CN106572208A - Housing and making method thereof, and mobile terminal - Google Patents

Housing and making method thereof, and mobile terminal Download PDF

Info

Publication number
CN106572208A
CN106572208A CN201610958424.8A CN201610958424A CN106572208A CN 106572208 A CN106572208 A CN 106572208A CN 201610958424 A CN201610958424 A CN 201610958424A CN 106572208 A CN106572208 A CN 106572208A
Authority
CN
China
Prior art keywords
metal portion
ink
housing
coating
protective layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201610958424.8A
Other languages
Chinese (zh)
Other versions
CN106572208B (en
Inventor
李静
吉斌
袁于才
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangdong Oppo Mobile Telecommunications Corp Ltd
Original Assignee
Guangdong Oppo Mobile Telecommunications Corp Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangdong Oppo Mobile Telecommunications Corp Ltd filed Critical Guangdong Oppo Mobile Telecommunications Corp Ltd
Priority to CN201610958424.8A priority Critical patent/CN106572208B/en
Publication of CN106572208A publication Critical patent/CN106572208A/en
Application granted granted Critical
Publication of CN106572208B publication Critical patent/CN106572208B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a housing and a making method thereof, and a mobile terminal; the housing comprises a metal part and a non-metal part fixedly connected with the metal part; one side, facing a user, of the non-metal part is attached by a coating; the coating color is consistent with the color of the surface, facing the user, of the metal part. The coating is attached to one side, facing the user, of the non-metal part; the coating color is consistent with the color of the surface, facing the user, of the metal part; therefore, the housing can have consistent integral housing appearance performance, thus improving user experiences.

Description

Housing, method for producing shell and mobile terminal
The application is that the Application No. 201610812276.9, applying date is September in 2016 8 days, applies for entitled《Housing, Method for producing shell and mobile terminal》Patent application divisional application.
Technical field
The present invention relates to the communications field, more particularly to a kind of housing, method for producing shell and mobile terminal.
Background technology
With the extensive application of mobile phone metal shell, appearance requirement more and more higher of the people to phone housing is more and more People's clock be intended to phone housing outward appearance integration.However, at present majority mobile phone is limited by communication function or limited by processing technique, Phone housing is caused all to there is metal portion and non-metal portion.Material composition is differed with metal portion because non-metal portion is adopted, is led Cause the appearance color of non-metal portion inconsistent with the appearance color of metal portion, so that the outward appearance overall performance of phone housing is not Height, and then cause Consumer's Experience not high.
The content of the invention
The present invention provides a kind of antenna assembly and mobile terminal that can improve Consumer's Experience.
The present invention provides a kind of antenna assembly, wherein, the housing includes metal portion and is fixedly connected the metal portion Non-metal portion, the non-metal portion is attached to coating towards user side, and the color of the coating is with the metal portion towards use The surface color at family is consistent.
The present invention also provides a kind of method for producing shell, wherein, the method for producing shell includes:
Housing product with metal portion and non-metal portion, the metal portion and the polished process of the non-metal portion are provided Afterwards and Jing blasting treatments again;
Set up coating, the color of the coating in the region for being located at the non-metal portion in the appearance surfaces of the housing product With the appearance surfaces solid colour of the metal portion.
The present invention also provides a kind of mobile terminal, wherein, the mobile terminal includes above-mentioned housing, the mobile terminal Also include the mainboard being fixed in the housing and the functional part being arranged on the mainboard.
The housing of the present invention, method for producing shell and mobile terminal, by attached towards user side in the non-metal portion Coating is provided with, and the color using the coating is consistent towards the surface color of user with the metal portion, so that described Housing overall appearance performance is consistent, and then improves Consumer's Experience.
Description of the drawings
In order to be illustrated more clearly that technical scheme, the accompanying drawing to be used needed for embodiment will be made below Simply introduce, it should be apparent that, drawings in the following description are only some embodiments of the present invention, general for this area For logical technical staff, on the premise of not paying creative work, can be with according to these other accompanying drawings of accompanying drawings acquisition.
Fig. 1 is the schematic diagram of the housing that the present invention is provided;
Fig. 2 is the enlarged diagram of the II parts of the housing of Fig. 1;
Fig. 3 is the schematic diagram of the housing of Fig. 1;
Fig. 4 is the machining sketch chart of the housing of Fig. 1;
Fig. 5 is the machining sketch chart of the housing of Fig. 1;
Fig. 6 is the machining sketch chart of the housing of Fig. 1;
Fig. 7 is the machining sketch chart of the housing of Fig. 1;
Fig. 8 is the schematic diagram of the housing of Fig. 1;
Fig. 9 is the schematic diagram of the housing of Fig. 1;
Figure 10 is the top view of the housing of Fig. 9;
Figure 11 is the schematic diagram of the housing of Fig. 1;
Figure 12 is the schematic flow sheet of the method for producing shell that the present invention is provided;
Figure 13 is the machining sketch chart of Fig. 1 housings;
Figure 14 is the schematic diagram of the mobile terminal that the present invention is provided.
Specific embodiment
Below in conjunction with the accompanying drawing in embodiment of the present invention, the technical scheme in embodiment of the present invention is carried out clearly Chu, it is fully described by.
Refer to Fig. 1 and Fig. 2, a kind of housing 100 that the present invention is provided.The housing 100 includes metal portion 10 and fixes Connect the non-metal portion 20 of the metal portion 10, the non-metal portion 10 is attached to coating 30, the coating towards user side 30 color is consistent towards the surface color of user with the metal portion 10.It is understood that the housing 100 can conduct The shell of mobile terminal 200, the mobile terminal 200 can be mobile phone, panel computer, notebook computer etc..
By being attached to coating 30 towards user side in the non-metal portion 20, and the color using the coating 30 with The metal portion 10 is consistent towards the surface color of user, so that the overall appearance performance of the housing 100 is consistent, Jin Erti High Consumer's Experience.
In present embodiment, the housing 100 is plate-like.The non-metal portion 20 is fixed on the side of the metal portion 10. The non-metal portion 20 can be distributed in the housing 100 by preset shape.The metal portion 10 can be by complete gold Category plate cutting is formed.The non-metal portion 20 can be fixed on the metal portion 10 by techniques such as injection or bondings.For The bulk metal texture of the increase housing 100, region shared by the non-metal portion 20 is shared less than the metal portion 10 Region.Certainly, in other embodiments, region can also with region shared by the metal portion 10 shared by the non-metal portion 20 It is identical, or more than region shared by the metal portion 10.
In present embodiment, the coating 30 is mixture.The coating 30 is uniformly layed in the court of the non-metal portion 20 To the surface of user.The coating 30 is in the orthographic projection region of the non-metal portion 20 with the non-metal portion 20 towards user's Surface region coincides.So as to the coating 30 covers completely the non-metal portion 20, will the non-metal portion 20 be hidden in Under the coating 30.The non-metal portion 20 is covered completely using the coating 30, so that user observes the housing 100 Outward appearance, only it is observed that the metal portion 10 and the coating 30, and the color of the coating 30 and the court of the metal portion 10 Surface color to user is consistent, so that the overall appearance performance of the housing 100 is consistent, improves Consumer's Experience.Can be with It is understood by, the color of the coating 30 and the metal portion 10 consistent be expressed as user and directly see towards the surface color of user The color appearance of the coating 30 seen is consistent towards the surface color outward appearance of user with the metal portion 10, i.e., described coating The surface perception solid colour of 20 perception color and the metal portion 10 towards user.Certainly, in other embodiments, institute State 30 overlay areas of coating and can also be exterior surface area more than the non-metal portion 20.
Further, the coating 30 is made up of the ink 33 for being mixed into metallic 31 and colorant 32.In present embodiment, By being mixed into metallic 31 in ink 33 so that the coating 30 have with the identical metal of the metal portion 10 outside See, and by being mixed into colorant 32 in the ink 33 so that the integral color of the coating 30 is improved, so that described The appearance color of coating 30 is consistent with the appearance color of the metal 10.And utilize the coating 30 main by the structure of the ink 33 Into, so as to facilitate the coating 30 to take shape in the non-metal portion 20, you can with the overlay area of coating described in precise control 30, So as to improve the appearance property of the housing 100.It is understood that the coating 30 can adopt spraying coating process, screen printing Dataller's skill or be that exposure imaging mode is taken shape on the non-metal portion 20.The metallic 31 and the colorant 32 can To be mixed into the ink 33 according to certain predetermined ratio, the metallic 31 can be aluminum or silver or ferrum or titanium or magnesium The metal alloy of any one metal or multiple combination, such as described metallic 31 can be aluminium powder, argentum powder or titanium valve, aluminum conjunction Bronze or Titanium Powder or Al-Mg alloy powder or titanium magnesium alloy powder.In other embodiments, the metallic 31 may be used also Being using stainless steel particles.
Further, Fig. 3 is referred to, the coating 30 is attached to ink protective layer 40 towards user side.
In present embodiment, the material of the ink protective layer 40 is ink.The ink protective layer 40 has light transmission. The appearance color light for alloing the coating 30 is observed through the ink protective layer 40 for user, that is, avoid the ink Protective layer 40 affects the outward appearance of the coating 30, that is, ensure that the overall appearance performance of the housing 100.The ink protective layer 40 have higher surface tensile stress, so as to the ink protective layer 40 has wear-resisting, the corrosion-resistant and resistance to performance such as come off.It is described Housing 100 sets one layer of coating 30 and one layer of ink protective layer 40 on the non-metal portion 20.The ink protection The 40 orthographic projection region in the coating 30 of layer coincide with the coating 30, so that the ink protective layer 40 can be with Accurately it is attached to the coating 30, and then ensure that the appearance property of the housing 100, prevent the coating 30 from scratching, coming off, Or erode, and reduce production cost.In other embodiments, the non-metal portion 20 is laminated with coating described in multilamellar 30 or/and ink protective layer 40 described in multilamellar, so that the color in the non-metal portion 20 of the housing 100 is purer Just, and outward appearance barrier propterty is more excellent.
Further, the ink protective layer 40 is resist sandblasting ink.
In present embodiment, in order to ensure the overall appearance planarization of the housing 100, and in order that the housing 100 surface obtains certain cleannes and different roughness, and by the appearance surfaces in the metal portion 10 sandblasting is carried out Process, and then improved the appearance surfaces mechanical performance of the housing 100, the appearance surfaces for improving the housing 100 resist Fatigability.But before carrying out at sandblasting to the metal portion 10, if the ink protective layer 40 has been attached to the painting On layer 30, then the ink protective layer 40 needs to adopt resist sandblasting ink, so as to surface is being carried out at sandblasting to the metal 10 During reason, the ink protective layer 40 is damaged, so as to affect the surface structure performance of the housing 100.Certainly, in other embodiment party In formula, the coating 30 can also adopt resist sandblasting ink, so as to further increase the surface structure performance of the housing 100.
Further, the ink 33 and the ink protective layer 40 are exposure ink.In present embodiment, the painting Layer 30 and the ink protective layer 40 take shape in the non-metal portion 20 using exposure imaging mode.Specifically, first, refer to Fig. 4, lays one layer of coloring printing ink 30a, to the colored oil jointly in the outer surface of the metal portion 10 and the non-metal portion 20 Black 30a is toasted 20 minutes under 70 degrees Celsius;Then, Fig. 5 is referred to, on the coloring printing ink 30a after baking institute is laid State protection ink 40a;Subsequently, Fig. 6 is referred to, film film 40b, film film 40b is pasted on the protection ink 40a With default shadow region 40c, the default shadow region 40c coincides with the non-metal portion 20, and by light source 40d institute is irradiated Film film 40b is stated, so that the protection ink 40a and coloring printing ink 30a is corresponding with the shadow region 40c Part generation photopolymerization reaction, and the protection ink 40a and coloring printing ink 30a corresponding with the metal portion 10 area Then there is no photopolymerization reaction in domain;Subsequently, Fig. 7 is referred to, using alkali liquor to the protection ink 40a and the coloring printing ink There is no photopolymerization reaction part and corroded in 30a, so as to only retain on the non-metal portion 20 the protection ink 40a and The coloring printing ink 30a.Finally, to remaining in the protection ink 40a and the coloring printing ink 30a of the non-metal portion 20 180 degrees Celsius of baking-curings are carried out, so that remaining in the protection ink 40a of the non-metal portion 20 and the coloring Ink 30a forms respectively the coating 30 and the ink protective layer 40.
Further, the ink protective layer 40 has the matte surface towards user.In present embodiment, due to the gold Category portion 10 towards user one side through blasting treatment so that the appearance surfaces of the metal portion 10 can be presented many concavo-convex Uneven pitting, i.e., the appearance of described metal portion 10 can be presented diffuse-reflectance.And in order that the housing 100 is described non- The appearance property that appearance property at metal portion 20 is held in the metal portion 10 is consistent, so as to by the ink protective layer 40 carry out matte management towards user's one side, and then cause the ink protective layer 40 to be presented concavo-convex towards user's one side Uneven pitting, i.e., described ink protective layer 40 can also be that diffuse-reflectance is presented towards user's one side.
Further, the non-metal portion 20 is to form the antenna headroom region of the housing 100.
In present embodiment, because region shared by the metal portion 10 is more than region shared by the non-metal portion 20.And work as When the housing 100 is applied to mobile terminal 200, the antenna inside the mobile terminal 200 is needed through the spoke of the housing 100 Radio magnetic signal.The metal portion 10 is unavoidably shielded due to metal properties to antenna electromagnetic signal, it is therefore desirable to will The clearance zone of the non-metal portion 20 and the coating 30 and ink protective layer 40 being arranged on the non-metal portion 20 as antenna Domain, so as to increase the radiance of antenna.Specifically, the non-metal portion 20 adopts non-signal shielding material.As one kind compared with Excellent embodiment, the material of the non-metal portion 20 adopts plastic cement.Certainly, in other embodiments, the non-metal portion 20 Material can also be carbon fiber or organic resin or glass fibre etc..
Further, Fig. 8 is referred to, the metal portion 10 is provided with anodic oxide coating 11, the anode towards user side The solid colour of the color of oxide layer 11 and the coating 30.
In present embodiment, in order that the metal portion 10 has the color required for user, by the metal Portion 10 carries out anodized towards user side, so as to realize that the metal portion 10 is carried out towards user side " Color ", and then cause the metal portion 10 that the effect of pre-set color is reached towards user side.Certainly, in other embodiments, Can also be using plating mode or corroded surface processing mode so that the metal portion 10 reach towards user side it is default The effect of color.
Further, the anodic oxide coating 11 has the sandblasting face 12 towards user.In present embodiment, by institute State metal portion 10 to process to be formed after the anodic oxide coating 11 towards user side, sandblasting is being carried out to the anodic oxide coating 11 Surface treatment so that the anodic oxide coating 11 has the sandblasting face 12 towards user.And so that the anodic oxide coating 11 It is wholely set with the metal portion 11, so as to strengthen the adhesive force of the anodic oxide coating 11 and the metal portion 10, it is to avoid institute State anodic oxide coating 11 to come off, affect the appearance property of housing 100.I.e. described anodic oxide coating 11 is by the metal portion 10 Metal material oxidation form, and the material of the metal portion 10 be aluminum or silver or rustless steel or aluminium alloy or titanium alloy, Or magnesium alloy or magnalium etc..Specifically, sand blasted surface process is carried out to the anodic oxide coating 11, can is described Ink protective layer 40 is attached to after the coating 30.Certainly, in other embodiments, or in ink protection Layer 40 is attached to before the coating 30, and to the anodic oxide coating 11 sand blasted surface process is carried out.
Further, the non-metal portion 20 is wholely set with the metal portion 10.
In present embodiment, the non-metal portion 20 is integrally formed with the metal portion 10 using nano injection technique.It is first First the side 13 of the metal portion 10 is existed described nonmetallic 20 raw material direct injection after nmization process On the side 13 of the metal portion 10, so that the metal portion 10 can be with integrally formed with the non-metal portion 20.So as to The non-metal portion 20 is effectively consolidated with the metal portion 10 to combine.
Further, Fig. 9 and Figure 10 is referred to, the non-metal portion 20 forms at least one slit of the housing 100 Band 50, the slit is made up of with 50 a plurality of slit 51 separately, and the metal portion 10 includes being separated by slit band 50 At least two metallic plates 14 for going out and a plurality of bonding jumper 15.
In present embodiment, the slit with 50 along the housing 100 width straight-line extension.The housing 100 One slit band 50 is set so that the metal portion 10 has two metallic plates 14 and a plurality of bonding jumper 15.Due to The slit is made up of with 50 a plurality of spaced slit 51, so that the non-metal portion 20 positioned at the slit 51 It is difficult observes and there is aberration with the metal portion 10 with the coating 30, and the ink protective layer 40, it is described so as to improve The appearance property of housing 100.Specifically, the seam width L of the slit 51 is 0.2mm~3.0mm.Due to forming the slit band 50 The non-metal portion 20 have it is larger take up room, such that it is able to improve the area in the antenna headroom region of the housing 100, So as to improve the electromagnetic radiation performance of the housing 100.In other embodiments, the slit band 50 can be with along the shell The length direction of body 100 extends, and the housing 100 can also arrange two slit bands 50.
Further, Figure 11 is referred to, the housing 100 is by back-cover 60 and the side for being integrally formed at the periphery of the back-cover 60 Frame 70 is constituted, and the frame 70 is formed at the curved edges of the periphery of the back-cover 60.
In present embodiment, the housing 100 is used as the bonnet of the mobile terminal 200.The inner side of the housing 100 is to hold Carry battery, mainboard and the other functions part of the mobile terminal 200.Specifically, the rectangular plate of the back-cover 60, the side The relatively described back-cover 60 of frame 70 bends.The frame 70 and the back-cover 60 can be Jing CNC milling machine Milling Process one into Type.And described 20 pairs of metal portions 10 of non-metal portion are separated.In other embodiments, the frame 70 and the back of the body Lid 60 can also be split production, assembling machine-shaping.
Further, Figure 12 is referred to, the present invention also provides a kind of method for producing shell, the method for producing shell can be with The housing 100 is made, the method for producing shell includes step:
S01:The housing product 100a with metal portion 10 (see Figure 13) and non-metal portion 20 (see Figure 13) is provided (see figure 13)。
In present embodiment, the metal portion 10 and the non-metal portion 20 are integrally formed rear shape using nano injection technique Into the housing product 100a.Specifically, metal derby 101 (see Figure 13) and nonmetal block 201 (see Figure 13) are first provided, will be described Nonmetal block 201 adopts nano injection technological forming on the metal derby 101, so that the metal derby 101 and the non-gold Category block 201 constitutes plate 100b (see Figure 13).Then to the upper surface 100c (see Figure 13) and lower surface of the plate 100b 100d (see Figure 13) carries out Milling Process, i.e., carry out numerical control milling jointly to the metal derby 101 and the nonmetal block 201 and add Work, so that the metal derby 101 and the nonmetal block 201 form respectively the metal portion 10 and the non-metal portion 20, and And cause the housing product 100a that there are the appearance surfaces of accurate dimension.Finally, to the metal portion 10 and described nonmetallic Portion 20 is surface-treated, so that the appearance surfaces of the housing product 100 are smooth, and with good adhesive force and resisting fatigue Performance.A kind of embodiment is provided, it can first carry out that surface treatment is carried out to the metal portion 10 and the non-metal portion 20 Carry out blasting treatment after polishing again.Certainly, in other embodiments, or only to the metal portion 10 and the non-gold Category portion 20 carries out sanding and polishing process.
S02:The housing product 100a appearance surfaces be located at the non-metal portion 20 region set up coating 30 (see Fig. 3), the appearance surfaces solid colour of the color of the coating 30 and the metal portion 10.
In present embodiment, in the appearance surfaces of the metal portion 10 and the non-metal portion 20 blasting treatment is polished Afterwards, the outer surface of the outer surface of the metal portion 10 and the non-metal portion 20 is respectively provided with good adhesion, so as to convenient in institute The appearance surfaces for stating metal portion 10 and the non-metal portion 20 are coated with ink.It is described so as to be formed by being processed to the ink Coating 30.Protect to be formed to the coating 30, the coating 30 that is located also is attached to ink protective layer towards user side 40.Specifically, first, Fig. 4 is referred to, in common one layer of the spraying of the outer surface of the metal portion 10 and the non-metal portion 20 Color ink 30a, coloring printing ink 30a is made up of the ink for being mixed into metallic and colorant.It is Celsius 70 to coloring printing ink 30a The lower baking of degree 20 minutes, so that coloring printing ink 30a solidifications;Then, Fig. 5 is referred to, in the coloring printing ink 30a after baking It is upper to spray the protection ink 40a, so that the protection ink 40a solidifications;Subsequently, Fig. 6 is referred to, in the protection ink Film film 40b is pasted on 40a, film film 40b has default shadow region 40c, and the default shadow region 40c is non-with described Metal portion 20 coincides, and by light source the film film 40b is irradiated, so that the protection ink 40a and the coloring Ink 30a part generation photopolymerization reactions corresponding with the shadow region 40c, and the protection ink 40a and the coloring Then there is no photopolymerization reaction in ink 30a corresponding with the metal portion 10 region;Subsequently, Fig. 7 is referred to, using carbonic acid There is no photopolymerization reaction part and corrode in sodium solution, to the protection ink 40a and coloring printing ink 30a so as to only exist Retain the protection ink 40a and coloring printing ink 30a on the non-metal portion 20.Finally, it is described nonmetallic to remaining in The protection ink 40a and the coloring printing ink 30a in portion 20 carries out 180 degrees Celsius of baking-curings, so that remaining in institute The protection ink 40a and the coloring printing ink 30a for stating non-metal portion 20 forms respectively the coating 30 and ink guarantor Sheath 40.
S03:The metal portion 10 is surface-treated towards the side of user, so that the metal portion 10 is towards user Side forms anodic oxide coating 11 (see Fig. 8).
In present embodiment, surface anodization process is carried out towards user side to the metal portion 10, so that The metal portion 10 towards user side formed anodic oxide coating 11, and then realize to the metal portion 10 towards user outward appearance Surface carries out " coloring ", so that the metal portion 10 reaches the effect of pre-set color towards user side.Certainly, implement at other In mode, if to the metal portion 10 not carrying out blasting treatment before being coated with the coating 30 on the non-metal portion 20, In order to further lift the appearance property of the metal portion 10, in addition it is also necessary to carry out blasting treatment to the anodic oxide coating 11, Then require when the non-metal portion 20 is coated with the coating 30 and the ink protective layer 40 simultaneously, the coating 30 and described Ink protective layer 40 adopts resist sandblasting ink.
Figure 14 is referred to, the present invention also provides a kind of mobile terminal 200, and the mobile terminal 200 includes the housing 100, the mobile terminal 200 also includes the mainboard 80 being fixed in the housing 100 and the work(being arranged on the mainboard 80 Energy part 81, and the protecgulum 90 mutually covered with the housing 100.It is understood that the functional part 81 can be day Line, battery or central processing unit etc..The protecgulum 90 is made up of euphotic cover plate 91 with the display screen 92 for being fixed on euphotic cover plate 91. The periphery of the protecgulum 90 is fixedly connected with the frame 70 of the housing 100, so that the protecgulum 90 and the housing 100 Collectively form the shell of the mobile terminal 200.
The housing of the present invention, method for producing shell and mobile terminal, by attached towards user side in the non-metal portion Coating is provided with, and the color using the coating is consistent towards the surface color of user with the metal portion, so that described Housing overall appearance performance is consistent, and then improves Consumer's Experience.
The above is the preferred embodiment of the present invention, it is noted that for those skilled in the art For, under the premise without departing from the principles of the invention, some improvements and modifications can also be made, these improvements and modifications are also considered as Protection scope of the present invention.

Claims (29)

1. a kind of housing, it is characterised in that the housing includes metal portion and the non-metal portion for being fixedly connected the metal portion, institute State non-metal portion and be attached to coating towards user side, the surface color of the color of the coating and the metal portion towards user Unanimously.
2. housing according to claim 1, it is characterised in that the coating is by the ink structure for being mixed into metallic and colorant Into.
3. housing according to claim 2, it is characterised in that the metallic is appointing for aluminum or silver or ferrum or titanium A kind of metal alloy of metal or multiple combination.
4. housing according to claim 2, it is characterised in that the coating is attached to ink protection towards user side Layer.
5. housing according to claim 4, it is characterised in that the ink protective layer is resist sandblasting ink.
6. housing according to claim 4, it is characterised in that the ink and the ink protective layer are exposure oil Ink.
7. housing according to claim 4, it is characterised in that the ink protective layer has the matte surface towards user.
8. housing according to claim 4, it is characterised in that the non-metal portion be laminated with coating described in multilamellar or/and Ink protective layer described in multilamellar.
9. the housing according to claim 1~8 any one, it is characterised in that the non-metal portion is described to be formed The antenna headroom region of housing.
10. housing according to claim 9, it is characterised in that the non-metal portion adopts non-signal shielding material.
11. housings according to claim 9, it is characterised in that the material of the non-metal portion be plastic cement or carbon fiber, Or organic resin or glass fibre etc..
12. housings according to claim 1~8 any one, it is characterised in that the metal portion sets towards user side There is an anodic oxide coating, the solid colour of the color of the anodic oxide coating and the coating.
13. housings according to claim 12, it is characterised in that the anodic oxide coating has the sandblasting towards user Face.
14. housings according to claim 12, it is characterised in that the anodic oxide coating and metal portion one.
15. housings according to claim 12, it is characterised in that the metal portion material be aluminum silver or rustless steel, Or aluminium alloy or titanium alloy or magnesium alloy or magnalium etc..
16. housings according to claim 1, it is characterised in that the non-metal portion is wholely set with the metal portion.
17. housings according to claim 1, it is characterised in that the non-metal portion forms at least one of the housing Slit band, the slit band is made up of a plurality of slit separately, the metal portion include by the slit band be separated out to Few two metallic plates and a plurality of bonding jumper.
18. housings according to claim 17, it is characterised in that a width of 0.2mm~3.0mm of seam of the slit.
19. housings according to claim 1, it is characterised in that the housing is by back-cover and is integrally formed at the back-cover The frame of periphery is constituted, and the frame is formed at the curved edges of the back-cover periphery.
20. a kind of method for producing shell, it is characterised in that the method for producing shell includes:
Housing product with metal portion and non-metal portion is provided, after the metal portion and the polished process of the non-metal portion and Jing blasting treatments again;
Set up coating, the color of the coating and institute in the region for being located at the non-metal portion in the appearance surfaces of the housing product State the appearance surfaces solid colour of metal portion.
21. method for producing shell according to claim 20, it is characterised in that the metal portion is adopted with the non-metal portion It is integrally formed with nano injection technique.
22. method for producing shell according to claim 20, it is characterised in that the coating is by being mixed into metallic and color The ink of material is constituted.
23. method for producing shell according to claim 22, it is characterised in that set up towards user side in the coating Ink protective layer.
24. method for producing shell according to claim 23, it is characterised in that the housing product appearance surfaces according to It is secondary to set up coloring printing ink and protection ink, and it is pointed to the coloring printing ink in the metal portion region and institute through exposure imaging technique State protection ink to be corroded, so that the coloring printing ink and protection ink that remain in the non-metal portion region form respectively described Coating and the ink protective layer.
25. method for producing shell according to claim 24, it is characterised in that to the coloring printing ink in preset duration After carrying out preset temperature baking, then the protection ink is attached on the coloring printing ink.
26. method for producing shell according to claim 24, it is characterised in that to remaining in the non-metal portion region Coloring printing ink and protection ink carry out forming the coating and the ink protective layer after baking-curing respectively.
27. method for producing shell according to claim 20, it is characterised in that the method for producing shell also includes:
The metal portion is surface-treated towards the side of user, so that the metal portion forms anode towards user side Oxide layer.
28. method for producing shell according to claim 27, it is characterised in that the anodic oxide coating is carried out at sandblasting Reason.
29. a kind of mobile terminals, it is characterised in that the mobile terminal includes the shell described in claim 1~19 any one Body, the mobile terminal also includes the mainboard being fixed in the housing and the functional part being arranged on the mainboard.
CN201610958424.8A 2016-09-08 2016-09-08 Shell, method for producing shell and mobile terminal Expired - Fee Related CN106572208B (en)