CN106758912A - 碳纤维氯化聚乙烯橡塑粉末合成胶板 - Google Patents
碳纤维氯化聚乙烯橡塑粉末合成胶板 Download PDFInfo
- Publication number
- CN106758912A CN106758912A CN201611119219.9A CN201611119219A CN106758912A CN 106758912 A CN106758912 A CN 106758912A CN 201611119219 A CN201611119219 A CN 201611119219A CN 106758912 A CN106758912 A CN 106758912A
- Authority
- CN
- China
- Prior art keywords
- carbon fiber
- plastic powder
- rubber
- haloflex
- offset plate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了碳纤维氯化聚乙烯橡塑粉末合成胶板,一种由网格式碳纤维的高韧性、耐高温、耐低温、防断裂添加氯化聚乙烯的附着性、高密度、耐酸碱防渗漏及橡塑粉末的高韧性、高密度、耐高温、耐低温、耐酸碱、耐磨损、抗重力等合成形成成型的胶板,修补因受热胀冷缩和受力年久及沉降与磨损老化等造成断裂、裂痕、裂口等构成的指示错觉和模糊不清及时维护修补更换。利用取氯化聚乙烯先期加热溶解与橡塑粉末(视产品添加发光材料)充分均匀稀释置入相应模具槽;而后平铺添加网格式碳纤维进行合成;置入相应模具槽进行冷却形成规格的碳纤维氯化聚乙烯橡塑粉末合成胶板。
Description
技术领域
本发明专利涉及一种危险警示安全提示主体标识等多领域用途的交通路标及导向,公路、高速路面、路基、路沿、出入口、减速、限速、目的地、景点、服务区及反光标识易受热胀冷缩、磨损及沉降,形成断裂、裂痕、裂口等造成模糊不清,指示错觉,必须经常维护及时修补,利用碳纤维加氯化聚乙烯加橡塑粉末合成的成型胶板(简称“碳纤维氯化聚乙烯橡塑粉末合成胶板)。
背景技术
基于现有公路、高速路面、路基、路沿、出入口、减速、限速、目的地、景点、服务区及反光标识等,受热胀冷缩和受力年久及沉降与磨损自然老化等影响,形成断裂、裂痕、裂口等造成指示错觉和模糊不清且经常维护不便。
发明内容
利用网格式碳纤维的韧性、耐高温、耐低温、防断裂添加氯化聚乙烯的附着性、高
密度防渗及橡塑粉末的高韧性、高密度、耐高温、耐低温、耐酸碱、耐磨损、抗重力等合成形成成型胶板,修补因受热胀冷缩和受力年久及沉降与磨损自然老化等造成断裂、裂痕、裂口等构成的指示错觉和模糊不清及时维护修补更换。
本发明所述一种碳纤维氯化聚乙烯橡塑粉末合成胶板包括:网格式碳纤维、氯化聚乙烯、橡塑粉末等组成。
具体实施方式
以下结合实施技术发明专利进行详细说明。
本发明所述一种碳纤维氯化聚乙烯橡塑粉末合成胶板包括:网格式碳纤维、氯化聚乙烯、橡塑粉末等组成。
本发明网格式碳纤维的特性:高韧性、耐高温、耐低温、防断裂、增强拉力;提高受力强度等。
氯化聚乙烯的特性:附着性、高密度、防渗、防漏、耐常温、耐酸碱等。
橡塑粉末特性:高韧性、高密度、耐高温、耐低温、耐酸碱、耐磨损、抗重力等。
碳纤维氯化聚乙烯橡塑粉末合成胶板特点:产品标准化,颜色多元化,可模印字形,可切割雕刻,施工方便快捷,边缘没有棱角,边角具有斜度等。
实施例1
本发明由网格式碳纤维的高韧性、耐高温、耐低温、防断裂添加氯化聚乙烯的附着性、高密度耐酸碱防渗漏及橡塑粉末的高韧性、高密度、耐高温、耐低温、耐酸碱、耐磨损、抗重力等合成形成成型胶板,修补因受热胀冷缩和受力年久及沉降与磨损老化等造成断裂、裂痕、裂口等构成的指示错觉和模糊不清及时维护修补更换。
本发明所述一种碳纤维氯化聚乙烯橡塑粉末合成胶板包括:网格式碳纤维、氯化聚
乙烯、橡塑粉末等组成。
加工方法:取氯化聚乙烯先期加热溶解与橡塑粉末(视产品添加发光材料)充分均匀
稀释置入相应模具槽;而后平铺添加网格式碳纤维进行合成;置入相应模具槽进行冷却形成规格的碳纤维氯化聚乙烯橡塑粉末合成胶板。
应用作业:取碳纤维氯化聚乙烯合橡塑粉末成胶板通过高温加热溶解表面对主体进
行粘合构成标识、导向、修补等作业。
现场施工方案:取氯化聚乙烯先期加热溶解加入反光剂添加橡塑粉末充分稀释置入
相应设备槽再添加平铺网格式碳纤维进行合成对主体作业面粘合,形成快速的、规格的碳纤维氯化聚乙烯橡塑粉末合成标识、导向、修补等作业。
Claims (5)
1.一种碳纤维氯化聚乙烯橡塑粉末合成胶板,由网格式碳纤维的高韧性、耐高温、耐低温、防断裂添加氯化聚乙烯的附着性、高密度、耐酸碱防渗漏及橡塑粉末的高韧性、高密度、耐高温、耐低温、耐酸碱、耐磨损、抗重力等合成形成成型胶板,修补因受热胀冷缩和受力年久及沉降与磨损老化等造成断裂、裂痕、裂口等构成的指示错觉和模糊不清及时维护修补更换。
2.根据权利要求所述的碳纤维氯化聚乙烯橡塑粉末合成胶板,其特征在于:碳纤维。
3.根据权利要求所述的碳纤维氯化聚乙烯橡塑粉末合成胶板,其特征在于:氯化聚乙烯。
4.根据权利要求所述的碳纤维氯化聚乙烯橡塑粉末合成胶板,其特征在于:橡塑粉末。
5.根据权利要求所述的碳纤维氯化聚乙烯橡塑粉末合成胶板,其特征在于:碳纤维加氯化聚乙烯橡塑粉末合成的胶板。