CN106864157A - A kind of aircraft passenger compartment wallpaper damage revamping method - Google Patents

A kind of aircraft passenger compartment wallpaper damage revamping method Download PDF

Info

Publication number
CN106864157A
CN106864157A CN201710046809.1A CN201710046809A CN106864157A CN 106864157 A CN106864157 A CN 106864157A CN 201710046809 A CN201710046809 A CN 201710046809A CN 106864157 A CN106864157 A CN 106864157A
Authority
CN
China
Prior art keywords
wallpaper
ink
repairing
gummed paper
damage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710046809.1A
Other languages
Chinese (zh)
Inventor
黄志勇
杜卫峰
王建国
崔军
韩宁
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangzhou Aircraft Maintenance Engineering Co Ltd
Original Assignee
Guangzhou Aircraft Maintenance Engineering Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangzhou Aircraft Maintenance Engineering Co Ltd filed Critical Guangzhou Aircraft Maintenance Engineering Co Ltd
Priority to CN201710046809.1A priority Critical patent/CN106864157A/en
Publication of CN106864157A publication Critical patent/CN106864157A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of civil aircraft main cabin wallpaper damage revamping method, including step:S1, allocates ink:S1 1, gathers existing wallpaper color data, and set up color database by Ai Seli spectroscopes;S1 2, toning:Primary colours ratio needed for analyzing repairing wallpaper using spectroscope, is mixed colours in proportion, and the primary colours meet the requirement of Boeing specification BMS10 73;S2, takes the clean damaged wallpaper surface dirt of cleansing tissue cleaning, and repair on technical condition damage field is protected to damage field surrounding patch one side gummed paper;S3, repairing position is applied to writing brush by step S1 gained ink, smoothens and make ink thickness to be differed with surrounding wallpaper thickness no more than 0.2mm;S4, removes one side gummed paper;S5, ink dry times 6 to 8 hours under normal temperature, or using thermal chimney low temperature shelves, air duct mouthful apart from the uniform heating of 10 to 15 centimeters of distances of mend 10 to 15 minutes.The present invention has easily operated, and repairing is time-consuming short, and repair efficiency is good, nonpoisonous and tasteless advantage.

Description

A kind of aircraft passenger compartment wallpaper damage revamping method
Technical field
The present invention relates to a kind of aircraft passenger compartment wallpaper damage revamping method.
Background technology
Civil aircraft main cabin wallpaper, if there is breakage, can be to be continuing with the case where aviation safety is not influenceed 's.But the part of breakage can influence its attractive in appearance, if changing whole wallpaper because of the small breakage of its appearance, not only increase maintenance Cost, also increases maintenance cycle.
Prior art is repaired by the way of digging, and it has following weak point:1st, digging effect is bad, There is apparent border;2nd, special digging instrument need to be used, is taken;3rd, the repairing of curved surface wallpaper can not be met.
The content of the invention
The present invention does the technical problem to be solved, and is just to provide a kind of civil aircraft main cabin wallpaper damage revamping method.
Above-mentioned technical problem is solved, the technical solution adopted in the present invention is as follows:
A kind of civil aircraft main cabin wallpaper damage revamping method, it is characterized in that comprising the following steps:
S1, allocates ink
S1-1, gathers existing wallpaper color data, and set up color database by Ai Seli spectroscopes;
S1-2, toning:Primary colours ratio needed for analyzing repairing wallpaper using spectroscope, is mixed colours in proportion, the primary colours Meet the requirement of Boeing specification BMS10-73;
S2, takes the clean damaged wallpaper surface dirt of cleansing tissue cleaning, and repair on technical condition damage field is pasted to damage field surrounding One side gummed paper is protected;
S3, repairing position is applied to writing brush by step S1 gained ink, smoothens and make ink thickness thick with surrounding wallpaper Degree difference is no more than 0.2mm;
S4, removes one side gummed paper;
S5, ink dry times 6 to 8 hours under normal temperature, or using thermal chimney low temperature shelves, air duct mouthful apart from mend 10 Uniformly heated 10 to 15 minutes to 15 centimeters of distances.
The beneficial effects of the invention are as follows:This method for repairing and mending has easily operated, and repairing is time-consuming short, and repair efficiency is good, nontoxic Tasteless advantage.
Specific embodiment
Embodiment one, sets up primary colours database such as table 1 below,
The primary colours database (part) of table 1
BAC93203 decorative patterns BAC93203 background colors
Specification number Piece number Weight Specification number Piece number Weight
BMS10-107BL 5587470018 0.222g BMS10-107BL 5587470018 0.017g
BMS10-107RO 5587470223 0.003g BMS10-107RO 5587470223 0.006g
BMS10-107YG 5587470222 0.122g BMS10-107YG 5587470222 0.045g
BMS10-107W 5587470112 29.653g BMS10-107W 5587470112 29.932g
Damaged wallpaper is analyzed using spectroscope, and draws required ink ratio such as table 2 below, adjusted in proportion Color;
The primary colours ratio of table 2
Repaired using the ink for mixing up color, according to the following steps:A, take the damaged wallpaper surface ash of clean cleansing tissue cleaning Dirt, repair on technical condition damage field, and damage field surrounding patch one side gummed paper is protected.B, ink is applied to writing brush is repaiied Cover is put, and smoothens and make ink to be differed with surrounding wallpaper thickness no more than 0.2mm;C, removal one side gummed paper;Ink under d, normal temperature 6 hours drying times.
Embodiment two, allotment ink is with embodiment one, repairing:A, the damaged wallpaper surface dirt of clean cleansing tissue cleaning is taken, Repair on technical condition damage field, and damage field surrounding patch one side gummed paper is protected.B, ink is applied to repairing with writing brush Position, smoothens and makes ink to be differed with surrounding wallpaper thickness no more than 0.2mm;C, removal one side gummed paper;Ink dries under d, normal temperature 8 hours dry time.
Embodiment three, allotment ink is with embodiment one, repairing:A, the damaged wallpaper surface dirt of clean cleansing tissue cleaning is taken, Repair on technical condition damage field, and damage field surrounding patch one side gummed paper is protected.B, ink is applied to repairing with writing brush Position, smoothens and makes ink to be differed with surrounding wallpaper thickness no more than 0.2mm;C, removal one side gummed paper;It is d, low using thermal chimney Warm shelves, air duct mouthful was apart from the uniform heating of 10 to 15 centimeters of distances of mend 10 to 15 minutes.
Three kinds of repairing results of method:Surface bonding is firm, and repairing color is basically identical with wallpaper color.

Claims (1)

1. a kind of civil aircraft main cabin wallpaper damage revamping method, it is characterized in that comprising the following steps:
S1, allocates ink
S1-1, gathers existing wallpaper color data, and set up color database by Ai Seli spectroscopes;
S1-2, toning:Primary colours ratio needed for analyzing repairing wallpaper using spectroscope, is mixed colours in proportion, and the primary colours meet The requirement of Boeing specification BMS10-73;
S2, takes the clean damaged wallpaper surface dirt of cleansing tissue cleaning, and repair on technical condition damage field pastes one side to damage field surrounding Gummed paper is protected;
S3, repairing position is applied to writing brush by step S1 gained ink, smoothens and make ink thickness with surrounding wallpaper thickness phase Difference is no more than 0.2mm;
S4, removes one side gummed paper;
S5, ink dry times 6 to 8 hours under normal temperature, or using thermal chimney low temperature shelves, air duct mouthful apart from mend 10 to 15 The uniform heating of centimetre distance 10 to 15 minutes.
CN201710046809.1A 2017-01-22 2017-01-22 A kind of aircraft passenger compartment wallpaper damage revamping method Pending CN106864157A (en)