CN106124742A - A kind of pigment and the method for inspection - Google Patents
A kind of pigment and the method for inspection Download PDFInfo
- Publication number
- CN106124742A CN106124742A CN201610536465.8A CN201610536465A CN106124742A CN 106124742 A CN106124742 A CN 106124742A CN 201610536465 A CN201610536465 A CN 201610536465A CN 106124742 A CN106124742 A CN 106124742A
- Authority
- CN
- China
- Prior art keywords
- pigment
- porcelain
- inspection
- damaged
- product
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to the production technical field of high tension insulator, concretely relate to a kind of method of inspection checked the whether damaged pigment of porcelain body and use this pigment.Manufacture method is by weight with basic fuchsin and the ethanol mix homogeneously of 100 parts of 0.8~1.5 part;Using method is: above-mentioned pigment brush is spread upon the position that porcelain piece is to be checked, treat that product pigment is dried, whether perusal porcelain facing has abnormal, have and manufacture advantage easy, with low cost, use this decompression method to have not and destroy or polluted product, easily operation, accurately and rapidly advantage.
Description
Technical field
The present invention relates to the production technical field of high tension insulator, concretely relate to a kind of check porcelain body whether damaged
Pigment and use the method for inspection of this pigment.
Background technology
In the prior art, whether breakage generally uses perusal to inspection porcelain body, observes whether porcelain body has crackle, accordingly
Judging whether to crush, but crackle is the most tiny sometimes, naked eyes are difficult to observe, it occur frequently that detection leakage phenomenon, make semi-finished product flow into
Next procedure, impact is normal to be produced, and increases production cost.
Summary of the invention
The purpose of the present invention is aiming at disadvantages mentioned above, it is provided that whether the inspection porcelain body of a kind of with low cost, easy manufacture
Damaged pigment, also provides for a kind of method of inspection using this pigment can accurately detect damaged insulator.A kind of inspection porcelain body
The most damaged pigment is achieved in that it to include by weight and mixes with the basic fuchsin of 0.8~1.5 part and the ethanol of 100 parts
Close uniformly.A kind of method using this pigment inspection insulator the most damaged is achieved in that brushes above-mentioned pigment
Son spreads upon the position that porcelain piece is to be checked, and treats that product pigment is dried, and whether perusal porcelain facing has abnormal.The present invention has
Benefit effect is: so manufacture method of pigment has the advantage that manufacture is easy, with low cost, uses this decompression method to have not
Destroy or polluted product, easily operation, accurately and rapidly advantage.
Detailed description of the invention
Embodiment 1 takes the basic fuchsin of 0.8 gram and the ethanol mixing of 100 grams, obtains this inspection raw material.By above-mentioned pigment
Spreading upon, with brush, the position that porcelain piece is to be checked, treat that product pigment is dried, whether perusal porcelain facing has abnormal, mainly sees
Seeing if there is color accumulation position, if there being accumulation position, may often be such that the place of breakage, experienced reviewer's meeting here
Easily determine whether damaged, the pigment above insulator that inexperienced personnel can be used cloth to wipe with, see and see if there is leave over deep
Color vestige, if any may determine that insulator is damaged.Described basic fuchsin is to have another name called magenta, Aniline Red, Aniline Red, Flos Rosae Rugosae
Anilinechloride, manufacturer has Shanghai this reddening chemical product company limited, Xingtai City rainbow Chemical Co., Ltd., Tianjin to shake
Numerous producers such as emerging great achievement chemical dyestuff company limited.
Claims (4)
1. checking the pigment that porcelain body is whether damaged, it includes by weight with the basic fuchsin of 0.8~1.5 part and 100 parts
Ethanol mix homogeneously.
Pigment the most according to claim 1, is characterized in that: it includes by weight with the basic fuchsin and 100 of 1~1.2 part
The ethanol mix homogeneously of part.
3. the method that the inspection insulator of an above-mentioned pigment is the most damaged is: above-mentioned pigment brush is spread upon porcelain piece to check
Position, treat that product pigment is dried, whether perusal porcelain facing has abnormal.
Method the most according to claim 3, is characterized in that: the pigment above the porcelain body that also includes using cloth to wipe with after drying.