CN107386681A - 刮腻子及刷乳胶漆的施工工艺 - Google Patents
刮腻子及刷乳胶漆的施工工艺 Download PDFInfo
- Publication number
- CN107386681A CN107386681A CN201710685784.XA CN201710685784A CN107386681A CN 107386681 A CN107386681 A CN 107386681A CN 201710685784 A CN201710685784 A CN 201710685784A CN 107386681 A CN107386681 A CN 107386681A
- Authority
- CN
- China
- Prior art keywords
- metope
- brush
- emulsion paint
- puttying
- construction technology
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
本发明公开一种刮腻子及刷乳胶漆的施工工艺,其目的在于:填补墙体细小孔洞和缝隙,使之满足表面光滑度的要求,遮蔽裂痕,本发明通过清理墙面、修补墙面将墙面底面修补干净平整,填补墙体细小孔洞和缝隙,刮腻子通过刷三遍乳胶漆来达到表面的光滑平整,使之满足表面光滑度的要求,遮蔽裂痕。
Description
技术领域
本发明涉及一种建筑施工工艺,具体涉及一种刮腻子及刷乳胶漆的施工工艺。
背景技术
建筑腻子是装修中必不可少的建材产品之一,是施涂于建筑物内外墙面,起弥补基层缺陷或表现多样化花纹和质感作用的涂装基层材料。腻子按产品用途主要分为:平壁型、浮雕型、拉花型、瓷砖专用型、高弹抗裂型等。其中,平壁型按其适用场合可分为三种,找平型、平面型和光面型。找平型主要使基层获得所需的平整度;光面型主要使基层获得光滑、细腻的表面质感;平面型界于两者之间,即可做平基面,又可做光基面,但是单方面的效用不如前两者,适用于普通应用场合;一般光面型腻子应在使用找平型腻子找平的基面上使用。按产品有无弹性,外墙建筑腻子可分为刚性和弹性(或称柔性)两大类,其中弹性腻子适用于抗裂或防裂的场合。
发明内容
针对上述问题,本发明提供了一种刮腻子及刷乳胶漆的施工工艺,其目的在于:填补墙体细小孔洞和缝隙,使之满足表面光滑度的要求,遮蔽裂痕。
本发明的技术解决方案:
刮腻子及刷乳胶漆的施工工艺,其特征在于包括如下步骤:
步骤一,清理墙面:将墙面起皮及松动处清除干净,并用水泥砂浆补抹,将残留灰渣铲干净,然后将墙面扫净。
步骤二,修补墙面:用水石膏将墙面磕碰处及坑洼缝隙等处找平,干燥后用砂纸凸出处磨掉,将浮尘扫净。
步骤三,刮腻子:刮腻子遍数可由墙面平整程度决定,一般情况为三遍,厨房、厕所、浴室用聚醋酸乙烯乳液:水泥:水=1:5:1耐水性腻子;刷第一遍乳胶漆:涂刷顺序是先刷顶板后刷墙面,墙面是先上后下,干燥后复补腻子,再干燥后用砂纸磨光,清扫干净;
刷第二遍乳胶漆:操作要求同第一遍,使用前充分搅拌,如不很稠,不宜加水,以防透底,漆膜干燥后,用细砂纸将墙面小疙瘩和排笔毛打磨掉,磨光滑后清扫干净。
根据步骤三中的刮腻子,刷第三遍乳胶漆:做法同第二遍乳胶漆,由于乳胶漆膜干燥较快,应连续迅速操作,涂刷时从一头开始,逐渐刷向另一头,要上下顺刷互相衔接,后一排笔紧接前一排笔,避免出现干燥后接头。
本发明的有益效果:
本发明通过清理墙面、修补墙面将墙面底面修补干净平整,填补墙体细小孔洞和缝隙,刮腻子通过刷三遍乳胶漆来达到表面的光滑平整,使之满足表面光滑度的要求,遮蔽裂痕。
具体实施方式
下面结合实施例来对本发明做进一步描述:
刮腻子及刷乳胶漆的施工工艺,包括如下步骤:
步骤一,清理墙面:将墙面起皮及松动处清除干净,并用水泥砂浆补抹,将残留灰渣铲干净,然后将墙面扫净。
步骤二,修补墙面:用水石膏将墙面磕碰处及坑洼缝隙等处找平,干燥后用砂纸凸出处磨掉,将浮尘扫净。
步骤三,刮腻子:刮腻子遍数可由墙面平整程度决定,一般情况为三遍,厨房、厕所、浴室用聚醋酸乙烯乳液:水泥:水=1:5:1耐水性腻子;刷第一遍乳胶漆:涂刷顺序是先刷顶板后刷墙面,墙面是先上后下,干燥后复补腻子,再干燥后用砂纸磨光,清扫干净;
刷第二遍乳胶漆:操作要求同第一遍,使用前充分搅拌,如不很稠,不宜加水,以防透底。漆膜干燥后,用细砂纸将墙面小疙瘩和排笔毛打磨掉,磨光滑后清扫干净。
根据步骤三中的刮腻子,刷第三遍乳胶漆:做法同第二遍乳胶漆,由于乳胶漆膜干燥较快,应连续迅速操作,涂刷时从一头开始,逐渐刷向另一头,要上下顺刷互相衔接,后一排笔紧接前一排笔,避免出现干燥后接头。
综上,本发明达到预期目的。
Claims (2)
1.刮腻子及刷乳胶漆的施工工艺,其特征在于:包括如下步骤:
步骤一,清理墙面:将墙面起皮及松动处清除干净,并用水泥砂浆补抹,将残留灰渣铲干净,然后将墙面扫净;
步骤二,修补墙面:用水石膏将墙面磕碰处及坑洼缝隙等处找平,干燥后用砂纸凸出处磨掉,将浮尘扫净;
步骤三,刮腻子:刮腻子遍数可由墙面平整程度决定,一般情况为三遍,厨房、厕所、浴室用聚醋酸乙烯乳液:水泥:水=1:5:1耐水性腻子;刷第一遍乳胶漆:涂刷顺序是先刷顶板后刷墙面,墙面是先上后下,干燥后复补腻子,再干燥后用砂纸磨光,清扫干净;
刷第二遍乳胶漆:操作要求同第一遍,使用前充分搅拌,如不很稠,不宜加水,以防透底,漆膜干燥后,用细砂纸将墙面小疙瘩和排笔毛打磨掉,磨光滑后清扫干净。
2.根据权利要求1所述的刮腻子及刷乳胶漆的施工工艺,其特征在于:根据步骤三中的刮腻子,刷第三遍乳胶漆:做法同第二遍乳胶漆,由于乳胶漆膜干燥较快,应连续迅速操作,涂刷时从一头开始,逐渐刷向另一头,要上下顺刷互相衔接,后一排笔紧接前一排笔,避免出现干燥后接头。