CN107721285A - 一种更环保的混凝土配方 - Google Patents
一种更环保的混凝土配方 Download PDFInfo
- Publication number
- CN107721285A CN107721285A CN201711268653.8A CN201711268653A CN107721285A CN 107721285 A CN107721285 A CN 107721285A CN 201711268653 A CN201711268653 A CN 201711268653A CN 107721285 A CN107721285 A CN 107721285A
- Authority
- CN
- China
- Prior art keywords
- environmentally friendly
- concrete formulation
- friendly concrete
- water
- straw
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明是一种更环保的混凝土配方,配方中的原料按重量百分比组成分别是:水泥36‑38%,粉煤灰33‑35%,工业废渣25‑27%,磷渣17‑19%,稻草11‑13%,激发剂7‑11%,抗凝剂9‑11%,粘合剂12‑18%,水20‑24%,通过本方法制备的产品,成本低廉,较为环保。
Description
技术领域
本发明公开了一种更环保的混凝土配方。
背景技术
混凝土是指由胶凝材料将骨料胶结成整体的工程复合材料的统称,一般用于工程之中,市场上的混凝土性价比不高。
发明内容
针对上述现有技术存在的问题,本发明提供一种更环保的混凝土配方,环保性能更好,成本较低。
为了实现上述目的,本发明通过以下技术方案实现:一种更环保的混凝土配方,配方中的原料按重量百分比组成分别是:水泥36-38%,粉煤灰33-35%,工业废渣25-27%,磷渣17-19%,稻草11-13%,激发剂7-11%,抗凝剂9-11%,粘合剂12-18%,水20-24%。
有益效果:通过本方法制备的产品,成本较低,原料更环保。
具体实施方式
一种更环保的混凝土配方,配方中的原料按重量百分比组成分别是:水泥36-38%,粉煤灰33-35%,工业废渣25-27%,磷渣17-19%,稻草11-13%,激发剂7-11%,抗凝剂9-11%,粘合剂12-18%,水20-24%。
实施例1
一种更环保的混凝土配方,配方中的原料按重量百分比组成分别是:36%水泥,33%粉煤灰,25%工业废渣,17%磷渣,11%稻草,7%激发剂,9%抗凝剂,12%粘合剂,20%水,此时更环保的混凝土配方成本较低但不够稳定。
实施例2
一种更环保的混凝土配方,配方中的原料按重量百分比组成分别是:38%水泥,35%粉煤灰,27%工业废渣,19%磷渣,13%稻草,11%激发剂,11%抗凝剂,18%粘合剂,24%水,此时更环保的混凝土配方提高了稳定性,但是成本较高。
实施例3
一种更环保的混凝土配方,配方中的原料按重量百分比组成分别是:37%水泥,34%粉煤灰,26%工业废渣,18%磷渣,12%稻草,9%激发剂,10%抗凝剂,15%粘合剂,22%水,此时更环保的混凝土配方性价比更高。
Claims (4)
1.一种更环保的混凝土配方,其特征在于,配方中的原料按重量百分比组成分别是:水泥36-38%,粉煤灰33-35%,工业废渣25-27%,磷渣17-19%,稻草11-13%,激发剂7-11%,抗凝剂9-11%,粘合剂12-18%,水20-24%。
2.根据权利要求1所述的更环保的混凝土配方,其特征在于,配方中的原料按重量百分比组成分别是:36%水泥,33%粉煤灰,25%工业废渣,17%磷渣,11%稻草,7%激发剂,9%抗凝剂,12%粘合剂,20%水。
3.根据权利要求1所述的更环保的混凝土配方,其特征在于,配方中的原料按重量百分比组成分别是:38%水泥,35%粉煤灰,27%工业废渣,19%磷渣,13%稻草,11%激发剂,11%抗凝剂,18%粘合剂,24%水。
4.根据权利要求1所述的更环保的混凝土配方,其特征在于,配方中的原料按重量百分比组成分别是:37%水泥,34%粉煤灰,26%工业废渣,18%磷渣,12%稻草,9%激发剂,10%抗凝剂,15%粘合剂,22%水。