CN106955983A - A kind of device for reducing slab nose - Google Patents
A kind of device for reducing slab nose Download PDFInfo
- Publication number
- CN106955983A CN106955983A CN201710338859.7A CN201710338859A CN106955983A CN 106955983 A CN106955983 A CN 106955983A CN 201710338859 A CN201710338859 A CN 201710338859A CN 106955983 A CN106955983 A CN 106955983A
- Authority
- CN
- China
- Prior art keywords
- roll shaft
- water
- sparge pipe
- slab
- axis
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a kind of device for reducing slab nose, including roller support, water tank and roll shaft, roll shaft is fixedly mounted on rollers, and roll shaft is arranged in the casing of the water tank, sparge pipe is additionally provided with water tank, sparge pipe is located at the sidepiece of roll shaft, sparge pipe is parallel with roll shaft to be installed, the vertical height of sparge pipe axis is more than the vertical height of roll shaft axis, 35 hole for water sprayings are further opened with sparge pipe, the axis of hole for water spraying is vertical with the axis of roll shaft, water is also placed with water tank, and water surface elevation will be at least flooded at 1/3 below roll shaft, during work, sprayed water on the top of running water roll shaft in sparge pipe;The phenomenon that the present invention easily produces nose for existing continuous casting steel billet in process of production is improved, and the present invention has the characteristics of production cost is low, device is simple, substantially increases the safety in production performance and quality of slab.
Description
Technical field
The present invention relates to metal smelt sheet billet continuous casting field, more particularly to a kind of device for reducing slab nose.
Background technology
Cast is a key link in steel manufacture process, is responsible for and molten steel is become the important of definite shape finished product
Task.Slab, due to its special cooling characteristics, after slab passes through withdrawal straightening machine, is transported in continuous casting production process on roll shaft
In row course of conveying, the radiating of slab plane is uneven due to above and below, it may appear that nose phenomenon.Slab nose can give continuous casting
Adversely affect, show:1st, nose is too high can cause slab can not can cause production by gas flame cuttiug region, when serious
Stop;2nd, the slab of nose, because Action of Gravity Field can be popped up, may break the equipment such as cutting gun at the end of cutting;3、
Nose can cause slab outward appearance not good enough, if nose is above standard, and product quality be influenceed, particularly in special metal material sheet material
Continuous casting steel billet production process in, occur slab nose it is even more serious, when serious, can cause production pause accident, be based on
There is provided a kind of device for reducing slab nose for the defect of technology people in existing sheet billet continuous casting.
A kind of device for reducing slab nose disclosed by the invention can effectively solve the problem that the phenomenon of continuous casting steel billet nose so that
Slab can smoothly enter next road slab cutting action, improve the product quality of sheet material.
The content of the invention
It is an object of the invention to overcome the deficiencies of the prior art and provide a kind of device for reducing continuous casting steel billet nose,
To solve, existing continuous casting steel billet slab upper and lower surface in course of conveying is uneven in temperature to cause the technical problem of slab nose.
The present invention is achieved by the following technical solutions:The invention discloses a kind of device for reducing slab nose, bag
Roll shaft, roller support and water tank are included, roll shaft is fixedly mounted on rollers, and roll shaft is arranged in the casing of water tank, water
Sparge pipe is additionally provided with case, sparge pipe is located at the sidepiece of roll shaft, and sparge pipe is parallel with roll shaft to be installed, the vertical height of sparge pipe axis
Degree, which is more than on the vertical height of roll shaft axis, sparge pipe, is further opened with 3-5 hole for water spraying, the axis of hole for water spraying and the axis of roll shaft
Vertically, water is also placed with water tank, and water surface elevation will be at least flooded at 1/3 below roll shaft, during work, in sparge pipe from
Water is sprayed water to the top of the roll shaft.
Further, according to the difference of the production requirement of slab length, the number of roll shaft is 3-6, between roll shaft mutually
It is arranged in parallel, the distance between sparge pipe and roll shaft are 3-5cm.
Further, in order to preferably realize the radiating of roll shaft so that the upper and lower surface radiating of slab is uniform, sparge pipe
Installation site is at the 1/3-2/5 of roll shaft top.
The course of work is:Slab, by the thrust of withdrawal straightening machine, is sent to roll shaft simultaneously by the slab of continuous casting after withdrawal straightening machine
Move forward, because roll shaft is contacted all the time with slab, the time one is grown, the temperature rise of roll shaft, in prolonged operation,
Cause the radiating of slab top and bottom uneven, occur as soon as slab nose phenomenon, when serious, the production thing that production can be caused to pause
Barrier, by the application of the present apparatus, one is to carry out cooling processing by tank roll shaft, and two be the water jet roll shaft by sparge pipe
Water spray, is cooled again, at this moment roll shaft water spray, and one is due to that distance between roll shaft and slab is very short, and the temperature of roll shaft is very
Height, the water being sprayed onto on roll shaft can be gasificated into vapor, risen by vapor and cooled to below slab, and two be roll shaft water spray,
Roll temperatures can be reduced, when being contacted below slab with roll shaft, also partial heat can be taken away by roll shaft, also function to slab
Below play thermolysis, reach that the radiating of slab top and bottom is uneven, efficiently solve the slab nose phenomenon of continuous casting, adopt
With this indirect cool-down method, slab can not only be made to smoothly enter down cutting action together, it is ensured that slab cutting
It is smooth, and indirect cool-down method, cooling is gently, it is ensured that the uniformity of the immanent structure of special steel material, improves sheet material
Product quality.
It is disclosed by the invention it is a kind of reduce continuous casting steel billet nose device, can roll shaft radiated in time, improve
The radiating efficiency of roll shaft so that the upper and lower surface radiating of slab is balanced, improves the quality of continuous casting steel billet, substantially increases production
Security performance, can smoothly enter down together slab cutting action.
Brief description of the drawings
Fig. 1 is that sheet billet continuous casting produces schematic diagram;
Fig. 2 is sparge pipe and roll shaft scheme of installation;
Fig. 3 is sparge pipe structural representation.
Embodiment
Embodiments of the invention are elaborated below, the present embodiment is carried out lower premised on technical solution of the present invention
Implement, give detailed embodiment and specific operating process, but protection scope of the present invention is not limited to following implementations
Example.
Embodiment 1
Embodiment 1 discloses a kind of device for reducing continuous casting steel billet nose, as shown in Figure 1-2, including roll shaft 2, roll shaft branch
Seat 21 and water tank 1, roll shaft 2 is fixedly mounted on rollers 21, and roll shaft 2 is arranged in the casing of water tank 1, on water tank 1
Sparge pipe 3 is additionally provided with, the number that sparge pipe 3 is located at sparge pipe 3 and roll shaft 2 in the sidepiece of roll shaft 2, embodiment 1 is 3,
Arranged in parallel between roll shaft, the distance between sparge pipe 3 and roll shaft 2 are 3-5cm.Sparge pipe 3 is parallel with roll shaft 2 to be installed,
The vertical height of the axis of sparge pipe 3 is more than the vertical height of the axis of roll shaft 2, as shown in figure 3, being further opened with 4 sprays on sparge pipe 3
Water hole 31, the axis of hole for water spraying 31 is vertical with the axis of roll shaft 2, and water is also placed with water tank 1, and water surface elevation will at least flood
At the 1/3 of the lower section of roll shaft 2, during work, the top of the running water roll shaft 2 in sparge pipe 3 is sprayed water.The installation position of sparge pipe 3
It is set at the top of roll shaft 2 1/3.During work, the slab 5 of continuous casting is after withdrawal straightening machine, by the thrust of withdrawal straightening machine, by slab 5
It is sent to roll shaft 2 and moves forward, because roll shaft 2 is contacted all the time with the slab 5 of temperature hyperpyrexia, the time one is grown, the temperature of roll shaft 2
Degree rise, in prolonged operation, causes the radiating of the top and bottom of slab 5 uneven, occurs as soon as slab nose phenomenon, so will
Running water is passed through in toward sparge pipe 3, running water carries out spray cooling by the top of the roll shaft 2 of hole for water spraying 31, and then slab enters
Enter gas flame cuttiug process 4 to be cut, realize the continuous production of continuous casting steel billet.
Embodiment 2
Embodiment 2 discloses a kind of device for reducing continuous casting steel billet nose, including roll shaft 2, roller support 21 and water tank 1,
Roll shaft 2 is fixedly mounted on rollers 21, and roll shaft 2 is arranged in the casing of water tank 1, and sparge pipe is additionally provided with water tank 1
3, the number that sparge pipe 3 is located at sparge pipe 3 and roll shaft 2 in the sidepiece of roll shaft 2, embodiment 2 is 6, between roll shaft mutually
It is arranged in parallel, the distance between sparge pipe 3 and roll shaft 2 are 3-5cm.Sparge pipe 3 is parallel with roll shaft 2 to be installed, the axis of sparge pipe 3
Vertical height is more than the vertical height of the axis of roll shaft 2, is further opened with 4 hole for water sprayings 31 on sparge pipe 3, the axis of hole for water spraying 31 with
The axis of roll shaft 2 is vertical, and water is also placed with water tank 1, and water surface elevation will be at least flooded at the 1/3 of the lower section of roll shaft 2, work
When, the top of the running water roll shaft 2 in sparge pipe 3 is sprayed water.The installation site of sparge pipe 3 is at the top of roll shaft 2 2/5.Work
When making, slab 5, by the thrust of withdrawal straightening machine, is sent to roll shaft 2 and moved forward by the slab 5 of continuous casting after withdrawal straightening machine, by
Contacted all the time with the slab 5 of temperature hyperpyrexia in roll shaft 2, the time one is grown, the temperature rise of roll shaft 2 is being run for a long time
In, cause the radiating of the top and bottom of slab 5 uneven, occur as soon as slab nose phenomenon, so will be toward being passed through originally in sparge pipe 3
Water, running water carries out spray cooling by the top of the roll shaft 2 of hole for water spraying 31, and slab is carried out subsequently into gas flame cuttiug process 4
Cutting, realizes the continuous production of continuous casting steel billet.
Claims (3)
1. a kind of device for reducing slab nose, it is characterised in that including roller support, water tank and roll shaft, the roll shaft is fixed
On the rollers, and the roll shaft is arranged in the casing of the water tank, and water spray is additionally provided with the water tank
Pipe, the sparge pipe is located at the sidepiece of the roll shaft, and the sparge pipe is parallel with the roll shaft to be installed, the sparge pipe axis
Vertical height, which is more than on the vertical height of the roll shaft axis, the sparge pipe, is further opened with 3-5 hole for water spraying, the hole for water spraying
Axis it is vertical with the axis of the roll shaft, be also placed with water in the water tank, and water surface elevation will be at least flooded below roll shaft
1/3 at, during work, the running water in the sparge pipe is sprayed water to the top of the roll shaft.
2. the device of slab nose is reduced as claimed in claim 1, it is characterised in that the number of the roll shaft is 3-6, institute
State arranged in parallel between roll shaft and roll shaft, the distance between the sparge pipe and described roll shaft are 3-5cm.
3. the device of slab nose is reduced as claimed in claim 1, it is characterised in that the sparge pipe installation site is roll shaft
At the 1/3-2/5 of top.