CN106739400A - A kind of Optical transparent adhesive applying method - Google Patents

A kind of Optical transparent adhesive applying method Download PDF

Info

Publication number
CN106739400A
CN106739400A CN201611060831.3A CN201611060831A CN106739400A CN 106739400 A CN106739400 A CN 106739400A CN 201611060831 A CN201611060831 A CN 201611060831A CN 106739400 A CN106739400 A CN 106739400A
Authority
CN
China
Prior art keywords
substrate
tool
transparent adhesive
optical transparent
laminating
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201611060831.3A
Other languages
Chinese (zh)
Other versions
CN106739400B (en
Inventor
黄建发
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Ningbo Vision Optoelectronics Co Ltd
Original Assignee
Ningbo Vision Optoelectronics Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ningbo Vision Optoelectronics Co Ltd filed Critical Ningbo Vision Optoelectronics Co Ltd
Priority to CN201611060831.3A priority Critical patent/CN106739400B/en
Publication of CN106739400A publication Critical patent/CN106739400A/en
Application granted granted Critical
Publication of CN106739400B publication Critical patent/CN106739400B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention provides a kind of Optical transparent adhesive applying method, belong to coating technique field.The method includes for first substrate being attached to the first laminating platform surface, is arranged side by side in the first direction with tool;Roller of fitting is acted on into the second film layer positioned at Optical transparent adhesive first end, drives laminating roller to roll the second film layer so that the one side of the glue-line of Optical transparent adhesive fits in the first surface of tool and first substrate;By the first end of second substrate close to tool first surface;Roller of fitting is acted on the first end of second substrate, drives laminating roller to roll second substrate so that second substrate fits in the first face of glue-line.By introducing tool, the bubble and edge glue-line that the Optical transparent adhesive edge during laminating between first substrate and second substrate is introduced damage the harmful effect brought to product and are transferred to tool, are effectively improved the yield of optical clear glue laminating.

Description

A kind of Optical transparent adhesive applying method
Technical field
The present invention relates to coating technique field, in particular to a kind of Optical transparent adhesive applying method.
Background technology
Optical transparent adhesive (Optically Clearance Adhesive, OCA) is to make without base optics acrylic glue Material, is a kind of two-sided glue band without matrix material then in upper and lower bottom one layer of release film of each laminating.Because it possesses High light transmittance, adhesion high, high durable and water resistance, high temperature resistant, uvioresistant, caliper uniformity are good, for a long time using will not Produce yellow (xanthochromia), stripping and rotten characteristic and be used widely.OCA edges may during existing OCA laminatings Introduce bubble and even result in the glue-line damage of OCA edges, influence the binding yield of product.
The content of the invention
In view of this, it is an object of the invention to provide a kind of Optical transparent adhesive applying method, effectively to improve above-mentioned Problem.
A kind of Optical transparent adhesive applying method is the embodiment of the invention provides, the Optical transparent adhesive includes what is be stacked First film layer, glue-line and the second film layer.Methods described includes:First substrate is attached to the first laminating platform surface, near pre- The tool of the first laminating platform is first arranged on, and is arranged side by side in the first direction with the tool, wherein, the tool Difference between the thickness of thickness and the first substrate is within a preset range;The optics after first film layer will be peeled off First surface of the first end of transparent adhesive tape close to the tool;Laminating roller is acted on positioned at the Optical transparent adhesive first end Second film layer, drive it is described laminating roller along the first direction roll second film layer so that the optical clear The glue-line of glue fits in the first surface of the tool and the first surface of the first substrate;Peel off the Optical transparent adhesive Second film layer to expose the glue-line, by the first end of second substrate close to the tool first surface;The laminating is rolled Wheel acts on the first end of the second substrate, drive the laminating roller along the first direction roll the second substrate with The second substrate is set to fit in surface of the glue-line away from the first substrate.
Further, the opposite side of the first laminating platform is provided with the second laminating platform, and described will peel off institute State the first end of the Optical transparent adhesive after the first film layer close to the tool first surface the step of, including:Will be described Second film layer of Optical transparent adhesive is attached to the surface relative with the described first laminating platform of the second laminating platform;By the light The first film layer for learning transparent adhesive tape is peeled off;The second laminating platform is inclined so that the first end of the Optical transparent adhesive is described in The first surface of tool.
Further, described the second film layer acted on roller of fitting positioned at the Optical transparent adhesive first end, drives The dynamic laminating roller rolls second film layer so that the glue-line of the Optical transparent adhesive fits in described controlling in the first direction The step of first surface of the first surface of tool and the first substrate, including:Laminating roller is acted on positioned at the optics Second film layer of transparent adhesive tape first end;Drive the second laminating platform relative to the described first laminating platform along the first party To motion;The laminating roller is driven to roll second film along the first direction with the motion of the described second laminating platform Layer, so that second film layer departs from the second laminating platform, and makes the glue-line of the Optical transparent adhesive fit in described controlling The first surface of the first surface of tool and the first substrate.
Further, the second film layer of the described stripping Optical transparent adhesive to be to expose the glue-line, by second substrate First end close to the tool first surface the step of, including:Second film layer of the Optical transparent adhesive is peeled off to reveal Go out the glue-line;The second substrate is attached to the table relative with the described first laminating platform of the second laminating platform Face;Incline it is described second laminating platform so that the second substrate first end close to the tool first surface.
Further, it is described the step of second film layer of the Optical transparent adhesive is peeled off, including:Dyestripping roller is made For the second film layer of the first end positioned at the Optical transparent adhesive;Drive the dyestripping roller from the Optical transparent adhesive One end, move to peel off second film layer along the first direction.
Further, the described first end that the laminating roller is acted on the second substrate, drives the laminating Roller rolls the second substrate so that the second substrate fits in the glue-line away from described first along the first direction After the step of surface of substrate, methods described also includes:Second base of the removal on the first surface of the tool Plate and the glue-line.
Further, the second film layer of the described stripping Optical transparent adhesive to be to expose the glue-line, by second substrate First end close to the tool first surface the step of before, methods described also includes:Removal is fitted in the tool The Optical transparent adhesive of first surface.
Further, the step of Optical transparent adhesive of the first surface that described removal is fitted in the tool, bag Include:The Optical transparent adhesive is cut open along the tool with the junction of the first substrate;Stripping is fitted in the tool First surface Optical transparent adhesive.
Further, the first surface of the tool posts the mould release membrance that one or more layers does not stay cull in advance.Described The step of Optical transparent adhesive of the first surface that stripping is fitted in the tool, including:Remove and be fitted in the tool in advance The mould release membrance of first surface is peeling off the Optical transparent adhesive being fitted on the mould release membrance.
Further, the described first end that the laminating roller is acted on the second substrate, drives the laminating Roller rolls the second substrate so that the second substrate fits in the glue-line away from described first along the first direction After the step of surface of substrate, methods described also includes:Second base of the removal on the first surface of the tool Plate.
Optical transparent adhesive applying method provided in an embodiment of the present invention by introducing tool, by first substrate during laminating The bubble and edge glue-line that Optical transparent adhesive edge and second substrate between is introduced damage the harmful effect brought to product Tool is transferred to, the yield of optical clear glue laminating is effectively improved.
Brief description of the drawings
Technical scheme in order to illustrate more clearly the embodiments of the present invention, below will be attached to what is used needed for embodiment Figure is briefly described, it will be appreciated that the following drawings illustrate only certain embodiments of the present invention, thus be not construed as it is right The restriction of scope, for those of ordinary skill in the art, on the premise of not paying creative work, can also be according to this A little accompanying drawings obtain other related accompanying drawings.
Fig. 1 shows the method flow diagram of the Optical transparent adhesive applying method that first embodiment of the invention is provided;
Fig. 2 shows first substrate and tool that first embodiment of the invention provides in the first arrangement fitted on platform Put schematic diagram;
Fig. 3 shows a kind of work of the Optical transparent adhesive applying method of first embodiment of the invention offer in application scenarios Skill flow chart;
Fig. 4 shows the method flow diagram of the Optical transparent adhesive applying method that second embodiment of the invention is provided;
Fig. 5 shows a kind of work of the Optical transparent adhesive applying method of second embodiment of the invention offer in application scenarios Skill flow chart;
Fig. 6 shows a kind of work of the Optical transparent adhesive applying method of third embodiment of the invention offer in application scenarios Skill flow chart;
Fig. 7 shows the A-A sectional views of Fig. 6.
Specific embodiment
Optical transparent adhesive (Optically Clearance Adhesive, OCA) includes the heavy mould release membrance, the glue that are stacked Layer and light mould release membrance, are widely used in laminating of the soft base material to the laminating (such as volume to volume), soft base material and hard base material of soft base material Processing procedure.When the laminating processing procedure such as flexible film for being applied to soft base material and hard base material attaches hard substrate, laminating flow is usually: Hard base material is fixed on platform surface by vacuum suction;The light mould release membrance of OCA is removed, by the close hard base material of OCA one end Initiating terminal;Roller is acted on the OCA of the initiating terminal of hard base material, driving rolls is pushed so that one end of OCA is fitted in The initiating terminal of hard base material;Driving rolls rolls the other end to OCA so that the glue-line of OCA is fitted in hard base material from one end of OCA Surface;The heavy mould release membrance for removing the OCA for being fitted in hard substrate surface exposes glue-line;By one end of soft base material near hard base material The glue-line of initial end surfaces;Roller acts on one end of the soft base material, driving rolls push cause one end of soft base material with The glue-line laminating of the initial end surfaces of hard base material;Driving rolls rolls the other end to OCA so that soft base from one end of soft base material Material laminating film surface.
In above-mentioned laminating flow, due to when the light mould release membrance of OCA is removed with weight mould release membrance, driving rolls push by Bubble may be introduced when fitting to OCA film surfaces when OCA fits to hard substrate surface and by soft base material very at OCA edges To the damage for causing edge OCA glue-lines.Subsequent configuration OCA deaeration techniques are generally needed, the bubble produced during laminating is removed. Additionally, edge glue-line damages the defect brought to product to be difficult to repair, the yield of OCA laminatings is significantly reduced.
In consideration of it, the embodiment of the invention provides a kind of Optical transparent adhesive applying method, be mainly used in flexible base board with The laminating of hard substrate, OCA edges introduce bubble and the damage of OCA edges glue-line etc. no in effectively improving existing laminating processing procedure The low problem of the good OCA binding yields for causing.
Optical transparent adhesive applying method provided in an embodiment of the present invention will be described in detail below.Obviously, it is described Embodiment be a part of embodiment of the invention, rather than whole embodiments.Generally described and illustrated in accompanying drawing herein The component of the embodiment of the present invention can be arranged and designed with a variety of configurations.Therefore, below in the accompanying drawings providing The detailed description of embodiments of the invention is not intended to limit the scope of claimed invention, but is merely representative of the present invention Selected embodiment.Based on the embodiment in the present invention, those of ordinary skill in the art are not making creative work premise Lower obtained every other embodiment, belongs to the scope of protection of the invention.
It should be noted that:Similar label and letter represents similar terms in following accompanying drawing, therefore, once a certain Xiang Yi It is defined in individual accompanying drawing, then it need not be further defined and explained in subsequent accompanying drawing.
In the description of the invention, it is necessary to explanation, term " on ", the orientation of the instruction such as D score or position relationship be base In orientation shown in the drawings or position relationship, or the orientation usually put when using of the invention product or position relationship, only It is to be described with simplified for the ease of the description present invention, must be with specific rather than the device or element for indicating or imply meaning Orientation, with specific azimuth configuration and operation, therefore be not considered as limiting the invention.Additionally, term " first ", " the Two " etc. it is only used for distinguishing description, and it is not intended that indicating or implying relative importance.
In the description of the invention, in addition it is also necessary to explanation, unless otherwise clearly defined and limited, term " setting ", " connection " should be interpreted broadly, for example, it may be being fixedly connected, or being detachably connected, or be integrally connected;Can be Mechanically connect, or electrically connect;Can be joined directly together, it is also possible to be indirectly connected to by intermediary, can be two The connection of element internal.For the ordinary skill in the art, with concrete condition above-mentioned term can be understood in the present invention In concrete meaning.
Fig. 1 shows the method flow diagram of the Optical transparent adhesive applying method that first embodiment of the invention is provided.Refer to Fig. 1, Optical transparent adhesive applying method provided in an embodiment of the present invention includes:
Step S110, the first laminating platform surface is attached to by first substrate, is fitted near being set in advance in described first The tool of platform, and be arranged side by side in the first direction with the tool;
In cartesian coordinate system (X, Y, Z) shown in Fig. 2, the first laminating platform is located on X/Y plane, and X-direction is the first patch The length direction of platform is closed, Y-direction is the width of the first laminating platform, and Z-direction is perpendicular to the side of the first laminating platform To.Tool 400 can be set in advance on the first laminating platform, the size of the first substrate 200 that its size is fitted as needed Set.Specifically, the difference between the thickness (Z-direction) of the tool 400 and the thickness (Z-direction) of the first substrate 200 Within a preset range.The preset range is acceptable error range, within the range, will not be brought to OCA binding yields Influence, can specifically determine according to many experiments.Certainly, thickness of the thickness of tool 400 preferably with first substrate 200 is equal. Additionally, for effect of preferably being fitted, the width (Y of the width (Y-direction) more than or equal to first substrate 200 of tool 400 Direction).
Specifically, first substrate 200 can be attached into the first laminating using the method for vacuum suction or other means Platform surface.As shown in Fig. 2 the first direction described in step S110 can be X-direction, first substrate 200 exists with tool 400 It is arranged side by side in X-direction.Wherein, the second side 220 of first substrate 200 fits with the first side 420 of tool 400.Need It is noted that when the first side 420 of tool 400 and the second side 220 of first substrate 200 are respectively provided with flatness higher When, can be similar between first side 420 and second side 220 very close to each other;When first side 420 or second side 220 Flatness it is relatively low when, might have gap between the two, but in order to reach preferable OCA laminatings effect, the gap is less than 2 millis Rice is preferably.
Step S120, will peel off the first end of the Optical transparent adhesive after first film layer close to the of the tool One surface;
Wherein, Optical transparent adhesive (OCA) includes the first film layer 450, the film layer 150 of glue-line 300 and second that are stacked.The One film layer 450 is the light mould release membrance of OCA, and the second film layer 150 is the heavy mould release membrance of OCA.It should be appreciated that in order to paste OCA damage of edges and edge introducing bubble etc. are bad caused by closing is transferred to the surface of tool 400, employed in the present embodiment Length of the length of OCA more than first substrate 200.Also, consider on material from being saved, width and the first substrate 200 of OCA Width is adapted to, length of the difference between the length of OCA and the length of first substrate 200 less than or equal to tool 400.
Traditional OCA applying methods, the OCA sizes for using are consistent with the size of the i.e. first substrate 200 of product, in laminating Need aligning accuracy higher.And the length of the OCA that this OCA applying methods are used is more than the length of first substrate 200, to laminating Aligning accuracy requirement before is relatively low.
OCA is fitted with first substrate 200, it is necessary to first remove the first film layer 450, be then by the first end of the OCA First surface 410 of the first end of the glue-line 300 of OCA close to tool 400.It should be noted that in the present embodiment, it is " close " to answer Make the understanding of broad sense, can be very close to but do not contact, or contact.That is, the now first end of OCA 310 can with the first surface 410 of tool 400 very close to but do not contact, it is also possible to the first surface 410 with tool 400 It is in contact.
In a kind of application scenarios of Optical transparent adhesive applying method provided in an embodiment of the present invention, such as by the optical lens When gelatin applying method is applied to OCA make-up machines, the opposite side of the first laminating platform is provided with the second laminating platform 50, and the One laminating platform and the second laminating platform 50 can be moved in 6 dimensions, you can be put down with X-direction, Y-direction, Z-direction Move, rotated in XZ directions, YZ directions and XY directions.
Now, as shown in figure 3, the concrete technology flow process of step S120 can be:
Second film layer 150 of OCA is attached to the surface relative with the first laminating platform 100 of the second laminating platform 50, As shown in (I) figure in Fig. 2.For example, the second laminating platform 50 can adsorb OCA by way of vacuum suction.Wherein, OCA Length and the length of first substrate 200 between difference be δ L1, the length of tool 400 is L, δ L1≤L.
First film layer 450 of OCA is peeled off.Specifically, as shown in (I) figure in Fig. 3, can be by dyestripping roller 350 First film layer 450 of OCA is peeled off, dyestripping roller 350 is contacted the first film layer 450 positioned at OCA first ends 310, by dyestripping The film-tear adhesive band on the surface of roller 350 in the first direction gets off first film layer 450 of OCA from the sur-face peeling of glue-line 300.
The first laminating laminating platform 50 of platform 100 and second is driven to be aligned, when completion is aligned, in Fig. 3 (II) shown in figure, incline second and fit platform 50 so that the first end 310 for being adsorbed in the OCA on the surface of the second laminating platform 50 is approached The first surface 410 of tool 400.Wherein, the first surface 410 of tool 400 is tool 400 away from the first laminating platform 100 Surface.That is so that first surface 410 of the glue-line 300 of the first end 310 of OCA close to tool 400.
Because the active position of dyestripping roller 350 is the first end 310 of OCA, and the first end 310 of OCA is not in the first base On plate 200, but positioned at the first surface 410 of tool 400.Relative to existing applying method, the laminating step is enabled to Issuable bad such as bubble, glue-line 300 are damaged and focused on the OCA of the first surface 410 for being fitted in tool 400.
Step S130, second film layer positioned at the Optical transparent adhesive first end is acted on by roller of fitting, and is driven The laminating roller rolls second film layer so that the glue-line of the Optical transparent adhesive fits in the tool in the first direction First surface and the first substrate first surface;
Due to laminating roller 250 have certain zone of action, therefore, in order to will it is above-mentioned it is bad (bubble, glue-line damage Deng) surface of tool 400 is transferred to, the OCA (including the second film layer 150 and glue-line 300) of the first surface laminating of tool 400 exists The length in the X direction of the zone of action when length of X-direction should be pressurized according to laminating roller 250 is set.The present embodiment In, the OCA of the first surface laminating of tool 400 is preferably not less than 1 centimetre in the length of X-direction, it is clear that tool 400 is in X-direction Length L nor less than 1 centimetre.
In above-mentioned application scenarios, step S130 can specifically include below scheme:
Such as (II) figure in Fig. 3, roller 250 of fitting is acted on into the second film layer 150 positioned at OCA first ends 310, driven Laminating roller 250 is pushed so that the glue-line 300 for being located at OCA first ends 310 is fitted with the first surface 410 of tool 400.Due to patch The depressed position of roller 250 is closed not on first substrate 200, but positioned at the first surface 410 of tool 400.Relative to existing Applying method, enables to the issuable bad such as bubble of the laminating step, the damage of glue-line 300 to focus on and be fitted in tool On the OCA of 400 first surface 410.
Such as (III) figure and (IV) figure in Fig. 3, second is driven to fit its heeling condition of holding of platform 50 relative to the first patch Platform 100 is closed to move in the first direction;And drive laminating roller 250 to be rolled in the first direction with the motion of the second laminating platform 50 The second film layer 150 is pressed, so that the second film layer 150 departs from the second laminating platform 50, and the glue-line 300 of OCA is fitted in tool 400 First surface 410 and first substrate 200 first surface 210.
Step S140, peels off the second film layer of the Optical transparent adhesive to expose the glue-line, by the first of second substrate Hold the first surface close to the tool;
The length in the X direction of second substrate 550 should be greater than length of the first substrate 200 in X-direction.In order to save as far as possible Material, the width that the width in the Y direction of second substrate 550 can be with first substrate 200 in the Y direction is adapted to, and second Difference of the length and first substrate 200 in the X direction of substrate 550 between the length of X-direction can be less than or equal to tool 400 length in the X direction.
By the one side of the glue-line 300 of OCA and the first surface 410 of tool 400 and the first surface 210 of first substrate 200 , it is necessary to further second substrate 550 is fitted with the another side of the glue-line 300 after laminating.First second film layer 150 of OCA is shelled From the glue-line 300, Ran Houzai of the first surface 210 for exposing the first surface 410 and first substrate 200 for being fitted in tool 400 The contraposition of first end 551 of second substrate 550 is fitted on the glue-line 300 of the first surface 410 of tool 400.
In above-mentioned application scenarios, step S140 can specifically include below scheme:
Second film layer 150 of the Optical transparent adhesive is peeled off to expose the glue-line 300.Such as (V) figure institute in Fig. 3 Show, second film layer 150 of OCA can be peeled off by dyestripping roller 350, dyestripping roller 350 is acted on positioned at OCA first ends 310 the second film layer 150, drives dyestripping roller 350 from the first end 310 of OCA, moves in the first direction, by dyestripping roller The film-tear adhesive band on 350 surfaces gets off second film layer 150 of OCA from the sur-face peeling of glue-line 300.Similarly, relative to existing patch Conjunction method so that the laminating step is issuable bad to be focused on and be fitted in tool 400 as bubble, glue-line 300 are damaged etc. On the OCA of first surface 410.
The second substrate 550 is attached to the relative with the described first laminating platform 100 of the second laminating platform 50 Surface, as shown in (V) figure in Fig. 3.Specifically, second substrate 550 can be attached into by way of vacuum suction Two laminating platform 50 surfaces.Difference between the length of second substrate 550 and the length of first substrate 200 is δ L2, tool 400 Length be L, δ L2≤L.
The first laminating laminating platform 50 of platform 100 and second is driven to be aligned, when completion is aligned, in Fig. 3 (VI) shown in figure, incline second fit platform 50 so that second substrate 550 first end 551 close to tool 400 first surface 410.That is so that glue-line 300 of the first end 551 of second substrate 550 close on the first surface 410 of tool 400.
Step S150, the laminating roller is acted on the first end of the second substrate, drives the laminating roller edge The first direction rolls the second substrate so that the second substrate fits in the glue-line away from the first substrate Surface.
Laminating roller 250 is acted on the second substrate 550 on the surface of tool 400, drives laminating roller 250 to push So that being fitted with the glue-line 300 on the first surface 410 of tool 400 positioned at the first end 551 of second substrate 550.Drive laminating Roller 250 is slow in the first direction to roll second substrate 550 so that second substrate 550 is pasted with the another side of the glue-line 300 of OCA Close, complete first substrate 200 and fitted with the OCA between second substrate 550.Similarly, because the laminating depressed position of roller 250 does not exist On first substrate 200, but positioned at the first surface 410 of tool 400.Relative to existing applying method, the patch is enabled to The issuable bad such as bubble of step, the damage of glue-line 300 is closed to focus on and be fitted on the OCA on the surface of tool 400.
In above-mentioned application scenarios, step S150 can specifically include below scheme:Such as (VI) figure in Fig. 3, the is driven Two laminating platforms 50 keep its heeling condition to be moved in the first direction relative to the first laminating platform 100;And drive laminating roller 250 is in the first direction v directions rolling second substrate 550 in Fig. 3 (III) near the with the motion of the second laminating platform 50 The surface of two laminating platforms 50, so that second substrate 550 departs from the second laminating platform 50, and makes second substrate 550 and tool 400 First surface 410 and first substrate 200 first surface 210 on glue-line 300 fit, complete first substrate 200 and the OCA laminatings between two substrates 550, as shown in (VII) figure in Fig. 3.
Step S160, the second substrate and the glue-line of the removal on the first surface of the tool.
After the completion of laminating, in tool 400 and the junction of first substrate 200, second substrate 550 (containing glue-line 300) is cut Isolate, the second substrate 550 and glue-line 300 that will be fitted in the surface of tool 400 are cleared up as waste material, first substrate 200 The second substrate 550 of surface laminating is the part for really bringing product into, as shown in (VIII) figure in Fig. 3.
In the present embodiment, first substrate 200 is hard substrate, and second substrate 550 is flexible base board.For example, first substrate 200 can be optical glass, and second substrate 550 can be Grating Film.In the present embodiment, the material to tool 400 is not limited, Can be metal, alloy material, plastic material, glass substrate etc., the first side 420 of its close first substrate 200 is (with plane ZOY is parallel) it is smoother surface.
It is understood that after tool 400 is reused many times, substantial amounts of OCA glue-lines 300 fit to the of tool 400 Tool 400 can be caused gradually thickening during one surface 410, even more than the thickness h of first substrate 200.Due to reach preferably Laminating effect, it is necessary to the difference of the thickness of thickness and the first substrate 200 of tool 400 within a preset range, accordingly, it would be desirable to periodically Waste material to the surface of tool 400 is purged or changes tool 400.
First embodiment of the invention provide Optical transparent adhesive applying method by introducing tool 400, during laminating The bubble and edge glue-line 300 that Optical transparent adhesive edge between first substrate 200 and second substrate 550 is introduced are damaged to product The harmful effect that product bring is transferred to tool 400, is effectively improved the yield of optical clear glue laminating.Also, through repeatedly examination Checking is bright, and the product fitted using the Optical transparent adhesive applying method, the bubble being visible by naked eyes is being normally applied occasion Pressurization deaeration technique can be saved, is conducive to simplifying the process of attaching process, improve laminating efficiency.
Fig. 4 shows the method flow diagram of the Optical transparent adhesive applying method that second embodiment of the invention is provided.Refer to Fig. 4, Optical transparent adhesive applying method provided in an embodiment of the present invention includes:
Step S210, first substrate is attached to the first laminating platform surface and is set in advance in described first and fits platform Tool be close to, and be arranged side by side in the first direction with the tool;
Wherein, the difference between the thickness of the thickness of the tool 400 and the first substrate 200 is within a preset range.
Step S220, will peel off the first end of the Optical transparent adhesive after first film layer close to the of the tool One surface;
Step S230, second film layer positioned at the Optical transparent adhesive first end is acted on by roller of fitting, and is driven The laminating roller rolls second film layer so that the glue-line of the Optical transparent adhesive fits in the tool in the first direction First surface and the first substrate first surface;
Step S210 is referred to step S110 in above-mentioned first embodiment extremely to the specific embodiment of step S230 S130, here is omitted.
Step S240, removal is fitted in the Optical transparent adhesive of the first surface of the tool.
Specific embodiment can be:Optical transparent adhesive is cut open along tool 400 with the junction of first substrate 200; Stripping is fitted in the OCA (including the second film layer 150 and glue-line 300) of the first surface 410 of tool 400, (V) figure in such as Fig. 5 It is shown.
The OCA of the first surface 410 of tool 400 is fitted in for the ease of removal, can be in the surface of tool 400 laminating OCA Before, i.e., before above-mentioned steps S220, the first surface 410 of tool 400 paste in advance one or more layers do not stay cull from Type film, now, the OCA (including the second film layer 150 and glue-line 300) that the first surface 410 of tool 400 is fitted in step S230 is real Matter is fitted on the mould release membrance that the surface of tool 400 is fitted in advance.When the first surface 410 for needing stripping to be fitted in tool 400 OCA (including the second film layer 150 and glue-line 300) when, it is only necessary to remove the first surface 410 for being fitted in tool 400 in advance One layer of mould release membrance, it is possible to which the OCA that will rapidly be fitted in mould release membrance surface is peeled off in the lump, and cull is not stayed.
Step S250, peels off the second film layer of the Optical transparent adhesive to expose the glue-line, by the first of second substrate Hold the first surface close to the tool;
Step S260, the laminating roller is acted on the first end of the second substrate, drives the laminating roller edge The first direction rolls the second substrate so that the second substrate fits in the glue-line away from the first substrate Surface.
The specific embodiment of step S250 and step S260 be referred to step S140 in above-mentioned first embodiment and Step S150, difference is that the glue-line 300 of the first surface 410 of tool 400 is removed in above-mentioned steps S240, such as Shown in (V), (VI), (VII) figure in Fig. 5, no longer step S250 and step S260 are repeated herein.
Step S270, the second substrate of the removal on the first surface of the tool.
After the completion of laminating, in tool 400 and the junction of first substrate 200, second substrate 550 is cut open to come, will paste Close the second substrate 550 on the surface of tool 400 to be cleared up as waste material, the second substrate 550 of the surface of first substrate 200 laminating Really to bring the part of product into, as shown in (VIII) figure in Fig. 5 and (Ⅸ) figure.
Based on above-mentioned first embodiment, the Optical transparent adhesive applying method that second embodiment of the invention is provided is by the second base Before plate 550 is fitted with OCA glue-lines 300, OCA (including the second film layer 150 and the glue-line of the first surface 410 of tool 400 are first removed 300), be conducive to alleviating due to the poor influence to effect of fitting of the flatness of the glue-line 300 positioned at OCA first ends 310.
Fig. 6 shows that third embodiment of the invention provides a kind of process chart of Optical transparent adhesive applying method.Such as Shown in Fig. 6, the technological process of the Optical transparent adhesive applying method that third embodiment of the invention is provided includes:
The deposition step of first substrate 200.(I) figure in Fig. 6 show under a kind of state of the step top view (XY put down Face).(I) figure in Fig. 7 shows the A-A sectional views (XZ planes) of (I) figure in Fig. 6.It should be noted that due to being used in figure In the first substrate 200 and the thinner thickness of tool 400 illustrated, in Fig. 7 part-structure non-cross-hatching clear in order to illustrate. Region representation tool 400 a little is filled in Fig. 6.As shown in (I) figure in (I) figure and Fig. 7 in Fig. 6, by first substrate 200 First is placed side by side on tool 400 to fit the surface of platform 100, and by way of vacuum suction or stopping means is to first Substrate 200 and tool 400 are fixed.If first substrate 200 is fitted with first, the contact area of platform 100 is much larger than tool 400 contacts area for fitting platform 100 with first, after first substrate 200 is fixed, tool 400 can not be fixed.If first Frictional force after being contacted between laminating platform 100 and first substrate 200 is sufficient for the fixation of first substrate 200, the first laminating Platform 100 can be without vacuum suction function or stopping means.
The laminating step of OCA and first substrate 200.(II) figure in Fig. 6 shows bowing under a kind of state of the step View.(II) figure in Fig. 7 shows the A-A sectional views of (II) figure in Fig. 6.Area filled with oblique line in (II) figure of Fig. 6 Domain representation OCA.As shown in (II) figure in (II) figure and Fig. 7 in Fig. 6, by the side of the first film layer 450 of OCA towards the first base The first surface 210 of plate 200 is placed on first substrate 200, and OCA is aligned with first substrate 200, and makes the of OCA One end 310 is located at the first surface 410 of tool 400.In the first end 310 such as aa ' positions adhesive tape of OCA after the completion of contraposition Be fixed, will OCA be pasted onto the surface of tool 400.Open the first film layer 450 of aa ' sides, the first film layer 450 is from aa ' One lateral offside is gradually peeled off.Laminating roller 250 is driven to act on OCA positioned at the first surface 410 of tool 400, and from aa ' Lateral offside is rolled, and OCA (including the film layer 150 of glue-line 300 and second) is fitted in into the first surface of first substrate 200 210, shown in (III) in (III) and Fig. 7 in such as Fig. 6.To avoid introducing bubble, the speed of rolling is unsuitable too fast, before rolling The glue-line 300 of OCA is not readily accessible to first substrate 200.Further, can be by beyond many of the second end of first substrate 200 Remaining OCA removals, as shown in (IV) figure in Fig. 7.
The laminating step of second substrate 550 and OCA.(IV) figure in Fig. 6 shows bowing under a kind of state of the step View.(IV) figure in Fig. 7 shows the A-A sectional views of (IV) figure in Fig. 6.Area filled with oblique line in (IV) figure of Fig. 6 Field surface second substrate 550.As shown in (IV) figure in (IV) figure and Fig. 7 in Fig. 6, second substrate 550 is placed in the of OCA On two film layers 150, second substrate 550 is aligned with the OCA glue-lines 300 of the first surface 410 of tool 400, and make second The first end 551 of substrate 550 is arranged at the first surface 410 of tool 400.After completing contraposition, with adhesive tape by second substrate 550 first end 551 is fixed on the first surface 410 of tool 400.It should be noted that the work illustrated at (III) of Fig. 6 After skill flow terminates, if tool 400 and first substrate 200 intersection by OCA (including the second film layer 150 and glue-line 300) cut off, be especially turned off the second film layer 150, it is also possible to which second substrate 550 is affixed directly to second film layer 150 of OCA On.Then the second film layer 150 is opened from aa ' sides, the second film layer 150 is gradually peeled off from the lateral offsides of aa '.Drive laminating The suppressing action of roller 250 drives laminating roller 250 from aa ' in the second substrate 550 positioned at the first surface 410 of tool 400 Lateral offside is rolled, and second substrate 550 is come into contact with glue-line 300, and second substrate 550 is fitted in into glue-line 300 Surface, completes first substrate 200 and is fitted with the OCA of second substrate 550, as shown in (V) figure in (V) figure and Fig. 7 in Fig. 6. To avoid bubble, the speed of rolling is unsuitable too fast, and second substrate 550 can not touch glue-line 300 before rolling.
Waste material removal step.(VI) figure in Fig. 6 shows the top view of product after removal waste material.(VI) figure in Fig. 7 Show the A-A sectional views of (VI) figure in Fig. 6.After the completion of laminating, by the waste material on periphery (including beyond the side of first substrate 200 The OCA and second substrate 550 of edge) remove the product obtained as shown in (VI) figure in Fig. 7.Thus can effectively by laminating During OCA edges introduce bubble and edge glue-line 300 damage etc. it is bad be transferred to outside product, be especially transferred to and control On tool 400, will finally be removed with above-mentioned bad glue-line 300 and the second substrate 550 fitted with the glue-line 300, you can with It is effectively improved the yield of optical clear glue laminating.
The preferred embodiments of the present invention are the foregoing is only, is not intended to limit the invention, for the skill of this area For art personnel, the present invention can have various modifications and variations.It is all within the spirit and principles in the present invention, made any repair Change, equivalent, improvement etc., should be included within the scope of the present invention.

Claims (10)

1. a kind of Optical transparent adhesive applying method, it is characterised in that the first film layer that the Optical transparent adhesive includes being stacked, Glue-line and the second film layer, methods described include:
First substrate is attached to the first laminating platform surface, near the tool for being set in advance in the first laminating platform, and It is arranged side by side in the first direction with the tool, wherein, the difference between the thickness of the thickness of the tool and the first substrate Value is within a preset range;
The first end of the Optical transparent adhesive after first film layer close to the first surface of the tool will be peeled off;
Roller of fitting is acted on into second film layer positioned at the Optical transparent adhesive first end, the laminating roller edge is driven The first direction rolls second film layer so that the glue-line of the Optical transparent adhesive fits in the first surface of the tool And the first surface of the first substrate;
The second film layer of the Optical transparent adhesive is peeled off to expose the glue-line, by the first end of second substrate close to the tool First surface;
The laminating roller is acted on the first end of the second substrate, drives the laminating roller to be rolled along the first direction The second substrate is pressed so that the second substrate fits in surface of the glue-line away from the first substrate.
2. method according to claim 1, it is characterised in that the opposite side of the first laminating platform is provided with second Laminating platform, the described first end that will peel off the Optical transparent adhesive after first film layer is close to the first of the tool The step of surface, including:
Second film layer of the Optical transparent adhesive is attached to the table relative with the described first laminating platform of the second laminating platform Face;
First film layer of the Optical transparent adhesive is peeled off;
Incline it is described second laminating platform so that the Optical transparent adhesive first end close to the tool first surface.
3. method according to claim 2, it is characterised in that described acts on positioned at the optical lens laminating roller Second film layer of gelatin first end, drives the laminating roller to roll second film layer so that institute along the first direction State Optical transparent adhesive glue-line fit in the tool first surface and the first substrate first surface the step of, bag Include:
Roller of fitting is acted on the second film layer positioned at the Optical transparent adhesive first end;
The second laminating platform is driven to be moved along the first direction relative to the described first laminating platform;
The laminating roller is driven to roll second film layer along the first direction with the motion of the described second laminating platform, So that second film layer departs from the second laminating platform, and the glue-line of the Optical transparent adhesive is set to fit in the tool The first surface of first surface and the first substrate.
4. method according to claim 3, it is characterised in that the second film layer of the described stripping Optical transparent adhesive with Expose the glue-line, by the first end of second substrate close to the tool first surface the step of, including:
Second film layer of the Optical transparent adhesive is peeled off to expose the glue-line;
The second substrate is attached to the surface relative with the described first laminating platform of the second laminating platform;
Incline it is described second laminating platform so that the second substrate first end close to the tool first surface.
5. method according to claim 4, it is characterised in that described the second film layer by the Optical transparent adhesive is peeled off The step of, including:
Dyestripping roller is acted on the second film layer of the first end positioned at the Optical transparent adhesive;
The dyestripping roller is driven to move to peel off described second from the first end of the Optical transparent adhesive, along the first direction Film layer.
6. method according to claim 1, it is characterised in that described acts on second base by the laminating roller The first end of plate, drives the laminating roller to roll the second substrate along the first direction so that the second substrate is fitted After the step of surface of the glue-line away from the first substrate, methods described also includes:
The second substrate and the glue-line of the removal on the first surface of the tool.
7. method according to claim 1, it is characterised in that the second film layer of the described stripping Optical transparent adhesive with Expose the glue-line, by the first end of second substrate close to the tool first surface the step of before, methods described is also wrapped Include:
Removal is fitted in the Optical transparent adhesive of the first surface of the tool.
8. method according to claim 7, it is characterised in that described removal is fitted in the first surface of the tool The step of Optical transparent adhesive, including:
The Optical transparent adhesive is cut open along the tool with the junction of the first substrate;
Stripping is fitted in the Optical transparent adhesive of the first surface of the tool.
9. method according to claim 8, it is characterised in that the first surface of the tool posts one or more layers in advance Not the step of not staying the mould release membrance of cull, the Optical transparent adhesive of the first surface that described stripping is fitted in the tool, including:
The mould release membrance for being fitted in the first surface of the tool in advance is removed to peel off the light being fitted on the mould release membrance Learn transparent adhesive tape.
10. method according to claim 7, it is characterised in that described acts on described second by the laminating roller The first end of substrate, drives the laminating roller to roll the second substrate along the first direction so that the second substrate is pasted Together in the glue-line away from the first substrate surface the step of after, methods described also includes:
The second substrate of the removal on the first surface of the tool.
CN201611060831.3A 2016-11-28 2016-11-28 A kind of Optical transparent adhesive applying method Active CN106739400B (en)