CN108044960A - A kind of dyeing of plastic plate - Google Patents
A kind of dyeing of plastic plate Download PDFInfo
- Publication number
- CN108044960A CN108044960A CN201711298514.XA CN201711298514A CN108044960A CN 108044960 A CN108044960 A CN 108044960A CN 201711298514 A CN201711298514 A CN 201711298514A CN 108044960 A CN108044960 A CN 108044960A
- Authority
- CN
- China
- Prior art keywords
- plastic plate
- toner
- dyeing
- aldehyde
- except
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to a kind of dyeings of plastic plate, it would be desirable to which the plastic plate of printing and dyeing is first mixed;Appropriate plastic plate is chosen to carry out playing colour table processing;When beating colour table, toner configuration first is carried out to the color that needs are printed and dyed, will carry out beating colour table by a certain percentage with plastic plate with the toner postponed, adjust the configuration of toner afterwards, be allowed to finally identical with the color for needing to print and dye;The weight for the total plastic plate printed and dyed as needed carries out proportional arrangement toner, and by total toner equivalent in multiple packaging bags;By the toner of each packaging bag correspond to therewith weight ratio plastic plate mix after be put into mixer and stir evenly;Plastic plate after stirring evenly is put into injection molding in injection molding machine;The plastic plate handled well, which is put into high steam, to be baked, and plastic plate is made to be not easy to fade;Plastic plate be put into except carried out in aldehyde pond except aldehyde handle.Present invention process is simple, reduces dyeing cost.
Description
Technical field
The present invention relates to plastic products technology field, it particularly relates to the dyeing of plastic plate.
Background technology
Plastics are a kind of plastic synthesis high molecular materials of tool.It is formd now with synthetic rubber, synthetic fibers
Indispensable three big synthetic material of daily life.Specifically, plastics are using natural or synthetic resin as main component, are added in
Various additives can mould under the conditions of certain temperature and pressure etc. and definite shape is made, and keep shape invariance at normal temperatures
Material.Plastic plate industry is the pillar industry of China's light industry.At present, the plastic plate industry faces opportunity to develop in China,
But many challenges can be also run into, it is leading that this, which is needed using market, enterprise, and government is being subject to policy guide, together to plastic plate
Power strides forward.The inherently simple resin of some plastics, such as polyethylene, polystyrene are known as one-component plastics.Some
Plastics, also containing other auxiliary materials, such as plasticizer, stabilizer, colorant, various fillers, claim in addition to synthetic resin
For multi-component plastics.The production of plastic plate for many years develops at high speed all over the world.And in order to obtain the modeling of different colours
Flitch material then needs to be processed.
The content of the invention
In view of this, the object of the present invention is to provide a kind of dyeing of plastic plate, to solve prior art printing and dyeing
Speed is slowly.
The present invention solves above-mentioned technical problem by the following technical programs:
A kind of dyeing of plastic plate, includes the following steps:
S1.5, the plastic plate for needing to print and dye first is mixed, carries out packing of weighing in a manner of quantitative afterwards;
S2, the appropriate plastic plate of selection carry out playing colour table processing;
S3, when beating colour table, toner configuration first is carried out to the color that needs are printed and dyed, by with the toner postponed with plastic plate by certain
Ratio carries out beating colour table, adjusts the configuration of toner afterwards, is allowed to finally identical with the color for needing to print and dye;
S4, the weight for the total plastic plate printed and dyed as needed carry out proportional arrangement toner, and total toner equivalent are mounted in
In multiple packaging bags;
S5, the toner of each packaging bag is corresponded to therewith be put into mixer after the plastic plate mixing of weight ratio stir it is equal
It is even;
S6, the plastic plate after stirring evenly is put into injection molding in injection molding machine;
S7, the plastic plate handled well are put into high steam and are baked, and plastic plate is made to be not easy to fade;
S8, after plastic plate cooling after be put into except carried out in aldehyde pond except aldehyde handle.
Often the weight of bag plastic plate is 1.56kg in the step 1.5.
Toner weight in the step 4 in each packaging bag is 1.5kg.
The weight ratio of toner and plastic plate is 1.5 in the step 5:400.
The temperature except aldehyde is 22 ~ 28 DEG C, except the time of aldehyde is 25 ~ 35min.
It is described except in aldehyde pond filled with removing aldehyde liquid, except aldehyde liquid is mixed by biological enzyme and medical stone, biological enzyme and wheat meal
The weight ratio of stone is 1.5:5.
The beneficial effects of the present invention are:Present invention process is simple, and it is convenient to prepare, and can quickly and effectively complete to print and dye, make
It is good with effect.The stamp of plastic plate, color and luster is bright and beautiful, and is not easy to fade.
Specific embodiment
In order to facilitate the understanding of those skilled in the art, below in conjunction with embodiment, the present invention will be further described.
Embodiment is only for example, not being limitation of the invention, the step of not illustrated in embodiment to the invention
It is prior art, is not described in detail herein.
Embodiment one
A kind of dyeing of plastic plate, includes the following steps:
S1.5, the plastic plate for needing to print and dye first is mixed, carries out packing of weighing in a manner of quantitative afterwards;
S2, the appropriate plastic plate of selection carry out playing colour table processing;
S3, when beating colour table, toner configuration first is carried out to the color that needs are printed and dyed, by with the toner postponed with plastic plate by certain
Ratio carries out beating colour table, adjusts the configuration of toner afterwards, is allowed to finally identical with the color for needing to print and dye;
S4, the weight for the total plastic plate printed and dyed as needed carry out proportional arrangement toner, and total toner equivalent are mounted in
In multiple packaging bags;
S5, the toner of each packaging bag is corresponded to therewith be put into mixer after the plastic plate mixing of weight ratio stir it is equal
It is even;
S6, the plastic plate after stirring evenly is put into injection molding in injection molding machine;
S7, the plastic plate handled well are put into high steam and are baked, and plastic plate is made to be not easy to fade;
S8, after plastic plate cooling after be put into except carried out in aldehyde pond except aldehyde handle.
Often the weight of bag plastic plate is 1.56kg in the step 1.5.
Toner weight in the step 4 in each packaging bag is 1.5kg.
The weight ratio of toner and plastic plate is 1.5 in the step 5:400.
The temperature except aldehyde is 22 DEG C, except the time of aldehyde is 25min.
It is described except in aldehyde pond filled with removing aldehyde liquid, except aldehyde liquid is mixed by biological enzyme and medical stone, biological enzyme and wheat meal
The weight ratio of stone is 1.5:5.
Present invention process is simple, and it is convenient to prepare, and can quickly and effectively complete to print and dye, and the stamp of plastic plate, color and luster is bright and beautiful,
And it is not easy to fade.
Embodiment one
A kind of dyeing of plastic plate, includes the following steps:
S1.5, the plastic plate for needing to print and dye first is mixed, carries out packing of weighing in a manner of quantitative afterwards;
S2, the appropriate plastic plate of selection carry out playing colour table processing;
S3, when beating colour table, toner configuration first is carried out to the color that needs are printed and dyed, by with the toner postponed with plastic plate by certain
Ratio carries out beating colour table, adjusts the configuration of toner afterwards, is allowed to finally identical with the color for needing to print and dye;
S4, the weight for the total plastic plate printed and dyed as needed carry out proportional arrangement toner, and total toner equivalent are mounted in
In multiple packaging bags;
S5, the toner of each packaging bag is corresponded to therewith be put into mixer after the plastic plate mixing of weight ratio stir it is equal
It is even;
S6, the plastic plate after stirring evenly is put into injection molding in injection molding machine;
S7, the plastic plate handled well are put into high steam and are baked, and plastic plate is made to be not easy to fade;
S8, after plastic plate cooling after be put into except carried out in aldehyde pond except aldehyde handle.
Often the weight of bag plastic plate is 1.56kg in the step 1.5.
Toner weight in the step 4 in each packaging bag is 1.5kg.
The weight ratio of toner and plastic plate is 1.5 in the step 5:400.
The temperature except aldehyde is 28 DEG C, except the time of aldehyde is 35min.
It is described except in aldehyde pond filled with removing aldehyde liquid, except aldehyde liquid is mixed by biological enzyme and medical stone, biological enzyme and wheat meal
The weight ratio of stone is 1.5:5.
Present invention process is simple, and it is convenient to prepare, and can quickly and effectively complete to print and dye, and the stamp of plastic plate, color and luster is bright and beautiful,
And it is not easy to fade.
Claims (6)
1. a kind of dyeing of plastic plate, it is characterised in that comprise the following steps:
S1.5, the plastic plate for needing to print and dye first is mixed, carries out packing of weighing in a manner of quantitative afterwards;
S2, the appropriate plastic plate of selection carry out playing colour table processing;
S3, when beating colour table, toner configuration first is carried out to the color that needs are printed and dyed, by with the toner postponed with plastic plate by certain
Ratio carries out beating colour table, adjusts the configuration of toner afterwards, is allowed to finally identical with the color for needing to print and dye;
S4, the weight for the total plastic plate printed and dyed as needed carry out proportional arrangement toner, and total toner equivalent are mounted in
In multiple packaging bags;
S5, the toner of each packaging bag is corresponded to therewith be put into mixer after the plastic plate mixing of weight ratio stir it is equal
It is even;
S6, the plastic plate after stirring evenly is put into injection molding in injection molding machine;
S7, the plastic plate handled well are put into high steam and are baked, and plastic plate is made to be not easy to fade;
S8, after plastic plate cooling after be put into except carried out in aldehyde pond except aldehyde handle.
2. the dyeing of the plastic plate as described in claim 1.5, it is characterised in that:Per plastic material in the step 1.5
The weight of plate is 1.56kg.
3. the dyeing of the plastic plate as described in claim 1.5, it is characterised in that:Each packaging bag in the step 4
In toner weight be 1.5kg.
4. the dyeing of the plastic plate as described in claim 1.5, it is characterised in that:Toner and plastics in the step 5
The weight ratio of plate is 1.5:400.
5. the dyeing of the plastic plate as described in claim 1.5, it is characterised in that:The temperature except aldehyde is 22 ~ 28
DEG C, except the time of aldehyde is 25 ~ 35min.
6. the dyeing of the plastic plate as described in claim 1.5, it is characterised in that:Described remove in aldehyde pond is filled with except aldehyde
Liquid, except aldehyde liquid is mixed by biological enzyme and medical stone, the weight ratio of biological enzyme and medical stone is 1.5:5.