CN106281037A - A kind of environment protection oil paint and preparation method thereof - Google Patents

A kind of environment protection oil paint and preparation method thereof Download PDF

Info

Publication number
CN106281037A
CN106281037A CN201610760853.4A CN201610760853A CN106281037A CN 106281037 A CN106281037 A CN 106281037A CN 201610760853 A CN201610760853 A CN 201610760853A CN 106281037 A CN106281037 A CN 106281037A
Authority
CN
China
Prior art keywords
parts
paint
environment protection
protection oil
butanol
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610760853.4A
Other languages
Chinese (zh)
Inventor
裴寿益
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201610760853.4A priority Critical patent/CN106281037A/en
Publication of CN106281037A publication Critical patent/CN106281037A/en
Pending legal-status Critical Current

Abstract

The present invention relates to a kind of environment protection oil paint and preparation method thereof, in parts by weight, described environment protection oil paint includes 10 parts of 20 parts of rosin resins, 2 parts of 3 parts of titanium dioxides, 10 parts of 20 parts of polyvinyl butyral resins, 30 parts 50 parts paints powder, 1 part of 3 parts of phosphoric acid, 10 parts of 15 parts of butanol, 3 parts of 4 parts of oil, 1 part of 2 parts of plasticizers, 1 part of 3 parts of triethanolamine, 2 parts of 3 parts of zeolite powders, 10 parts of 20 parts of deionized waters.The environment protection oil paint of the present invention is dried rapidly, difficult drop-off, protection against the tide, anticorrosion, safety and environmental protection, raw material is easy to get, low cost.

Description

A kind of environment protection oil paint and preparation method thereof
Technical field
The present invention relates to new material technology field, be specifically related to a kind of environment protection oil paint and preparation method thereof.
Background technology
Paint is the staple product of modern industry, all has extensive and substantial amounts of on the various modern production of all trades and professions Use.In general, paint has a certain degree of harm to human body and animals and plants, because containing a large amount of in common paint Industrial chemicals, such as polyesters composition etc..And the paint using toxic composition to be made in a large number, necessarily endanger the mankind With other vegeto-animal health.
Summary of the invention
The technical problem to be solved is for the deficiencies in the prior art, it is provided that a kind of environment protection oil paint and preparation thereof Method.
The technical scheme is that a kind of environment protection oil paint, in parts by weight, including 10 -20 parts of rosin resins of part, 2 parts of-3 parts of titanium dioxides, 10 parts of-20 parts of polyvinyl butyral resins, 30 parts-50 parts paints powder, 1 part of-3 parts of phosphorus Acid, 10 parts of-15 parts of butanol, 3 parts of-4 parts of oil, 1 part of-2 parts of plasticizer, 1 part of-3 parts of triethanolamine, 2 parts of-3 parts of zeolite powders, 10 -20 parts of deionized waters of part.
The invention has the beneficial effects as follows: the environment protection oil paint of the present invention is dried rapidly, difficult drop-off, protection against the tide, anticorrosion, safety collar Protecting, raw material is easy to get, low cost.
On the basis of technique scheme, the present invention can also do following improvement.
Further, in parts by weight, including 10 parts of rosin resins, 2 parts of titanium dioxides, 10 parts of polyvinyl butyral resins, 30 parts Paint powder, 1 part of phosphoric acid, 10 parts of butanol, 3 parts of oil, 1 part of plasticizer, 1 part of triethanolamine, 2 parts of zeolite powders, 10 parts of deionized waters.
Further, in parts by weight, including 20 parts of rosin resins, 3 parts of titanium dioxides, 20 parts of polyvinyl butyral resins, 50 parts Paint powder, 3 parts of phosphoric acid, 15 parts of butanol, 4 parts of oil, 2 parts of plasticizers, 3 parts of triethanolamine, 3 parts of zeolite powders, 20 parts of deionized waters.
Further, in parts by weight, including 15 parts of rosin resins, 2.5 parts of titanium dioxides, 15 parts of polyvinyl butyral resins, 40 Part paint powder, 2 parts of phosphoric acid, 12 parts of butanol, 3.5 parts of oil, 1.5 parts of plasticizers, 2 parts of triethanolamine, 2.5 parts of zeolite powders, 15 parts go Ionized water.
Further, described antibacterial is at least one of zinc oxide, copper oxide, ammonium dihydrogen phosphate and lithium carbonate.
The preparation method of a kind of environment protection oil paint described above, comprises the following steps:
1) deionized water and paint powder being added in stirred tank, carry out heated and stirred, whipping temp is 60 DEG C-70 DEG C, obtains Mixed liquor;
2), after cooling, in initial paint liquid, rosin resin, titanium dioxide, polyvinyl butyral resin, phosphoric acid, butanol, increasing are added After moulding agent, triethanolamine, zeolite powder, after stirring, initially painted liquid;
3) initial paint liquid is filtered, prepare environment protection oil paint.
The invention has the beneficial effects as follows: the method for the present invention is simple, production suitable for industrialized.
Further, described mixing time is 40-60min.
Detailed description of the invention
Principle and feature to the present invention are described below, and example is served only for explaining the present invention, is not intended to limit Determine the scope of the present invention.
Embodiment 1
A kind of environment protection oil paint of the present embodiment, in parts by weight, including 10 parts of rosin resins, 2 parts of titanium dioxides, 10 parts of poly-second Enol butyral, 30 parts of paint powder, 1 part of phosphoric acid, 10 parts of butanol, 3 parts of oil, 1 part of plasticizer, 1 part of triethanolamine, 2 parts of zeolite powders, 10 parts of deionized waters.
The environment protection oil paint of the present embodiment is dried rapidly, difficult drop-off, protection against the tide, anticorrosion, safety and environmental protection, raw material is easy to get, cost Low.
The preparation method of the environment protection oil paint a kind of described above of the present embodiment, comprises the following steps:
1) deionized water and paint powder being added in stirred tank, carry out heated and stirred, whipping temp is 60 DEG C-70 DEG C, obtains Mixed liquor;Described mixing time is 40-60min.
2), after cooling, in initial paint liquid, rosin resin, titanium dioxide, polyvinyl butyral resin, phosphoric acid, butanol, increasing are added After moulding agent, triethanolamine, zeolite powder, after stirring, initially painted liquid;
3) initial paint liquid is filtered, prepare environment protection oil paint.
The method of the present embodiment is simple, production suitable for industrialized.
Embodiment 2
A kind of environment protection oil paint of the present embodiment, in parts by weight, including 20 parts of rosin resins, 3 parts of titanium dioxides, 20 parts of poly-second Enol butyral, 50 parts of paint powder, 3 parts of phosphoric acid, 15 parts of butanol, 4 parts of oil, 2 parts of plasticizers, 3 parts of triethanolamine, 3 parts of zeolite powders, 20 parts of deionized waters.
The environment protection oil paint of the present embodiment is dried rapidly, difficult drop-off, protection against the tide, anticorrosion, safety and environmental protection, raw material is easy to get, cost Low.
The preparation method of the environment protection oil paint a kind of described above of the present embodiment, comprises the following steps:
1) deionized water and paint powder being added in stirred tank, carry out heated and stirred, whipping temp is 60 DEG C-70 DEG C, obtains Mixed liquor;Described mixing time is 40-60min.
2), after cooling, in initial paint liquid, rosin resin, titanium dioxide, polyvinyl butyral resin, phosphoric acid, butanol, increasing are added After moulding agent, triethanolamine, zeolite powder, after stirring, initially painted liquid;
3) initial paint liquid is filtered, prepare environment protection oil paint.
The method of the present embodiment is simple, production suitable for industrialized.
Embodiment 3
A kind of environment protection oil paint of the present embodiment, in parts by weight, including 15 parts of rosin resins, 2.5 parts of titanium dioxides, 15 parts gather Vinyl butyral, 40 parts of paint powder, 2 parts of phosphoric acid, 12 parts of butanol, 3.5 parts of oil, 1.5 parts of plasticizers, 2 parts of triethanolamine, 2.5 Part zeolite powder, 15 parts of deionized waters.
The environment protection oil paint of the present embodiment is dried rapidly, difficult drop-off, protection against the tide, anticorrosion, safety and environmental protection, raw material is easy to get, cost Low.
The preparation method of the environment protection oil paint a kind of described above of the present embodiment, comprises the following steps:
1) deionized water and paint powder being added in stirred tank, carry out heated and stirred, whipping temp is 60 DEG C-70 DEG C, obtains Mixed liquor;Described mixing time is 40-60min.
2), after cooling, in initial paint liquid, rosin resin, titanium dioxide, polyvinyl butyral resin, phosphoric acid, butanol, increasing are added After moulding agent, triethanolamine, zeolite powder, after stirring, initially painted liquid;
3) initial paint liquid is filtered, prepare environment protection oil paint.
The method of the present embodiment is simple, production suitable for industrialized.
The foregoing is only presently preferred embodiments of the present invention, not in order to limit the present invention, all spirit in the present invention and Within principle, any modification, equivalent substitution and improvement etc. made, should be included within the scope of the present invention.

Claims (6)

1. an environment protection oil paint, it is characterised in that in parts by weight, including 10 parts of-20 parts of rosin resins, 2 parts of-3 parts of titanium dioxides, 10 parts of-20 parts of polyvinyl butyral resins, 30 parts-50 parts paint powder, 1 part of-3 parts of phosphoric acid, 10 parts of-15 parts of butanol, 3 parts of-4 parts of oil, 1 Part-2 parts of plasticizers, 1 part of-3 parts of triethanolamine, 2 parts of-3 parts of zeolite powders, 10 parts of-20 parts of deionized waters.
A kind of environment protection oil paint, it is characterised in that in parts by weight, including 10 parts of rosin resins, 2 Part titanium dioxide, 10 parts of polyvinyl butyral resins, 30 parts of paint powder, 1 part of phosphoric acid, 10 parts of butanol, 3 parts of oil, 1 part of plasticizer, 1 part three Ethanolamine, 2 parts of zeolite powders, 10 parts of deionized waters.
A kind of environment protection oil paint, it is characterised in that in parts by weight, including 20 parts of rosin resins, 3 Part titanium dioxide, 20 parts of polyvinyl butyral resins, 50 parts of paint powder, 3 parts of phosphoric acid, 15 parts of butanol, 4 parts of oil, 2 parts of plasticizers, 3 part three Ethanolamine, 3 parts of zeolite powders, 20 parts of deionized waters.
A kind of environment protection oil paint, it is characterised in that in parts by weight, including 15 parts of rosin resins, 2.5 parts of titanium dioxides, 15 parts of polyvinyl butyral resins, 40 parts of paints powder, 2 parts of phosphoric acid, 12 parts of butanol, 3.5 parts of oil, 1.5 parts of plasticising Agent, 2 parts of triethanolamine, 2.5 parts of zeolite powders, 15 parts of deionized waters.
5. the preparation method of environment protection oil paint as described in any one of Claims 1-4, it is characterised in that comprise the following steps:
1) deionized water and paint powder being added in stirred tank, carry out heated and stirred, whipping temp is 60 DEG C-70 DEG C, is mixed Liquid;
2) after cooling, add in initial paint liquid rosin resin, titanium dioxide, polyvinyl butyral resin, phosphoric acid, butanol, plasticizer, After triethanolamine, zeolite powder, after stirring, initially painted liquid;
3) initial paint liquid is filtered, prepare environment protection oil paint.
The preparation method of a kind of environment protection oil paint, it is characterised in that described mixing time is 40- 60min。
CN201610760853.4A 2016-08-30 2016-08-30 A kind of environment protection oil paint and preparation method thereof Pending CN106281037A (en)