CN107737811A - 一种铝合金导线拉制工艺 - Google Patents
一种铝合金导线拉制工艺 Download PDFInfo
- Publication number
- CN107737811A CN107737811A CN201710964630.4A CN201710964630A CN107737811A CN 107737811 A CN107737811 A CN 107737811A CN 201710964630 A CN201710964630 A CN 201710964630A CN 107737811 A CN107737811 A CN 107737811A
- Authority
- CN
- China
- Prior art keywords
- aluminium alloy
- alloy conductor
- wire
- drawing machine
- machine
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明是一种铝合金导线拉制工艺,包括的如下步骤:1)铝合金导线的拉制在一般的拉丝机上进行,制的范围在10~0.12mm;2)金属拉丝机基本上分成两类:滑动式拉丝机和非滑动式拉丝机;3)拉制10.00~2.00mm线径的导线多采用非滑动式拉丝机,拉制2.00mm以下线径的导线采用滑动式拉丝机。本发明所述一种铝合金导线拉制工艺,保持电缆的优良传输性能,还能有效地降低原材料的消耗,可使成本下降40%左右。
Description
技术领域
本发明涉及铝合金导线拉制领域,尤其涉及一种铝合金导线拉制工艺。
背景技术
铝合金导线应用于电力架空传输线已有近六十年的历史。这种铝合金主要基于铝-镁-硅,由于具有额定载流量大,损耗小、安装及维修简单等优点,使铝合金架空导线得到了广泛的应用。本文将详细介绍应用于CATV电缆外导体编织的铝合金导线的拉制工艺。
铝合金导线的制造工艺为:铸合金-浇铸及轧制成杆-固溶热处理-淬火-拉制-人工时效处理。
为此,设计一种铝合金导线拉制工艺,解决以上问题。
发明内容
本发明为克服以上不足,提供一种铝合金导线拉制工艺,包括的如下步骤:
1)铝合金导线的拉制在一般的拉丝机上进行,制的范围在10~0.12mm;
2)金属拉丝机基本上分成两类:滑动式拉丝机和非滑动式拉丝机;
3)拉制10.00~2.00mm线径的导线多采用非滑动式拉丝机,拉制2.00mm以下线径的导线采用滑动式拉丝机。
进一步,所述拉丝机的拉丝速度一般在10~30m/s,即600~1800m/min。
本发明的有益效果是:
本发明所述一种铝合金导线拉制工艺,保持电缆的优良传输性能,还能有效地降低原材料的消耗,可使成本下降40%左右。
具体实施方式
以下将结合本发明的实施例进行详细叙述。
一种铝合金导线拉制工艺,包括的如下步骤:
1)铝合金导线的拉制在一般的拉丝机上进行,制的范围在10~0.12mm;
2)金属拉丝机基本上分成两类:滑动式拉丝机和非滑动式拉丝机;
3)拉制10.00~2.00mm线径的导线多采用非滑动式拉丝机,拉制2.00mm以下线径的导线采用滑动式拉丝机。
进一步,所述拉丝机的拉丝速度一般在10~30m/s,即600~1800m/min。
以上所述仅是本发明的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本发明的保护范围。
Claims (2)
1.一种铝合金导线拉制工艺,其特征在于,包括的如下步骤:
1)铝合金导线的拉制在一般的拉丝机上进行,制的范围在10~0.12mm;
2)金属拉丝机基本上分成两类:滑动式拉丝机和非滑动式拉丝机;
3)拉制10.00~2.00mm线径的导线多采用非滑动式拉丝机,拉制2.00mm以下线径的导线采用滑动式拉丝机。
2.根据权利要求1所述的一种铝合金导线拉制工艺,其特征在于,所述拉丝机的拉丝速度一般在10~30m/s,即600~1800m/min。