CN106076776A - A kind of mahogany furniture painting technology - Google Patents
A kind of mahogany furniture painting technology Download PDFInfo
- Publication number
- CN106076776A CN106076776A CN201610582164.9A CN201610582164A CN106076776A CN 106076776 A CN106076776 A CN 106076776A CN 201610582164 A CN201610582164 A CN 201610582164A CN 106076776 A CN106076776 A CN 106076776A
- Authority
- CN
- China
- Prior art keywords
- mahogany furniture
- furniture
- paint
- mahogany
- painting technology
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The open a kind of mahogany furniture painting technology of the present invention, comprises the following steps: (1) dries;(2) PROCESS FOR TREATMENT;(3) varnish is uniformly sprayed;(4) removing surface;(5) spray-applied primer;(6) surface processes.The present invention is easy to make, and hardening time is fast, with low cost, can preserve for a long time, can produce on a large scale, and scratch resistance capability more wear-resisting than general paint, and service life is long, the surface of our furniture of significantly more efficient guarantee, the addition of iron powder can ensure that metope damage.
Description
Technical field
The invention belongs to paint technology field, be specifically related to a kind of mahogany furniture painting technology.
Background technology
Paint is that one can firmly cover at body surface, and the chemical mixture coating of other specific uses, have anticorrosion,
The functions such as Water-proof and oil-proof, chemicals-resistant, fast light, heatproof.Object is exposed among air, by the erosion of oxygen, moisture etc.,
Cause the breakoff phenomenons such as corrosion of metal, foxiness, cement air slaking.It is coated with coating at object surface, forms layer protecting film, energy
Enough stop or postpone generation and the development of these breakoff phenomenons, make extend the service life of various material.So, protective effect is
One Main Function of coating.
The paint property the most wear-resisting, scratch resistant of furniture is bad now, accidentally will stay and shine into depainting, or occurs one
The cut that bar is the biggest, has not only broken up attractive in appearance and has caused the protection of furniture to be affected, and some paints because of poor quality,
Breathability is bad, causes the temperature in furniture effectively not discharge, and trips out a lot of projections on surface, the most also holds
Easily inside of furniture material is shone into destruction.
Summary of the invention
For solving above-mentioned technical problem present in prior art, the invention provides a kind of mahogany furniture painting technology.
The purpose of the present invention is achieved through the following technical solutions: a kind of mahogany furniture painting technology, described method step
Including:
(1), the surface of mahogany furniture is carried out Surface heat-treatent so that it is the moisture in furniture sufficiently evaporates;
(2), mahogany furniture surface is carried out PROCESS FOR TREATMENT;
(3), on mahogany furniture surface uniformly spray varnish, described varnish adds preservative, wait it to be dried;
(4), polish, polish, removing surface;
(5) coat, again on mahogany furniture surface and spray polyurethane priming paint, wait its dry solidification;
(6), again by mahogany furniture surface process, wait its dry solidification;
(7), in surface pattern-making so that it is more attractive in appearance, then surface cleaning process is carried out.
Preferably, described polyurethane priming paint is contained within firming agent and additive, makes the time of the dry solidification of paint shorten,
Described additive can be effectively ensured the most long-time preservation of paint.
Preferably, described varnish contains the iron powder of 10%-15%.
The medicine have the advantages that the present invention is easy to make, hardening time is fast, with low cost, can preserve for a long time, can be big
The production of scale, and scratch resistance capability more wear-resisting than general paint, and service life is long, significantly more efficient guarantee we
The surface of furniture, the addition of iron powder can ensure that metope damage.
Detailed description of the invention
The present invention is described further in conjunction with the embodiments.
A kind of mahogany furniture painting technology, described method step includes:
(1), the surface of mahogany furniture is carried out Surface heat-treatent so that it is the moisture in furniture sufficiently evaporates;
(2), mahogany furniture surface is carried out PROCESS FOR TREATMENT;
(3), on mahogany furniture surface uniformly spray varnish, described varnish adds preservative, wait it to be dried;
(4), polish, polish, removing surface;
(5) coat, again on mahogany furniture surface and spray polyurethane priming paint, wait its dry solidification;
(6), again by mahogany furniture surface process, wait its dry solidification;
(7), in surface pattern-making so that it is more attractive in appearance, then surface cleaning process is carried out.
Preferably, described polyurethane priming paint is contained within firming agent and additive, makes the time of the dry solidification of paint shorten,
Described additive can be effectively ensured the most long-time preservation of paint.
Preferably, described varnish contains the iron powder of 10%-15%.
The present invention is easy to make, and hardening time is fast, with low cost, can preserve for a long time, can produce on a large scale, and ratio is typically
Paint is the most wear-resisting and scratch resistance capability, and service life is long, the surface of our furniture of significantly more efficient guarantee, iron powder
Add and can ensure that metope damage.
In this description, the present invention is described with reference to its specific embodiment.But it is clear that still can make
Various modifications and alterations are without departing from the spirit and scope of the present invention.Therefore, description is considered as illustrative rather than limits
Property processed.
Claims (3)
1. a mahogany furniture painting technology, it is characterised in that comprise the following steps:
(1), the surface of mahogany furniture is carried out Surface heat-treatent so that it is the moisture in furniture sufficiently evaporates;
(2), mahogany furniture surface is carried out PROCESS FOR TREATMENT;
(3), on mahogany furniture surface uniformly spray varnish, described varnish adds preservative, wait it to be dried;
(4), polish, polish, removing surface;
(5) coat, again on mahogany furniture surface and spray polyurethane priming paint, wait its dry solidification;
(6), again by mahogany furniture surface process, wait its dry solidification;
(7), in surface pattern-making so that it is more attractive in appearance, then surface cleaning process is carried out.
Mahogany furniture painting technology the most according to claim 1, it is characterised in that described polyurethane priming paint is contained within solidification
Agent and additive, make the time of the dry solidification of paint shorten, and described additive can be effectively ensured the most long-time guarantor of paint
Deposit.
Mahogany furniture painting technology the most according to claim 1, it is characterised in that containing 10%-15%'s in described varnish
Iron powder.