CN106739027A - 一种热塑性塑料阀门的退火工艺 - Google Patents
一种热塑性塑料阀门的退火工艺 Download PDFInfo
- Publication number
- CN106739027A CN106739027A CN201710051505.4A CN201710051505A CN106739027A CN 106739027 A CN106739027 A CN 106739027A CN 201710051505 A CN201710051505 A CN 201710051505A CN 106739027 A CN106739027 A CN 106739027A
- Authority
- CN
- China
- Prior art keywords
- valve
- thermoplastic
- annealing process
- mineral oil
- plastic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供一种热塑性塑料阀门的退火工艺,涉及塑料阀门加工技术领域,其步骤如下:将塑料阀门放入有底容器中,向其中加入矿物油,使得塑料阀门完全浸没在矿物油中,将容器放入微波加热装置的加热室中,微波加热至130‑140℃,取出,风冷至常温。本发明方法能够很好的消除热塑性塑料中的应变力,退火效果好,从而保持热塑性阀门的物理和化学性能,有很好的推广应用价值。
Description
技术领域
本发明涉及塑料阀门加工技术领域,具体涉及一种热塑性塑料阀门的退火工艺。
背景技术
塑料阀门具有质量轻、耐腐蚀、不吸附水垢、可与塑料管路一体化连接和使用寿命长等优点,塑料阀门在给水(尤其是热水与采暖)和工业用其他流体的塑料管路系统中,其应用方面的优势是其他阀门无法相比的。
塑料阀门加工步骤一般包括配料、注塑、退火、机加工等步骤。其中,退火的目的是除去或消除热塑性塑料中的应变力,防止在后期加工和应用过程中产生裂缝或者碎裂。目前塑料阀门的常规退火工艺是直接加热塑料阀门再自然慢慢冷却来实现退火,退火效果并不是很理想,且退火过程中热塑性塑料会发生收缩。
发明内容
针对现有技术的不足,本发明提供了一种热塑性塑料阀门的退火工艺。
为实现以上目的,本发明通过以下技术方案予以实现:
一种热塑性塑料阀门的退火工艺,步骤如下:将塑料阀门放入有底容器中,向其中加入矿物油,使得塑料阀门完全浸没在矿物油中,将容器放入微波加热装置的加热室中,微波加热至130-140℃,取出,风冷至常温。
优选地,所述塑料阀门材质为聚丙烯或聚乙烯。
优选地,所述塑料阀门的壁厚为3-12mm。
优选地,所述载物容器材质为高硼硅耐热玻璃或不锈钢。
优选地,所述微波加热时间为1-5min。
本发明有益效果:本发明方法热量更容易穿透阀门材质内部,使得阀门各部位受热均匀,且将其放于矿物油中微波加热,意外发现其热缩形变小,从而能够很好的消除热塑性塑料中的应变力,退火效果好,能够很好保持热塑性阀门的物理和化学性能,有很好的推广应用价值。
具体实施方式
为使本发明实施例的目的、技术方案和优点更加清楚,下面将结合本发明实施例,对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有作出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。
实施例1:
一种热塑性塑料阀门的退火工艺,步骤如下:将壁厚为5mm的聚丙烯塑料阀门放入材质为高硼硅耐热玻璃的有底容器中,向其中加入矿物油,使得塑料阀门完全浸没在矿物油中,将容器放入微波加热装置的加热室中,微波加热至135℃,加热时间为2.5min,取出,风冷至常温。
实施例2:
一种热塑性塑料阀门的退火工艺,步骤如下:将壁厚为12mm的聚丙烯塑料阀门放入材质为不锈钢的有底容器中,向其中加入矿物油,使得塑料阀门完全浸没在矿物油中,将容器放入微波加热装置的加热室中,微波加热至140℃,加热时间为5min,取出,风冷至常温。
实施例3:
一种热塑性塑料阀门的退火工艺,步骤如下:将壁厚为5mm的聚乙烯塑料阀门放入材质为高硼硅耐热玻璃的有底容器中,向其中加入矿物油,使得塑料阀门完全浸没在矿物油中,将容器放入微波加热装置的加热室中,微波加热至130℃,加热时间为3min,取出,风冷至常温。
实施例4:
一种热塑性塑料阀门的退火工艺,步骤如下:将壁厚为3mm的聚乙烯塑料阀门放入材质为不锈钢的有底容器中,向其中加入矿物油,使得塑料阀门完全浸没在矿物油中,将容器放入微波加热装置的加热室中,微波加热至135℃,加热时间为1min,取出,风冷至常温。
实施例5:
一种热塑性塑料阀门的退火工艺,步骤如下:将壁厚为8mm的聚丙烯塑料阀门放入材质为不锈钢的有底容器中,向其中加入矿物油,使得塑料阀门完全浸没在矿物油中,将容器放入微波加热装置的加热室中,微波加热至140℃,加热时间为4min,取出,风冷至常温。
需要说明的是,在本文中,诸如第一和第二等之类的关系术语仅仅用来将一个实体或者操作与另一个实体或操作区分开来,而不一定要求或者暗示这些实体或操作之间存在任何这种实际的关系或者顺序。而且,术语“包括”、“包含”或者其任何其他变体意在涵盖非排他性的包含,从而使得包括一系列要素的过程、方法、物品或者设备不仅包括那些要素,而且还包括没有明确列出的其他要素,或者是还包括为这种过程、方法、物品或者设备所固有的要素。在没有更多限制的情况下,由语句“包括一个……”限定的要素,并不排除在包括所述要素的过程、方法、物品或者设备中还存在另外的相同要素。
以上实施例仅用以说明本发明的技术方案,而非对其限制;尽管参照前述实施例对本发明进行了详细的说明,本领域的普通技术人员应当理解:其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换;而这些修改或者替换,并不使相应技术方案的本质脱离本发明各实施例技术方案的精神和范围。
Claims (5)
1.一种热塑性塑料阀门的退火工艺,其特征在于,步骤如下:将塑料阀门放入有底容器中,向其中加入矿物油,使得塑料阀门完全浸没在矿物油中,将容器放入微波加热装置的加热室中,微波加热至130-140℃,取出,风冷至常温。
2.如权利要求1所述的热塑性塑料阀门的退火工艺,其特征在于,所述塑料阀门材质为聚丙烯或聚乙烯。
3.如权利要求2所述的热塑性塑料阀门的退火工艺,其特征在于,所述塑料阀门的壁厚为3-12mm。
4.如权利要求1所述的热塑性塑料阀门的退火工艺,其特征在于,所述载物容器材质为高硼硅耐热玻璃或不锈钢。
5.如权利要求1所述的热塑性塑料阀门的退火工艺,其特征在于,所述微波加热时间为1-5min。