间隙3的的宽度为1~3mm。
在上述基础上,所述覆块2呈算盘珠状。
本发明的有益效果:包覆本所述焊条的药渣由覆块2组成,并且留有间隙3,间隙便于弯折过程中的补偿,本焊条独特的结构保护了焊条本身在弯折过程中不受损坏。在焊工进行焊接的过程中能随意对焊条进行弯折操作,在弯折的过程中不会掉渣,便于焊工进行多元化的焊接操作。
附图说明
图1是所述便于弯折的焊条直的状态的示意图。
图2是所述便于弯折的焊条被折弯的状态的示意图。
具体实施方式
以下结合附图与具体实施例对本发明作进一步描述。
图1、2中:焊芯1、覆块2、间隙3。
一种便于弯折的焊条,其特征在于,所述便于弯折的焊条包括焊芯1、包覆于所述焊芯1的覆层结构,所述覆层结构由直线排列的覆块2组成,所述覆块2之间留有间隙3,所述间隙3的的宽度为1~3mm。所述覆块2呈算盘珠状。
图1是所述便于弯折的焊条直的状态的示意图。当需要对焊条进行弯折时,弯折至如图2所示的状态,如图2即是所述便于弯折的焊条被折弯的状态的示意图。包覆本所述焊条的药渣由覆块2组成,并且留有间隙3,便于弯折过程中的补偿,本焊条独特的结构保护了焊条本身在弯折过程中不受损坏。
Claims (2)
1.一种便于弯折的焊条,其特征在于,所述便于弯折的焊条包括焊芯(1)、包覆于所述焊芯(1)的覆层结构,所述覆层结构由直线排列的覆块(2)组成,所述覆块(2)之间留有间隙(3),所述间隙(3)的的宽度为1~3mm。
2.根据权利要求1所述的一种便于弯折的焊条,其特征在于,所述覆块(2)呈算盘珠状。