CN107029958A - A kind of construction technology for fitting up special wood wax oil - Google Patents

A kind of construction technology for fitting up special wood wax oil Download PDF

Info

Publication number
CN107029958A
CN107029958A CN201710304349.8A CN201710304349A CN107029958A CN 107029958 A CN107029958 A CN 107029958A CN 201710304349 A CN201710304349 A CN 201710304349A CN 107029958 A CN107029958 A CN 107029958A
Authority
CN
China
Prior art keywords
wax oil
wood wax
ensured
construction technology
wood
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201710304349.8A
Other languages
Chinese (zh)
Inventor
施享
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Maanshan Niuze Technology Service Co Ltd
Original Assignee
Maanshan Niuze Technology Service Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Maanshan Niuze Technology Service Co Ltd filed Critical Maanshan Niuze Technology Service Co Ltd
Priority to CN201710304349.8A priority Critical patent/CN107029958A/en
Publication of CN107029958A publication Critical patent/CN107029958A/en
Withdrawn legal-status Critical Current

Abstract

The present invention relates to a kind of construction technology for fitting up special wood wax oil, its processing step is as follows:A stirrings, B are brushed for the first time, C clear up wait to do, D is brushed for second, E third times are brushed.Present invention process is simple, easy to operate, uses the stirring of preceding strength degree, ensure that coating is uniform and thin, plus the control of ventilated environment, make coating fast drying, three layers of brushing make its absorption fuller, color and luster is more anxious vivid, guarantee period viscosity and stability, effective waterproof and dustproof, mould proof etc., effectively save the usage amount of wood wax oil for a long time, it is cost-effective, increase economic efficiency.

Description

A kind of construction technology for fitting up special wood wax oil
Technical field
The present invention relates to a kind of construction technology for fitting up special wood wax oil.
Background technology
Wood wax oil is liked as the new coating for replacing painting by consumers in general.Wax in traditional wood wax oil is not Be dissolved in oil, in oil be in suspended state, the temperature of wood wax oil it is too high or it is too low can all influence decentralization of the wax in oil, cause Inequality is embrocated after construction, wood wax oil construction quality is influenceed.In addition, the drying temperature after the viscosity of wood wax oil and construction also can Directly influence the final construction quality of wood wax oil.The construction technology of current wood wax oil does not do strict rule to process above parameter Fixed, this, which also directly results in, is influenceed by workmen is different with construction environment, and wood wax oil construction quality alternates betwwen good and bad.
The content of the invention:
A kind of construction technology for fitting up special wood wax oil is provided the invention aims to overcome the shortcomings of the above.
Technical scheme includes:A kind of construction technology for fitting up special wood wax oil, its construction technology is as follows:
A, wood wax oil stirred, rest on 30min under 16-25 DEG C of ventilated environment;
B, use in room temperature and draughty environment, please Yi Zesi wood wax oils thoroughly stir before brushing, matter is used The brushing of measured mane bruss or artificial hairbrush uniform and thin is brushed in wood surface according to the grain direction of timber;
C, the wood wax oil for cleaning out with non-dust cloth residual, are placed in room temperature, the environment of drying 6-8 hours;
D, such as above-mentioned step B carry out second and brushed, it is ensured that uniform and thin, it is ensured that well-ventilated, 6-10 are placed at room temperature small When, after thorough drying to be coated, lightly polish wood surface using scouring pad;
E, such as above-mentioned step B carry out third time brushing, it is ensured that uniform and thin, it is ensured that well-ventilated, 8-12 are placed at room temperature small When, gently polish wood surface using scouring pad after drying.
Further improvement of the present invention is:The wood wax oil is being 400-600r/min using preceding stir speed (S.S.).
Further improvement of the present invention is:The ambient temperature control is at 18-26 DEG C.
Beneficial effects of the present invention:
Present invention process is simple, easy to operate, uses the stirring of preceding strength degree, it is ensured that coating is uniform and thin, adds ventilated environment Control, makes coating fast drying, and brushing for three layers makes that its absorption is fuller, and color and luster is more anxious vivid, it is ensured that phase viscosity and stability, Effective waterproof and dustproof, mould proof etc., effectively save the usage amount of wood wax oil for a long time, cost-effective, save manpower, improve economy Benefit.
Embodiment:
In order to deepen the understanding of the present invention, below in conjunction with embodiment, the invention will be further described, and the embodiment is only used In explaining the present invention, it is not intended to limit the scope of the present invention..
Embodiment 1
A kind of construction technology for fitting up special wood wax oil, its construction technology is as follows:
A, wood wax oil stirred, rest on 30min under 20 DEG C of ventilated environment;
B, use in room temperature and draughty environment, please Yi Zesi wood wax oils thoroughly stir before brushing, matter is used The brushing of measured mane bruss or artificial hairbrush uniform and thin is brushed in wood surface according to the grain direction of timber;
C, the wood wax oil for cleaning out with non-dust cloth residual, are placed in room temperature, the environment of drying 8 hours;
D, such as above-mentioned step B carry out second and brushed, it is ensured that uniform and thin, it is ensured that well-ventilated, 10 are placed at room temperature small When, after thorough drying to be coated, lightly polish wood surface using scouring pad;
E, such as above-mentioned step B carry out third time brushing, it is ensured that uniform and thin, it is ensured that well-ventilated, place 12 hours at room temperature, Gently wood surface is polished after drying using scouring pad.
Wherein wood wax oil is being 600r/min using preceding stir speed (S.S.)., ambient temperature control is at 20 DEG C.
Embodiment 2
A kind of construction technology for fitting up special wood wax oil, its construction technology is as follows:
A, wood wax oil stirred, rest on 30min under 16 DEG C of ventilated environment;
B, use in room temperature and draughty environment, please Yi Zesi wood wax oils thoroughly stir before brushing, matter is used The brushing of measured mane bruss or artificial hairbrush uniform and thin is brushed in wood surface according to the grain direction of timber;
C, the wood wax oil for cleaning out with non-dust cloth residual, are placed in room temperature, the environment of drying 6 hours;
D, such as above-mentioned step B carry out second and brushed, it is ensured that uniform and thin, it is ensured that well-ventilated, place 6 hours at room temperature, After thorough drying to be coated, lightly wood surface is polished using scouring pad;
E, such as above-mentioned step B carry out third time brushing, it is ensured that uniform and thin, it is ensured that well-ventilated, place 8 hours at room temperature, Gently wood surface is polished after drying using scouring pad.
Wherein wood wax oil is being 400r/min using preceding stir speed (S.S.)., ambient temperature control is at 18 DEG C.
Embodiment 3
A kind of construction technology for fitting up special wood wax oil, its construction technology is as follows:
A, wood wax oil stirred, rest on 30min under 25 DEG C of ventilated environment;
B, use in room temperature and draughty environment, please Yi Zesi wood wax oils thoroughly stir before brushing, matter is used The brushing of measured mane bruss or artificial hairbrush uniform and thin is brushed in wood surface according to the grain direction of timber;
C, the wood wax oil for cleaning out with non-dust cloth residual, are placed in room temperature, the environment of drying 8 hours;
D, such as above-mentioned step B carry out second and brushed, it is ensured that uniform and thin, it is ensured that well-ventilated, place 9 hours at room temperature, After thorough drying to be coated, lightly wood surface is polished using scouring pad;
E, such as above-mentioned step B carry out third time brushing, it is ensured that uniform and thin, it is ensured that well-ventilated, place 10 hours at room temperature, Gently wood surface is polished after drying using scouring pad.
Wherein wood wax oil is being 500r/min using preceding stir speed (S.S.)., ambient temperature control is at 26 DEG C.
Embodiment 4
A kind of construction technology for fitting up special wood wax oil, its construction technology is as follows:
A, wood wax oil stirred, rest on 30min under 20 DEG C of ventilated environment;
B, use in room temperature and draughty environment, please Yi Zesi wood wax oils thoroughly stir before brushing, matter is used The brushing of measured mane bruss or artificial hairbrush uniform and thin is brushed in wood surface according to the grain direction of timber;
C, the wood wax oil for cleaning out with non-dust cloth residual, are placed in room temperature, the environment of drying 7 hours;
D, such as above-mentioned step B carry out second and brushed, it is ensured that uniform and thin, it is ensured that well-ventilated, place 9 hours at room temperature, After thorough drying to be coated, lightly wood surface is polished using scouring pad;
E, such as above-mentioned step B carry out third time brushing, it is ensured that uniform and thin, it is ensured that well-ventilated, place 11 hours at room temperature, Gently wood surface is polished after drying using scouring pad.
Wherein wood wax oil is being 550r/min using preceding stir speed (S.S.)., ambient temperature control is at 21 DEG C.
Embodiment 5
A kind of construction technology for fitting up special wood wax oil, its construction technology is as follows:
A, wood wax oil stirred, rest on 30min under 22 DEG C of ventilated environment;
B, use in room temperature and draughty environment, please Yi Zesi wood wax oils thoroughly stir before brushing, matter is used The brushing of measured mane bruss or artificial hairbrush uniform and thin is brushed in wood surface according to the grain direction of timber;
C, the wood wax oil for cleaning out with non-dust cloth residual, are placed in room temperature, the environment of drying 8 hours;
D, such as above-mentioned step B carry out second and brushed, it is ensured that uniform and thin, it is ensured that well-ventilated, 10 are placed at room temperature small When, after thorough drying to be coated, lightly polish wood surface using scouring pad;
E, such as above-mentioned step B carry out third time brushing, it is ensured that uniform and thin, it is ensured that well-ventilated, place 10 hours at room temperature, Gently wood surface is polished after drying using scouring pad.
Wherein wood wax oil is being 600r/min using preceding stir speed (S.S.)., ambient temperature control is at 22 DEG C.
Embodiment 6
A kind of construction technology for fitting up special wood wax oil, its construction technology is as follows:
A, wood wax oil stirred, rest on 30min under 25 DEG C of ventilated environment;
B, use in room temperature and draughty environment, please Yi Zesi wood wax oils thoroughly stir before brushing, matter is used The brushing of measured mane bruss or artificial hairbrush uniform and thin is brushed in wood surface according to the grain direction of timber;
C, the wood wax oil for cleaning out with non-dust cloth residual, are placed in room temperature, the environment of drying 7 hours;
D, such as above-mentioned step B carry out second and brushed, it is ensured that uniform and thin, it is ensured that well-ventilated, place 9 hours at room temperature, After thorough drying to be coated, lightly wood surface is polished using scouring pad;
E, such as above-mentioned step B carry out third time brushing, it is ensured that uniform and thin, it is ensured that well-ventilated, place 12 hours at room temperature, Gently wood surface is polished after drying using scouring pad.
Wherein wood wax oil is being 500r/min using preceding stir speed (S.S.)., ambient temperature control is at 26 DEG C.
Explanation embodiments of the present invention are the foregoing is only, are not intended to limit the invention, for the technology of this area For personnel, within the spirit and principles of the invention, any modification, equivalent substitution and improvements made etc. should be included in Within protection scope of the present invention.

Claims (3)

1. a kind of construction technology for fitting up special wood wax oil, it is characterised in that:Its construction technology is as follows:
A, wood wax oil stirred, rest on 30min under 16-25 DEG C of ventilated environment;
B, use in room temperature and draughty environment, please Yi Zesi wood wax oils thoroughly stir before brushing, matter is used The brushing of measured mane bruss or artificial hairbrush uniform and thin is brushed in wood surface according to the grain direction of timber;
C, the wood wax oil for cleaning out with non-dust cloth residual, are placed in room temperature, the environment of drying 6-8 hours;
D, such as above-mentioned step B carry out second and brushed, it is ensured that uniform and thin, it is ensured that well-ventilated, 6-10 are placed at room temperature small When, after thorough drying to be coated, lightly polish wood surface using scouring pad;
E, such as above-mentioned step B carry out third time brushing, it is ensured that uniform and thin, it is ensured that well-ventilated, 8-12 are placed at room temperature small When, gently polish wood surface using scouring pad after drying.
2. a kind of construction technology for fitting up special wood wax oil according to claim 1, it is characterised in that:The wood wax oil exists The use of preceding stir speed (S.S.) is 400-600r/min.
3. a kind of construction technology for fitting up special wood wax oil according to claim 1, it is characterised in that:The ambient temperature Control is at 18-26 DEG C.
CN201710304349.8A 2017-05-03 2017-05-03 A kind of construction technology for fitting up special wood wax oil Withdrawn CN107029958A (en)