CN107696773A - A kind of noble metal letters and preparation method thereof - Google Patents

A kind of noble metal letters and preparation method thereof Download PDF

Info

Publication number
CN107696773A
CN107696773A CN201711030934.XA CN201711030934A CN107696773A CN 107696773 A CN107696773 A CN 107696773A CN 201711030934 A CN201711030934 A CN 201711030934A CN 107696773 A CN107696773 A CN 107696773A
Authority
CN
China
Prior art keywords
noble metal
rope
paper tinsel
shell
metal paper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201711030934.XA
Other languages
Chinese (zh)
Inventor
许楚瀚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shenzhen Jinbaoying Culture Co Ltd
Original Assignee
Shenzhen Jinbaoying Culture Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shenzhen Jinbaoying Culture Co Ltd filed Critical Shenzhen Jinbaoying Culture Co Ltd
Priority to CN201711030934.XA priority Critical patent/CN107696773A/en
Publication of CN107696773A publication Critical patent/CN107696773A/en
Pending legal-status Critical Current

Abstract

The present invention relates to a kind of noble metal letters and preparation method thereof.This noble metal letters include noble metal paper tinsel, the rope for series connection and the transparent shell of the lengthy motion picture shape with patterned layer, noble metal paper tinsel at least two panels, width parallel arranged of the noble metal paper tinsel along itself;Rope has at least two, and every rope doubling and noble metal paper tinsel are clipped between two parts rope formed after doubling, sandwich noble metal paper tinsel between rope in parallel to each other;Shell is divided into lid and lower cover, and shell corresponds with noble metal paper tinsel, and noble metal paper tinsel and rope are capped and clamped with lower cover simultaneously.The structure of the present invention avoids needs each rope is knotted during assembling, simplifies assembling process, produces time-consuming reduction, and efficiency improves, is more beneficial for producing in enormous quantities, meets the market demand.

Description

A kind of noble metal letters and preparation method thereof
Technical field
The present invention relates to noble metal collectibles, more particularly to a kind of noble metal letters and preparation method thereof.
Background technology
In collectibles field, noble metal is the common selection of people, such as gold, silver, noble metal collectibles common are gold/ Silver-colored banknote/coin, stamp, porcelain, bowls and chopsticks, operation card etc..Several years ago there are a kind of golden letters of imitative inscriptions on bamboo slips letter structure, into For the one of which kind of noble metal collectibles.It is the gold plaque or silver strip that surface is printed on pattern/word inside golden letters, outside It is the shell of layer of transparent, all shells side by side are made letters in a row by enclosure by winding rope.This structure The shortcomings that be outside winding rope when mounted, rope need to be knotted once by often filling a shell, then be refilled next Shell, this process is comparatively laborious, time-consuming, is unfavorable for accelerating production, has much room for improvement.
The content of the invention
The defects of it is an object of the invention to overcome prior art, and a kind of noble metal letters are provided, structure-improved with Simplify assembling process, reduce time-consuming.
To achieve the above object, the present invention uses following technical scheme:
A kind of noble metal letters, it include the noble metal paper tinsel of lengthy motion picture shape with patterned layer, the rope for series connection and Transparent shell, noble metal paper tinsel at least two panels, width parallel arranged of the noble metal paper tinsel along itself;Rope has at least two Bar, every rope doubling and noble metal paper tinsel are clipped between two parts rope formed after doubling, between rope in parallel to each other Sandwich noble metal paper tinsel;Shell is divided into lid and lower cover, and shell corresponds with noble metal paper tinsel, and noble metal paper tinsel and rope are simultaneously upper Lid and lower cover clamp;The upper lid and lower cover of shell are fixed by ultrasonic bonding and are bonded.
Further, the outer casing upper cover corresponding to the bending place of rope doubling is respectively equipped with lower cover and led to for what rope passed through Hole, a rope sequentially pass through two through holes corresponding with rope, and rope passes through the through hole of upper lid from the inside to the outside, rope from outside to The interior through hole through lower cover.
Further, the one side of upper lid and lower cover towards the noble metal paper tinsel of shell is equipped with the groove for covering rope.
Further, shell on be covered with two dops, the lower lid of shell is provided with the hole clipping of corresponding dop, upper lid with Lower cover is inserted in hole clipping by dop and realizes that relative position is fixed.
Further, shell is acrylic shell.
Further, a tasselled are equipped with same one end of two ropes.
Further, noble metal paper tinsel thickness range:0.004mm~0.01mm.
The invention also discloses the preparation method of noble metal letters, comprise the following steps:
The rolling of noble metal raw material is cut into the noble metal paper tinsel of required thickness and shape size, then disposably in your gold Overall oil pressure goes out layout on category paper tinsel;
Noble metal paper tinsel that oil pressure is crossed disposably is cut into the noble metal paper tinsel of a plurality of lengthy motion picture shape using cutting die;
By noble metal paper tinsel lay out in parallel at least above two ropes, then by rope doubling, then by noble metal paper tinsel and Rope is put on the lower lid of shell, and lower cover and the noble metal paper tinsel of shell correspond, and then cover the upper lid of shell in lower cover Go up and fix relative position;
The semi-finished product that previous step is made, which are integrally put into ultrasonic welding machine, carries out ultrasonic bonding so that upper lid with Lower cover achieves a fixed connection.
Further, the outer casing upper cover corresponding to the bending place of rope doubling is respectively equipped with lower cover and led to for what rope passed through Hole;Before by rope doubling, need that rope is first passed through to the through hole of upper lid from the inside to the outside, then pass through down rope from outside to inside The through hole of lid.
Further, after ultrasonic welding step completes, a tasselled need to be assembled in the end of rope.
Further, shell on be covered with two dops, the lower lid of shell is provided with the hole clipping of corresponding dop;By outside The upper lid of shell is covered in lower cover, and the dop of upper lid is inserted respectively into the hole clipping of lower cover and realizes that relative position is fixed.
Further, the one side of upper lid and lower cover towards the noble metal paper tinsel of shell is equipped with the groove for covering rope; When noble metal paper tinsel, rope and shell assemble, rope need to be allowed to be placed on the position of respective slot.
Further, cutting die cutting is completed using cross cutting hydraulic cutting presser.
Compared with the prior art, the invention has the advantages that:
The present invention directly sandwiches rope on noble metal paper tinsel, then clamps rope and noble metal paper tinsel with lid lower cover, is producing During assembling, rope, noble metal paper tinsel are put well on lower lid, by it is upper cover and with lower cover fasten, finally carry out lid and lower cover It is fixedly connected, so just avoid needs each rope is knotted during assembling, simplifies assembling process, Production is time-consuming to be reduced, and efficiency improves, and is more beneficial for producing in enormous quantities, meets the market demand.
Brief description of the drawings
Fig. 1 is noble metal letters exploded view of the present invention.
Fig. 2 is noble metal letters rope bending place structure section view position view of the present invention.
Fig. 3 is outer casing upper cover of the present invention, lower cover and noble metal paper tinsel exploded view.
Fig. 4 is noble metal letters assembling stereogram of the present invention.
Embodiment
In order to more fully understand the technology contents of the present invention, technical scheme is made with reference to specific embodiment It is further described and illustrates.
The concrete structure of the embodiment of the present invention is as Figure 1-4.
As shown in figure 1, noble metal letters include noble metal paper tinsel 20, the rope for series connection of the lengthy motion picture shape with patterned layer 30 and transparent acrylic shell 10.
As shown in figure 1, at least two panels of noble metal paper tinsel 20, in the present embodiment, noble metal paper tinsel 20 has 14 side by side, noble metal Width parallel arranged of the paper tinsel 20 along itself.The thickness range of noble metal paper tinsel 20:0.004mm~0.01mm.Noble metal paper tinsel 20 Making step:Roll, cut, oil pressure pattern, finally cutting into lengthy motion picture shape.
As shown in figure 1, the rope 30 of the present embodiment has two.As shown in Figure 1, 2, every doubling of rope 30 and noble metal Paper tinsel 20 is clipped between two parts rope 30 formed after doubling.Noble metal paper tinsel 20 is sandwiched in parallel to each other between two ropes 30.
As shown in figure 1, shell 10 corresponds with noble metal paper tinsel 20, there are 14 shells 10 in the present embodiment.Such as Fig. 1,3 institutes Show, the upper lid 11 and lower cover 12 that shell 10 divides to be mutually permanently connected.The upper lid 11 of shell 10 is provided with two dops 111, shell 10 lower cover 12 is provided with the hole clipping 121 of corresponding dop 111, and upper lid 11 is inserted real in hole clipping 121 with lower cover 12 by dop 111 Existing relative position is fixed.Upper lid 11 is fixed by ultrasonic bonding after being covered with the relative positioning of lower cover 12 and is bonded.
As shown in Figure 1, 2, 3, noble metal paper tinsel 20 and rope 30 be capped simultaneously 11 and lower cover 12 clamp.The upper lid of shell 10 11 and lower cover 12 towards noble metal paper tinsel 20 one side be respectively provided with covering rope groove 112,122.
As shown in Fig. 2 lid 11 is respectively equipped with for rope with lower cover 12 on shell 10 corresponding to the bending place of the doubling of rope 30 The through hole 113,123 that son 30 passes through.One rope 30 sequentially pass through with 30 corresponding two through holes 113,123 of rope, specifically, Rope 30 passes through the through hole 113 of upper lid 11 from the inside to the outside, and then rope 30 is finally restricted from the outside of shell 10 below lower cover 12 Son 30 returns to the lower section of noble metal paper tinsel 20 through the through hole 123 of lower cover 12 from outside to inside.Such structure can avoid shell 10 Split away off from rope 30.
Noble metal letters after assembling are as shown in figure 4, each shell 10 is wrapped in a noble metal paper tinsel (not shown), and two Bar rope 30 connects all shells 10, all laid out in parallel of shell 10, two ropes 30 relative to the another of bending end A tasselled (not shown) is equipped with one end.
The preparation method of the present embodiment noble metal letters, is made up of following steps:
(1) rolling of noble metal raw material is cut into the noble metal paper tinsel of required thickness and shape size, then disposably existed Overall oil pressure goes out layout on noble metal paper tinsel;
(2) noble metal paper tinsel that oil pressure is crossed disposably is cut into the noble metal paper tinsel of a plurality of lengthy motion picture shape using cutting die;
(3) by noble metal paper tinsel lay out in parallel on two ropes, then by rope doubling, then by noble metal paper tinsel and rope Son is put on the lower lid of shell, and lower cover and the noble metal paper tinsel of shell correspond, and then cover the upper lid of shell on lower lid And fixed relative position;
(4) semi-finished product for making previous step, which are integrally put into ultrasonic welding machine, carries out ultrasonic bonding so that on Lid achieves a fixed connection with lower cover;
(5) a tasselled are assembled in the end of rope.
In step (1), noble metal raw material can be gold or silver, and by precious metal material, repeatedly rolling thickness is Noble metal paper tinsel between 0.004mm~0.01mm, need to carry out stress relief annealing process every time between rolling.Make ultra-thin expensive Metal foil, grammes per square metre can be greatly reduced, reduce the cost of product, reduced purchase threshold, be advantageous to high-volume market sale.Reach After required thickness, noble metal paper tinsel is carried out to cut into required size and shape.Then noble metal paper tinsel is entered using hydraulic press The disposable oil pressure of row, designed pattern is carved with the mould of hydraulic press, after carrying out oil pressure to noble metal paper tinsel, noble metal paper tinsel Just designed pattern is had on surface.Reduce procedure of processing in disposable overall oil pressure molding pattern, improve processing Speed, improve production efficiency.
In step (2), cutting die cutting is completed using cross cutting hydraulic cutting presser, and cutting is out the lengthy motion picture shape of multi-disc formed objects Noble metal paper tinsel.The method that this first oil pressure pattern is disposably cut again, make mould compared to monolithic and carry out oil pressure figure again The mode of case, speed of production are improved, and pattern integrity is guaranteed.
In step (3), the outer casing upper cover corresponding to the bending place of rope doubling is respectively equipped with lower cover to be passed through for rope Through hole.Thus, before by rope doubling, need that rope is first passed through to the through hole of upper lid from the inside to the outside, then by rope from outer To the interior through hole for passing through lower cover, by lower cover be put into corresponding to below that noble metal paper tinsel, then doubling rope, upper lid is put into pair It is upper to be covered on lower lid above that the noble metal paper tinsel answered.After this, then by remaining noble metal paper tinsel and rope and other Shell is assembled.
It has been observed that shell on be covered with two dops, the lower lid of shell is provided with the hole clipping of corresponding dop.In step (3) in, when the upper lid of shell is covered in lower cover, the dop of upper lid need to be inserted respectively into the hole clipping of lower cover and realizes phase Position is fixed, is now still removable between upper lid and lower cover, does not realize and completely fix non-disconnectable connection.
It has been observed that the one side of upper lid and lower cover towards the noble metal paper tinsel of shell is equipped with the groove for covering rope. In step (3), when noble metal paper tinsel, rope and shell assemble, rope need to be allowed to be placed on the position of respective slot, otherwise clamped Rope can be allowed to produce larger pressure to noble metal paper tinsel and damage during rope.
In step (4), semi-finished product obtained by previous step are put into inside the mould of ultrasonic welding machine, matched moulds, Ran Houjin Row integral ultrasonic is welded so that upper lid realizes fixed, non-disconnectable connection with lower cover.The side of this integral ultrasonic welding Formula, compared to manual wire rope handling assembling mode, speed of production is improved, and advantageously reduces processing cost.
The technology contents set forth above that the present invention is only further illustrated with embodiment, in order to which reader is easier to understand, But embodiments of the present invention are not represented and are only limitted to this, any technology done according to the present invention extends or recreation, is sent out by this Bright protection.

Claims (10)

1. a kind of noble metal letters, it is characterised in that it includes the noble metal paper tinsel of the lengthy motion picture shape with patterned layer, for series connection Rope and transparent shell, the noble metal paper tinsel at least two panels, the noble metal paper tinsel are parallel along the width of itself Arrangement;The rope has at least two, every rope doubling and noble metal paper tinsel be clipped in two parts rope for being formed after doubling it Between, noble metal paper tinsel is sandwiched between the rope in parallel to each other;The shell is divided into lid and lower cover, shell and noble metal paper tinsel one One correspondence, the noble metal paper tinsel and rope are capped simultaneously to be clamped with lower cover;The upper lid and lower cover of the shell pass through ultrasonic wave It is welded and fixed fitting.
2. noble metal letters as claimed in claim 1, it is characterised in that the shell corresponding to the bending place of the rope doubling Upper lid is respectively equipped with the through hole passed through for rope with lower cover, and a rope sequentially passes through two through holes corresponding with rope, The rope passes through the through hole of upper lid from the inside to the outside, and the rope passes through the through hole of lower cover from outside to inside.
3. noble metal letters as claimed in claim 1, it is characterised in that the upper lid and lower cover of the shell are towards noble metal paper tinsel One side be equipped with groove for covering rope.
4. noble metal letters as claimed in claim 1, it is characterised in that two dops are covered with the shell, it is described The lower lid of shell is provided with the hole clipping of the corresponding dop, and the upper lid is inserted in hole clipping with lower cover by dop realizes relative position Put fixation.
5. the preparation method of noble metal letters as claimed in claim 1, it is characterised in that it comprises the following steps:
The rolling of noble metal raw material is cut into the noble metal paper tinsel of required thickness and shape size, then disposably in noble metal paper tinsel Upper overall oil pressure goes out layout;
Noble metal paper tinsel that oil pressure is crossed disposably is cut into the noble metal paper tinsel of a plurality of lengthy motion picture shape using cutting die;
By noble metal paper tinsel lay out in parallel at least above two ropes, then by rope doubling, then by noble metal paper tinsel and rope Put on the lower lid of shell, lower cover and the noble metal paper tinsel of shell correspond, and then cover the upper lid of shell on lower lid simultaneously Fixed relative position;
The semi-finished product that previous step is made, which are integrally put into ultrasonic welding machine, carries out ultrasonic bonding so that upper lid and lower cover Achieve a fixed connection.
6. preparation method as claimed in claim 5, it is characterised in that on the shell corresponding to the bending place of the rope doubling Lid is respectively equipped with the through hole passed through for rope with lower cover;Before by rope doubling, need that rope is first passed through into upper lid from the inside to the outside Through hole, then by rope from outside to inside pass through lower cover through hole.
7. preparation method as claimed in claim 5, it is characterised in that after ultrasonic welding step completes, need to restrict The end of son assembles a tasselled.
8. preparation method as claimed in claim 5, it is characterised in that two dops are covered with the shell, it is described outer The lower lid of shell is provided with the hole clipping of the corresponding dop;When the upper lid of shell is covered in lower cover, by the dop of upper lid point It is not inserted into the hole clipping of lower cover and realizes that relative position is fixed.
9. preparation method as claimed in claim 5, it is characterised in that the upper lid and lower cover of the shell are towards noble metal paper tinsel Simultaneously it is equipped with the groove for covering rope;When noble metal paper tinsel, rope and shell assemble, rope need to be allowed to be placed on described in correspondence On the position of groove.
10. preparation method as claimed in claim 5, it is characterised in that cutting die cutting is completed using cross cutting hydraulic cutting presser.
CN201711030934.XA 2017-10-30 2017-10-30 A kind of noble metal letters and preparation method thereof Pending CN107696773A (en)