CN107266104A - A kind of gold copy trailing its repair handicraft repair member - Google Patents

A kind of gold copy trailing its repair handicraft repair member Download PDF

Info

Publication number
CN107266104A
CN107266104A CN201710351757.9A CN201710351757A CN107266104A CN 107266104 A CN107266104 A CN 107266104A CN 201710351757 A CN201710351757 A CN 201710351757A CN 107266104 A CN107266104 A CN 107266104A
Authority
CN
China
Prior art keywords
handicraft
repair member
gold
repair
glue
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710351757.9A
Other languages
Chinese (zh)
Inventor
刘志钧
刘冠辰
张晓菲
晋文龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201710351757.9A priority Critical patent/CN107266104A/en
Publication of CN107266104A publication Critical patent/CN107266104A/en
Pending legal-status Critical Current

Abstract

A kind of gold is copied decoration restorative procedure, it is characterised in that:Step is:With alcohol or the incomplete handicraft section of supersonic wave cleaning machine cleaning;The quality proportioning of modulation cloud stone glue, glue and curing agent is 100:1‑4;Above-mentioned cloud stone glue is filled into the reparation area of handicraft repair member;It will be dried in handicraft repair member air at room temperature, make marble adhesive curing;Handicraft repair member is surface-treated.The invention also discloses a kind of handicraft repair member for decoration restorative procedure reparation of being copied using above-mentioned gold.Relative to prior art, technique effect of the invention is that the present invention is replacing lacquer to be bonded and paint spachtling with cloud stone glue, in the case where ensureing no chemical contamination, reduces flash-off time, improves efficiency and reduce cost.

Description

A kind of gold copy trailing its repair handicraft repair member
Technical field
Gold involved in the present invention is copied, and is the reparation for being derived from a Japan art, is used the materials pair such as natural lacquer, goldleaf Bonding reparation is carried out at implements incompleteness, it is ornamental stronger.But different with common renovation technique, gold is copied not exclusively technology, more It is an art, this needs have certain understanding to implements.The implements of catcher have much all been broken into several pieces, by broken place " breaking gold size " engages, and implements is returned to intact form again, recovers attractive in appearance with using function again, is to repair teacher " the Secondary creation ".Gold technique of copying has the very wide scope of application, serves as porcelain and boccaro ware is in the majority, be also used as in addition In articles made of bamboo, ivory, smallclothes woodenware, jadeware etc..
Background technology
It is that porcelain repairs stronger one kind of decoration technique in decoration technology that gold, which is copied, is used not only for the reparation decoration of ceramics, The reparation to bamboo and wood, tooth, boccaro, jadeware can also be applied to decorate, while this method is more conform with Asian aesthetic reason Read.If using proper gimmick, graceful design, the original work that can have also not only crushed originally can also increase another on the contrary Plant beyond expression " incomplete U.S. ".
Copied with gold reparation, it is important to use such natural glue(Majority is lacquer), there is no chemical contamination after drying. The general cycle is repaired at 20 days or so with lacquer, and the part of last gold lacquer can be completed for about 5 days, the foundation of paint before Spend or so two weeks.And the work of this part is hidden under bright and new appearance, there is suitable skin in lacquer manufacturing process Anaphylaxis, and be difficult to cure, only only a few people is immune to this, there is high health and safety hidden danger.
The content of the invention
The technical problem to be solved in the present invention is:The foundation of paint(Exactly dry part)Or so two weeks is spent, no Only the time is longer, and the shady room that need to be more than 70% in humidity is dried, and temperature, humidity environment require very high.
Copied restorative procedure it is an object of the invention to provide a kind of new gold, reduce flash-off time, environmental requirement is dried in reduction.
Technical scheme is specially:
A kind of gold is copied decoration restorative procedure, it is characterised in that:Step is:
With alcohol or the incomplete handicraft section of supersonic wave cleaning machine cleaning;
The quality proportioning of modulation cloud stone glue, glue and curing agent is 100:1-4;
Above-mentioned cloud stone glue is filled into the reparation area of handicraft repair member;
It will be dried in handicraft repair member air at room temperature, make marble adhesive curing;
Handicraft repair member is surface-treated.
A kind of handicraft repair member for decoration restorative procedure reparation of being copied using above-mentioned gold, handicraft repair member is porcelain, purple Sand device, articles made of bamboo, ivory or jadeware.
Relative to prior art, technique effect of the invention is that the present invention is replacing lacquer bonding and paint ash with cloud stone glue Putty, in the case where ensureing no chemical contamination, reduces flash-off time, reduces and dry environmental requirement, in no tradition While lacquer cutaneous anaphylaxis, process safety is improved, efficiency is improved and reduces cost.
Embodiment
A kind of gold is copied restorative procedure, and step is:
1. with alcohol or the incomplete handicraft section of supersonic wave cleaning machine cleaning.
2. modulating cloud stone glue, the quality proportioning of glue and curing agent is 100:1-4.The modulation comparative maturity of current cloud stone glue, Be mainly used in building stone industry, cloud stone glue performance it is excellent be mainly reflected in hardness, it is toughness, rapid curing, polishability, resistance to Wait, it is corrosion-resistant in terms of.This modulation is consistent with method, the proportioning of the Nian Jie stone material of modulation.The quality proportioning of glue and curing agent is 100:It is optimal during 2-4.
3. above-mentioned cloud stone glue is filled into in the reparation area of handicraft decorative repair member, the step technique of being copied with existing gold Approximately, gold lacquer is simply changed to cloud stone glue.
4. will be dried in handicraft decorative repair member air at room temperature, make marble adhesive curing.After marble adhesive curing 24 hours, just Powerful cohesive force can be kept, even if water soaks 10 hours, then boiling water boiling 5 hours, remain in that powerful cohesive force.
5. handicraft decorative repair member is surface-treated, this prior art is the same.
Handicraft decorative repair member can be porcelain, boccaro ware, articles made of bamboo, ivory, jadeware.
The present invention is replacing lacquer with cloud stone glue, and flash-off time is to need 24 hours, reduces flash-off time;Without guarantor That holds high humility dries environment, reduces and dries environmental requirement, while no traditional lacquer cutaneous anaphylaxis, improves effect Rate and cost is reduced, integrally brought conveniently.
Above-described is only the preferred embodiment of the present invention, it is noted that for those skilled in the art, Under the premise of general idea of the present invention is not departed from, some changes and improvements can also be made, these should also be considered as the present invention's Protection domain.

Claims (2)

  1. The trailing 1. a kind of gold is copied, it is characterised in that:Step is:
    With the spot of alcohol or the incomplete handicraft section of supersonic wave cleaning machine cleaning;
    The quality proportioning of modulation cloud stone glue, glue and curing agent is 100:1-4;
    Above-mentioned cloud stone glue is filled into the reparation area of handicraft repair member;
    It will be dried in handicraft repair member air at room temperature, make marble adhesive curing;
    Handicraft repair member is surface-treated.
  2. The handicraft repair member of trailing reparation 2. the gold described in a kind of usage right requirement 1 is copied, it is characterised in that:Handicraft Repair member is porcelain, boccaro ware, articles made of bamboo, ivory or jadeware.
CN201710351757.9A 2017-05-18 2017-05-18 A kind of gold copy trailing its repair handicraft repair member Pending CN107266104A (en)