CN106047393A - 一种低比例主焦煤参与的炼焦配煤方法 - Google Patents
一种低比例主焦煤参与的炼焦配煤方法 Download PDFInfo
- Publication number
- CN106047393A CN106047393A CN201610513121.5A CN201610513121A CN106047393A CN 106047393 A CN106047393 A CN 106047393A CN 201610513121 A CN201610513121 A CN 201610513121A CN 106047393 A CN106047393 A CN 106047393A
- Authority
- CN
- China
- Prior art keywords
- coal
- coking
- coking coal
- index
- value
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种低比例主焦煤参与的炼焦配煤方法,炼焦煤包括主焦煤、肥煤、三分之一焦煤、瘦煤、气煤,所述主焦煤单种成焦M10指标小于9%,CSR指标大于60%,所述肥煤的粘结指数G值大于85,干燥无灰基挥发份Vdaf小于32%,胶质层最大厚度Y值大于25mm,单种成焦CSR指标大于45%,所述三分之一焦煤的粘结指数G值大于80,单种成焦CSR指标大于45%,所述瘦煤的粘结指数G值大于20,所述气煤的粘结指数G值大于55,其特征在于:各炼焦煤的重量百分比为:主焦煤15~25,肥煤20~25,三分之一焦煤35~42,瘦煤13~18,气煤0~6,且配合煤中主焦煤+肥煤总比例为40%以上,且配合煤的G值为75~85,挥发份为Vdaf=28%~30%。
Description
技术领域
本发明属于炼焦配煤技术领域,具体指一种低比例主焦煤参与的炼焦配煤方法,特别地涉及一种顶装焦炉炼焦工艺主焦煤配比低于25%参与的炼焦配煤方法。
技术背景
钢铁行业产能过剩,经济效益下滑,作为钢铁联合企业的焦化厂面临降低配煤成本的紧迫任务。但为了保证高炉系统低成本稳定运行,在降低配煤成本的同时,要保证焦炭质量不下降。主焦煤是炼焦配煤中的骨干炼焦煤煤种,其质量最好、价格最高,因此我们要持续优化炼焦配煤,降低高价主焦煤配比,通过其它低价煤种的搭配,在保证焦炭质量不下降的前提下,降低配煤成本。
发明内容
本发明所要解决的技术问题是提供一种低比例主焦煤参与的炼焦配煤方法,该方法可以降低价格最高的主焦煤配比,降低配煤成本,且炼焦出的焦炭质量不下降。
为解决上述技术问题,本发明采用如下技术方案:
一种低比例主焦煤参与的炼焦配煤方法,炼焦煤包括主焦煤、肥煤、三分之一焦煤、瘦煤、气煤,所述主焦煤单种成焦M10指标小于9%,CSR指标大于60%,所述肥煤的粘结指数G值大于85,干燥无灰基挥发份Vdaf小于32%,胶质层最大厚度Y值大于25mm,单种成焦CSR指标大于45%,所述三分之一焦煤的粘结指数G值大于80,单种成焦CSR指标大于45%,所述瘦煤的粘结指数G值大于20,所述气煤的粘结指数G值大于55,其特征在于:各炼焦煤的重量百分比为:主焦煤15~25,肥煤20~25,三分之一焦煤35~42,瘦煤13~18,气煤0~6,且配合煤中主焦煤+肥煤总比例为40%以上, 且配合煤的G值为75~85,挥发份为Vdaf=28%~30%。
本发明以配合煤中主焦煤+肥煤总比例为控制指标,以优质主焦煤和肥煤为骨干,通过调节配合煤中主焦煤、肥煤、三分之一焦煤、瘦煤和气煤的用量,不仅可以降低价格最高主焦煤的用量,合理利用煤质资源,大幅降低配煤成本,而且在无分级破碎、型煤工艺或捣固炼焦等工艺条件下, 4.3米、6米顶装、全干熄焦焦炉所炼焦炭的CSR大于64%。
具体实施方式
以下结合实施例对本发明的有关技术问题作进一步的详细说明。
一种低比例主焦煤参与的炼焦配煤方法,包括将主焦煤、肥煤、三分之一焦煤、瘦煤和气煤混配的步骤,各单种煤煤质分析结果见表1:
表1 单种煤煤质分析结果
各炼焦煤的重量百分比为:主焦煤:15~25%;肥煤:20~25%;三分之一焦煤:35~42%;瘦煤:13~18%;气煤:0~6%;且配合煤中主焦煤+肥煤总比例为40%以上。
配煤方案的具体实施例见表2。
表2 配煤方案
实施例1、实施例2、实施例3、实施例4所得焦炭均在无分级破碎、型煤工艺或捣固炼焦等工艺条件下, 4.3米、6米顶装、全干熄焦焦炉制得。
以上所述仅是本发明的优选实施方式,在本发明所公开的实验条件参数范围内取值的任意组合都可以实施本发明。
Claims (1)
1.一种低比例主焦煤参与的炼焦配煤方法,炼焦煤包括主焦煤、肥煤、三分之一焦煤、瘦煤、气煤,所述主焦煤单种成焦M10指标小于9%,CSR指标大于60%,所述肥煤的粘结指数G值大于85,干燥无灰基挥发份Vdaf小于32%,胶质层最大厚度Y值大于25mm,单种成焦CSR指标大于45%,所述三分之一焦煤的粘结指数G值大于80,单种成焦CSR指标大于45%,所述瘦煤的粘结指数G值大于20,所述气煤的粘结指数G值大于55,其特征在于:各炼焦煤的重量百分比为:主焦煤15~25,肥煤20~25,三分之一焦煤35~42,瘦煤13~18,气煤0~6,且配合煤中主焦煤+肥煤总比例为40%以上, 且配合煤的G值为75~85,挥发份为Vdaf=28%~30%。