CN107044996B - Heat insulating property test device and test method - Google Patents

Heat insulating property test device and test method Download PDF

Info

Publication number
CN107044996B
CN107044996B CN201611077878.0A CN201611077878A CN107044996B CN 107044996 B CN107044996 B CN 107044996B CN 201611077878 A CN201611077878 A CN 201611077878A CN 107044996 B CN107044996 B CN 107044996B
Authority
CN
China
Prior art keywords
battery
thermocouple
temperature
insulating property
heat insulating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201611077878.0A
Other languages
Chinese (zh)
Other versions
CN107044996A (en
Inventor
倪备
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Changzhou Haoda Technology Co Ltd
Original Assignee
Changzhou Haoda Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Changzhou Haoda Technology Co Ltd filed Critical Changzhou Haoda Technology Co Ltd
Priority to CN201611077878.0A priority Critical patent/CN107044996B/en
Publication of CN107044996A publication Critical patent/CN107044996A/en
Application granted granted Critical
Publication of CN107044996B publication Critical patent/CN107044996B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to heat insulating property test device field more particularly to heat insulating property test device and test methods.Pass through external module and internal module;The external module includes computer and moisture recorder, and internal module includes high-and-low temperature humid heat test box, battery, the pedestal of PP plate and accumulator protecting set;Accumulator protecting is arranged with outside the battery to cover and pass through on the bracket that pedestal is arranged in high-and-low temperature humid heat test box, at least one aperture is provided on the battery cap of the battery;It is equipped with the first thermocouple in the aperture, mounting device is equipped between the first thermocouple and aperture;The second thermocouple is provided between the battery and accumulator protecting set;First, second thermocouple stretches out one end of battery and the moisture recorder outside high-and-low temperature humid heat test box connects, and moisture recorder is connect with computer;Make heat insulating property test device when testing accumulator protecting set heat-proof quality, conveniently observes and records temperature change, and facilitate fixed thermocouple.

Description

Heat insulating property test device and test method
Technical field
The present invention relates to heat insulating property test device field more particularly to heat insulating property test device and test methods.
Background technique
It generally will use accumulator protecting set when in automobile using battery, to realize the protection to battery;With vapour The development in vehicle field, the requirement to accumulator protecting set is also higher and higher, surveys to the heat-proof quality that accumulator protecting covers When examination, staff is needed to observe and record in real time the variation of temperature, it is not only time-consuming and laborious, but also it is easy to produce mistake Difference, and thermocouple is fixed more inconvenient, is easy to cause thermocouple to be corroded, influences service life.
Summary of the invention
The object of the present invention is to provide when testing accumulator protecting set heat-proof quality, temperature change is conveniently observed and recorded, And facilitate the heat insulating property test device and test method of fixed thermocouple.
Technical scheme is as follows:
Heat insulating property test device, which is characterized in that including external module and internal module;The external module includes electricity Brain and moisture recorder, internal module include high-and-low temperature humid heat test box, battery, the pedestal of PP plate and accumulator protecting set; It is arranged with accumulator protecting outside the battery to cover and pass through on the bracket that pedestal is arranged in high-and-low temperature humid heat test box, the storage At least one aperture is provided on the battery cap of battery;The first thermocouple, the first thermocouple and aperture are equipped in the aperture Between be equipped with mounting device;The second thermocouple is provided between the battery and accumulator protecting set;First, second heat Galvanic couple stretches out one end of battery and the moisture recorder outside high-and-low temperature humid heat test box connects, and moisture recorder and computer connect It connects.
There are three apertures for setting on the battery cap of the battery, and three apertures are transversely arranged.
The mounting device includes the first support plate, which is equipped with the first installation of the first thermocouple of installation Hole;The first thermocouple above first mounting hole is equipped with stop nut, on the first thermocouple below the first mounting hole Equipped with limit sleeve.
The mounting device includes the second support plate, which is equipped with the second installation of the first thermocouple of installation Hole;Second support plate bottom surface is fixed with the rubber sleeve with aperture transition fit, which is equipped with and the second mounting hole The jack being used cooperatively;The aperture inner wall is equipped with the annular protrusion being used cooperatively with rubber sleeve.
The rubber sleeve is hemispherical.
Branch the first fagging bottom surface is equipped with adhesive tape.
Third thermocouple is equipped in the high-and-low temperature humid heat test box, third thermocouple stretches out high-and-low temperature humid heat test box One end is connect with moisture recorder.
The test method of heat insulating property test device, characterized in that it comprises the following steps:
Step 1: the dilute sulfuric acid in battery being poured out and uses each slot in water repeated flushing battery;
Step 2: water is put into battery to battery five/everywhere;
Step 3: accumulator protecting to be measured being covered into confirmation sponge and attaches position;
Step 4: the first thermocouple being arranged on battery cap, the second thermocouple is arranged in battery and accumulator protecting Between set;
Step 5: placing the pedestal that PP plate surrounds on the bracket of high-and-low temperature humid heat test box, battery is put in PP board bottom On seat;
Step 6: accumulator protecting set is set on battery;
Step 7: the liquid temperature in confirmation battery, by 90 DEG C of temperature setting in high-and-low temperature humid heat test box;When height is warm and humid When temperature in wet heating testing case rises, the temperature of the first, second thermocouple of moisture recorder start recording;
Step 8: confirmation 10-15min temperature elapses situation, and testing after starting 5 hours terminates;
Step 9: saving data.
The first thermocouple is adjusted in the step 4 makes temperature measurement fraction at aperture center.
Confirm that the initial temperature in battery is maintained at 17 DEG C -28 DEG C in the step 7.
The beneficial effects of the present invention are: the temperature of baking oven is controlled, in order to electric power storage by setting high-and-low temperature humid heat test box The heat-proof quality test of accumulator protecting set is detected in set temperature in pond;Liquid in battery is detected by the first thermocouple Real time temperature, the second thermocouple detects the real time temperature between battery and accumulator protecting set, and two real time temperatures are passed Moisture recorder is passed, data are recorded by moisture recorder and passes data to computer, on computers displays temperature curve Variation diagram facilitates operator intuitively to observe the variation of temperature;Due to having detected liquid in battery respectively when detecting temperature Temperature between real time temperature and battery and the accumulator protecting set of body, facilitates and compares two temperature, with better The heat-proof quality of judgement material;By the way that the pedestal of PP plate is arranged, with simulated automotive internal structure, so that the temperature data obtained is more Precisely.
Detailed description of the invention
Through the following detailed description taken in conjunction with the accompanying drawings, present invention objects, features and advantages above-mentioned and other will become Obviously.
Wherein: Fig. 1 is schematic structural view of the invention;
Fig. 2 is the first supporting plate structure schematic diagram of the invention;
Fig. 3 is limit sleeve structural schematic diagram of the present invention;
Fig. 4 is the second supporting plate structure schematic diagram of the invention;
In attached drawing, 1 is computer, and 2 be moisture recorder, and 3 be high-and-low temperature humid heat test box, and 4 be battery, and 5 be pedestal, 6 It is bracket for accumulator protecting set, 7,9 be the first thermocouple, and 10 be the second thermocouple, and 11 be the first support plate, and 13 be limit spiral shell Mother, 14 be limit sleeve, and 15 be the second support plate, and 17 be upper plate, and 18 be lower plate, and 19 be the first stiffening plate, and 20 be the second stiffening plate.
Specific embodiment
It is shown in Figure 1, heat insulating property test device, which is characterized in that including external module and internal module;It is described outer Portion's module includes computer 1 and moisture recorder 2, and internal module includes the pedestal of high-and-low temperature humid heat test box 3, battery 4, PP plate 5 and accumulator protecting set 6;Accumulator protecting is arranged with outside the battery to cover and be arranged by pedestal in high-and-low temperature humid heat test On bracket 7 in case, at least one aperture is provided on the battery cap of the battery;The first thermocouple is equipped in the aperture 9, mounting device is equipped between the first thermocouple and aperture;The second thermoelectricity is provided between the battery and accumulator protecting set Even 10;First, second thermocouple stretches out one end of battery and the moisture recorder outside high-and-low temperature humid heat test box connects, Moisture recorder is connect with computer.By the way that high-and-low temperature humid heat test box is arranged, the temperature of baking oven is controlled, in order to which battery is being set Determine the heat-proof quality test of detection accumulator protecting set in temperature;The real-time temperature of liquid in battery is detected by the first thermocouple Degree, the second thermocouple detects the real time temperature between battery and accumulator protecting set, and two real time temperatures are passed to temperature Recorder is spent, data are recorded by moisture recorder and passes data to computer, the figure of displays temperature curvilinear motion on computers, Operator is facilitated intuitively to observe the variation of temperature;Due to having detected the reality of liquid in battery respectively when detecting temperature Temperature between Shi Wendu and battery and accumulator protecting set, facilitates and compares two temperature, preferably to judge material The heat-proof quality of material;By the way that the pedestal of PP plate is arranged, with simulated automotive internal structure, so that the temperature data obtained is more accurate.
There are three apertures for setting on the battery cap of the battery, and three apertures are transversely arranged.Pass through setting three Aperture is each provided with first thermocouple in corresponding three apertures, convenient to reality to detect the temperature of liquid in battery Shi Wendu is compared, so that obtained material thermal insulation performance is more accurate;It is transversely arranged due to being open, facilitate the first thermocouple Installation.
The mounting device includes the first support plate 11, which is equipped with the first peace of the first thermocouple of installation Fill hole;The first thermocouple above first mounting hole is equipped with stop nut 13, the first thermoelectricity below the first mounting hole Idol is equipped with limit sleeve 14.By the way that the first support plate is arranged, the fixation to the first thermocouple location on the one hand may be implemented, it is another Aspect can be realized the sealing to tapping;It must be cooperated by stop nut and limit sleeve, fix the position of the first thermocouple, So that the first thermocouple is located at the middle part of battery, avoids contact with the bottom end of battery;It transversely arranged is opened when using three Kong Shi, the first support plate due to be also it is transversely arranged continuous first support plate can be used, can guarantee three first in this way The height of thermocouple is identical, certainly when using two transversely arranged apertures, it is possible to use continuous to obtain the first support plate.
The mounting device includes the second support plate 15, which is equipped with the second peace of the first thermocouple of installation Fill hole;Second support plate bottom surface is fixed with the rubber sleeve with aperture transition fit, which is equipped with and the second installation The jack that hole is used cooperatively;The aperture inner wall is equipped with the annular protrusion being used cooperatively with rubber sleeve.By rubber sleeve with The limit to rubber sleeve may be implemented in the cooperation of annular protrusion;Due to being provided with jack on rubber sleeve, the insertion of the first thermocouple is inserted In hole, since the frictional force of rubber sleeve is larger, to realize the limit to the first thermocouple, the first heat is fixed in this way Galvanic couple, on the one hand fish installation easy to disassemble, on the other hand facilitates the depth for adjusting the insertion of the first thermocouple;Jack can use Bellmouth, effect are more preferable.
The rubber sleeve is hemispherical.Since rubber sleeve is in dome-type, so that rubber sleeve dream is preferably stuck in aperture.
Branch the first fagging bottom surface is equipped with adhesive tape.Facilitate the installation of the first support plate, enhancing sealing by the way that adhesive tape is arranged Effect.
First support plate includes the first enhancement layer 19 between upper plate 17, lower plate 18 and upper and lower plate;Described first Enhancement layer is one layer of wavy first stiffening plate.By the way that the first stiffening plate is arranged, and it is wavy, the first support plate of enhancing Intensity.
Second support plate includes the second enhancement layer 20 between top panel, lower panel and upper and lower panel;Described Two enhancement layers are one layer of wavy second stiffening plate.
Third thermocouple is equipped in the high-and-low temperature humid heat test box, third thermocouple stretches out high-and-low temperature humid heat test box One end is connect with moisture recorder.By in setting third thermocouple measurement experimental box temperature in order to participating in pair of temperature Than.
The test method of heat insulating property test device, characterized in that it comprises the following steps:
Step 1: the dilute sulfuric acid in battery being poured out and uses each slot in water repeated flushing battery;
Step 2: water is put into battery to battery five/everywhere;
Step 3: accumulator protecting to be measured being covered into confirmation sponge and attaches position;
Step 4: the first thermocouple being arranged on battery cap, the second thermocouple is arranged in battery and accumulator protecting Between set;
Step 5: placing the pedestal that PP plate surrounds on the bracket of high-and-low temperature humid heat test box, battery is put in PP board bottom On seat;
Step 6: accumulator protecting set is set on battery;
Step 7: the liquid temperature in confirmation battery, by 90 DEG C of temperature setting in high-and-low temperature humid heat test box;When height is warm and humid When temperature in wet heating testing case rises, the temperature of the first, second thermocouple of moisture recorder start recording;
Step 8: confirmation 10-15min temperature elapses situation, and testing after starting 5 hours terminates;
Step 9: saving data.By the first thermocouple and the second thermocouple to measure the measurement realized to real time temperature; The test of accumulator protecting set thermal insulation performance is carried out using the ambient temperature of high-and-low temperature humid heat test box control battery.
The first thermocouple is adjusted in the step 4 makes temperature measurement fraction at aperture center.The first thermocouple is allowed to be arranged in aperture At center, so that the temperature of test is more acurrate, but also the first thermocouple is not easy to be corroded.
Confirm that the initial temperature in battery is maintained at 17 DEG C -28 DEG C in the step 7.Initial temperature in battery is not Easily too low, too low influence heating rate is easy to cause experimental result less than normal;As experiment starts, battery temp is gradually risen, Heating rate is gradually reduced, so that initial temperature is smaller on experimental result influence, at 23 ± 5 DEG C (18 DEG C -28 DEG C), to reality It is minimum to test result influence.
First aluminium is put into the battery after rinsing in the step 2.The corruption of aluminium is observed in battery by the way that aluminium to be put into Erosion degree, to test whether internal storage battery cleans up.
The above is only presently preferred embodiments of the present invention, not does limitation in any form to the present invention, it is all according to According to any simple modification to the above embodiments in technical spirit of the invention, equivalent variations, guarantor of the invention is each fallen within Within the scope of shield.

Claims (3)

1. the test method of heat insulating property test device, characterized in that it comprises the following steps:
Step 1: the dilute sulfuric acid in battery being poured out and uses each slot in water repeated flushing battery;
Step 2: water is put into battery to battery five/everywhere;
Step 3: accumulator protecting to be measured being covered into confirmation sponge and attaches position;
Step 4: the first thermocouple being arranged on battery cap, the second thermocouple, which is arranged, covers it in battery and accumulator protecting Between;
Step 5: placing the pedestal that PP plate surrounds on the bracket of high-and-low temperature humid heat test box, battery is put in PP board bottom seat On;
Step 6: accumulator protecting set is set on battery;
Step 7: the liquid temperature in confirmation battery, by 90 DEG C of temperature setting in high-and-low temperature humid heat test box;When the damp and hot examination of high/low temperature When temperature in tryoff rises, the temperature of the first, second thermocouple of moisture recorder start recording;
Step 8: confirmation 10-15min temperature elapses situation, and testing after starting 5 hours terminates;
Step 9: saving data.
2. the test method of heat insulating property test device according to claim 1, which is characterized in that adjusted in the step 4 Whole first thermocouple makes temperature measurement fraction at aperture center.
3. the test method of heat insulating property test device according to claim 1, which is characterized in that in the step 7 really The initial temperature recognized in battery is maintained at 17 DEG C -28 DEG C.
CN201611077878.0A 2016-11-29 2016-11-29 Heat insulating property test device and test method Active CN107044996B (en)