CN1070224C - 多功能隔离剂及其制造方法 - Google Patents

多功能隔离剂及其制造方法 Download PDF

Info

Publication number
CN1070224C
CN1070224C CN97100938A CN97100938A CN1070224C CN 1070224 C CN1070224 C CN 1070224C CN 97100938 A CN97100938 A CN 97100938A CN 97100938 A CN97100938 A CN 97100938A CN 1070224 C CN1070224 C CN 1070224C
Authority
CN
China
Prior art keywords
agent
water
isolating
caustic soda
soya
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN97100938A
Other languages
English (en)
Other versions
CN1163926A (zh
Inventor
张喜林
Original Assignee
WANG WUEHUAN
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WANG WUEHUAN filed Critical WANG WUEHUAN
Priority to CN97100938A priority Critical patent/CN1070224C/zh
Publication of CN1163926A publication Critical patent/CN1163926A/zh
Application granted granted Critical
Publication of CN1070224C publication Critical patent/CN1070224C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

多功能隔离剂及其制造方法,隔离剂由皂剂、滑石粉组成,皂剂:滑石粉=7∶3,皂剂由豆油渣、水、苛性钠、苯甲酸钠组成,以上各成分的含量为:豆油渣为10kg、水为10kg、苛性钠为1kg、苯甲酸钠为0.1kg。其制造方法为,将水加热到60-70℃,放入豆油渣待溶解后加入苛性钠、苯甲酸钠后煮沸2-4分钟。液体皂剂取出后与滑石粉混合搅拌均匀。本发明的隔离剂无毒、无三废污染、隔离性强,不但能用于湿凝土制品,还能用于水泥制品及其它需用模在常温下浇铸成型产品的隔离之用。其制造方法简单、成本低、便于运输。

Description

多功能隔离剂及其制造方法
多功能隔离剂主要用于水泥制品或混凝土等制品浇铸成型过程中与模隔离,便于脱模之用。
现有的隔离剂是以棉油渣为主要原料,其颜色为棕黑色,不能用于水泥制品的浇铸成型,用于混凝土产品浇铸成型时其成本又很高,它是液体状态,室外雨天不能使用,运输也很不方便。
本发明的目的是研制一种以豆油渣为主要原料的多功能隔离剂,该隔离剂不但能用于混凝土产品浇铸成型,而且还能用于水泥制品及其它用模在常温下浇铸成型制品的隔离之用。同时提供它的制造方法。
本发明的隔离剂由皂剂、化石粉组成,按容量百分比,皂剂为70-80、化石粉为20-30。皂剂由豆油渣、水、苛性钠、苯甲酸钠组成,按容量百分比,豆油渣为40-60、水为40-60、苛性钠为9-12、苯甲酸钠为0.1-0.2。
其制造方法为:将水放入容器内加热到60℃-70℃,再放入豆油渣后继续加温,待豆油渣溶解后放入苛性钠和苯甲酸钠,煮沸2-4分钟即成皂剂。液体皂剂取出后与化石粉混合,充分搅拌后成固体隔离剂。
使用时需再向固体隔离剂内加水溶解,其容积比例关系为,固体隔离剂∶水=1∶7-9。
本发明的隔离剂无毒、无易燃易爆性,无三废污染。它具有适用范围广,隔离性强、对被隔离产品本身质量无影响,成本低、使用运输方便的优点。它不但适用于混凝土产品浇铸成型,而且还适用于水泥产品及其它需用模在常温下浇铸成型产品的隔离之用。适用环境条件低,如雨天室外也能使用。其制造方法简单,生产中不产生三废污染,而且其主要原料豆油渣是废物利用。
实施例:取10Kg水放到铁锅内,将水加热到60℃-70℃,再取豆油渣10Kg放入铁锅的水中,继续加热,待豆油渣溶解后放入1Kg的苛性钠、0.1Kg的苯甲酸钠到内的溶液内,煮沸3分钟即成皂剂。液体皂剂取出后与化石粉混合,皂剂∶化石粉=7∶3,充分搅拌均匀后即成固体隔离剂。使用时再向固体隔离剂内添水,搅拌成糊状即可使用,固体隔离剂∶水=1∶8。

Claims (3)

1、多功能隔离剂,它由皂剂、滑石粉组成,其特征在于皂剂∶滑石粉=7∶3;皂剂由豆油渣、水、苛性钠、苯甲酸钠组成,以上各成份的含量为:豆油渣为10kg、水为10kg、苛性钠为1kg、苯甲酸钠为0.1kg。
2、根据权利要求1所述的多功能隔离剂,其特征在于在使用时需再向固体隔离剂内加水溶解,其比例关系为,固体隔离剂∶水=1∶7-9。
3、多功能隔离剂的制造方法,其特征在于将水放入容器内加热到60-70℃,再放入豆油渣后继续加温,待豆油渣溶解后放入苛性钠和苯甲酸酸钠,煮沸2-4分钟即成皂剂;液体皂剂取出后与滑石粉混合,充分搅拌后成固体隔离剂。
CN97100938A 1997-03-03 1997-03-03 多功能隔离剂及其制造方法 Expired - Fee Related CN1070224C (zh)