CN108298829A - Glass plate painting line and lacquer spraying technique - Google Patents
Glass plate painting line and lacquer spraying technique Download PDFInfo
- Publication number
- CN108298829A CN108298829A CN201810107641.5A CN201810107641A CN108298829A CN 108298829 A CN108298829 A CN 108298829A CN 201810107641 A CN201810107641 A CN 201810107641A CN 108298829 A CN108298829 A CN 108298829A
- Authority
- CN
- China
- Prior art keywords
- station
- spray
- glass plate
- glass
- room
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to spraying equipment fields, more particularly to glass plate painting line and lacquer spraying technique, including spray booth, it is set in spray booth for carrying out pretreated preprocessing station to glass, it is connected to several spray stations of preprocessing station for painting in a side surface of glass or both side surface, it is connected to the post-processing station of spray station, it is connected to the discharge station of post-processing station, it is connected to the conveyer belt for transporting glass between each station, further include being set to the fixture that bearing glass is used on conveyer belt, drive the power station of conveyer belt movement;For the preprocessing station perpendicular to the line of several spray stations, the line of several spray stations is parallel to post-processing station.The present invention can improve the performance of glass plate, space availability ratio height, high degree of automation, the efficient high-quality and functional diversities of spray painting.
Description
Technical field
The present invention relates to spraying equipment fields, more particularly to glass plate painting line and lacquer spraying technique.
Background technology
Glass is amorphous inorganic non-metallic material, and usually with a variety of inorganic minerals, (such as quartz sand, borax, boric acid, weight are brilliant
Stone, barium carbonate, lime stone, feldspar, soda ash etc.) it is primary raw material, it additionally incorporates made of a small amount of auxiliary material.It it is main at
It is divided into silica and other oxides.
Since with excellent properties such as good perspectivity, translucency, sound-proofing, heat insulating abilities, it is each to be widely used in each row
Industry, such as electronics industry, glass are commonly used to make touch screen.
The glass plate for applying to touch screen, has the following deficiencies, on the one hand, in use, user passes through hand
Refer to touch-control touch screen to have been controlled, however usually there are the ingredients such as sweat, oil stain spot in finger, these ingredients are attached to touch
Screen surfaces cause touch screen unintelligible, when these penetrations enter inside touch screen, the electronic component of corrodible inside,
Touch screen job insecurity is caused, it is inconvenient to use.Second aspect, glass belong to fragile article, bad mechanical strength, fragment more cutting edge of a knife or a sword
Profit, fragment directive user can damage user, and security risk is big.The third aspect has in the visible light that touch screen is sent out big
The irregular shortwave blue light of amount, in particular, the high energy shortwave just between 360nm-500nm maximum to eye injury is blue
Light.It can be directed through the through retina of cornea, cause retina to generate free radicals, free radical can lead to retinal pigment epithelium
Apoptosis then allows photosensitive cell to lack nutrient so as to cause vision impairment, generates maculopathy, squeeze and shrink crystalline lens,
Myopia is caused to even result in this section macular disease, especially 450nm-460nm, injury is maximum.
Invention content
To solve the above problems, the present invention provides, a kind of performance that can improve glass plate, space availability ratio be high, automation journey
Degree is high, paint efficient high-quality and functional diversities glass plate painting line and lacquer spraying technique.
Technical solution is used by invention:Glass plate painting line, including spray booth, be set in spray booth and be used for
To glass carry out pretreated preprocessing station, be connected to preprocessing station for a side surface of glass or both side surface into
Several spray stations of row spray painting, the post-processing station for being connected to spray station, are connected to the discharge station of post-processing station,
Be connected to the conveyer belt that transporting glass is used between each station, further include be set to fixture on conveyer belt for bearing glass,
Drive the power station of conveyer belt movement;The preprocessing station perpendicular to several spray stations line, it is described several
The line of spray station is parallel to post-processing station.
To being further improved as the spray station includes spray room, the stream that conveyer belt sequentially passes through for above-mentioned technical proposal
One-storey house, baking room and cooling room, further include several spray guns being set in spray room;The conveyer belt is sprayed in the connection of bending
Room, levelling room, baking room and cooling room.
To being further improved as the fixture is plastic cement fixture, and is equipped between fixture and glass for above-mentioned technical proposal
Adhesive-layer.
To being further improved as temperature is 60 DEG C -90 DEG C in the baking room for above-mentioned technical proposal.
To being further improved as the spray station is anti-blue light spray station or enhancing Spray Painter for above-mentioned technical proposal
Position or oil rub resistance spray station, the spray station are four, respectively the first spray station, the second spray station, third spray
Lacquerer position and the 4th spray station.
To being further improved as first spray station, the second spray station, third Spray Painter for above-mentioned technical proposal
It is all provided with having heaters in the baking room of position, UV curing apparatus is equipped in the baking room of the 4th spray station.
To being further improved as the preprocessing station is equipped with dehumidifier, and post-processing station is equipped with for above-mentioned technical proposal
Heater.
Anti- blue light glass plate lacquer spraying technique includes using the glass plate spray painting production described in any one of claim 1-7
Line is sprayed, and includes a, pretreatment, b, several times spraying, c, post-processing and d, blanking successively.
Beneficial effects of the present invention are:
1, on the one hand, several spray stations are equipped with, can be sprayed in the one or both sides of glass plate according to different product characteristic
The paint with certain function is applied, to improve the performance of glass plate, such as anti-blue light, resistance to oily stain and resistance to falls impact resistance, function
Diversification.Second aspect shifts glass by conveyer belt between different station, and each spray station paints automatically, work
Make efficient.The third aspect is pre-processed before spray painting, is post-processed after spray painting, so that the glass plate after spraying can expire
Sufficient different manufacturers requirement, coating quality is good, applied widely.Fourth aspect, preprocessing station is perpendicular to several spray stations
Line, the line of several spray stations is parallel to post-processing station, and all stations are straggly to be distributed in spray booth, space utilization
Rate is high.
2, spray station includes spray room, levelling room, baking room and the cooling room that conveyer belt sequentially passes through, and further includes being set to
Several spray guns in spray room;The conveyer belt is in the connection spray room of bending, levelling room, baking room and cooling room.It is painting
Station first paints to glass by several spray guns in spray room, then carries out levelling so that paint is evenly applied to glass
Surface, then dried so that paint curing forms a tunic in glass surface, finally cools down, spray efficiency height, coating quality
It is good, one layer of uniform and stable functional film can be formed to improve the performance of glass in glass surface.
3, fixture is plastic cement fixture, will not be caused damages to glass plate, and coating quality is high, is equipped between fixture and glass viscous
Glue-line realizes being stably connected with for fixture and glass by adhesive-layer, is smoothed out convenient for what is subsequently sprayed, further ensures that spraying
Efficiency and coating quality.
4, the temperature of baking room is 60 DEG C -90 DEG C, and preferably 80 DEG C, temperature is too low to cause baking and curing effect poor, temperature
Du Taigao can cause plastic cement fixture to damage, and 80 DEG C of temperature, solidification effect is good at this time, and will not damage fixture.
5, spray station is anti-blue light spray station or enhancing spray station or oil rub resistance spray station, the spray station
It is four, respectively the first spray station, the second spray station, third spray station and the 4th spray station.It can be according to difference
Different spray stations is arranged in the requirement of product, and such as the first spray station sprays the anti-blue light paint of first layer, the second spray station spray the
Two layers of anti-blue light paint, third spray station spray the anti-blue light paint of third layer, and the 4th spray station is sprayed in another side surface of glass plate
Enhancing paint, is painted by four times, to improve the anti-blue light performance and mechanical strength of glass plate.As the first spray station sprays first layer
Anti- blue light paint, the second spray station spray the anti-blue light paint of the second layer, and third spray station is anti-in the spray of the second layer anti-blue light paint surface
Greasy dirt paint, the 4th spray station is painted in another side surface of glass plate spray enhancing paint by four times, to improve the anti-of glass plate
Blue light, resistance to oily stain and mechanical strength.
6, it is all provided with having heaters in the baking room of the first spray station, the second spray station, third spray station, described
It is equipped with UV curing apparatus in the baking room of four spray stations, is cured by UV curing apparatus after last side spray paint, cures
Effect is good, and can guarantee each layer function paint stabilization is attached to glass plate, and spraying effect is good.
7, preprocessing station is equipped with dehumidifier, and the moisture of glass surface is removed before being painted, convenient for subsequent paint
Uniform and stable, post-processing station is equipped with heater, is further cured, and solidification effect is good, can guarantee that each layer function paint is stablized
Be attached to glass plate, spraying effect is good.
8, anti-blue light glass plate lacquer spraying technique includes using the glass plate spray painting life described in any one of claim 1-7
Producing line is sprayed, and includes a, pretreatment, b, several times spraying, c, post-processing and d, blanking successively.Can according to different requirements,
The one or both sides of glass plate spray the different numbers of plies or different types of paint, preferably to improve performance, the space profit of glass plate
With rate height, high degree of automation, paint efficient high-quality and functional diversities.
Description of the drawings
Fig. 1 is the structural schematic diagram of the glass plate painting line of the present invention;
Fig. 2 is the structural schematic diagram of the spray station of the present invention.
Specific implementation mode
Invention is further described below in conjunction with attached drawing.
As depicted in figs. 1 and 2, it is the structure of the structural schematic diagram and spray station of the glass plate painting line of the present invention
Schematic diagram.
Glass plate painting line 100, including spray booth 110, be set in spray booth 110 for being located in advance to glass
The preprocessing station 120 of reason is connected to what preprocessing station 120 was used to paint in a side surface of glass or both side surface
Several spray stations 130, the post-processing station 140 for being connected to spray station 130 are connected to the blanking of post-processing station 140
Station 150 is connected to the conveyer belt 160 for transporting glass between each station, further includes being set on conveyer belt 160 for holding
Carry the fixture of glass, the power station that driving conveyer belt 160 moves;The preprocessing station 120 is perpendicular to several Spray Painter
The line of the line of position 130, several spray stations 130 is parallel to post-processing station 140.
Spray station 130 includes spray room 131, levelling room 132, baking room 133 and the cooling that conveyer belt 160 sequentially passes through
Room 134 further includes several spray guns 135 being set in spray room 131;The conveyer belt 160 is in the connection spray room of bending
131, levelling room 132, baking room 133 and cooling room 134.Spray gun 135 is preferably salt pan spray gun or Graco spray gun.
In spray station 130, first painted to glass by several spray guns 135 in spray room 131, then flowed
It is flat so that paint is evenly applied to glass surface, then is dried so that paint curing forms a tunic in glass surface, most
Postcooling, spray efficiency is high, coating quality is good, can form one layer of uniform and stable functional film in glass surface to improve glass
The performance of glass.
Fixture is plastic cement fixture, will not be caused damages to glass plate, and coating quality is high, and viscose glue is equipped between fixture and glass
Layer is realized being stably connected with for fixture and glass by adhesive-layer, is smoothed out convenient for what is subsequently sprayed, further ensures that spraying effect
Rate and coating quality.
The temperature of baking room 133 is 60 DEG C -90 DEG C, and preferably 80 DEG C, temperature is too low to cause baking and curing effect poor, temperature
Du Taigao can cause plastic cement fixture to damage, and 80 DEG C of temperature, solidification effect is good at this time, and will not damage fixture.
Spray station 130 is anti-blue light spray station 130 or enhancing spray station 130 or oil rub resistance spray station 130, institute
It is four to state spray station 130, respectively the first spray station 130a, the second spray station 130b, third spray station 130c
With the 4th spray station 130d.
First spray station 130a, the second spray station 130b, third spray station 130c baking room 133 in be all provided with
Having heaters, the baking room 133 of the 4th spray station 130d is interior to be equipped with UV curing apparatus, passes through UV after last side spray paint
Curing apparatus is cured, and solidification effect is good, and can guarantee each layer function paint stabilization is attached to glass plate, and spraying effect is good.
Preprocessing station 120 is equipped with dehumidifier, and the moisture of glass surface is removed before being painted, convenient for subsequent paint
Uniform and stable, post-processing station 140 is equipped with heater, is further cured, solidification effect is good, can guarantee that each layer function paint is steady
Fixed is attached to glass plate, and spraying effect is good.
Anti- blue light glass plate lacquer spraying technique includes using the glass plate spray painting production described in any one of claim 1-7
Line 100 is sprayed, and includes a, pretreatment, b, several times spraying, c, post-processing and d, blanking successively.Can according to different requirements,
The different numbers of plies or different types of paint are sprayed in the one or both sides of glass plate, preferably to improve performance, the space of glass plate
Utilization rate height, high degree of automation, paint efficient high-quality and functional diversities.
When being painted, in each spray station 130, conveyer belt passes through levelling room 132, baking room 133 and cooling room 134
Length and the time can according to the size of glass, thickness and spray painting require depending on.
On the one hand, several spray stations 130 are equipped with, it can be according to different product characteristic, in the one or both sides of glass plate
The paint with certain function is sprayed, to improve the performance of glass plate, such as anti-blue light, resistance to oily stain and resistance to falls impact resistance, work(
It can diversification.Second aspect shifts glass by conveyer belt 160 between different station, and each spray station 130 carries out automatically
Spray painting, work efficiency is high.The third aspect is pre-processed before spray painting, is post-processed after spray painting, so that the glass after spraying
Plate can meet different manufacturers requirement, and coating quality is good, applied widely.Fourth aspect, preprocessing station 120 is perpendicular to several
The line of the line of spray station 130, several spray stations 130 is parallel to post-processing station 140, straggly point of all stations
It is high to be distributed in spray booth 110, space availability ratio.
Embodiment one:
If there are four spray station 130, the first spray station 130a sprays the anti-blue light paint of first layer, the second spray station 130b
The anti-blue light paint of the second layer is sprayed, third spray station 130c sprays the anti-blue light paint of third layer, and the 4th spray station 130d sprays anti-blue light paint,
It is sprayed by four times so that glass plate has preferable anti-blue light effect.
Embodiment two:
If there are four spray station 130, the first spray station 130a sprays first layer oil rub resistance paint, the second spray station 130b
Second layer oil rub resistance paint is sprayed, third spray station 130c sprays third layer oil rub resistance paint, and the 4th spray station 130d sprays oil rub resistance paint,
It is sprayed by four times so that glass plate has preferable oil rub resistance effect.
Embodiment three:
If there are four spray station 130, the first spray station 130a spray first layer enhancing paints, the second spray station 130b sprays
Second layer enhancing paint, third spray station 130c spray third layer enhancing paints, the 4th spray station 130d spray the 4th layer of enhancing paint,
It is sprayed by four times, greatly strengthens the mechanical strength of glass plate, improve the impact resistance of glass plate.
Example IV:
If there are four spray station 130, the first spray station 130a sprays the anti-blue light paint of first layer, the second spray station 130b
The anti-blue light paint of the second layer is sprayed, third spray station 130c is to spray oil rub resistance paint, the 4th Spray Painter on the second layer anti-blue light paint surface
Position 130d is painted, to improve anti-blue light, the oil rub resistance of glass plate in another side surface of glass plate spray enhancing paint by four times
Property and mechanical strength.
The several embodiments invented above described embodiment only expresses, the description thereof is more specific and detailed, but not
It can therefore be construed as limiting the scope of the patent.It should be pointed out that for those of ordinary skill in the art,
Under the premise of not departing from inventive concept, various modifications and improvements can be made, these are all within the scope of protection of the present invention.
Therefore, the protection domain of patent of invention should be determined by the appended claims.
Claims (8)
1. glass plate painting line, it is characterised in that:Including spray booth, it is set in spray booth for being located in advance to glass
The preprocessing station of reason is connected to several for painting in a side surface of glass or both side surface of preprocessing station
Spray station, the post-processing station for being connected to spray station, be connected to post-processing station discharge station, be connected to each station it
Between be used for transporting glass conveyer belt, further include be set on conveyer belt for bearing glass fixture, driving conveyer belt movement
Power station;The preprocessing station is perpendicular to the line of several spray stations, the line of several spray stations
It is parallel to post-processing station.
2. glass plate painting line according to claim 1, it is characterised in that:The spray station include conveyer belt according to
The secondary spray room passed through, levelling room, baking room and cooling room, further include several spray guns being set in spray room;The conveyer belt
In the connection spray room of bending, levelling room, baking room and cooling room.
3. glass plate painting line according to claim 2, it is characterised in that:The fixture is plastic cement fixture, and is pressed from both sides
Adhesive-layer is equipped between tool and glass.
4. glass plate painting line according to claim 3, it is characterised in that:In the baking room temperature be 60 DEG C-
90℃。
5. glass plate painting line according to claim 4, it is characterised in that:The spray station paints for anti-blue light
Station or enhancing spray station or oil rub resistance spray station, the spray station are four, respectively the first spray station, second
Spray station, third spray station and the 4th spray station.
6. glass plate painting line according to claim 5, it is characterised in that:First spray station, the second spray
Lacquerer position, third spray station baking room in be all provided with having heaters, it is solid equipped with UV in the baking room of the 4th spray station
Change equipment.
7. glass plate painting line according to claim 6, it is characterised in that:The preprocessing station is equipped with dehumidifying
Device, post-processing station are equipped with heater.
8. anti-blue light glass plate lacquer spraying technique, it is characterised in that:Include using the glass plate described in any one of claim 1-7
Painting line is sprayed, and includes a, pretreatment, b, several times spraying, c, post-processing and d, blanking successively.