CN107268812A - A kind of anti-dropout exterior wall with anticreep rod - Google Patents
A kind of anti-dropout exterior wall with anticreep rod Download PDFInfo
- Publication number
- CN107268812A CN107268812A CN201710714105.7A CN201710714105A CN107268812A CN 107268812 A CN107268812 A CN 107268812A CN 201710714105 A CN201710714105 A CN 201710714105A CN 107268812 A CN107268812 A CN 107268812A
- Authority
- CN
- China
- Prior art keywords
- proof
- anticreep rod
- anticreep
- layer
- rod
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a kind of anti-dropout exterior wall with anticreep rod, belong to building field.A kind of anti-dropout exterior wall with anticreep rod, including wall, cement layer is equipped with the wall, anticreep rod is inserted with the cement layer, the anticreep rod runs proof including first, stayed mast and second runs proof, described first, which runs proof, is fixedly connected on one end of stayed mast, described second, which runs proof, is fixedly connected on second other end run proof, described first runs proof, stayed mast, the second outside run proof are enclosed with antiseptic rubber, the antiseptic rubber and first run proof, stayed mast, second run proof between space in be filled with cement based powders.It can realize the addition anticreep rod between exterior wall and heat-insulation layer, increase the steadiness of heat-insulation layer, while can be moistureproof, simplify existing construction technology, without fixed components such as anchoring piece, rack plating zinc wire nettings, form of construction work is simpler, and cost is lower.
Description
Technical field
The present invention relates to building field, more specifically to a kind of anti-dropout exterior wall with anticreep rod.
Background technology
Coming off for external wall not only influences attractive in appearance, and the exterior wall come off drops from eminence and very likely results in personnel's wound
Event is died, existing exterior wall is mainly coming off for heat-insulation layer.
In the prior art, the reason for exterior wall comes off is mainly:Styrofoam uses a little viscous mode, bond area not pedal plate
The 5% of face;There is no anchoring piece, cause heat-insulation layer large area to come off;Adhesive mortar is of poor quality, the adhesion strength of styrofoam and mortar
Less than 0.1Mpa;The way of styrofoam external hanging ceramic tile make it that wall thermal insulating deadweight is excessive;There is no a rack plating zinc wire netting, and with anchoring
Part is reliably connected.
Existing external wall construction cost is high, and of low quality, and the phenomenon come off of making moist takes place frequently life, can not meet existing
In the demand of building.
The content of the invention
1. the technical problem to be solved
For problems of the prior art, it is an object of the invention to provide a kind of anti-dropout exterior wall with anticreep rod,
It can realize the addition anticreep rod between exterior wall and heat-insulation layer, increase the steadiness of heat-insulation layer, while can be moistureproof, simplify existing
There is construction technology, without fixed components such as anchoring piece, rack plating zinc wire nettings, form of construction work is simpler, and cost is lower.
2. technical scheme
To solve the above problems, the present invention is adopted the following technical scheme that.
Cement layer, the cement layer are equipped with a kind of anti-dropout exterior wall with anticreep rod, including wall, the wall
Anticreep rod is inside inserted with, the anticreep rod runs proof including first, stayed mast and second runs proof, described first runs proof fixation
One end of stayed mast is connected to, described second, which runs proof, is fixedly connected on second other end run proof, described first run proof,
Stayed mast, the second outside run proof are enclosed with antiseptic rubber, the antiseptic rubber and first run proof, stayed mast, second prevent
It is filled with space between de- ball on cement based powders, the antiseptic rubber and offers multiple through holes, multiple through holes is equal
Even to be arranged on antiseptic rubber, one end of the anticreep rod is located in cement layer, and the other end of the anticreep rod is located at cement layer
Outside, the one end of the cement layer away from wall is equipped with adhesive layer, and the one end of the adhesive layer away from cement layer is equipped with insulation
Layer, and anticreep rod the other end be located at heat-insulation layer in, one end of anticreep rod is fixed by the low cement layer of firm, cost, prevent
The other end of de- rod is directly embedded in heat-insulation layer, and coming off for heat-insulation layer is prevented by the pulling force of anticreep rod, and first runs proof and the
Two run proof be sphere, relative volume with the contact surface of cement layer and heat-insulation layer under, contact area is maximum, and lifting surface area is most
Greatly, anticreep rod is hardly damaged, and the antiseptic rubber on anticreep rod surface is flexible, is not good feelings in heat-insulation layer heat insulation effect
Under condition, the contact surface of anticreep rod and cement layer and heat-insulation layer can normally expand with heat and contract with cold, and be difficult to form cracking, increase heat-insulation layer
Steadiness, once after heat-insulation layer formation cracking, antiseptic rubber is stretched, thru-hole distortion, cement based powders, is scattering into slit
In gap, cement based powders become cement base and are covered in cracking slit surfaces after making moist, and slow down heat-insulation layer and further make moist cracking.
Preferably, the antiseptic rubber uses chlorinated rubber, and the surface of antiseptic rubber scribbles hydrophilic layer, chlorinated rubber tool
There are excellent film forming, adhesiveness, corrosion resistance, anti-flammability and insulating properties, antiseptic rubber is hardly damaged, expose cement original washing powder
End.
Preferably, mixed with water-absorbent resin powder in the cement based powders, water-absorbent resin powder keeps cement based powders
Dry.
Preferably, described first run proof positioned at one end of anticreep rod, and first runs proof in cement layer, described
Two run proof positioned at the other end of anticreep rod, and second runs proof in heat-insulation layer, and first runs proof runs proof with second makes
Stress surface is sphere, increases lifting surface area, and anticreep rod is hardly damaged, and improves anticreep rod service life.
Preferably, the thickness of the of length no more than heat-insulation layer of the other end of the anticreep rod, second runs proof fills with heat-insulation layer
Tap is touched, and increases lifting surface area.
3. beneficial effect
Compared to prior art, the advantage of the invention is that:
(1)This programme fixes one end of anticreep rod by the low cement layer of firm, cost, and the other end of anticreep rod is directly embedded to
In heat-insulation layer, coming off for heat-insulation layer is prevented by the pulling force of anticreep rod, first runs proof runs proof and cement layer and guarantor with second
Under the contact surface of warm layer is sphere, relative volume, contact area is maximum, and lifting surface area is maximum, and anticreep rod is hardly damaged, and anti-
The antiseptic rubber on de- rod surface is flexible, in the case of heat-insulation layer heat insulation effect is not well, anticreep rod and cement layer and
The contact surface of heat-insulation layer can normally expand with heat and contract with cold, and be difficult to form cracking, increase the steadiness of heat-insulation layer, once heat-insulation layer is formed
After cracking, antiseptic rubber is stretched, and thru-hole distortion cement based powders are scattering into cracking gap, and cement based powders become after making moist
Cracking slit surfaces are covered in into cement base, slows down heat-insulation layer and further makes moist cracking;
(2)Antiseptic rubber uses chlorinated rubber, and the surface of antiseptic rubber scribbles hydrophilic layer, and chlorinated rubber has excellent film forming
Property, adhesiveness, corrosion resistance, anti-flammability and insulating properties, antiseptic rubber are hardly damaged, and expose cement based powders;
(3)Mixed with water-absorbent resin powder in cement based powders, water-absorbent resin powder keeps the drying of cement based powders;
(4)First runs proof positioned at one end of anticreep rod, and first runs proof in cement layer, and described second, which runs proof, is located at
The other end of anticreep rod, and second run proof in heat-insulation layer, first runs proof runs proof with second makes stress surface be ball
Face, increases lifting surface area, and anticreep rod is hardly damaged, and improves anticreep rod service life;
(5)The thickness of the of length no more than heat-insulation layer of the other end of anticreep rod, second runs proof fully contacts with heat-insulation layer, increase by
Power area;
(6)Simplify existing construction technology, without fixed components such as anchoring piece, rack plating zinc wire nettings, form of construction work is simpler, cost
It is lower.
Brief description of the drawings
Fig. 1 is structural representation of the invention;
Fig. 2 is the structural representation of anticreep rod of the present invention;
Fig. 3 is located at structural representation when in water soluble film for anticreep rod of the present invention;
Fig. 4 is structural representation when wall of the present invention lays cement layer;
Fig. 5 is fixed on the structural representation on cement layer for anticreep rod in Fig. 4;
Fig. 6 is the structural representation after water soluble film thawing in Fig. 5.
Label declaration in figure:
1 first runs proof, 2 stayed masts, 3 second run proof, 4 water soluble films, 5 cement layers, 6 walls, 7 anticreep rods, 8 heat-insulation layers, 9 water
Mud based powders, 10 through holes, 11 antiseptic rubbers, 12 adhesive layers.
Embodiment
Below in conjunction with the accompanying drawing in the embodiment of the present invention;Technical scheme in the embodiment of the present invention is carried out clear, complete
Site preparation is described;Obviously;Described embodiment is only a part of embodiment of the invention;Rather than whole embodiments.It is based on
Embodiment in the present invention;It is every other that those of ordinary skill in the art are obtained under the premise of creative work is not made
Embodiment;Belong to the scope of protection of the invention.
Embodiment 1:
Refer to and be equipped with cement layer 5, water on Fig. 1-6, a kind of anti-dropout exterior wall with anticreep rod, including wall 6, wall 6
It is inserted with anticreep rod 7 in mud layer 5, anticreep rod 7 runs proof 3 including the first 1, stayed mast 2 and second that runs proof, first run proof 1,
Stayed mast 2 and second is run proof and 3 is made using stainless steel, and intensity is high, good corrosion resistance, and first, which runs proof, 1 is fixedly connected on
One end of stayed mast 2, second run proof 3 be fixedly connected on second run proof 3 the other end, first runs proof 1, stayed mast 2,
Two run proof 3 outsides are enclosed with antiseptic rubber 11, antiseptic rubber 11 and first run proof 1, stayed mast 2, second run proof 3 it
Between space in be filled with cement based powders 9, mixed with water-absorbent resin powder in cement based powders 9, water-absorbent resin powder keeps water
The drying of mud based powders 9, antiseptic rubber 11 uses chlorinated rubber, and the surface of antiseptic rubber 11 scribbles the parent that hydrophilic coating is formed
Water layer, chlorinated rubber has excellent film forming, adhesiveness, corrosion resistance, anti-flammability and an insulating properties, the not rapid wear of antiseptic rubber 11
It is bad, expose and multiple through holes 10 are offered on cement based powders 9, antiseptic rubber 11, multiple through holes 10 are evenly spaced in antiseptic rubber
On 11, one end of anticreep rod 7 is located in cement layer 5, and the other end of anticreep rod 7 is located at outside cement layer 5, and cement layer 5 is away from wall 6
One end be equipped with adhesive layer 12, the one end of adhesive layer 12 away from cement layer 5 is equipped with heat-insulation layer 8, and the other end of anticreep rod 7
In heat-insulation layer 8, first run proof 1 be located at anticreep rod 7 one end, and first run proof 1 be located at cement layer 5 in, second prevent
De- ball 3 is located at the other end of anticreep rod 7, and second runs proof and 3 be located in heat-insulation layer 8, and first, which runs proof, 1 and second runs proof 3
It is sphere to make stress surface, increases lifting surface area, anticreep rod 7 is hardly damaged, and improves the service life of anticreep rod 7, anticreep rod 7 it is another
The thickness of the of length no more than heat-insulation layer 8 in one end, second runs proof 3 fully contacts with heat-insulation layer 8, increases lifting surface area.
A kind of anti-dropout external wall construction technique with anticreep rod,
First, cement layer 5 is laid on the surface of wall 6, before cement layer 5 does not solidify, escapement is layered on the surface of cement layer 5
And press one end of anticreep rod 7 into cement layer 5, escapement includes water soluble film 4 and anticreep rod 7, and water soluble film 4 uses 2min
With regard to the normal temperature water soluble film that can be completely dissolved, the other end of anticreep rod 7 is bonded in water soluble film 4, anticreep rod 7 and the table of water soluble film 4
Face keeps vertical, and the uniform branch of anticreep rod 7 is in water soluble film 4, without anticreep rod 7 is injected in cement layer 5 one by one, time saving province
Power;
2nd, after cement layer 5 solidifies, a small amount of water is sprayed to the surface of water soluble film 4 using atomizing shower nozzle, until water soluble film 4 is complete
Stop water spray after moistening, wait 2min, after water soluble film 4 has dissolved, expose the other end of anticreep rod 7, remove water soluble film 4, prevent
4 pairs of constructions of water soluble film are interfered, and water soluble film compares other films, and water can be recycled to remove after the coagulation forming of cement layer 5,
Remove the surface of cement layer 5 after water soluble film 4 smooth, space will not be left during bonding and thermal insulation layer 8, using other films in cement layer 5
Torn off before coagulation forming and easily take anticreep rod 7 out of, while it is crude to will also result in the surface of cement layer 5, sky is left during bonding and thermal insulation layer 8
Gap, causes the later stage of heat-insulation layer 8 to come off, and other films are fixed on cement layer 5 after the coagulation forming of cement layer 5, it is difficult to tear clean, shadow
Ring the fastness of bonding and thermal insulation layer 8;
3rd, reuse atomizing shower nozzle and a small amount of water is sprayed to another end surfaces of anticreep rod 7, until the other end table of anticreep rod 7
Stop water spray after the moistening completely of face, the cement based powders 9 during water spray at through hole 10 become cement base sealant and seal through hole 10, keep away
Exempt from water into the inner side of antiseptic rubber 11;
4th, after the surface of wait anticreep rod 7 is dried completely, adhesive layer 12 is painted on the surface of cement layer 5, then in adhesive layer 12
Surface laying heat-insulation layer 8, the other end of anticreep rod 7 is laid on to the inside of heat-insulation layer 8 during laying heat-insulation layer 8.
Cement layer 5 is laid on wall 6, by adding anticreep rod 7 between cement layer 5 and heat-insulation layer 8, anticreep rod 7 will
Heat-insulation layer 8 is fixed on cement layer 5, increases the steadiness of heat-insulation layer 8, while the cement based powders 9 in anticreep rod 7 can prevent
Simplify existing construction technology in tide, work progress, without fixed components such as anchoring piece, rack plating zinc wire nettings, made using water soluble film 4
Form of construction work is simpler, and once after the formation cracking of heat-insulation layer 8, antiseptic rubber 11 is stretched, and through hole 10 is deformed, and is formed during construction
Cement base sealant come off from through hole 10, through hole 10 is no longer sealed, and the cement based powders 9 of the inner side of antiseptic rubber 11 are scattering into
Ftracture in gap, cement based powders 11 become cement base and are covered in cracking slit surfaces after making moist, slow down heat-insulation layer 8 further by
Tide cracking, time saving and energy saving, cost is lower.
More than;Preferably embodiment only of the invention;But protection scope of the present invention is not limited thereto;It is any
Those familiar with the art the invention discloses technical scope in;Technique according to the invention scheme and its improvement
Design is subject to equivalent substitution or change;It should all cover within the scope of the present invention.
Claims (6)
1. a kind of anti-dropout exterior wall with anticreep rod, it is characterised in that:Including wall(6), the wall(6)On be equipped with water
Mud layer(5), the cement layer(5)Inside it is inserted with anticreep rod(7), the anticreep rod(7)Run proof including first(1), stayed mast
(2)Run proof with second(3), described first runs proof(1)It is fixedly connected on stayed mast(2)One end, described second runs proof
(3)Second is fixedly connected on to run proof(3)The other end, described first runs proof(1), stayed mast(2), second run proof(3)
Outside be enclosed with antiseptic rubber(11), the antiseptic rubber(11)Run proof with first(1), stayed mast(2), second run proof
(3)Between space in be filled with cement based powders(9), the antiseptic rubber(11)On offer multiple through holes(10), it is multiple
The through hole(10)It is evenly spaced in antiseptic rubber(11)On, the anticreep rod(7)One end be located at cement layer(5)It is interior, it is described
Anticreep rod(7)The other end be located at cement layer(5)Outside, the cement layer(5)Away from wall(6)One end be equipped with adhesive layer
(12), the adhesive layer(12)Away from cement layer(5)One end be equipped with heat-insulation layer(8), and anticreep rod(7)The other end be located at
Heat-insulation layer(8)It is interior.
2. a kind of anti-dropout exterior wall with anticreep rod according to claim 1, it is characterised in that:The antiseptic rubber
(11)Using chlorinated rubber, and antiseptic rubber(11)Surface scribble hydrophilic layer.
3. a kind of anti-dropout exterior wall with anticreep rod according to claim 1, it is characterised in that:The cement based powders
(9)It is interior mixed with water-absorbent resin powder.
4. a kind of anti-dropout exterior wall with anticreep rod according to claim 1, it is characterised in that:
Described first runs proof(1)Positioned at anticreep rod(7)One end, and first run proof(1)Positioned at cement layer(5)It is interior, it is described
Second runs proof(3)Positioned at anticreep rod(7)The other end, and second run proof(3)Positioned at heat-insulation layer(8)It is interior.
5. a kind of anti-dropout exterior wall with anticreep rod according to claim 1, it is characterised in that:The anticreep rod(7)
The of length no more than heat-insulation layer of the other end(8)Thickness.
6. a kind of anti-dropout exterior wall with anticreep rod according to claim 1, it is characterised in that:
The escapement includes water soluble film(4)With anticreep rod(7), the anticreep rod(7)The other end be fixedly connected on it is water-soluble
Film(4)On, the anticreep rod(7)With water soluble film(4)Surface keep vertical, and anticreep rod(7)Uniform branch is in water soluble film(4)
On.