CN107083523A - A kind of handware steel - Google Patents
A kind of handware steel Download PDFInfo
- Publication number
- CN107083523A CN107083523A CN201710407675.1A CN201710407675A CN107083523A CN 107083523 A CN107083523 A CN 107083523A CN 201710407675 A CN201710407675 A CN 201710407675A CN 107083523 A CN107083523 A CN 107083523A
- Authority
- CN
- China
- Prior art keywords
- parts
- steel
- handware
- iron
- weight
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of handware steel, using iron as raw material, include the component of following parts by weight:0.12 0.25 parts of platinum;0.25 0.55 parts of magnesium;0.2 0.35 parts of palladium;0.22 0.34 parts of chromium;0.12 0.35 parts of tungsten, 0.3 0.5 parts of lithium.The beneficial effects of the invention are as follows:Using iron as main metal element, proportioning is scientific and reasonable, and the platinum and elemental lithium of addition increase the intensity of steel, and the tungsten of addition can strengthen the corrosion resistance of steel, improves the stability of steel, and security performance is high.
Description
Technical field
The present invention relates to a kind of metal material, more particularly to a kind of handware steel.
Background technology
With the continuous improvement of science and technology, hardware industry also constantly emerges, and iron-based handware is due to price at this stage
Cheap therefore most widely used, while iron-based handware, which also possesses, preferable use value, then iron-based handware makes
There is more defect during, such as:Easily it is oxidized, is easily corroded, and for drawbacks described above, at present using copper-plated
Mode, but during copper facing in the prior art, its quality is poor, density metal is not enough, increased number of stomata so that the quality of product
It is poor, it is impossible to meet the demand of all trades and professions.
Therefore, to solve the above problems, special provide a kind of new technical scheme.
The content of the invention
The present invention provides a kind of handware steel.
The technical solution adopted by the present invention is:
A kind of handware steel, using iron as raw material, include the component of following parts by weight:0.12-0.25 parts of platinum;0.25-
0.55 part of magnesium;0.2-0.35 parts of palladium;0.22-0.34 parts of chromium;0.12-0.35 parts of tungsten, 0.3-0.5 parts of lithium.
Further, the parts by weight of the iron are 70-80 parts.
Further, the parts by weight of the magnesium are 0.3-0.4 parts.
Further, the parts by weight of the platinum are 0.2 part.
Further, the parts by weight of the tungsten are 0.25 part.
Further, the parts by weight of the lithium are 0.4 part.
The beneficial effects of the invention are as follows:Using iron as main metal element, proportioning is scientific and reasonable, and the platinum and elemental lithium of addition add
The big intensity of steel, the tungsten of addition can strengthen the corrosion resistance of steel, improve the stability of steel, and security performance is high.
Embodiment
In order to deepen the understanding of the present invention, below in conjunction with embodiment, the invention will be further described, the embodiment
It is only used for explaining the present invention, does not constitute the restriction to protection scope of the present invention.
Embodiment 1
A kind of handware steel, using iron as raw material, the parts by weight of iron are 70 parts, include the component of following parts by weight:
0.12 part of platinum;0.25 part of magnesium;0.2 part of palladium;0.22 part of chromium;0.12 part of tungsten, 0.3 part of lithium.
The beneficial effects of the invention are as follows:Using iron as main metal element, proportioning is scientific and reasonable, and the platinum and elemental lithium of addition add
The big intensity of steel, the tungsten of addition can strengthen the corrosion resistance of steel, improve the stability of steel, and security performance is high.
Embodiment 2
A kind of handware steel, using iron as raw material, the parts by weight of iron are 75 parts, include the component of following parts by weight:
0.18 part of platinum;0.4 part of magnesium;0.28 part of palladium;0.28 part of chromium;0.22 part of tungsten, 0.4 part of lithium.
The beneficial effects of the invention are as follows:Using iron as main metal element, proportioning is scientific and reasonable, and the platinum and elemental lithium of addition add
The big intensity of steel, the tungsten of addition can strengthen the corrosion resistance of steel, improve the stability of steel, and security performance is high.
Embodiment 3
A kind of handware steel, using iron as raw material, the parts by weight of iron are 80 parts, include the component of following parts by weight:
0.25 part of platinum;0.55 part of magnesium;0.35 part of palladium;0.34 part of chromium;0.35 part of tungsten, 0.5 part of lithium.
The beneficial effects of the invention are as follows:Using iron as main metal element, proportioning is scientific and reasonable, and the platinum and elemental lithium of addition add
The big intensity of steel, the tungsten of addition can strengthen the corrosion resistance of steel, improve the stability of steel, and security performance is high.
The above described is only a preferred embodiment of the present invention, being not the limit for making any other form to the present invention
System, and any modification made according to technical spirit of the invention or equivalent variations, still fall within model claimed of the invention
Enclose.
Claims (6)
1. a kind of handware steel, it is characterised in that:Using iron as raw material, include the component of following parts by weight:0.12-0.25
The platinum of part;0.25-0.55 parts of magnesium;0.2-0.35 parts of palladium;0.22-0.34 parts of chromium;0.12-0.35 parts of tungsten, 0.3-0.5
The lithium of part.
2. a kind of handware steel according to claim 1, it is characterised in that:The parts by weight of the iron are 70-80
Part.
3. a kind of handware steel according to claim 1, it is characterised in that:The parts by weight of the magnesium are 0.3-
0.4 part.
4. a kind of handware steel according to claim 1, it is characterised in that:The parts by weight of the platinum are 0.2 part.
5. a kind of handware steel according to claim 1, it is characterised in that:The parts by weight of the tungsten are 0.25
Part.
6. a kind of handware steel according to claim 1, it is characterised in that:The parts by weight of the lithium are 0.4 part.